CN104072890A CN201410290214.7A CN201410290214A CN104072890A CN 104072890 A CN104072890 A CN 104072890A CN 201410290214 A CN201410290214 A CN 201410290214A CN 104072890 A CN104072890 A CN 104072890A
Authority
CN
China
Prior art keywords
parts
resistant
ethylene propylene
diene monomer
propylene diene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410290214.7A
Other languages
English (en)
Inventor
杨存俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Ningguo Shangding Rubber & Plastic Products Co Ltd
Original Assignee
Anhui Ningguo Shangding Rubber & Plastic Products Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Ningguo Shangding Rubber & Plastic Products Co Ltd filed Critical Anhui Ningguo Shangding Rubber & Plastic Products Co Ltd
Priority to CN201410290214.7A priority Critical patent/CN104072890A/zh
Publication of CN104072890A publication Critical patent/CN104072890A/zh
Pending legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
    • C08L23/00Compositions of homopolymers or copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond; Compositions of derivatives of such polymers
    • C08L23/02Compositions of homopolymers or copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond; Compositions of derivatives of such polymers not modified by chemical after-treatment
    • C08L23/16Elastomeric ethene-propene or ethene-propene-diene copolymers, e.g. EPR and EPDM rubbers
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08KUse of inorganic or non-macromolecular organic substances as compounding ingredients
    • C08K2201/00Specific properties of additives
    • C08K2201/002Physical properties
    • C08K2201/003Additives being defined by their diameter
    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08KUse of inorganic or non-macromolecular organic substances as compounding ingredients
    • C08K2201/00Specific properties of additives
    • C08K2201/011Nanostructured additives

Landscapes

  • Chemical & Material Sciences (AREA)
  • Health & Medical Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Medicinal Chemistry (AREA)
  • Polymers & Plastics (AREA)
  • Organic Chemistry (AREA)
  • Compositions Of Macromolecular Compounds (AREA)

Abstract

本发明公开了一种耐磨耐撕裂三元乙丙橡胶材料,其原料按重量份包括:三元乙丙橡胶30-40份,氯丁橡胶10-18份,LH-C96硫化剂0.8-1.5份,N,N'-间苯基双马来酰亚胺0.5-1.5份,促进剂TMTD1.5-1.8份,氧化镁2-4份,硬脂酸1-3份,偏苯三酸三辛酯5-10份,环保阻燃剂FR-T8012.5-4份,三氧化二锑0.8-1.6份,纳米氧化锌20-40份,煤矸石粉15-30份,煅烧陶土20-30份,防老剂RD2-3份,防老剂NBC0.5-1.3份。本发明具有优异的耐磨耐撕裂性能,耐老化性能好。

Description

一种耐磨耐撕裂三元乙丙橡胶材料
技术领域
本发明涉及橡胶材料技术领域,尤其涉及一种耐磨耐撕裂三元乙丙橡胶材料。
背景技术
三元乙丙橡胶是乙烯、丙烯和非共轭二烯烃的三元共聚物,二烯烃具有特殊的结构,只有两键之一的才能共聚,不饱和的双键主要是作为交链处,另一个不饱和的不会成为聚合物主链,只会成为边侧链,使三元乙丙橡胶的主要聚合物链是完全饱和的。这个特性使得三元乙丙橡胶可以抵抗热、光、氧气,尤其是臭氧。三元乙丙橡胶本质上是无极性的,对极性溶液和化学物具有抗性,吸水率低,具有良好的绝缘特性。在所有橡胶当中,三元乙丙橡胶具有最低的比重,还能吸收大量的填料和油而影响特性不大,因此可以制作成本低廉的橡胶化合物。由于其优异的相容性和绝缘性能,而被电缆行业所广泛使用,但三元乙丙橡胶的耐磨耐撕裂性能并不理想,需要通过加入辅料以提高其性能。
发明内容
基本背景技术存在的技术问题,本发明提出了一种耐磨耐撕裂三元乙丙橡胶材料,具有优异的耐磨耐撕裂性能,耐老化性能好。
本发明提出的一种耐磨耐撕裂三元乙丙橡胶材料,其原料按重量份包括:
优选地,三元乙丙橡胶与氯丁橡胶的重量比为35:15。
优选地,LH-C96硫化剂、N,N'-间苯基双马来酰亚胺及促进剂TMTD的重量比为1.2:1.2:1.6。
优选地,纳米氧化锌中,粒径为10-20nm的占40-60wt%,粒径为50-60nm的占10-30wt%,粒径为70-100nm的占10-30wt%。
本发明以三元乙丙橡胶、氯丁橡胶为主料,采用N,N'-间苯基双马来酰亚胺作为三元乙丙橡胶、氯丁橡胶的过氧化物硫化助剂,不仅可以提高硫化过程的交联速度,还可以有效抑制聚合物的歧化和断链,从而改善产品的综合性能;而且N,N'-间苯基双马来酰亚胺针对三元乙丙橡胶不仅起硫化剂的作用,而且还是老化过程中的结构稳定剂,可减弱硫化返原性;加入氧化镁、三氧化二锑、纳米氧化锌、煤矸石粉和煅烧陶土作为补强剂,辅以偏苯三酸三辛酯和硬脂酸,提高了主料和补强剂的相容性,提高产品的耐磨、抗撕裂性能,还提高产品的强度和硬度,降低了产品的成本,其中纳米氧化锌易分散在基料中,作为活性剂、硫化剂、补强剂及填充剂,促进硫化过程,使产品具有良好的耐磨耐撕裂性能及弹性,而煤矸石粉即为氧化铝、二氧化硅和氧化镁的混合物,其挥发成分高达27%,有半补强效能,俗称硅铝炭黑,易混入橡胶中,分散性好,可替代部分炭黑作补强剂使用。
具体实施方式
下面,通过具体实施例对本发明的技术方案进行详细说明。
在实施例1-4中,本发明提出的一种耐腐蚀耐氧化橡胶材料的原料按重量份如下表所示组成。
实施例1中纳米氧化锌中,粒径为10-20nm的占60wt%,粒径为50-60nm的占10wt%,粒径为70-100nm的占30wt%。
实施例2中纳米氧化锌中,粒径为10-20nm的占40wt%,粒径为50-60nm的占30wt%,粒径为70-100nm的占30wt%。
实施例4中纳米氧化锌中,粒径为10-20nm的占60wt%,粒径为50-60nm的占30wt%,粒径为70-100nm的占10wt%。
以上所述,仅为本发明较佳的具体实施方式,但本发明的保护范围并不局限于此,任何熟悉本技术领域的技术人员在本发明揭露的技术范围内,根据本发明的技术方案及其发明构思加以等同替换或改变,都应涵盖在本发明的保护范围之内。

Claims (5)

1.一种耐磨耐撕裂三元乙丙橡胶材料,其特征在于,其原料按重量份包括:
2.根据权利要求1所述的耐磨耐撕裂三元乙丙橡胶材料,其特征在于,其原料按重量份包括:
3.根据权利要求1或2所述的耐磨耐撕裂三元乙丙橡胶材料,其特征在于,三元乙丙橡胶与氯丁橡胶的重量比为35:15。
4.根据权利要求1-3任一项所述的耐磨耐撕裂三元乙丙橡胶材料,其特征在于,LH-C96硫化剂、N,N'-间苯基双马来酰亚胺及促进剂TMTD的重量比为1.2:1.2:1.6。
5.根据权利要求1-4任一项所述的耐磨耐撕裂三元乙丙橡胶材料,其特征在于,纳米氧化锌中,粒径为10-20nm的占40-60wt%,粒径为50-60nm的占10-30wt%,粒径为70-100nm的占10-30wt%。
CN201410290214.7A 2014-06-24 2014-06-24 一种耐磨耐撕裂三元乙丙橡胶材料 Pending CN104072890A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410290214.7A CN104072890A (zh) 2014-06-24 2014-06-24 一种耐磨耐撕裂三元乙丙橡胶材料

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410290214.7A CN104072890A (zh) 2014-06-24 2014-06-24 一种耐磨耐撕裂三元乙丙橡胶材料

Publications (1)

Publication Number Publication Date
CN104072890A true CN104072890A (zh) 2014-10-01

Family

ID=51594515

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410290214.7A Pending CN104072890A (zh) 2014-06-24 2014-06-24 一种耐磨耐撕裂三元乙丙橡胶材料

Country Status (1)

Country Link
CN (1) CN104072890A (zh)

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104177714A (zh) * 2014-09-10 2014-12-03 安徽弘毅电缆集团有限公司 一种高拉伸性能的煤矸石改性橡胶
CN104558862A (zh) * 2014-12-24 2015-04-29 合肥协知行信息系统工程有限公司 一种耐磨阻燃橡胶配方
CN104592704A (zh) * 2015-02-06 2015-05-06 苏州欢颜电气有限公司 电气工程用防潮绝缘材料
CN105001523A (zh) * 2015-06-30 2015-10-28 桐城市诚信木塑科技材料有限公司 一种阻燃耐磨耐撕裂三元乙丙橡胶材料
CN105017587A (zh) * 2015-07-06 2015-11-04 安徽创宇电力设备有限公司 一种耐撕裂耐磨阻燃绝缘子
CN105348653A (zh) * 2015-09-30 2016-02-24 安徽酷米智能科技有限公司 一种手机外壳用高硬度耐磨耐热材料
CN105400088A (zh) * 2015-12-11 2016-03-16 重庆可益荧新材料有限公司 一种三元乙丙橡胶与氯丁橡胶共硫化材料及其制备方法
CN105949511A (zh) * 2016-05-05 2016-09-21 华北科技学院 一种煤矸石复合型pvc阻燃剂、阻燃材料及其制备方法
CN113248836A (zh) * 2021-05-24 2021-08-13 大冢材料科技(上海)有限公司 一种三元乙丙橡胶组合物及其制备方法

Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1386788A (zh) * 2002-06-12 2002-12-25 上海工程技术大学 含有纳米氧化锌的橡胶及其混炼方法
CN1746211A (zh) * 2004-09-06 2006-03-15 刘明辉 一种阻燃橡胶板材
CN101891905A (zh) * 2009-11-18 2010-11-24 九江学院 一种无骨雨刷胶条及其制备方法
CN101921434A (zh) * 2010-09-19 2010-12-22 无锡宝通带业股份有限公司 一种用于耐高温钢网输送带芯胶的制备方法
CN102993575A (zh) * 2012-12-04 2013-03-27 天津鹏翎胶管股份有限公司 一种低硬度注胶用耐低温的三元乙丙组合物
CN102993520A (zh) * 2012-11-13 2013-03-27 安徽文峰电子科技集团有限公司 一种港机蓄缆筐吊具电缆护套绝缘材料及其制备方法
CN103613810A (zh) * 2013-11-22 2014-03-05 芜湖集拓橡胶技术有限公司 一种改进型氯丁橡胶
CN103665496A (zh) * 2013-11-27 2014-03-26 东营中一橡胶有限公司 耐火橡胶

Patent Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1386788A (zh) * 2002-06-12 2002-12-25 上海工程技术大学 含有纳米氧化锌的橡胶及其混炼方法
CN1746211A (zh) * 2004-09-06 2006-03-15 刘明辉 一种阻燃橡胶板材
CN101891905A (zh) * 2009-11-18 2010-11-24 九江学院 一种无骨雨刷胶条及其制备方法
CN101921434A (zh) * 2010-09-19 2010-12-22 无锡宝通带业股份有限公司 一种用于耐高温钢网输送带芯胶的制备方法
CN102993520A (zh) * 2012-11-13 2013-03-27 安徽文峰电子科技集团有限公司 一种港机蓄缆筐吊具电缆护套绝缘材料及其制备方法
CN102993575A (zh) * 2012-12-04 2013-03-27 天津鹏翎胶管股份有限公司 一种低硬度注胶用耐低温的三元乙丙组合物
CN103613810A (zh) * 2013-11-22 2014-03-05 芜湖集拓橡胶技术有限公司 一种改进型氯丁橡胶
CN103665496A (zh) * 2013-11-27 2014-03-26 东营中一橡胶有限公司 耐火橡胶

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
张祥福等: "EPDM/CR共混物的研究", 《橡胶工业》, vol. 45, no. 1, 31 December 1998 (1998-12-31), pages 3 - 8 *

Cited By (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104177714A (zh) * 2014-09-10 2014-12-03 安徽弘毅电缆集团有限公司 一种高拉伸性能的煤矸石改性橡胶
CN104558862A (zh) * 2014-12-24 2015-04-29 合肥协知行信息系统工程有限公司 一种耐磨阻燃橡胶配方
CN104592704A (zh) * 2015-02-06 2015-05-06 苏州欢颜电气有限公司 电气工程用防潮绝缘材料
CN104592704B (zh) * 2015-02-06 2016-08-24 苏州欢颜电气有限公司 电气工程用防潮绝缘材料
CN105001523A (zh) * 2015-06-30 2015-10-28 桐城市诚信木塑科技材料有限公司 一种阻燃耐磨耐撕裂三元乙丙橡胶材料
CN105017587A (zh) * 2015-07-06 2015-11-04 安徽创宇电力设备有限公司 一种耐撕裂耐磨阻燃绝缘子
CN105348653A (zh) * 2015-09-30 2016-02-24 安徽酷米智能科技有限公司 一种手机外壳用高硬度耐磨耐热材料
CN105400088A (zh) * 2015-12-11 2016-03-16 重庆可益荧新材料有限公司 一种三元乙丙橡胶与氯丁橡胶共硫化材料及其制备方法
CN105949511A (zh) * 2016-05-05 2016-09-21 华北科技学院 一种煤矸石复合型pvc阻燃剂、阻燃材料及其制备方法
CN113248836A (zh) * 2021-05-24 2021-08-13 大冢材料科技(上海)有限公司 一种三元乙丙橡胶组合物及其制备方法

Similar Documents

Publication Publication Date Title
CN104072890A (zh) 一种耐磨耐撕裂三元乙丙橡胶材料
CN105331000B (zh) 高耐磨阻燃钢丝绳芯输送带用覆盖胶及制备方法
CN104086834A (zh) 一种耐油耐腐蚀橡胶材料
CN103524843A (zh) 一种控制信号电缆用护套料及其制备方法
US3136739A (en) Synthetic rubber compositions
CN103788514A (zh) 一种高强耐寒电缆护套材料
SA110310044B1 (ar) مخاليط المطاط المحتوية على السيلان
JP2017101218A (ja) タイヤトレッド用ゴム組成物及びこれを用いて製造したタイヤ
CN104086839A (zh) 一种高强耐磨耐撕裂橡胶材料
CN104017281A (zh) 一种船用高性能橡胶材料
JP2019172957A (ja) タイヤトレッド用ゴム組成物及びそれを含むタイヤ
CN104072830A (zh) 一种耐磨耐老化橡胶材料
KR101182208B1 (ko) 타이어 트레드용 고무 조성물 및 이를 이용하여 제조한 타이어
CN105419023A (zh) 一种工程车专用轮胎胎面胶
US2391742A (en) Synthetic rubber compositions
KR101170668B1 (ko) 양로 및 험로 겸용 트럭 타이어 트레드 고무 조성물 및 이를 이용하여 제조한 타이어
CN104693547A (zh) 一种耐油耐磨橡胶垫
CN104017282A (zh) 一种船用高强耐老化橡胶材料
CN104072839B (zh) 一种阻燃耐热橡胶材料
US20160272797A1 (en) Rubber Composition for Tire Treads and Tire Manufactured Using the Same
KR101917493B1 (ko) 타이어 트레드용 고무 조성물 및 이를 이용하여 제조한 타이어
KR102443664B1 (ko) 젖은 노면 제동 성능이 향상된 타이어 트레드 조성물 및 이를 이용하여 제조한 타이어
KR101787573B1 (ko) 타이어 트레드용 고무 조성물 및 이를 이용하여 제조한 타이어
JP5191687B2 (ja) タイヤトレッド用ゴム組成物
Hwang et al. Comparison of SBR/BR blend compound and ESBR copolymer having same butadiene contents

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20141001