CN109808407A - A kind of production method for painting plate iron picture - Google Patents
A kind of production method for painting plate iron picture Download PDFInfo
- Publication number
- CN109808407A CN109808407A CN201910086510.8A CN201910086510A CN109808407A CN 109808407 A CN109808407 A CN 109808407A CN 201910086510 A CN201910086510 A CN 201910086510A CN 109808407 A CN109808407 A CN 109808407A
- Authority
- CN
- China
- Prior art keywords
- paint
- iron picture
- lacquer
- painting
- plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of production methods for painting plate iron picture, it is related to painting production technical field, the present invention is coated with lacquer with cover gold in Qi Yi applies this skill and technique production bottom surface liner plate, silver, aluminum metallic foil powder make metalloid color bottom surface, transparent lacquer or transparent cashew nut paint coat with lacquer painting and surface, are allowed to show gentle bright and strong sense of texture characteristic, then the element that sculpture method and space are constituted is dissolved into iron picture, picture timing and spatial impression have promotion, keep picture more agile abundant.And iron picture is incorporated in paint plate with welding embedding technique, on Picture Showing, a variety of painting skills is incorporated, traditional Chinese Painting element is added on the basis of realistic, makes picture while having levels also more rich in artistic conception and entertaining.
Description
Technical field
The present invention relates to painting production method and technology fields, particularly relate to a kind of production method for painting plate iron picture.
Background technique
Iron picture refers to a kind of craftwork for being forged with iron plate and iron wire and being welded into picture, general painted black or brownish red.It is overgrown with weeds
Lake iron picture is ink with iron to hammer into shape as pen, and using anvil as paper, wrought iron is picture, superb craftsmanship, flavor day at.Wuhu iron picture is long-drawn-out with history
Long, unique style, exquisite workmanship, superb skill are world-famous for.But due to the limitation on iron material and creation subject, traditional iron
It is drawn in picture timing and spatial impression and there is shortcoming, and the agile rich deficiency of picture, in order to which Wuhu iron picture is hewed out one
Region specialty industries promote competitiveness of Wuhu iron picture in Chinese Art and Craft goods in the market, need to explore an iron picture and pass
System process innovation development.
Summary of the invention
In view of this, it is an object of the invention to propose a kind of production method for painting plate iron picture, to overcome existing conventional iron
The all or part of deficiency drawn.
Based on a kind of above-mentioned purpose production method for painting plate iron picture provided by the invention, described method includes following steps:
1) production of iron picture: Design Works original copy prepares out iron picture, the iron of production using sculpture or/and traditional Chinese Painting line drawing method
Component is drawn there are assembled portion, then the iron picture component of preparation is carried out derusting and colouring is handled by ease of assembly;
2) paint plate production: taking decorative bottom plate, roughly ground to bottom plate, coat with lacquer painting, and coating with lacquer coating layer thickness is 3~6mm, coating to be coated with lacquer
After drying to humidity < 10%, matel coated foil powder is spread, plate face is made to show silvery white tone, it is secondary to coat with lacquer painting after plate face is completely dried
Enter 5~7h of shade, coat with lacquer and be painted into shade 2~3 times, after being completely dried, the polishing of level skin texture is carried out to paint plate;
3) it assembles: the iron picture component of preparation is layered on paint plate according to design manuscript, it is whole after being filled by original set of locations
Body cover paint, after drying completely, integral manufacturing step is fully completed, and must paint plate iron picture.
In some optional embodiments, the assembled portion is stitch or screw-socket.
In some optional embodiments, the derusting is first to be cleaned using the diluted acid of concentration 20~40%, is then adopted
It is roasting in 800~1000 DEG C of fire with flame burner.
In some optional embodiments, the colouring is carried out using polyesters paint, hand self-spraying paint or resinae paint
Color.
In some optional embodiments, rough tool is 240# waterproof abrasive paper in described (2).
In some optional embodiments, painting is coated with lacquer in described (2) using transparent priming, including following weight percent at
Point: transparent lacquer or cashew nut paint 45~55%, diluent 45~55%.
In some optional embodiments, the metal foil powder is the silver foil and aluminium foil mixture that mass ratio is 1:2~5.
In some optional embodiments, in described (2) skin texture milling tools be fineness be respectively 800#, 1500#, 3000#,
5000# waterproof abrasive paper.
From the above it can be seen that a kind of production method for painting plate iron picture provided by the invention, by Chinese tradition lacquer painting
With merging for region iron picture, is coated with lacquer with cover gold in Qi Yi and apply this skill and technique production bottom surface liner plate, silver, aluminum metallic foil powder are made
Metalloid color bottom surface, transparent lacquer or transparent cashew nut paint coat with lacquer painting and surface, are allowed to show gentle bright and strong sense of texture spy
Property;Then the element that sculpture method and space are constituted is dissolved into iron picture, picture timing and spatial impression have promotion, make picture
Face is more agile abundant;And iron picture is incorporated in paint plate with welding embedding technique, on Picture Showing, incorporates a variety of drawing skills
Method adds traditional Chinese Painting element on the basis of realistic, makes picture while having levels also more rich in artistic conception and entertaining.
The present invention is a kind of new craftwork art form, wherein traditional lacquer painting is enumerated, the manufacture skill of traditional iron picture,
And new manufacture craft is added, modern painting thinking is added on traditional arts and crafts manufacture skill, makes iron picture and lacquer painting more
Kind painting element fusion, explores the road of a traditional handicraft innovation and development.
Detailed description of the invention
Fig. 1 is " fishing is returned " works of production of the embodiment of the present invention, the figure under no light;
Fig. 2 is " fishing is returned " works of production of the embodiment of the present invention, the figure under light.
Specific embodiment
To make the objectives, technical solutions, and advantages of the present invention clearer, below in conjunction with specific embodiment, and reference
Attached drawing, the present invention is described in more detail.
In order to overcome iron picture traditional in the prior art to there is shortcoming in picture timing and spatial impression, and picture is agile
The disadvantage of rich deficiency, a kind of production method for painting plate iron picture provided in an embodiment of the present invention, the method includes walking as follows
It is rapid:
1) production of iron picture: Design Works original copy prepares out iron picture, the iron of production using sculpture or/and traditional Chinese Painting line drawing method
Component is drawn there are assembled portion, then the iron picture component of preparation is carried out derusting and colouring is handled by ease of assembly;
2) paint plate production: taking decorative bottom plate, roughly ground to bottom plate, coat with lacquer painting, and coating with lacquer coating layer thickness is 3~6mm, coating to be coated with lacquer
After drying to humidity < 10%, matel coated foil powder is spread, plate face is made to show silvery white tone, it is secondary to coat with lacquer painting after plate face is completely dried
Enter 5~7h of shade, coat with lacquer and be painted into shade 2~3 times, after being completely dried, the polishing of level skin texture is carried out to paint plate;
3) it assembles: the iron picture component of preparation is layered on paint plate according to design manuscript, it is whole after being filled by original set of locations
Body cover paint, after drying completely, integral manufacturing step is fully completed, and must paint plate iron picture.
Further, a kind of production method for paint plate iron picture that one embodiment of the present invention provides, includes the following steps:
1) production of iron picture: making design manuscript in conjunction with picture, goes out contribution with traditional Chinese Painting or line drawing block face formal layout, hands over
It is made in iron picture master worker, manufacturing process embodies iron picture forging skill, incorporates the drawing member such as element or traditional Chinese Painting element of sculpture
Element keeps picture plentiful;Stitch or screw-socket assembled portion, ease of assembly, iron picture component are left after the iron picture component got
It after completing, is first cleaned using the diluted acid of concentration 35%, then using flame burner in the roasting derusting processing of 900 DEG C of fire;
Then it paints to iron picture component, paints and polyesters paint can be selected, hand self-spraying paint, resinae paint processing keeps a variety of colors, rich
Rich form of painting;
2) paint plate production: decorative bottom plate is taken, after first roughly grinding using 240# waterproof abrasive paper to bottom plate, (i.e. by transparent priming
Transparent lacquer or cashew nut paint 50%, diluent 50% reconcile) coat with lacquer and be applied to backplate surface, coating with lacquer coating layer thickness is 5mm, need by
It 24 hours or so, is taken out after coating with lacquer coating drying to humidity < 10%, paving applies silver, the aluminium mixed metal foil powder that mass ratio is 1:3,
Plate face is set to show silvery white tone, during applying foil powder, if surface only dries 7 percent, 80, powder absorbs priming paint
More, silvery white cannot reach bright instead, and if priming paint Tu get Tai is thin, completely solid, foil powder cannot then adhere to completely thereon;
After plate face is completely dried, secondary coat with lacquer is painted into 5~7h of shade, coats with lacquer and is painted into shady 2~3 times, after being completely dried, finally using 800#,
1500#, 3000#, 5000# waterproof abrasive paper are successively polished by design original text requirement, using polishing gimmick, polishing degree weight, make to paint plate
Surface shows different levels skin texture;
3) it assembles: the iron picture component of preparation being layered on paint plate according to design manuscript, is put on stitch or screw with colored paint
Mouthful set position, with small bit bore on stitch or screw in hole (or using super glue such as 502ab glue) by its
Fixed, the last layer can be done with matte varnish or gloss varnish by being completed rear the last layer cover paint, and be spontaneously dried,
Plate iron picture must be painted.
The present invention secondly embodiment with one embodiment, unlike, the present invention is secondly a kind of paint plate that embodiment provides
In the production method of iron picture:
1) it after the completion of iron picture establishment of component, is first cleaned using the diluted acid of concentration 20%, is then existed using flame burner
The roasting derusting processing of 800 DEG C of fire.
2) coating with lacquer coating layer thickness is 4mm, coats with lacquer painting using transparent priming, including following weight percent composition: transparent big
Paint or cashew nut paint 45%, diluent 55%, metal foil powder are the silver foil that mass ratio is 1:2 and aluminium foil mixture.
The present invention thirdly embodiment with one embodiment, unlike, the present invention is thirdly a kind of paint plate that embodiment provides
In the production method of iron picture:
1) it after the completion of iron picture establishment of component, is first cleaned using the diluted acid of concentration 40%, is then existed using flame burner
The roasting derusting processing of 1000 DEG C of fire.
2) coating with lacquer coating layer thickness is 6mm, coats with lacquer painting using transparent priming, including following weight percent composition: transparent big
Paint or cashew nut paint 55%, diluent 45%, metal foil powder are the silver foil that mass ratio is 1:5 and aluminium foil mixture.
Its of the invention four embodiment with one embodiment, unlike, a kind of paint plate that its four embodiment of the invention provides
In the production method of iron picture:
1) it after the completion of iron picture establishment of component, is first cleaned using the diluted acid of concentration 20%, is then existed using flame burner
The roasting derusting processing of 800 DEG C of fire.
2) coating with lacquer coating layer thickness is 6mm, coats with lacquer painting using transparent priming, including following weight percent composition: transparent big
Paint or cashew nut paint 55%, diluent 45%, metal foil powder are the silver foil that mass ratio is 1:5 and aluminium foil mixture.
Its of the invention five embodiment with one embodiment, unlike, a kind of paint plate that its five embodiment of the invention provides
In the production method of iron picture:
1) it after the completion of iron picture establishment of component, is first cleaned using the diluted acid of concentration 40%, is then existed using flame burner
The roasting derusting processing of 1000 DEG C of fire.
2) coating with lacquer coating layer thickness is 4mm, coats with lacquer painting using transparent priming, including following weight percent composition: transparent big
Paint or cashew nut paint 45%, diluent 55%, metal foil powder are the silver foil that mass ratio is 1:2 and aluminium foil mixture.
Fig. 1~2 are the works of entitled " fishing is returned " produced that is carried out using method in the embodiment of the present invention, works specification
90 × 60cm, " fishing is returned " works are the products of the fusion of Chinese industrial art traditional technology, in traditional arts and crafts manufacture skill
It is upper to add modern painting thinking, allow iron picture to merge with a variety of painting elements, an innovation and development road is walked out in trial.
It is Chinese tradition lacquer painting merges with iron picture, and the characteristic for having used the gentle bright sense of texture of lacquer painting strong is as bottom surface
Liner plate imposes color with paint powder, and silver-colored pearl powder is made in silver color bottom surface involvement paint and makes sense of texture, then by sculpture method and space
The element of composition is dissolved into iron picture, is allowed the picture timing of iron picture and spatial impression to have promotion, is kept picture rhythm cleverer
It is dynamic abundant.And iron picture is incorporated in paint plate with welding embedding technique, a variety of painting skills are incorporated on Picture Showing, are being write
Traditional Chinese Painting element is added on the basis of reality, so that picture is had artistic conception while also there are distant relationships.
This works is the trial of a new material, is the fusion and innovation of traditional technique, closes the road for development of own characteristic.
It should be understood by those ordinary skilled in the art that: the discussion of any of the above embodiment is exemplary only, not
It is intended to imply that the scope of the present disclosure (including claim) is limited to these examples;Under thinking of the invention, above embodiments
Or can also be combined between the technical characteristic in different embodiments, step can be realized with random order, and be existed such as
Many other variations of the upper different aspect of the invention, for simplicity, they are not provided in details.
The embodiment of the present invention be intended to cover fall into all such replacements within the broad range of appended claims,
Modifications and variations.Therefore, all within the spirits and principles of the present invention, any omission, modification, equivalent replacement, the improvement made
Deng should all be included in the protection scope of the present invention.
Claims (8)
1. a kind of production method for painting plate iron picture, which is characterized in that described method includes following steps:
1) production of iron picture: Design Works original copy prepares out iron picture, the iron picture group of production using sculpture or/and traditional Chinese Painting line drawing method
There are assembled portion, ease of assembly, and the iron picture component of preparation then to be carried out derusting and colouring is handled for part;
2) paint plate production: taking decorative bottom plate, roughly ground to bottom plate, coat with lacquer painting, and coating with lacquer coating layer thickness is 3~6mm, and coating to be coated with lacquer is dry
To humidity < 10%, matel coated foil powder is spread, so that plate face is showed silvery white tone, after plate face is completely dried, secondary coat with lacquer is painted into shade
5~7h is coated with lacquer and is painted into shade 2~3 times, after being completely dried, carries out the polishing of level skin texture to paint plate;
3) it assembles: the iron picture component of preparation is layered on paint plate according to design manuscript, after original set of locations dress, piece cover
Paint, after drying completely, integral manufacturing step is fully completed, and must paint plate iron picture.
2. the production method of paint plate iron picture according to claim 1, which is characterized in that the assembled portion is stitch or spiral shell
Silk mouth.
3. the production method of paint plate iron picture according to claim 1, which is characterized in that the derusting is first using concentration 20
~40% diluted acid is cleaned, then roasting in 800~1000 DEG C of fire using flame burner.
4. the production method of paint plate iron picture according to claim 1, which is characterized in that the colouring is using polyesters
Paint, hand self-spraying paint or resinae paint are painted.
5. the production method of paint plate iron picture according to claim 1, which is characterized in that rough tool is in (2)
240# waterproof abrasive paper.
6. it is according to claim 1 paint plate iron picture production method, which is characterized in that coated with lacquer in (2) painting using
Transparent priming, including following weight percent composition: transparent lacquer or cashew nut paint 45~55%, diluent 45~55%.
7. the production method of paint plate iron picture according to claim 1, which is characterized in that the metal foil powder is that mass ratio is
The silver foil and aluminium foil mixture of 1:2~5.
8. the production method of paint plate iron picture according to claim 1, which is characterized in that skin texture milling tools in (2)
It is respectively 800#, 1500#, 3000#, 5000# waterproof abrasive paper for fineness.