Publication number
CN105081485A
CN105081485A CN201510621815.6A CN201510621815A CN105081485A CN 105081485 A CN105081485 A CN 105081485A CN 201510621815 A CN201510621815 A CN 201510621815A CN 105081485 A CN105081485 A CN 105081485A
Authority
CN
China
Prior art keywords
diamondite
barred body
spark machined
tungsten alloy
bar body
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510621815.6A
Other languages
English (en)
Inventor
陈铮
张志娟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HENAN DADI ALLOY CO Ltd
Original Assignee
HENAN DADI ALLOY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HENAN DADI ALLOY CO Ltd filed Critical HENAN DADI ALLOY CO Ltd
Priority to CN201510621815.6A priority Critical patent/CN105081485A/zh
Publication of CN105081485A publication Critical patent/CN105081485A/zh
Pending legal-status Critical Current

Abstract

本发明公开一种电火花加工用碳化钨合金细棒,该碳化钨合金细棒用于电火花加工中作电极材料,包括棒体;所述棒体设置有冷却液从棒体的顶端注入、从棒体的底端涌出的中心孔,所述棒体为带中心孔的碳化钨合金棒体;所述棒体用制成电火花加工中的电极材料,所述中心孔可以注入冷却液,用于电火花加工中的冷却、润滑和排屑。棒体的长度≥100㎜,外径≤1.5㎜,中心孔直径≤0.6㎜。本发明的电火花加工用碳化钨合金细棒克服了现有技术的碳化钨合金细棒在高精度高速度加工情况下强度下降、刚性变差、使用寿命缩短、加工成本提高和排屑困难的缺陷。

Description

电火花加工用碳化钨合金细棒
技术领域
本发明涉及粉末冶金制造技术领域,具体地说涉及一种电火花加工用碳化钨合金细棒。
背景技术
在粉末冶金制造技术领域,由粉末硬质合金制成的细棒广泛用于玉石的机械打孔修整、印刷电路板(PCB-PrintedCircuitBoard)机械钻孔等。碳化钨合金细棒是硬质合金的一种,其结构特点是细棒为实心,直径小、长度长,长度尺寸公差范围较小且垂直度要求较高。
碳化钨合金细棒虽然在玉石的机械打孔修整、印刷电路板(PCB-PrintedCircuitBoard)机械钻孔等获得了成功,但很少有在电火花加工行业应用的记载,究其原因,在电火花加工过程中,电极材料的作用是输送加工脉冲,并以自身最小的损耗去蚀除工件,而碳化钨合金细棒由于细棒为实心棒材,导致细棒在电火花加工应用时排屑困难,局部温升过高,限制了碳化钨合金细棒在电火花加工行业的应用。
发明内容
本发明的目的在于提供一种电火花加工用碳化钨合金细棒,以期克服现有技术的碳化钨合金细棒在电火花加工行业应用的缺陷。
为实现上述目的,本发明采用了如下的技术方案:
一种电火花加工用碳化钨合金细棒,该碳化钨合金细棒用于电火花加工中作电极材料,包括棒体;所述棒体设置有使冷却液从棒体的顶端注入、从棒体的底端涌出的中心孔,所述棒体为带中心孔的碳化钨合金棒体;所述棒体用制成电火花加工中的电极材料,所述中心孔可以注入冷却液,用于电火花加工中的冷却、润滑和排屑。
作为对上述技术方案的改进,所述棒体的长度≥100㎜,外径≤1.5㎜,中心孔直径≤0.6㎜。
作为对上述技术方案的改进,上述碳化钨合金细棒用于电火花加工中作电极材料;所述细棒为带中心孔的碳化钨合金细棒。
作为对上述技术方案的改进,碳化钨合金自身的高杨氏模量>600MPa。
与现有技术相比,本发明所取得的有益效果是:
本发明的电火花加工用碳化钨合金细棒,用于电火花加工中作电极材料,碳化钨合金细棒的中部设置有使冷却液从棒体的顶端注入、从棒体的底端涌出的中心孔,所述中心孔可以注入冷却液,用于电火花加工中的冷却、润滑和排屑。
本碳化钨合金细棒用碳化钨合金混合料粉经混合、研磨、过滤干燥、挤压、烧结、收缩、冷却而成;碳化钨合金细棒中设置有中心孔,在使用的时候,可通入冷却液,一来可以将碳化钨合金细棒切削头部的磨屑排出,提高加工效率,二来实现对碳化钨合金细棒的冷却,使碳化钨合金细棒的温升下降,从而保证碳化钨合金细棒的强度、刚度,保证加工的质量和效率。碳化钨合金细棒可以直接开槽制成挫刀或用金刚石微粉涂层,以提高其耐磨性。
本发明的电火花加工用碳化钨合金细棒可广泛用于电火花加工行业,开拓了碳化钨合金细棒在电火花加工行业的应用,增加了碳化钨合金细棒的使用范围,其强度高、刚性好、使用寿命长,加工成本低;碳化钨合金自身的高杨氏模量(>600MPa)及中心孔进一步增加其电极的刚性,加上中心孔的排屑和冷却作用,这对要求高精度的小直径的深孔加工带来非常大的利益。
附图说明
构成本申请的一部分附图用来提供对本发明的进一步理解,本发明的示意性实施例及其说明用于解释本发明,并不构成对本发明的不当限定。
图1为本发明的结构示意图。
具体实施方式
下面结合附图对本发明作进一步详细说明。
实施例1:
如图1所示,本实施例的电火花加工用碳化钨合金细棒,该碳化钨合金细棒用于电火花加工中作电极材料,包括棒体1;所述棒体1设置有冷却液从棒体1的顶端注入、从棒体1的底端涌出的中心孔2,所述棒体1为带中心孔2的碳化钨合金棒体;所述棒体用制成电火花加工中的电极材料,所述中心孔2可以注入冷却液,用于电火花加工中的冷却、润滑和排屑。
该碳化钨合金细棒,包括棒体1,所述棒体1为带中心孔2的碳化钨合金棒体;所述棒体1的长度为100㎜,外径1.5㎜,中心孔2直径0.6㎜。
实施例2:
如图1所示,本实施例的电火花加工用碳化钨合金细棒,该碳化钨合金细棒用于电火花加工中作电极材料,包括棒体1;所述棒体1设置有冷却液从棒体1的顶端注入、从棒体1的底端涌出的中心孔2,所述棒体1为带中心孔2的碳化钨合金棒体;所述棒体用制成电火花加工中的电极材料,所述中心孔2可以注入冷却液,用于电火花加工中的冷却、润滑和排屑。
该碳化钨合金细棒,包括棒体1,所述棒体1为带中心孔2的碳化钨合金棒体;所述棒体1的长度110㎜,外径1.2㎜,中心孔2直径0.5㎜。
碳化钨合金自身的高杨氏模量>600MPa。
以上所述仅为本发明的较佳实施例而已,并不用以限制本发明,凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。

Claims (6)

1.一种电火花加工用碳化钨合金细棒,其特征在于:该碳化钨合金细棒用于电火花加工中作电极材料,包括棒体;所述棒体设置有使冷却液从棒体的顶端注入、从棒体的底端涌出的中心孔,所述棒体为带中心孔的碳化钨合金棒体;所述棒体用制成电火花加工中的电极材料,所述中心孔可以注入冷却液,用于电火花加工中的冷却、润滑和排屑。
2.根据权利要求1的述的电火花加工用碳化钨合金细棒,其特征在于:所述棒体的中心孔直径≤0.6㎜。
3.根据权利要求1的述的电火花加工用碳化钨合金细棒,其特征在于:所述棒体的外径≤1.5㎜。
4.根据权利要求1的述的电火花加工用碳化钨合金细棒,其特征在于:所述棒体的长度≥100㎜。
5.如权利要求2或3或4所述的电火花加工用碳化钨合金细棒,其特征在于:该碳化钨合金细棒用于电火花加工中作电极材料;所述细棒为带中心孔的碳化钨合金细棒。
6.如权利要求5所述的电火花加工用碳化钨合金细棒,其特征在于:碳化钨合金自身的高杨氏模量>600MPa。
CN201510621815.6A 2015-09-28 2015-09-28 电火花加工用碳化钨合金细棒 Pending CN105081485A (zh)