CN104294449A - Anti-pilling suede stretch wool fabric and manufacturing method thereof - Google Patents
Anti-pilling suede stretch wool fabric and manufacturing method thereof Download PDFInfo
- Publication number
- CN104294449A CN104294449A CN201410442896.9A CN201410442896A CN104294449A CN 104294449 A CN104294449 A CN 104294449A CN 201410442896 A CN201410442896 A CN 201410442896A CN 104294449 A CN104294449 A CN 104294449A
- Authority
- CN
- China
- Prior art keywords
- yarn
- weft yarn
- fibre
- suede
- antipilling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an anti-pilling suede stretch wool fabric. Warp and weft A of the fabric are formed by blending wool fibers and anti-pilling fibers, weft B of the fabric is covering yarn composed of elastic fibers serving as core yarn and wool fibers wrapping the elastic fibers, the proportion of the weft A and the weft B is 1:1, the weight percentage of the wool fibers in the warp and the weft A is 55-60%, and the weight percentage of the wool fibers in the weft B is 75-85%. The anti-pilling suede stretch wool fabric has high elasticity and excellent resilience, and is good in felting performance, exquisite in suede hand feel and excellent in anti-pilling performance.
Description
Technical field
The present invention relates to textiles and textile technology, be specifically related to a kind of ANTIPILLING suede elastic and preparation method thereof.
Background technology
Along with the development of society, improving constantly of people's living standard, not only pursues novel style to textiles, more focuses on the quality of fabric, only have the clothes of unique style, level top grade just can become the main flow in market, the dark favor by people.People more and more pay attention to the thickness of clothes, comfortableness and warmth retention property.Wool is the first-selected fabric of high-grade clothing, and the lightening of worsted fabric is one of its inevitable development trend.There is the undesirable shortcoming of feltability difference, pile effects in current common tweed fabric, and the shortcoming of easy pilling.
Summary of the invention
The object of the invention is to overcome the defect existed in prior art, the ANTIPILLING suede elastic that a kind of quality is frivolous, feel is fine and smooth, anti-pilling property is excellent is provided.
For realizing above-mentioned technique effect, technical scheme of the present invention is: a kind of ANTIPILLING suede elastic, it is characterized in that, the warp thread of described fabric and weft yarn A are formed by wool fibre and anti-pill fibre blending, the weft yarn B of described fabric is core silk with elastomer and the cladded yarn made of outsourcing wool fibre, in described weft yarn, the ratio of weft yarn A and weft yarn B is 1:1, in described warp thread and weft yarn A, shared by wool fibre, percentage by weight is 55 ~ 60%, and in described weft yarn B, shared by wool fibre, percentage by weight is 75 ~ 85%.
A preparation method for ANTIPILLING suede elastic, is characterized in that, described preparation method comprises the following steps:
The first step: prepare spinning ANTIPILLING suede elastic need raw material;
Second step: respectively wool fibre, anti-pill fibre and elastomer are dyeed;
3rd step: spinning, by the wool fibre after dyeing and anti-pill fibre by making blended yarn with hair, hacking, shredding, carding slivering, drafting, open-end spinning and automatic winding technique; Wool fibre after dyeing is made slubbing yarn by closing hair, carding, drafting, rove, open-end spinning and winding process, is then the spandex core-spun yarn that core silk spinning is made with elastomer on fine spining machine;
4th step: weave, to the 3rd step yarn weave on Rapier looms;
5th step: Final finishing, by the 3rd step the cloth knitted by grey cloth sizing, running boiling, move back dimension, crabbing, singe, braying, cropping, crease-resistant, hot light make finished product, wherein, the sizing of bad cloth adopts high-temperature shaping, speed: 42 ~ 48m/min, temperature 188 ~ 192 DEG C.
Wherein, in described second step, anti-pill fibre special Lay Wella dyeing adopts when 48 ~ 52 DEG C of low temperature, adds DISPERSE DYES and auxiliary agent running 4 ~ 6min; Then be rapidly heated to 90 ~ 91 DEG C with liter per minute 4 DEG C before this, then with the slow programming rate of 1min1 DEG C to 130 ~ 132 DEG C, then continue insulation 48 ~ 52min.
Wherein, described crease-resistant operation completes on setting machine, and the anti wrinkling agent that described crease-resistant operation uses is combined by polyamide and dimethyl silicone polymer, and in described anti wrinkling agent, the mass percent of polyamide is 65 ~ 75%.
Advantage of the present invention and beneficial effect are:
Of the present invention the employing of ANTIPILLING suede elastic has higher elasticity and excellent rebound performance, feltability is good, matte feel fine and smooth, anti-pilling property is excellent.
Detailed description of the invention
Below in conjunction with embodiment, the specific embodiment of the present invention is further described.Following examples only for technical scheme of the present invention is clearly described, and can not limit the scope of the invention with this.
Embodiment 1
A kind of ANTIPILLING suede elastic, the warp thread of fabric and weft yarn A are formed by wool fibre and anti-pill fibre blending, the weft yarn B of fabric is core silk with elastomer and the cladded yarn made of outsourcing wool fibre, in weft yarn, the ratio of weft yarn A and weft yarn B is 1:1, in warp thread and weft yarn A, shared by wool fibre, percentage by weight is 55%, and in weft yarn B, percentage by weight shared by wool fibre is 75%.
A preparation method for ANTIPILLING suede elastic, is characterized in that, preparation method comprises the following steps:
The first step: prepare spinning ANTIPILLING suede elastic need raw material;
Second step: respectively wool fibre, anti-pill fibre and elastomer are dyeed;
3rd step: spinning, by the wool fibre after dyeing and anti-pill fibre by making blended yarn with hair, hacking, shredding, carding slivering, drafting, open-end spinning and automatic winding technique; Wool fibre after dyeing is made slubbing yarn by closing hair, carding, drafting, rove, open-end spinning and winding process, is then the spandex core-spun yarn that core silk spinning is made with elastomer on fine spining machine;
4th step: weave, to the 3rd step yarn weave on Rapier looms;
5th step: Final finishing, by the 3rd step the cloth knitted by grey cloth sizing, running boiling, move back dimension, crabbing, singe, braying, cropping, crease-resistant, hot light make finished product, wherein, the sizing of bad cloth adopts high-temperature shaping, speed: 42m/min, temperature 188 DEG C.
Wherein, in second step, anti-pill fibre special Lay Wella dyeing adopts when 48 DEG C of low temperature, adds DISPERSE DYES and auxiliary agent running 4min; Then be rapidly heated to 90 DEG C with liter per minute 4 DEG C before this, then with the slow programming rate of 1min1 DEG C to 130 DEG C, then continue insulation 48min.
Wherein, crease-resistant operation completes on setting machine, and anti wrinkling agent is combined by polyamide and dimethyl silicone polymer, and in anti wrinkling agent, the mass percent of polyamide is 65%.
Embodiment 2
Embodiment 2 is with the difference of embodiment 1, and in warp thread and weft yarn A, shared by wool fibre, percentage by weight is 60%, and in weft yarn B, percentage by weight shared by wool fibre is 85%.
In embodiment 2 ANTIPILLING suede elastic preparation method's second step in anti-pill fibre special Lay Wella dyeing adopt when 52 DEG C of low temperature, add DISPERSE DYES and auxiliary agent running 6min; Then be rapidly heated to 91 DEG C with liter per minute 4 DEG C before this, then with the slow programming rate of 1min1 DEG C to 132 DEG C, then continue insulation 52min.
Wherein, crease-resistant operation completes on setting machine, and anti wrinkling agent is combined by polyamide and dimethyl silicone polymer, and in anti wrinkling agent, the mass percent of polyamide is 75%.
Freefit fabric soft, elasticity is moderate, moisture absorption, good permeability, comfortable and easy to wear.Comparatively be suitable as shirt fabric.
The above is only the preferred embodiment of the present invention; it should be pointed out that for those skilled in the art, under the prerequisite not departing from the technology of the present invention principle; can also make some improvements and modifications, these improvements and modifications also should be considered as protection scope of the present invention.
Claims (4)
1. an ANTIPILLING suede elastic, it is characterized in that, the warp thread of described fabric and weft yarn A are formed by wool fibre and anti-pill fibre blending, the weft yarn B of described fabric is core silk with elastomer and the cladded yarn made of outsourcing wool fibre, in described weft yarn, the ratio of weft yarn A and weft yarn B is 1:1, in described warp thread and weft yarn A, shared by wool fibre, percentage by weight is 55 ~ 60%, and in described weft yarn B, shared by wool fibre, percentage by weight is 75 ~ 85%.
2. a preparation method for ANTIPILLING suede elastic, is characterized in that, described preparation method comprises the following steps:
The first step: prepare spinning ANTIPILLING suede elastic need raw material;
Second step: respectively wool fibre, anti-pill fibre and elastomer are dyeed;
3rd step: spinning, by the wool fibre after dyeing and anti-pill fibre by making blended yarn with hair, hacking, shredding, carding slivering, drafting, open-end spinning and automatic winding technique; Wool fibre after dyeing is made slubbing yarn by closing hair, carding, drafting, rove, open-end spinning and winding process, is then the spandex core-spun yarn that core silk spinning is made with elastomer on fine spining machine;
4th step: weave, to the 3rd step yarn weave on Rapier looms;
5th step: Final finishing, by the 3rd step the cloth knitted by grey cloth sizing, running boiling, move back dimension, crabbing, singe, braying, cropping, crease-resistant, hot light make finished product, wherein, the sizing of bad cloth adopts high-temperature shaping, speed: 42 ~ 48m/min, temperature 188 ~ 192 DEG C.
3. ANTIPILLING suede elastic according to claim 2 and preparation method thereof, is characterized in that, in described second step, anti-pill fibre special Lay Wella dyeing adopts when 48 ~ 52 DEG C of low temperature, adds DISPERSE DYES and auxiliary agent running 4 ~ 6min; Then be rapidly heated to 90 ~ 91 DEG C with liter per minute 4 DEG C before this, then with the slow programming rate of 1min1 DEG C to 130 ~ 132 DEG C, then continue insulation 48 ~ 52min.
4. ANTIPILLING suede elastic according to claim 3 and preparation method thereof, it is characterized in that, described crease-resistant operation completes on setting machine, the anti wrinkling agent that described crease-resistant operation uses is combined by polyamide and dimethyl silicone polymer, and in described anti wrinkling agent, the mass percent of polyamide is 65 ~ 75%.