CN104493934A - Bamboo weaving softening agent and preparation technique thereof - Google Patents

Bamboo weaving softening agent and preparation technique thereof Download PDF

Info

Publication number
CN104493934A
CN104493934A CN201410757786.1A CN201410757786A CN104493934A CN 104493934 A CN104493934 A CN 104493934A CN 201410757786 A CN201410757786 A CN 201410757786A CN 104493934 A CN104493934 A CN 104493934A
Authority
CN
China
Prior art keywords
softening agent
agent
stearic acid
bamboo weaving
minutes
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410757786.1A
Other languages
Chinese (zh)
Other versions
CN104493934B (en
Inventor
王银
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shandong Yangxin Hualong Textile Technology Co.,Ltd.
Original Assignee
JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES filed Critical JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES
Priority to CN201410757786.1A priority Critical patent/CN104493934B/en
Publication of CN104493934A publication Critical patent/CN104493934A/en
Application granted granted Critical
Publication of CN104493934B publication Critical patent/CN104493934B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a bamboo weaving softening agent and a preparation method thereof. The preparation method comprises the following steps: putting glycerol, alcohol ether glucoside, polyethenoxy ether and a surfactant into a stirring tank, stirring for 30 minutes at 80 DEG C, adding glyoxal, formaldehyde and ammonium persulfate, simultaneously adding talcum powder, limestone flour and calcium carbonate, quickly stirring at 130 DEG C for 3 minutes, finally adding stearyl alcohol, stearic acid, ethyl carbamate and paraffin, stirring for 1 hour, and cooling to normal temperature. The softening agent prepared by the method has the advantages of favorable softening effect, no corrosion and better effects, enhances the strength and toughness of the softened part, and is convenient for popularization and use.

Description

Bamboo weaving softening agent and preparation technology thereof
Technical field:
The present invention relates to bamboo softening technology field, be specifically related to bamboo weaving softening agent and preparation technology thereof.
Background technology:
Existing bamboo weaving is softening generally all continues to use traditional approach, and fire is roasting, after roasting for bamboo fire, can carry out bending and be compiled into various articles for use, and this softening mode is too simple, and easily roasting disconnected bamboo, affects toughness and the intensity of bamboo.
Summary of the invention:
Technical problem to be solved by this invention is the defect overcoming prior art, provides a kind of bamboo weaving softening agent and preparation technology thereof.
Technical problem to be solved by this invention realizes by the following technical solutions.
Bamboo weaving softening agent, is characterized in that: comprise intensity modifying agent 28-34 part, form retention agent 41-48 part, softening agent 66-71 part, initator 16-19 part, reinforcing agent 10-16 part, water 130-140 part;
Intensity modifying agent: stearyl alcohol 60-70%, stearic acid 30-40%;
Form retention agent: stearic acid 15-25%, urethanes 60-65%, paraffin 15%-20% part;
Softening agent: glycerine 20-30%, alcohol ether glucoside 20-30%, APEO 20-30%, surfactant 20-30%;
Initator: glyoxal 15-25%, formaldehyde 20-25%, ammonium persulfate 55-60%;
Reinforcing agent: talcum powder 30-40%, agstone 30-40%, calcium carbonate 30-40%.
Bamboo weaving softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds glyoxal, formaldehyde, ammonium persulfate, put into talcum powder, agstone, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
Beneficial effect of the present invention is: the softening agent prepared by this law, and bating effect is good, corrosion-free, and strengthen intensity and the toughness of maceration, effect is better, is convenient to promote and use.
Detailed description of the invention:
The technological means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, below in conjunction with specific embodiment, setting forth the present invention further.
Embodiment 1: bamboo weaving softening agent, is characterized in that: comprise intensity modifying agent 28 parts, form retention agent 41 parts, softening agent 66 parts, initator 16 parts, reinforcing agent 10 parts, 130 parts, water;
Intensity modifying agent: stearyl alcohol 60%, stearic acid 40%;
Form retention agent: stearic acid 15%, urethanes 65%, 20% part, paraffin;
Softening agent: glycerine 20%, alcohol ether glucoside 20%, APEO 30%, surfactant 30%;
Initator: glyoxal 15%, formaldehyde 25%, ammonium persulfate 60%;
Reinforcing agent: talcum powder 40%, agstone 30%, calcium carbonate 30%.
Bamboo weaving softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds glyoxal, formaldehyde, ammonium persulfate, put into talcum powder, agstone, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
Through experiment, this law compares than following data with the common fire method of baking:
Tensile strength Compression strength Bending strength Coefficient of elasticity Bending angle
Fire is roasting 1300kg/m 2 800kg/m 2 1500kg/m 2 80000kg 40°
Softening agent 4300kg/m 2 1500kg/m 2 3600kg/m 2 200000kg 75°
Embodiment 2: bamboo weaving softening agent, is characterized in that: comprise intensity modifying agent 34 parts, form retention agent 48 parts, softening agent 71 parts, initator 19 parts, reinforcing agent 16 parts, 140 parts, water;
Intensity modifying agent: stearyl alcohol 70%, stearic acid 30%;
Form retention agent: stearic acid 25%, urethanes 65%, 15% part, paraffin;
Softening agent: glycerine 30%, alcohol ether glucoside 30%, APEO 20%, surfactant 20%;
Initator: glyoxal 25%, formaldehyde 20%, ammonium persulfate 55%;
Reinforcing agent: talcum powder 40%, agstone 30%, calcium carbonate 30%.
Bamboo weaving softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds glyoxal, formaldehyde, ammonium persulfate, put into talcum powder, agstone, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
Through experiment, this law compares than following data with the common fire method of baking:
Tensile strength Compression strength Bending strength Coefficient of elasticity Bending angle
Fire is roasting 1400kg/m 2 700kg/m 2 1500kg/m 2 80000kg 40°
Softening agent 4000kg/m 2 2000kg/m 2 3300kg/m 2 150000kg 80°
More than show and describe general principle of the present invention, principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and description just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (2)

1. bamboo weaving softening agent, is characterized in that: comprise intensity modifying agent 28-34 part, form retention agent 41-48 part, softening agent 66-71 part, initator 16-19 part, reinforcing agent 10-16 part, water 130-140 part;
Intensity modifying agent: stearyl alcohol 60-70%, stearic acid 30-40%;
Form retention agent: stearic acid 15-25%, urethanes 60-65%, paraffin 15%-20% part;
Softening agent: glycerine 20-30%, alcohol ether glucoside 20-30%, APEO 20-30%, surfactant 20-30%;
Initator: glyoxal 15-25%, formaldehyde 20-25%, ammonium persulfate 55-60%;
Reinforcing agent: talcum powder 30-40%, agstone 30-40%, calcium carbonate 30-40%.
2. bamboo weaving softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds glyoxal, formaldehyde, ammonium persulfate, put into talcum powder, agstone, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
CN201410757786.1A 2014-12-10 2014-12-10 Bamboo weaving softening agent and preparation technology thereof Active CN104493934B (en)