Prior art keywords
rectangular tube
antidote
fiber
reinforced resin
resin matrix
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201611042423.5A
Other languages
English (en)
Inventor
刘小平
刘灵通
郭超超
贾鹏军
张宁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Hengshen Co Ltd
Original Assignee
Jiangsu Hengshen Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Hengshen Co Ltd filed Critical Jiangsu Hengshen Co Ltd
Priority to CN201611042423.5A priority Critical patent/CN106799828A/zh
Publication of CN106799828A publication Critical patent/CN106799828A/zh
Pending legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B29WORKING OF PLASTICS; WORKING OF SUBSTANCES IN A PLASTIC STATE IN GENERAL
    • B29CSHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
    • B29C53/00Shaping by bending, folding, twisting, straightening or flattening; Apparatus therefor
    • B29C53/16Straightening or flattening
    • B29C53/20Straightening or flattening of tubes

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Shaping Of Tube Ends By Bending Or Straightening (AREA)

Abstract

本发明提供一种树脂基纤维增强复合材料拉挤矩形管的矫正方法,该方法通过加热复合材料制品到热变形温度以上,利用相应装置固定。保温一定时间,冷却后卸掉装置。这个过程中复合材料矩形管在原有弯曲量基础上反弯了一些变形,在回复弹性弯曲部分的变形后,复合材料矩形管趋于平直。该方法解决了矩形管难矫正的问题。

Description

一种纤维增强树脂基复合材料矩形管矫正方法
技术领域
本发明涉及的是一种纤维增强树脂基复合材料矩形管的矫正方法,具体是一种拉挤矩形管的矫正方法。
背景技术
复合材料矫正会降低复合材料性能,一般通过成型前的工艺控制来完成尺寸及尺寸偏差的控制。纤维增强树脂基复合材料型材成型过程中会因工艺控制及原材料不稳定等因素产生的直线度较差,热塑性复合材料在加热至热变形温度以上时能发生塑性变形。
发明内容
本发明提供一种纤维增强树脂基复合材料矩形管矫正方法,能够减少复合材料矩形管应矫正而引起的性能损失。
一种纤维增强树脂基复合材料矩形管矫正方法,在矫正平台上放上矩形管,在矩形管上垫上不同厚度的软质材料形成反弯曲线,并用夹具在两端固定住矩形管,通过加热复合材料矩形管到热变形温度以上,保温一定时间,冷却后松掉夹具。这个过程中复合材料矩形管在原有弯曲量基础上反弯了一些变形,在回复弹性弯曲部分的变形后,复合材料矩形管趋于平直。该方法可以直线度为4mm/M的矩形管矫正到直线度小于0.5mm/M。并且材料的性能保留率超过90%。
该矫正方法的夹具表面包裹一层耐温的硅橡胶层,在反弯过程中不至于破坏矩形管形状。
进一步的垫在矩形管下的的软质材料也为弹性材料,从而不致矩形管在反弯过程中局部应力过大而破坏。
该矫正过程中矩形管只有一面承受外力,这就最大限度的保持了复合材料的截面形状。
该方法矫正矩形管时,该装置不受矩形管本身长度的影响,只受加热空间大小影响,可以实现较长矩形管的变形。
该方法矫正可以利用两根弯曲的矩形管互相矫正,这样就节省了矫正平台。两根长度一致直线度相当时矫正效果好。
附图说明
图1位单根矩形管矫正示意图。
图2为双根矩形管矫正示意图。
图3为矩形管的示意图。
具体实施方式
下面结合附图详细说明本发明的优选实施例1
如图1,矫正一根矩形管时,在矫正平台4上放上矩形管2,按反弯曲线在不同位置垫上不同厚度的软质材料的垫片3,使矩形管向相反方向弯曲,再用夹具1在两端夹紧矩形管,然后放入到120℃烘箱中保持30min,冷却后取出拆卸夹具,矩形管回弹部分变形,矩形管被矫直。
下面结合附图详细说明本发明的优选实施例2
如图2,在两根需要矫正的矩形管2之间按反弯曲线在不同位置垫上不同厚度的垫片3,将矩形管反弯,在两端用夹具1夹住矩形管2,固定完成后放入120℃烘箱中保持30min,冷却后取出拆卸夹具,矩形管回弹部分变形,两根矩形管直线度较矫正前改善。

Claims (3)

1.一种纤维增强树脂基复合材料矩形管矫正方法,其特征在于:在矫正平台上放上矩形管,在矩形管上垫上不同厚度的软质材料形成反弯曲线,并用夹具在两端固定住矩形管,通过加热复合材料矩形管到热变形温度以上,保温一定时间,冷却后松掉夹具。
2.根据权利要求1所述的一种纤维增强树脂基复合材料矩形管矫正方法,其特征在于:垫在矩形管下的的软质材料也为弹性材料。
3.根据权利要求1所述的一种纤维增强树脂基复合材料矩形管矫正方法,其特征在于:夹具表面包裹一层耐温的硅橡胶层。
CN201611042423.5A 2016-11-23 2016-11-23 一种纤维增强树脂基复合材料矩形管矫正方法 Pending CN106799828A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201611042423.5A CN106799828A (zh) 2016-11-23 2016-11-23 一种纤维增强树脂基复合材料矩形管矫正方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201611042423.5A CN106799828A (zh) 2016-11-23 2016-11-23 一种纤维增强树脂基复合材料矩形管矫正方法

Publications (1)

Publication Number Publication Date
CN106799828A true CN106799828A (zh) 2017-06-06

Family

ID=58976289

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201611042423.5A Pending CN106799828A (zh) 2016-11-23 2016-11-23 一种纤维增强树脂基复合材料矩形管矫正方法

Country Status (1)

Country Link
CN (1) CN106799828A (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110549587A (zh) * 2019-10-18 2019-12-10 常州市新创智能科技有限公司 一种t型拉挤件自动校直装置及其控制方法
CN110920039A (zh) * 2019-12-04 2020-03-27 陈小风 一种塑料管材调直处理方法
CN112571772A (zh) * 2020-11-24 2021-03-30 宁波江丰复合材料科技有限公司 一种碳纤维复合材料的弯曲矫正方法

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS56120108A (en) * 1980-02-27 1981-09-21 Sadao Amijima Bending correction device for bar member supported by cantilever
JPH01272188A (ja) * 1988-04-25 1989-10-31 Matsushita Electric Works Ltd プリント配線板の反り矯正方法
JPH0334835A (ja) * 1989-06-30 1991-02-14 Daikyo Inc プラスチック成形体の歪修正装置
EP0514915A2 (de) * 1991-05-24 1992-11-25 GAO Gesellschaft für Automation und Organisation mbH Verfahren und Vorrichtung zur Nachbehandlung eines mehrschichtigen gewölbten Laminats
JPH11277620A (ja) * 1998-03-31 1999-10-12 Techno Chubu:Kk 可撓性筒体の直管方法および直管状筒体を主要部とする手動弁用スピンドルカバー

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS56120108A (en) * 1980-02-27 1981-09-21 Sadao Amijima Bending correction device for bar member supported by cantilever
JPH01272188A (ja) * 1988-04-25 1989-10-31 Matsushita Electric Works Ltd プリント配線板の反り矯正方法
JPH0334835A (ja) * 1989-06-30 1991-02-14 Daikyo Inc プラスチック成形体の歪修正装置
EP0514915A2 (de) * 1991-05-24 1992-11-25 GAO Gesellschaft für Automation und Organisation mbH Verfahren und Vorrichtung zur Nachbehandlung eines mehrschichtigen gewölbten Laminats
JPH11277620A (ja) * 1998-03-31 1999-10-12 Techno Chubu:Kk 可撓性筒体の直管方法および直管状筒体を主要部とする手動弁用スピンドルカバー

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110549587A (zh) * 2019-10-18 2019-12-10 常州市新创智能科技有限公司 一种t型拉挤件自动校直装置及其控制方法
CN110549587B (zh) * 2019-10-18 2021-11-16 常州市新创智能科技有限公司 一种t型拉挤件自动校直装置及其控制方法
CN110920039A (zh) * 2019-12-04 2020-03-27 陈小风 一种塑料管材调直处理方法
CN110920039B (zh) * 2019-12-04 2021-07-23 安徽神添海绵城市新材料科技有限公司 一种塑料管材调直处理方法
CN112571772A (zh) * 2020-11-24 2021-03-30 宁波江丰复合材料科技有限公司 一种碳纤维复合材料的弯曲矫正方法

Similar Documents

Publication Publication Date Title
CN106799828A (zh) 一种纤维增强树脂基复合材料矩形管矫正方法
CN205167531U (zh) 一种管材矫正装置
CN107058708A (zh) 一种弹簧片类零件热处理变形控制方法
CN203157130U (zh) 一种塑胶件矫正装置
CN103624107A (zh) 一种剪板机刀片火焰矫正工艺
CN108714639A (zh) 一种弯管工艺
CN104485270A (zh) 一种螺旋线行波管用慢波系统的制造工艺
CN207108809U (zh) 一种热弯机及其万向调节装置
CN105531396A (zh) 带背板的溅射靶材的翘曲矫正方法
CN109591335A (zh) 一种复合材料产品成型过程中金属件的预埋方法
CN108973099A (zh) 一种多曲面贴膜的方法
CN104493440A (zh) 一种波形膨胀节的制造工艺
JP6508568B2 (ja) タービンブレード用素材の形状矯正方法及びタービンブレード用素材の製造方法
CN207204905U (zh) 矫正装置
CN206925504U (zh) 一种用于板材焊接的辅助夹持装置
CN107673589A (zh) 一种挡风玻璃弯曲成形的方法
CN202259131U (zh) 一种行波管用螺旋线慢波系统的热压缩夹具
CN205167532U (zh) 一种管材轨道式矫正装置
CN105109024A (zh) 一种多曲率薄壁复合材料零件的热校形方法
CN104701223A (zh) 一种芯片压合设备
KR101165313B1 (ko) 카본원사 편직구조를 갖는 라켓용 샤프트 및 그 제조방법
JP2015030104A (ja) タイヤ加硫方法及びタイヤ加硫装置
CN110641009A (zh) 一种高分子发泡无缝缓冲管的制备方法
CN205169044U (zh) 非接触式预热装置
CN112571772A (zh) 一种碳纤维复合材料的弯曲矫正方法

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20170606