CN104862476A - 高银难解吸载金炭的解吸方法 - Google Patents
高银难解吸载金炭的解吸方法 Download PDFInfo
- Publication number
- CN104862476A CN104862476A CN201510282911.2A CN201510282911A CN104862476A CN 104862476 A CN104862476 A CN 104862476A CN 201510282911 A CN201510282911 A CN 201510282911A CN 104862476 A CN104862476 A CN 104862476A
- Authority
- CN
- China
- Prior art keywords
- loaded carbon
- gold
- desorption
- silver
- gold loaded
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种用于黄金行业中高银难解吸载金炭的解吸方法,该方法通过用清水冲洗高银难解吸载金炭,去除高银难解吸表面炭泥及絮凝剂等覆盖物,在低碱度1%~2%,低温75℃~85℃状态下解吸4~6个小时,然后升温至150℃解吸12~18小时即可完成解吸电解作业,对于高品位载金炭可添加解吸剂,使解吸更加彻底。该方法节能、环保,所用试剂无毒,价廉易得,大大提高金属回收率。
Description
技术领域
本发明涉及一种用于黄金行业中高银难解吸载金炭的解吸方法。
背景技术
在现有国内黄金炭浆工艺生产中,载金炭的主要解吸方法有常温常压解吸、中温中压无氰解吸、有机物洗脱法、去离子水洗脱法等。对于常规载金炭这些解吸方法几乎都能满足生产要求,但是对于高银载金炭(特别Ag、Au金属量比为3:1载金炭),这些方法都不能满足生产要求,贫炭金银品味过高。
发明内容
为了降低高银载金炭解吸后贫炭的金银品味,该发明提供一种高银难解吸载金炭的解吸方法,该方法可以解决高银载金炭难解吸问题,降低贫炭金银品位。
本发明的方法是:
首先利用清水冲洗高银难解吸载金炭,去除高银难解吸载金炭表面炭泥和絮凝剂覆盖物;
其次,在碱的质量百分比浓度为1%~2%、解吸温度75℃~85℃情况下解吸4~6个小时,然后升温至150℃解吸12~18小时即可完成解吸电解作业,对于高品位载金炭可添加解吸剂,使解吸更加彻底;所述的碱为氢氧化钠;所述的解吸剂为异辛醇。
所述的高品位载金炭为Ag:Au金属量比为3:1的载金炭。
本发明的有益效果是:
贫炭中金品位比传统解吸方法降低30%左右、银降低50%左右,大大降低了金银在系统内的滞留时间,金银回收率提高,给黄金企业带来了直观利润,而且该方法无污染物添加和产生,环保意义重大。
Claims (2)
1.一种高银难解吸载金炭的解吸方法,该方法是:
首先利用清水冲洗高银难解吸载金炭,去除高银难解吸载金炭表面炭泥和絮凝剂覆盖物;
其次,在碱的质量百分比浓度为1%~2%、解吸温度75℃~85℃情况下解吸4~6个小时,然后升温至150℃解吸12~18小时即可完成解吸电解作业,对于高品位载金炭可添加解吸剂,使解吸更加彻底;所述的碱为氢氧化钠;所述的解吸剂为异辛醇。
2.根据权利要求1所述的一种高银难解吸载金炭的解吸方法,其特征在于:所述的高品位载金炭为Ag:Au金属量比为3:1的载金炭。