CN105984869A - 乙二胺改性活性炭的制备方法 - Google Patents

乙二胺改性活性炭的制备方法 Download PDF

Info

Publication number
CN105984869A
CN105984869A CN201510052316.XA CN201510052316A CN105984869A CN 105984869 A CN105984869 A CN 105984869A CN 201510052316 A CN201510052316 A CN 201510052316A CN 105984869 A CN105984869 A CN 105984869A
Authority
CN
China
Prior art keywords
activated carbon
ethylenediamine
modified activated
steel cylinder
ethylenediamine modified
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510052316.XA
Other languages
English (en)
Inventor
刘加召
徐启生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
State Productivity Promotion Centre (limited)
Original Assignee
State Productivity Promotion Centre (limited)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by State Productivity Promotion Centre (limited) filed Critical State Productivity Promotion Centre (limited)
Priority to CN201510052316.XA priority Critical patent/CN105984869A/zh
Publication of CN105984869A publication Critical patent/CN105984869A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种乙二胺改性活性炭,其技术方案要点是,先购买椰壳制备的活性炭、乙二胺、N2,将活性炭放入到钢瓶中,并且持续对其升温,使钢瓶内的活性炭降温至100℃,持续通入1小时N2,在对其包装储存。将廉价的价廉的乙二胺偶联接枝到活性炭表面,将乙二胺对贵金属离子的鳌合特性与活性炭的高比表面积相结合,从而增加了现有技术中的活性炭的吸附性,以及产品的可塑性,从而能使其更好的对贵金属回收,大气PM2.5过滤,污染处理等领域。

Description

乙二胺改性活性炭的制备方法
技术领域
本发明涉及一种活性炭,尤其涉及一种乙二胺改性活性炭的制备方法。
背景技术
活性炭是一种具有丰富的孔隙结构、比表面积非常大的粉末状物质,其对贵金属离子具有非常强的吸附作用。活性炭吸附法回收金,工艺过程简单、回收率高、成本低廉,是目前贵金属选矿领域应用最为广泛的吸附回收方法之一。另外,由于可以采用很多种因地制宜的方法以煤、椰壳、杏核、甘蔗渣等制备活性炭,其成本较低,适合于规模化生产。因此,目前采用活性炭作为吸附剂回收金的方法得到了广泛应用。
但是现有技术中的活性炭的吸附能力一定,对一些贵金属离子的吸附性一般,或者吸附不完全,所以急需要提高活性炭的吸附能力。另外,活性炭的可塑性不强,无法制得要求形状的产品,也是在防止大气污染、治理污水方面需要解决的。
发明内容
本发明要解决的技术问题是,提供一种乙二胺改性化性炭的制备方法以克服现有技术中的缺陷。
为达到上述目的,本发明提供一种乙二胺改性活性炭的制备方法,包括以下步骤:
(1)采购活性炭、乙二胺、N2
(2)选择仪器:风机、流量计、钢瓶、鼓泡法制备吸附剂装置;
(3)将活性炭放入到钢瓶中,并且分别在300、400、500、600下采用鼓泡法通入乙二胺,升温速率为10℃/min;
(4)使钢瓶内的活性炭降温至100℃,持续通入1小时N2
(5)包装与储存。
作为本发明的进一步改进,所述步骤(1)中的活性炭为椰壳制备的活性炭。
作为本发明的进一步改进,所述步骤(1)中的N2为钢瓶装高纯N2
作为本发明的进一步改进,所述步骤(5)中的储存要在干燥、阴凉、洁净的环境中。
与现有技术相比,本发明的有益效果是:这样就将廉价的价廉的乙二胺偶联接枝到活性炭表面,将乙二胺对贵金属离子的鳌合特性与活性炭的高比表面积相结合,从而增加了现有技术中的活性炭的吸附性,从而能使其更好的对贵金属回收,并且还可以用于大气的PM2.5过滤,污水处理等领域。
具体实施方式
下面为本发明实施例,对本发明的具体实施方式作进一步详细描述。以下实施例用于说明本发明,但不用来限制本发明的范围。
本发明的一种本发明提供一种乙二胺改性活性炭的制备方法,包括以下步骤:
(1)采购活性炭、乙二胺、N2,活性炭为椰壳制备的活性炭,N2为钢瓶装高纯N2,椰壳制备的活性炭可保证生产出的乙二胺改性活性炭性能可靠稳定,而N2为钢瓶装高纯N2是为了保证其纯度和性能的稳定性;
(2)选择仪器:风机、流量计、钢瓶、鼓泡法制备吸附剂装置;
(3)将活性炭放入到钢瓶中,并且分别在300、400、500、600下采用鼓泡法通入乙二胺,升温速率为10℃/min;
(4)使钢瓶内的活性炭降温至100℃,持续通入1小时N2
(5)包装与储存,储存要在干燥、阴凉、洁净的环境中,是为了适合其无污染、性能稳定的要求。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围,包括后续设计本技术的后续产品的开发与应用。

Claims (4)

1.一种乙二胺改性活性炭的制备方法,其特征在于,包括以下步骤:
(1)采购活性炭、乙二胺、N2
(2)选择仪器:风机、流量计、钢瓶、鼓泡法制备吸附剂装置;
(3)将活性炭放入到钢瓶中,并且分别在300、400、500、600下采用鼓泡法通入乙二胺,升温速率为10℃/min;
(4)使钢瓶内的活性炭降温至100℃,持续通入1小时N2
(5)包装与储存。
2.根据权利要求1所述的乙二胺改性活性炭的制备方法,其特征在于:所述步骤(1)中的活性炭为椰壳制备的活性炭。
3.根据权利要求1所述的乙二胺改性活性炭的制备方法,其特征在于:所述步骤(1)中的N2为钢瓶装高纯N2
4.根据权利要求1所述的乙二胺改性活性炭的制备方法,其特征在于:所述步骤(5)中的储存要在干燥、阴凉、洁净的环境中。
CN201510052316.XA 2015-01-30 2015-01-30 乙二胺改性活性炭的制备方法 Pending CN105984869A (zh)