CN104526808A - Bamboo strip softener and preparation process thereof - Google Patents

Bamboo strip softener and preparation process thereof Download PDF

Info

Publication number
CN104526808A
CN104526808A CN201410757775.3A CN201410757775A CN104526808A CN 104526808 A CN104526808 A CN 104526808A CN 201410757775 A CN201410757775 A CN 201410757775A CN 104526808 A CN104526808 A CN 104526808A
Authority
CN
China
Prior art keywords
stearic acid
softener
stirring
softening agent
agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410757775.3A
Other languages
Chinese (zh)
Inventor
王银
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES
Original Assignee
JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES filed Critical JIESHOU XIANGYU BAMBOO WEAVING SPECIALIZED COOPERATIVES
Priority to CN201410757775.3A priority Critical patent/CN104526808A/en
Publication of CN104526808A publication Critical patent/CN104526808A/en
Pending legal-status Critical Current

Abstract

The invention provides a bamboo strip softener and a preparation process thereof. The bamboo strip softener is prepared by the following steps: weighing glycerol, alkylethoxyglucoside, polyoxyethylene ether and a surfactant, putting into a stirring tank, stirring for 30 minutes with the stirring temperature to be 80 DEG C, then adding potassium persulfate, formaldehyde and ammonium persulfate, simultaneously adding cobalt naphthenate, dimethylaniline and calcium carbonate, rapidly stirring for 3 minutes with the stirring temperature to be 130 DEG C, finally adding stearyl alcohol, stearic acid, stearic acid, urethane and paraffin, stirring for 1h, and cooling at room temperature. The bamboo strip softener has the beneficial effects that the prepared softener is good in softening effect without corrosion and good in effect, is capable of strengthening the strength and the toughness of the softening part and is convenient in popularization and using.

Description

Bamboo cane softening agent and preparation technology thereof
Technical field:
The present invention relates to bamboo softening technology field, be specifically related to bamboo cane softening agent and preparation technology thereof.
Background technology:
Existing bamboo cane is softening generally all continues to use traditional approach, and fire is roasting, after roasting for bamboo fire, can carry out bending and be compiled into various articles for use, and this softening mode is too simple, and easily roasting disconnected bamboo, affects toughness and the intensity of bamboo.
Summary of the invention:
Technical problem to be solved by this invention is the defect overcoming prior art, provides a kind of bamboo cane softening agent and preparation technology thereof.
Technical problem to be solved by this invention realizes by the following technical solutions.
Bamboo cane softening agent, is characterized in that: comprise intensity modifying agent 28-34 part, form retention agent 41-48 part, softening agent 66-71 part, initator 16-19 part, promoter 10-16 part, water 130-140 part;
Intensity modifying agent: stearyl alcohol 60-70%, stearic acid 30-40%;
Form retention agent: stearic acid 15-25%, urethanes 60-65%, paraffin 15%-20% part;
Softening agent: glycerine 20-30%, alcohol ether glucoside 20-30%, APEO 20-30%, surfactant 20-30%;
Initator: potassium peroxydisulfate 15-25%, formaldehyde 20-25%, ammonium persulfate 55-60%;
Promoter: cobalt naphthenate 30-40%, dimethylaniline 30-40%, calcium carbonate 30-40%.
Bamboo cane softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds potassium peroxydisulfate, formaldehyde, ammonium persulfate, put into cobalt naphthenate, dimethylaniline, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
Beneficial effect of the present invention is: the softening agent prepared by this law, and bating effect is good, corrosion-free, and strengthen intensity and the toughness of maceration, effect is better, is convenient to promote and use.
Detailed description of the invention:
The technological means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, below in conjunction with specific embodiment, setting forth the present invention further.
Embodiment 1: bamboo cane softening agent, is characterized in that: comprise intensity modifying agent 28 parts, form retention agent 41 parts, softening agent 66 parts, initator 16 parts, promoter 10 parts, 130 parts, water;
Intensity modifying agent: stearyl alcohol 60%, stearic acid 40%;
Form retention agent: stearic acid 15%, urethanes 65%, 20% part, paraffin;
Softening agent: glycerine 20%, alcohol ether glucoside 20%, APEO 30%, surfactant 30%;
Initator: potassium peroxydisulfate 15%, formaldehyde 25%, ammonium persulfate 60%;
Promoter: cobalt naphthenate 40%, dimethylaniline 30%, calcium carbonate 30%.
Bamboo cane softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds potassium peroxydisulfate, formaldehyde, ammonium persulfate, put into cobalt naphthenate, dimethylaniline, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
Through experiment, this law compares than following data with the common fire method of baking:
Tensile strength Compression strength Bending strength Coefficient of elasticity Bending angle
Fire is roasting 1100kg/㎡ 900kg/㎡ 1000kg/㎡ 100000kg 40°
Softening agent 4500kg/㎡ 2000kg/㎡ 4000kg/㎡ 140000kg 70°
Embodiment 2: bamboo cane softening agent, is characterized in that: comprise intensity modifying agent 34 parts, form retention agent 48 parts, softening agent 71 parts, initator 19 parts, promoter 16 parts, 140 parts, water;
Intensity modifying agent: stearyl alcohol 70%, stearic acid 30%;
Form retention agent: stearic acid 25%, urethanes 65%, 15% part, paraffin;
Softening agent: glycerine 30%, alcohol ether glucoside 30%, APEO 20%, surfactant 20%;
Initator: potassium peroxydisulfate 25%, formaldehyde 20%, ammonium persulfate 55%;
Promoter: cobalt naphthenate 40%, dimethylaniline 30%, calcium carbonate 30%.
Bamboo cane softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds potassium peroxydisulfate, formaldehyde, ammonium persulfate, put into cobalt naphthenate, dimethylaniline, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
Through experiment, this law compares than following data with the common fire method of baking:
Tensile strength Compression strength Bending strength Coefficient of elasticity Bending angle
Fire is roasting 1400kg/㎡ 700kg/㎡ 1500kg/㎡ 80000kg 40°
Softening agent 4000kg/㎡ 2000kg/㎡ 3300kg/㎡ 150000kg 80°
More than show and describe general principle of the present invention, principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and description just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (2)

1. bamboo cane softening agent, is characterized in that: comprise intensity modifying agent 28-34 part, form retention agent 41-48 part, softening agent 66-71 part, initator 16-19 part, promoter 10-16 part, water 130-140 part;
Intensity modifying agent: stearyl alcohol 60-70%, stearic acid 30-40%;
Form retention agent: stearic acid 15-25%, urethanes 60-65%, paraffin 15%-20% part;
Softening agent: glycerine 20-30%, alcohol ether glucoside 20-30%, APEO 20-30%, surfactant 20-30%;
Initator: potassium peroxydisulfate 15-25%, formaldehyde 20-25%, ammonium persulfate 55-60%;
Promoter: cobalt naphthenate 30-40%, dimethylaniline 30-40%, calcium carbonate 30-40%.
2. bamboo cane softening agent preparation method: it is characterized in that: get glycerine, alcohol ether glucoside, APEO, surfactant, put into agitator tank, stir 30 minutes, whipping temp is 80 DEG C, then adds potassium peroxydisulfate, formaldehyde, ammonium persulfate, put into cobalt naphthenate, dimethylaniline, calcium carbonate simultaneously, whipping temp 130 DEG C, rapid stirring 3 minutes, finally adds stearyl alcohol, stearic acid, stearic acid, urethanes and paraffin, stir 1 hour, normal temperature cools.
CN201410757775.3A 2014-12-10 2014-12-10 Bamboo strip softener and preparation process thereof Pending CN104526808A (en)