CN106696589A - Making process for lacquer painting with gold wires embedded in surface - Google Patents

Making process for lacquer painting with gold wires embedded in surface Download PDF

Info

Publication number
CN106696589A
CN106696589A CN201610960135.1A CN201610960135A CN106696589A CN 106696589 A CN106696589 A CN 106696589A CN 201610960135 A CN201610960135 A CN 201610960135A CN 106696589 A CN106696589 A CN 106696589A
Authority
CN
China
Prior art keywords
lacquer
lacquer painting
paint
spun gold
painting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610960135.1A
Other languages
Chinese (zh)
Inventor
魏佳
汪智强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Textile Vocational Technology College
Original Assignee
Nantong Textile Vocational Technology College
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nantong Textile Vocational Technology College filed Critical Nantong Textile Vocational Technology College
Priority to CN201610960135.1A priority Critical patent/CN106696589A/en
Publication of CN106696589A publication Critical patent/CN106696589A/en
Pending legal-status Critical Current

Abstract

The invention discloses a making process for a lacquer painting with gold wires embedded in the surface. By means of the steps of lacquer body preparation, primer preparation, primer coating, manuscript making, plant gum coating, filigreeing, japanning, grinding for showing, clear lacquer covering, pushing for brightening and clean wiping, the making process for the lacquer painting with the gold wires embedded in the surface is completed. The making process for the lacquer painting with the gold wires embedded in the surface has the beneficial effects that the final effect controllability of the lacquer painting can be effectively improved, the precision of stripe patterns of gold lines is guaranteed, the texture consistency of a plurality of frames is guaranteed, the batch production requirement is met, the rate of finished products is increased, and the process is convenient and fast, and is easy to master.

Description

A kind of lacquer painting manufacture craft of surface inserting spun gold
Technical field
The present invention relates to a kind of lacquer painting manufacture craft, and in particular to a kind of lacquer painting manufacture craft of surface inserting spun gold.
Background technology
Lacquer painting is one of more ancient picture kind of China, and its craft method is numerous, and the form of expression is various, often with gold and silver lines Depict personage, birds and flowers, landscape and symbolistic figure, pattern.But because painter's level is different, paint the smoothness of gold and silver lines Property, aesthetic degree have very big difference,
Its works effect has very big uncertainty, is not suitable for mass, standardized making, and this is accomplished by developing and uses More particularly suitable medium materials and means.
The content of the invention
A kind of deficiency it is an object of the invention to be directed to existing manifestation mode, there is provided final effect for effectively improving lacquer painting Controllability, it is ensured that the precision of gold thread bar grain pattern, it is ensured that multiple picture texture homogeneities, meets mass production requirement, improves Yield rate, technique is convenient, it is easy to the lacquer painting manufacture craft of the surface inserting spun gold of grasp.
In order to solve the above technical problems, the technical solution adopted by the present invention is:A kind of lacquer painting of surface inserting spun gold makes Technique, its innovative point is:By preparing paint tire, standby under-coating varnish, priming, bottoming original text, apply natural plant gum, wire inlay, coat with lacquer paint, grind Aobvious, the cover colored varnish, push away light and wipe clear step, complete the lacquer painting manufacture craft of surface inserting spun gold;It is described to comprise the following steps that:
(1)Prepare paint tire:Selected import five-ply board is smooth using liquid honing as base plate, then by latex in base plate On mount one layer of mull, unnecessary mull is dismissed after drying, standby, the thickness of the mull is 0.11-0.16mm;
(2)Standby under-coating varnish:Take raw lacquer, thin dark grey and reconcile uniform, be obtained under-coating varnish, the mixing quality ratio of the raw lacquer and thin dark grey It is 1:1-2;
(3)Prime:By the uniform scrubbing brush of under-coating varnish on paint tire, brush 3-5 times, it is every all over being spaced 24-36 hours, treat that priming paint is dried The silicon carbide paper for wrapping up in 600-800 mesh with plank afterwards is polished lacquer painting, makes lacquer painting smooth;
(4)Bottoming original text:Outlet original text is delineated with pencil on lacquer painting, embedded figure and the position of spun gold is determined;
(5)Apply natural plant gum:Will the part ribs of a leaf pen of mosaic gold silk be stained with natural plant gum, carried out on the lines that pencil is delineated Describe, the natural plant gum is bletilla striata liquid;
(6)Wire inlay:One section of spun gold is chosen, the position for having smeared natural plant gum is bonded at according to the pencil lines trend delineated in advance, borrowed Help tweezers to be bent to spun gold while viscous, make it accurately to be fitted on priming paint along pencil lines trend;Spun gold is all viscous The shady and cool dustless place of drying is lain against after good, 2-4 hours is stood, waits glue to parch;
(7)Coat with lacquer paint:By rough sketch requirement in the lacquer painting upper cover for pasted spun gold colored paint, wait lacquer painting parch after slightly polish, weight Paint step is coated with lacquer again 8-12 times, it is each lacquer painting before to be polished before paint is coated with lacquer, until spun gold turns into one with the lacquer painting on periphery Individual plane;
(8)Mill is aobvious:Carefully mill is carried out to lacquer painting with the mesh silicon carbide paper of 1200 mesh -1500 aobvious, to its lacquer painting and spun gold completely one Individual plane, and surface exquisiteness is bright and clean;
(9)The cover colored varnish:The colored varnish is uniformly brushed on lacquer painting surface with scrubbing brush, is kept flat, standing is dried in the shade, time of repose is 16- 26 hours, polished with 2000-2600 mesh silicon carbide papers;
(10)Push away light:Transparent polished lacquer is taken, dipped in cotton carries out pushing repeatedly on lacquer painting surface;
(11)Wipe clear:The first-class raw lacquer of upper addition raw vegetable oil is dipped in using absorbent cotton, smears uniform on lacquer painting, complete surface edge The lacquer painting manufacture craft of embedding spun gold.
Further, the step(6)In spun gold a width of 0.4mm-0.6mm, a height of 1.0mm-1.5mm.
Further, the step(11)In first-class paint mesad oil addition be 3-11%.
Beneficial effects of the present invention are as follows:Using the present invention, the final effect controllability of lacquer painting is effectively improved, it is ensured that gold The precision of lines grain pattern, it is ensured that multiple picture texture homogeneities, meets mass production requirement, improves yield rate, and technique is just It is prompt, it is easy to grasp.
Specific embodiment
Embodiments of the present invention are illustrated by particular specific embodiment below, those skilled in the art can be by this explanation Content disclosed by book understands other advantages of the invention and effect easily.
Embodiment 1
A kind of lacquer painting manufacture craft of surface inserting spun gold, by preparing paint tire, standby under-coating varnish, priming, bottoming original text, apply plant Glue, wire inlay, coat with lacquer paint, mill aobvious, the cover colored varnish, push away light and wipe clear step, completing the lacquer painting manufacture craft of surface inserting spun gold;Specifically Step is as follows:
(1)Prepare paint tire:Selected import five-ply board is smooth using liquid honing as base plate, then by latex in base plate On mount one layer of mull, unnecessary mull is dismissed after drying, standby, the thickness of the mull is 0.11mm;
(2)Standby under-coating varnish:Take raw lacquer, thin dark grey to reconcile uniformly, under-coating varnish is obtained, raw lacquer is 1 with the mixing quality ratio of thin dark grey: 1;
(3)Prime:By the uniform scrubbing brush of under-coating varnish paint tire on, brush 3 times, it is every all over interval 24 hours, after priming paint drying after with The silicon carbide paper that plank wraps up in 600 mesh is polished lacquer painting, makes lacquer painting smooth;
(4)Bottoming original text:Outlet original text is delineated with pencil on lacquer painting, embedded figure and the position of spun gold is determined;
(5)Apply natural plant gum:Will the part ribs of a leaf pen of mosaic gold silk be stained with natural plant gum, carried out on the lines that pencil is delineated Describe, natural plant gum is bletilla striata liquid;
(6)Wire inlay:One section of spun gold is chosen, the position for having smeared natural plant gum is bonded at according to the pencil lines trend delineated in advance, borrowed Help tweezers to be bent to spun gold while viscous, make it accurately to be fitted on priming paint along pencil lines trend;Spun gold is all viscous The shady and cool dustless place of drying is lain against after good, 2 hours are stood, waits glue to parch, a width of 0.4mm of spun gold, a height of 1.0mm;
(7)Coat with lacquer paint:By rough sketch requirement in the lacquer painting upper cover for pasted spun gold colored paint, wait lacquer painting parch after slightly polish, weight Paint step 8 time is coated with lacquer again, it is each lacquer painting before to be polished before paint is coated with lacquer, until spun gold turns into one with the lacquer painting on periphery putting down Face;
(8)Mill is aobvious:Carefully mill is carried out to lacquer painting with 1200 mesh silicon carbide papers aobvious, to its lacquer painting and spun gold completely in a plane, And surface exquisiteness is bright and clean;
(9)The cover colored varnish:The colored varnish is uniformly brushed on lacquer painting surface with scrubbing brush, is kept flat, standing is dried in the shade, time of repose is 16 small When, polished with 2000 mesh silicon carbide papers;
(10)Push away light:Transparent polished lacquer is taken, dipped in cotton carries out pushing repeatedly on lacquer painting surface;
(11)Wipe clear:The first-class raw lacquer of upper addition raw vegetable oil is dipped in using absorbent cotton, smears uniform on lacquer painting, complete surface edge The lacquer painting manufacture craft of embedding spun gold, the addition of first-class paint mesad oil is 3%.
Embodiment 2
A kind of lacquer painting manufacture craft of surface inserting spun gold, by preparing paint tire, standby under-coating varnish, priming, bottoming original text, apply plant Glue, wire inlay, coat with lacquer paint, mill aobvious, the cover colored varnish, push away light and wipe clear step, completing the lacquer painting manufacture craft of surface inserting spun gold;Specifically Step is as follows:
(1)Prepare paint tire:Selected import five-ply board is smooth using liquid honing as base plate, then by latex in base plate On mount one layer of mull, unnecessary mull is dismissed after drying, standby, the thickness of the mull is 0.16mm;
(2)Standby under-coating varnish:Take raw lacquer, thin dark grey to reconcile uniformly, under-coating varnish is obtained, raw lacquer is 1 with the mixing quality ratio of thin dark grey: 2;
(3)Prime:By the uniform scrubbing brush of under-coating varnish paint tire on, brush 5 times, it is every all over interval 36 hours, after priming paint drying after with The silicon carbide paper that plank wraps up in 800 mesh is polished lacquer painting, makes lacquer painting smooth;
(4)Bottoming original text:Outlet original text is delineated with pencil on lacquer painting, embedded figure and the position of spun gold is determined;
(5)Apply natural plant gum:Will the part ribs of a leaf pen of mosaic gold silk be stained with natural plant gum, carried out on the lines that pencil is delineated Describe, natural plant gum is bletilla striata liquid;
(6)Wire inlay:One section of spun gold is chosen, the position for having smeared natural plant gum is bonded at according to the pencil lines trend delineated in advance, borrowed Help tweezers to be bent to spun gold while viscous, make it accurately to be fitted on priming paint along pencil lines trend;Spun gold is all viscous The shady and cool dustless place of drying is lain against after good, 4 hours are stood, waits glue to parch, a width of 0.6mm of spun gold, a height of 1.5mm.
(7)Coat with lacquer paint:By rough sketch requirement in the lacquer painting upper cover for pasted spun gold colored paint, wait lacquer painting parch after slightly beat Paint step 12 time is coated with lacquer in mill, repetition, each lacquer painting before to be polished before paint is coated with lacquer, until spun gold turns into the lacquer painting on periphery One plane;
(8)Mill is aobvious:Carefully mill is carried out to lacquer painting with 1500 mesh silicon carbide papers aobvious, to its lacquer painting and spun gold completely in a plane, And surface exquisiteness is bright and clean;
(9)The cover colored varnish:The colored varnish is uniformly brushed on lacquer painting surface with scrubbing brush, is kept flat, standing is dried in the shade, time of repose is 26 small When, polished with 2600 mesh silicon carbide papers;
(10)Push away light:Transparent polished lacquer is taken, dipped in cotton carries out pushing repeatedly on lacquer painting surface;
(11)Wipe clear:The first-class raw lacquer of upper addition raw vegetable oil is dipped in using absorbent cotton, smears uniform on lacquer painting, complete surface edge The lacquer painting manufacture craft of embedding spun gold, the addition of first-class paint mesad oil is 11%.
Embodiment 3
A kind of lacquer painting manufacture craft of surface inserting spun gold, by preparing paint tire, standby under-coating varnish, priming, bottoming original text, apply plant Glue, wire inlay, coat with lacquer paint, mill aobvious, the cover colored varnish, push away light and wipe clear step, completing the lacquer painting manufacture craft of surface inserting spun gold;Specifically Step is as follows:
(1)Prepare paint tire:Selected import five-ply board is smooth using liquid honing as base plate, then by latex in base plate On mount one layer of mull, unnecessary mull is dismissed after drying, standby, the thickness of the mull is 0.15mm;
(2)Standby under-coating varnish:Take raw lacquer, thin dark grey to reconcile uniformly, under-coating varnish is obtained, raw lacquer is 1 with the mixing quality ratio of thin dark grey: 1.5;
(3)Prime:By the uniform scrubbing brush of under-coating varnish paint tire on, brush 4 times, it is every all over interval 30 hours, after priming paint drying after with The silicon carbide paper that plank wraps up in 700 mesh is polished lacquer painting, makes lacquer painting smooth;
(4)Bottoming original text:Outlet original text is delineated with pencil on lacquer painting, embedded figure and the position of spun gold is determined;
(5)Apply natural plant gum:Will the part ribs of a leaf pen of mosaic gold silk be stained with natural plant gum, carried out on the lines that pencil is delineated Describe, natural plant gum is bletilla striata liquid;
(6)Wire inlay:One section of spun gold is chosen, the position for having smeared natural plant gum is bonded at according to the pencil lines trend delineated in advance, borrowed Help tweezers to be bent to spun gold while viscous, make it accurately to be fitted on priming paint along pencil lines trend;Spun gold is all viscous The shady and cool dustless place of drying is lain against after good, 3 hours are stood, waits glue to parch, a width of 0.5mm of spun gold, a height of 1.3mm;
(7)Coat with lacquer paint:By rough sketch requirement in the lacquer painting upper cover for pasted spun gold colored paint, wait lacquer painting parch after slightly polish, weight Paint step 10 time is coated with lacquer again, it is each lacquer painting before to be polished before paint is coated with lacquer, until spun gold turns into one with the lacquer painting on periphery Plane;
(8)Mill is aobvious:Carefully mill is carried out to lacquer painting with 1300 mesh silicon carbide papers aobvious, to its lacquer painting and spun gold completely in a plane, And surface exquisiteness is bright and clean;
(9)The cover colored varnish:The colored varnish is uniformly brushed on lacquer painting surface with scrubbing brush, is kept flat, standing is dried in the shade, time of repose is 20 small When, polished with 2300 mesh silicon carbide papers;
(10)Push away light:Transparent polished lacquer is taken, dipped in cotton carries out pushing repeatedly on lacquer painting surface;
(11)Wipe clear:The first-class raw lacquer of upper addition raw vegetable oil is dipped in using absorbent cotton, smears uniform on lacquer painting, complete surface edge The lacquer painting manufacture craft of embedding spun gold, the addition of first-class paint mesad oil is 7%.
Following experimental data can obtain by above-mentioned 3 embodiments, data are as shown in the table:
By above-mentioned experimental data, it is known that, the gold thread of the lacquer painting of the surface inserting spun gold that the method for embodiment 1,2 and 3 is prepared Bar grain pattern precision and yield rate are much higher than the lacquer painting of the surface inserting spun gold that common process is prepared.
Using the present invention, the final effect controllability of lacquer painting is effectively improved, it is ensured that the precision of gold thread bar grain pattern, it is ensured that many Individual picture texture homogeneity, meets mass production requirement, improves yield rate, and technique is convenient, it is easy to grasp.
Above-described embodiment is presently preferred embodiments of the present invention, is not the limitation to technical solution of the present invention, as long as Without the technical scheme that creative work can be realized on the basis of above-described embodiment, it is regarded as falling into patent of the present invention Rights protection scope in.

Claims (3)

1. a kind of lacquer painting manufacture craft of surface inserting spun gold, it is characterised in that:Through preparation paint tire, standby under-coating varnish, prime, Bottoming original text, natural plant gum is applied, is wired inlay, is coated with lacquer paint, mill aobvious, the cover colored varnish, pushes away light and wipe clear step, the lacquer painting of completion surface inserting spun gold Manufacture craft;It is described to comprise the following steps that:
Prepare paint tire:Selected import five-ply board is smooth using liquid honing as base plate, is then mounted on base plate by latex One layer of mull, dismisses unnecessary mull after drying, standby, and the thickness of the mull is 0.11-0.16mm;
Standby under-coating varnish:Take raw lacquer, thin dark grey to reconcile uniformly, under-coating varnish is obtained, the raw lacquer is with the mixing quality ratio of thin dark grey 1:1-2;
Prime:By the uniform scrubbing brush of under-coating varnish on paint tire, brush 3-5 times, it is every all over being spaced 24-36 hours, after after priming paint drying Lacquer painting is polished with the silicon carbide paper that plank wraps up in 600-800 mesh, makes lacquer painting smooth;
Bottoming original text:Outlet original text is delineated with pencil on lacquer painting, embedded figure and the position of spun gold is determined;
Apply natural plant gum:Will the part ribs of a leaf pen of mosaic gold silk be stained with natural plant gum, retouched on the lines that pencil is delineated Paint, the natural plant gum is bletilla striata liquid;
Wire inlay:One section of spun gold is chosen, the position for having smeared natural plant gum is bonded at according to the pencil lines trend delineated in advance, by tweezer It is sub- spun gold is bent while viscous, make it accurately to be fitted on priming paint along pencil lines trend;After spun gold is all glued The shady and cool dustless place of drying is lain against, 2-4 hours is stood, waits glue to parch;
Coat with lacquer paint:By rough sketch requirement in the lacquer painting upper cover for pasted spun gold colored paint, wait lacquer painting parch after slightly polish, repetition coat with lacquer Paint step 8-12 times, it is each lacquer painting before to be polished before paint is coated with lacquer, until spun gold turns into one with the lacquer painting on periphery putting down Face;
Mill is aobvious:Carefully mill is carried out to lacquer painting with the mesh silicon carbide paper of 1200 mesh -1500 aobvious, it is flat completely at one to its lacquer painting and spun gold Face, and surface exquisiteness is bright and clean;
The cover colored varnish:The colored varnish is uniformly brushed on lacquer painting surface with scrubbing brush, is kept flat, standing is dried in the shade, time of repose is that 16-26 is small When, polished with 2000-2600 mesh silicon carbide papers;
Push away light:Transparent polished lacquer is taken, dipped in cotton carries out pushing repeatedly on lacquer painting surface;
Wipe clear:The first-class raw lacquer of upper addition raw vegetable oil is dipped in using absorbent cotton, smears uniform on lacquer painting, complete surface inserting gold The lacquer painting manufacture craft of silk.
2. the lacquer painting manufacture craft of a kind of surface inserting spun gold according to claim 1, it is characterised in that:The step (6)In spun gold a width of 0.4mm-0.6mm, a height of 1.0mm-1.5mm.
3. the lacquer painting manufacture craft of a kind of surface inserting spun gold according to claim 1, it is characterised in that:The step (11)In first-class paint mesad oil addition be 3-11%.
CN201610960135.1A 2016-10-28 2016-10-28 Making process for lacquer painting with gold wires embedded in surface Pending CN106696589A (en)