CN104131429A - 一种用定型轧车浸轧修正色光的修色工艺 - Google Patents

一种用定型轧车浸轧修正色光的修色工艺 Download PDF

Info

Publication number
CN104131429A
CN104131429A CN201410343362.0A CN201410343362A CN104131429A CN 104131429 A CN104131429 A CN 104131429A CN 201410343362 A CN201410343362 A CN 201410343362A CN 104131429 A CN104131429 A CN 104131429A
Authority
CN
China
Prior art keywords
color
padding machine
technology
shaping
padding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410343362.0A
Other languages
English (en)
Inventor
刘长申
彭新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinjiang Longxinglong Dyeing & Weaving Industrial Co Ltd
Original Assignee
Jinjiang Longxinglong Dyeing & Weaving Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jinjiang Longxinglong Dyeing & Weaving Industrial Co Ltd filed Critical Jinjiang Longxinglong Dyeing & Weaving Industrial Co Ltd
Priority to CN201410343362.0A priority Critical patent/CN104131429A/zh
Publication of CN104131429A publication Critical patent/CN104131429A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种用定型轧车浸轧修正色光的修色工艺,依次进行配布、抓取配方、浸轧修色和对色,如对色存在深浅差,则适当调整定型轧车的压力,重新进行浸轧修色3-5次,每次30-60min;如无深浅差,则进行成品检检包装。与现有技术相比,本发明的有益效果是:该工艺通过定型加色工艺处理后,可避免染色后色不对进缸重修或经后整后成品色不对无法返修的,可直接于定型轧车修色,大大降低生产成本,减少环境污染;经过本工艺生产的面料,其色泽更加鲜艳,手感更具有柔软滑爽感,广泛的应用于任何成衣服装面料。

Description

一种用定型轧车浸轧修正色光的修色工艺
技术领域
本发明涉及纺织技术领域,具体是一种用定型轧车浸轧修正色光的修色工艺。
背景技术
随着社会的进步,生活水平的提高,人们对环境也越来越重视,国家对环保的政策也越来越严,正进行大力整治,节能减排成为当前最重要的目标,同时水资源的缺乏,要求人们降低印染用量,降低单位染色损耗。而现有的染色工艺染色后会出现轻微色光,或者在后整处理过程后容易造成色光变异,因此需要多次进染缸重修颜色,其工作效率低,水、电、汽的消耗高,增加了生产成本,排污量增多,造成环境污染,而且布面色不稳定。
发明内容
本发明的目的在于提供一种用定型轧车浸轧修正色光的修色工艺,该工艺可以修正染色后轻微色光或因后整处理造成的色光变异。
为实现上述目的,本发明提供如下技术方案:
一种用定型轧车浸轧修正色光的修色工艺,包括以下步骤:
(1)配布:采用染后颜色不对或成品颜色不对的锦纶、涤纶或锦棉交织物,经纬密不限的坯布进行配布;
(2)抓取配方:取染后颜色不对或成品颜色不对的锦纶、涤纶或锦棉交织物的样品,然后在试验室中依色光差异调配红黄蓝涂料及渗透剂的配方,然后抓取配方; 
(3)浸轧修色:将步骤(2)抓取的配方设定于定型轧车进行修色处理,定型轧车的浸轧温度设定为175-195℃,车速保持30-60m/min;
(4)对色:取步骤(3)处理后的样品与标准样比对;如存在深浅差,则适当调整定型轧车的压力,重新进行浸轧修色3-5次,每次30--60min;如无深浅差,则进行成品检检包装;
(5)成品检检包装:对布进行检验,分等级后进行包装。
作为本发明进一步的方案:步骤(3)中定型轧车的浸轧温度设定为180-190℃,车速保持40-50m/min。
与现有技术相比,本发明的有益效果是:该工艺通过定型加色工艺处理后,可避免染色后色不对进缸重修或经后整后成品色不对无法返修的,可直接于定型轧车修色,大大降低生产成本,减少环境污染;经过本工艺生产的面料,其色泽更加鲜艳,手感更具有柔软滑爽感,广泛的应用于任何成衣服装面料。
具体实施方式
下面将结合本发明实施例,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
本发明实施例中,一种用定型轧车浸轧修正色光的修色工艺,包括以下步骤:
(1)配布:采用染后颜色不对或成品颜色不对的锦纶、涤纶或锦棉交织物,经纬密不限的坯布进行配布;
(2)抓取配方:取染后颜色不对或成品颜色不对的锦纶、涤纶或锦棉交织物的样品,然后在试验室中依色光差异调配红黄蓝涂料及渗透剂的配方,然后抓取配方; 
(3)浸轧修色:将步骤(2)抓取的配方设定于定型轧车进行修色处理,定型轧车的浸轧温度设定为175-195℃,车速保持30-60m/min;作为优选,定型轧车的浸轧温度设定为180-190℃,车速保持40-50m/min。
(4)对色:取步骤(3)处理后的样品与标准样比对;如存在深浅差,则适当调整定型轧车的压力,重新进行浸轧修色3-5次,每次30--60min;如无深浅差,则进行成品检检包装;
(5)成品检检包装:对布进行检验,分等级后进行包装。
对于本领域技术人员而言,显然本发明不限于上述示范性实施例的细节,而且在不背离本发明的精神或基本特征的情况下,能够以其他的具体形式实现本发明。因此,无论从哪一点来看,均应将实施例看作是示范性的,而且是非限制性的,本发明的范围由所附权利要求而不是上述说明限定,因此旨在将落在权利要求的等同要件的含义和范围内的所有变化囊括在本发明内。 
此外,应当理解,虽然本说明书按照实施方式加以描述,但并非每个实施方式仅包含一个独立的技术方案,说明书的这种叙述方式仅仅是为清楚起见,本领域技术人员应当将说明书作为一个整体,各实施例中的技术方案也可以经适当组合,形成本领域技术人员可以理解的其他实施方式。

Claims (2)

1.一种用定型轧车浸轧修正色光的修色工艺,其特征在于,包括以下步骤:
配布:采用染后颜色不对或成品颜色不对的锦纶、涤纶或锦棉交织物,经纬密不限的坯布进行配布;
抓取配方:取染后颜色不对或成品颜色不对的锦纶、涤纶或锦棉交织物的样品,然后在试验室中依色光差异调配红黄蓝涂料及渗透剂的配方,然后抓取配方; 
浸轧修色:将步骤(2)抓取的配方设定于定型轧车进行修色处理,定型轧车的浸轧温度设定为175-195℃,车速保持30-60m/min;
对色:取步骤(3)处理后的样品与标准样比对;如存在深浅差,则适当调整定型轧车的压力,重新进行浸轧修色3-5次,每次30--60min;如无深浅差,则进行成品检检包装;
成品检检包装:对布进行检验,分等级后进行包装。
2.根据权利要求1所述的用定型轧车浸轧修正色光的修色工艺,其特征在于,步骤(3)中定型轧车的浸轧温度设定为180-190℃,车速保持40-50m/min。
CN201410343362.0A 2014-07-18 2014-07-18 一种用定型轧车浸轧修正色光的修色工艺 Pending CN104131429A (zh)