CN103881543A - 一种耐候耐腐蚀涂料 - Google Patents

一种耐候耐腐蚀涂料 Download PDF

Info

Publication number
CN103881543A
CN103881543A CN201210565175.8A CN201210565175A CN103881543A CN 103881543 A CN103881543 A CN 103881543A CN 201210565175 A CN201210565175 A CN 201210565175A CN 103881543 A CN103881543 A CN 103881543A
Authority
CN
China
Prior art keywords
parts
coating material
resistance
epoxy resin
present
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201210565175.8A
Other languages
English (en)
Inventor
李光俊
李少香
刘来运
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
QINGDAO XUANWEI COATING MATERIAL CO Ltd
Original Assignee
QINGDAO XUANWEI COATING MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINGDAO XUANWEI COATING MATERIAL CO Ltd filed Critical QINGDAO XUANWEI COATING MATERIAL CO Ltd
Priority to CN201210565175.8A priority Critical patent/CN103881543A/zh
Publication of CN103881543A publication Critical patent/CN103881543A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种耐候耐腐蚀涂料,由以下重量份的成分组成:醇酸树脂30~60;环氧树脂5~10;阻燃剂10~15;聚磷酸铵10~20;增稠剂10~15;尿素5~10;丁基乳胶1~3;去离子水10~15。本发明采用的醇酸树脂具有干燥速度快和耐候性好的特点,使得制得的涂料干燥迅速,提高涂装效率;本发明采用的环氧树脂对多种基体介质有很好的附着力,它的加入提高了涂料对基体的附着力;本发明采用的萜烯树脂对氧、光和热都非常稳定,耐老化性能优异,使得涂料具有优良的耐候性能。

Description

一种耐候耐腐蚀涂料
技术领域
本发明涉及一种耐候耐腐蚀涂料。
背景技术
钢管在钢铁厂流水线上下线后,其表面耐蚀性能差,在储运过程中很容易被腐蚀,严重影响其性能和使用寿命。一旦其表面被腐蚀,其后续处理过程繁琐,工作量大。
发明内容
    针对现有技术存在的不足,本发明所要解决的技术问题是,提供一种适用多种施工方式且能自然干燥,与钢管结合力强和对钢管保护性能好的耐候耐腐蚀涂料。
为解决上述技术问题,本发明所采取的技术方案是:一种耐候耐腐蚀涂料,由以下重量份的成分组成:
醇酸树脂                          30~60;
环氧树脂                          5~10;
阻燃剂                            10~15;
聚磷酸铵                          10~20;
增稠剂                            10~15;
尿素                               5~10;
丁基乳胶                          1~3;
去离子水                          10~15。
本发明耐候耐腐蚀涂料的优点是:本发明采用的醇酸树脂具有干燥速度快和耐候性好的特点,使得制得的涂料干燥迅速,提高涂装效率;本发明采用的环氧树脂对多种基体介质有很好的附着力,它的加入提高了涂料对基体的附着力;本发明采用的萜烯树脂对氧、光和热都非常稳定,耐老化性能优异,使得涂料具有优良的耐候性能;本发明采用的防锈剂能在钢管表面形成致密、附着力强的保护层,通过隔离作用阻止或减缓环境中的氧和水的渗透,从而阻碍腐蚀微电池的产生,起到较好的防腐蚀保护作用。
具体实施方式
下面结合具体实施例对本发明做进一步详细说明;
一种耐候耐腐蚀涂料,由以下重量份的成分组成:
醇酸树脂                          30~60;
环氧树脂                          5~10;
阻燃剂                            10~15;
聚磷酸铵                          10~20;
增稠剂                            10~15;
尿素                               5~10;
丁基乳胶                           1~3;
去离子水                          10~15。
当然,上述说明并非是对本发明的限制,本发明也并不限于上述举例,本技术领域的普通技术人员,在本发明的实质范围内,作出的变化、改型、添加或替换,都应属于本发明的保护范围。

Claims (1)

1.一种耐候耐腐蚀涂料,其特征在于,由以下重量份的成分组成:
醇酸树脂                          30~60;
环氧树脂                          5~10;
阻燃剂                            10~15;
聚磷酸铵                          10~20;
增稠剂                            10~15;
尿素                               5~10;
丁基乳胶                          1~3;
去离子水                          10~15。
CN201210565175.8A 2012-12-24 2012-12-24 一种耐候耐腐蚀涂料 Pending CN103881543A (zh)