parts
shitosan
wet strength
strength agent
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410062900.9A
Other languages
English (en)
Other versions
CN103882773B (zh
Inventor
邓强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Jia run new material Co., Ltd.
Original Assignee
Suzhou Heng Kang New Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Heng Kang New Material Co Ltd filed Critical Suzhou Heng Kang New Material Co Ltd
Priority to CN201410062900.9A priority Critical patent/CN103882773B/zh
Publication of CN103882773A publication Critical patent/CN103882773A/zh
Application granted granted Critical
Publication of CN103882773B publication Critical patent/CN103882773B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Paper (AREA)

Abstract

本发明涉及一种壳聚糖湿强剂及其制备方法,壳聚糖湿强剂由以下成分按照重量比组成:壳聚糖为6~7份、羟丙基甲基纤维素为3~6份、聚丙烯酸异丁酯为4~8份、十四烷基苯磺酸钠为2~5份、丁二醇为6~7份、柠檬酸为1~2份、去离子水为205~215份。壳聚糖湿强剂的制备工艺包括各种原料机械混合、机械搅拌等步骤。制备得到的壳聚糖湿强剂可以提高纸张的抗撕裂强度和抗张强度,提高了纸制品的抗撕裂和抗张的性能。

Description

一种壳聚糖湿强剂及其制备方法
技术领域
本发明涉及一种湿强剂及其制备方法,特别是涉及一种可以显著提高纸张的抗撕裂强度和抗张强度的壳聚糖湿强剂及其制备方法。
背景技术
常规的纸张在使用过程中,遇到外力时,会有撕裂的现象。纸张的撕裂影响着人们的正常使用。在通常情况下,纸张的抗撕裂性能和抗张强度都较低,由于这两个缺陷的存在,一定范围内制约了纸张的使用。
纸张的撕裂性能和抗张强度和很多方面有关。纸张的材料、制浆的工艺、造纸助剂的使用都会对纸张的抗撕裂性能和抗张强度有较大的作用。在这其中,造纸助剂也有较大的作用,作为造纸助剂的一种,湿强剂在这其中也发挥着重要作用。湿强剂类型的选择进而影响着纸张的使用性能。
发明内容
要解决的技术问题:常规的纸张由于其造纸助剂性能较差,制备得到的纸张的抗撕裂性能和抗张强度较差,制约了纸张的使用的问题。
技术方案:本发明公开了一种壳聚糖湿强剂及其制备方法,壳聚糖湿强剂由以下成分按照重量比组成:壳聚糖为6~7份、羟丙基甲基纤维素为3~6份、聚丙烯酸异丁酯为4~8份、十四烷基苯磺酸钠为2~5份、丁二醇为6~7份、柠檬酸为1~2份、去离子水为205~215份。
一种壳聚糖湿强剂的制备方法,制备方法包括如下步骤:(1)将温度设定为60℃,取去离子水为205~215份,向水中加入壳聚糖为6~7份、羟丙基甲基纤维素为3~6份、丁二醇为6~7份、柠檬酸为1~2份,将5种成分用涡轮搅拌器进行混合搅拌,搅拌均匀后为混合液;(2)搅拌均匀后向混合液中加入十四烷基苯磺酸钠为2~5份,再次进行涡轮搅拌,搅拌时间为20min;(3)再向混合液中均匀缓慢添加聚丙烯酸异丁酯为4~8份,添加的同时进行涡轮搅拌,搅拌均匀;(4)将得到的混合液装罐保存,制备得到壳聚糖湿强剂。
制备过程中加入的羟丙基甲基纤维素优选为6份。
制备过程中加入的壳聚糖优选为7份。
制备过程中加入的聚丙烯酸异丁酯优选为6~8份。
有益效果:制备得到壳聚糖湿强剂后,应用在造纸工艺中后,纸张撕裂指数从5.7mN·m2/g升高至13.2mN·m2/g至14.6mN·m2/g,显著提高了纸张的抗撕裂性能。制备得到的纸张的干强抗张强度提高较大,干强抗张强度由未添加前的29.5N·m/g提高至44.7至47.5N·m/g,扩大了纸张的应用领域。
具体实施方式
实施例1
一种壳聚糖湿强剂的制备方法,制备方法包括如下步骤:(1)将温度设定为60℃,取去离子水为205kg,向水中加入壳聚糖为6kg、羟丙基甲基纤维素为3kg、丁二醇为7kg、柠檬酸为2kg,将5种成分用涡轮搅拌器进行混合搅拌,搅拌均匀后为混合液;(2)搅拌均匀后向混合液中加入十四烷基苯磺酸钠为2kg,再次进行涡轮搅拌,搅拌时间为20min;(3)再向混合液中均匀缓慢添加聚丙烯酸异丁酯为6kg,添加的同时进行涡轮搅拌,搅拌均匀;(4)将得到的混合液装罐保存,制备得到壳聚糖湿强剂。
实施例2
一种壳聚糖湿强剂的制备方法,制备方法包括如下步骤:(1)将温度设定为60℃,取去离子水为210kg,向水中加入壳聚糖为7kg、羟丙基甲基纤维素为4kg、丁二醇为7kg、柠檬酸为1kg,将5种成分用涡轮搅拌器进行混合搅拌,搅拌均匀后为混合液;(2)搅拌均匀后向混合液中加入十四烷基苯磺酸钠为4kg,再次进行涡轮搅拌,搅拌时间为20min;(3)再向混合液中均匀缓慢添加聚丙烯酸异丁酯为8kg,添加的同时进行涡轮搅拌,搅拌均匀;(4)将得到的混合液装罐保存,制备得到壳聚糖湿强剂。
实施例3
一种壳聚糖湿强剂的制备方法,制备方法包括如下步骤:(1)将温度设定为60℃,取去离子水为215kg,向水中加入壳聚糖为6kg、羟丙基甲基纤维素为6kg、丁二醇为6kg、柠檬酸为2kg,将5种成分用涡轮搅拌器进行混合搅拌,搅拌均匀后为混合液;(2)搅拌均匀后向混合液中加入十四烷基苯磺酸钠为5kg,再次进行涡轮搅拌,搅拌时间为20min;(3)再向混合液中均匀缓慢添加聚丙烯酸异丁酯为4kg,添加的同时进行涡轮搅拌,搅拌均匀;(4)将得到的混合液装罐保存,制备得到壳聚糖湿强剂。
将质量浓度为7.5wt%的阔叶浆充分搅拌均匀,向阔叶浆料中分别加入实施例1、实施例2、实施例3制备得到的壳聚糖湿强剂,壳聚糖湿强剂添加量为纸张重量的0.7wt%,另外再进行对比试验,不加入本发明的湿强剂,加入湿强剂后搅拌均匀,再将纸张进行抄片,纸张定量为35g/m2,纸张干燥后熟化,熟化温度为85℃,熟化时间为13min,熟化后冷却至室温,室温下测定实施例1、实施例2、实施例3的纸张的撕裂指数和干强抗张强度。结果如下。
Figure 2014100629009100002DEST_PATH_IMAGE001
添加了本发明制备的湿强剂后,纸张的撕裂指数和干强抗张强度得到显著提升,进而提高了纸品的质量,扩大了纸品的使用领域。

Claims (5)

1.一种壳聚糖湿强剂,其特征在于壳聚糖湿强剂由以下成分按照重量比组成:壳聚糖为6~7份、羟丙基甲基纤维素为3~6份、聚丙烯酸异丁酯为4~8份、十四烷基苯磺酸钠为2~5份、丁二醇为6~7份、柠檬酸为1~2份、去离子水为205~215份。
2. 根据权利要求1所述的一种壳聚糖湿强剂的制备方法,其特征在于制备方法包括如下步骤:(1)将温度设定为60℃,取去离子水为205~215份,向水中加入壳聚糖为6~7份、羟丙基甲基纤维素为3~6份、丁二醇为6~7份、柠檬酸为1~2份,将5种成分用涡轮搅拌器进行混合搅拌,搅拌均匀后为混合液;(2)搅拌均匀后向混合液中加入十四烷基苯磺酸钠为2~5份,再次进行涡轮搅拌,搅拌时间为20min;(3)再向混合液中均匀缓慢添加聚丙烯酸异丁酯为4~8份,添加的同时进行涡轮搅拌,搅拌均匀;(4)将得到的混合液装罐保存,制备得到壳聚糖湿强剂。
3.根据权利要求2所述的一种壳聚糖湿强剂的制备方法,其特征在于制备过程中加入的羟丙基甲基纤维素为6份。
4.根据权利要求2所述的一种壳聚糖湿强剂的制备方法,其特征在于制备过程中加入的壳聚糖为7份。
5.根据权利要求2所述的一种壳聚糖湿强剂的制备方法,其特征在于制备过程中加入的聚丙烯酸异丁酯为6~8份。
CN201410062900.9A 2014-02-25 2014-02-25 一种壳聚糖湿强剂及其制备方法 Active CN103882773B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410062900.9A CN103882773B (zh) 2014-02-25 2014-02-25 一种壳聚糖湿强剂及其制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410062900.9A CN103882773B (zh) 2014-02-25 2014-02-25 一种壳聚糖湿强剂及其制备方法

Publications (2)

Publication Number Publication Date
CN103882773A true CN103882773A (zh) 2014-06-25
CN103882773B CN103882773B (zh) 2016-04-20

Family

ID=50951876

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410062900.9A Active CN103882773B (zh) 2014-02-25 2014-02-25 一种壳聚糖湿强剂及其制备方法

Country Status (1)

Country Link
CN (1) CN103882773B (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105839451A (zh) * 2015-11-04 2016-08-10 山东太阳生活用纸有限公司 造纸助剂、造纸方法及纸巾

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1582314A (zh) * 2001-11-02 2005-02-16 三洋化成工业株式会社 复合树脂粒子
CN102105544A (zh) * 2007-07-02 2011-06-22 格林百奥生态材料科技(上海)有限公司 用于纤维素材料的粘合及改性的聚合物组合物
WO2011109174A1 (en) * 2010-02-18 2011-09-09 Dow Corning Corporation Surface -modified hydrogels and hydrogel microparticles
CN102373649A (zh) * 2010-08-23 2012-03-14 昆山钞票纸业有限公司 纸的生产工艺及其产品

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1582314A (zh) * 2001-11-02 2005-02-16 三洋化成工业株式会社 复合树脂粒子
CN102105544A (zh) * 2007-07-02 2011-06-22 格林百奥生态材料科技(上海)有限公司 用于纤维素材料的粘合及改性的聚合物组合物
WO2011109174A1 (en) * 2010-02-18 2011-09-09 Dow Corning Corporation Surface -modified hydrogels and hydrogel microparticles
CN102373649A (zh) * 2010-08-23 2012-03-14 昆山钞票纸业有限公司 纸的生产工艺及其产品

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105839451A (zh) * 2015-11-04 2016-08-10 山东太阳生活用纸有限公司 造纸助剂、造纸方法及纸巾
WO2017075917A1 (zh) * 2015-11-04 2017-05-11 山东太阳生活用纸有限公司 造纸助剂、造纸方法及纸巾

Also Published As

Publication number Publication date
CN103882773B (zh) 2016-04-20

Similar Documents

Publication Publication Date Title
CN104119021B (zh) 高效减水剂
CN104119027B (zh) 缓凝减水剂
CN106905744B (zh) 一种抗裂型外墙用腻子粉
CN106947029A (zh) 一种高性能聚羧酸保坍剂及其制备方法
CN105348396B (zh) 一种环保型壁纸胶粉用改性淀粉及其制备方法
CN104119026A (zh) 混凝土复合减水剂
EP2911991A1 (en) Composition of cellulose ether and gluconate salts for use in cement containing skim coats
CN103466985A (zh) 一种石墨烯水泥增强剂
CN104119013B (zh) 葡萄糖基缓凝减水剂的制备方法
CN104119023A (zh) 缓凝高效减水剂
CN104212391A (zh) 环氧树脂-丙烯酸酯共聚胶黏剂配方及其制备工艺
CN103882773B (zh) 一种壳聚糖湿强剂及其制备方法
CN104478287B (zh) 一种多功能混凝土增效剂及其制备方法
CN105293991A (zh) 填料用改性剂及其填料的制备方法
CN104790265A (zh) 一种混合纤维壁纸及其制造方法
CN103924456A (zh) 一种活性印花糊料的生产工艺
CN104261773A (zh) 耐水性水泥基自流平材料
CN103866630B (zh) 一种黄原胶湿强剂及其制备方法
US8920557B2 (en) Additive for skim coat mortar and skim coat mortar composition containing the same
WO2013097263A1 (zh) 一种天然乳胶与二氧化硅浆液共混的方法
CN103588417A (zh) 一种木质素磺酸钠盐混凝土减水剂的改性剂
CN104387830A (zh) 一种建筑腻子粉及其制备方法
CN104261717B (zh) 一种混凝土防冻剂
CN105110701B (zh) 一种适用于瓷砖胶粘剂的纤维素醚组合物
CN103483764B (zh) 一种耐酸碱红色母粒

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C41 Transfer of patent application or patent right or utility model
CB03 Change of inventor or designer information

Inventor after: Qiu Caijun

Inventor before: Deng Qiang

COR Change of bibliographic data
TA01 Transfer of patent application right

Effective date of registration: 20160321

Address after: 750000, the Ningxia Hui Autonomous Region, Yinchuan, Xingqing District, Xinhua East Street, Lishui homes, No. 42 business building, room 7

Applicant after: The Ningxia abundant mechanical Science and Technology Ltd. of letter

Address before: Baoan Xushuguan Town Road Suzhou City, Jiangsu province 215151 No. 196

Applicant before: Suzhou Heng Kang new material Co., Ltd

C14 Grant of patent or utility model
GR01 Patent grant
TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20181105

Address after: 313009 Jinma East Road, Ma Lok village, Nanxun Economic Development Zone, Huzhou, Zhejiang, 5

Patentee after: Huzhou Liming hardware Electromechanical Equipment Co. Ltd.

Address before: 750000 the Ningxia Hui Autonomous Region Yinchuan Xingqing District Xinhua East Street Lishui home 42 commercial and residential building 7

Patentee before: The Ningxia abundant mechanical Science and Technology Ltd. of letter

TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20191203

Address after: Room 512a, building 1, No. 98, Yingchun East Road, hailing Industrial Park, Taizhou City, Jiangsu Province

Patentee after: Jiangsu Wanglong Machinery Co., Ltd

Address before: 313009 No. 5 Jinma East Road, Mayao Village, Nanxun Economic Development Zone, Huzhou City, Zhejiang Province

Patentee before: Huzhou Liming hardware Electromechanical Equipment Co. Ltd.

TR01 Transfer of patent right

Effective date of registration: 20191226

Address after: 314000 NO.311, Washan Road, Zhapu Town, Jiaxing Port Area, Huzhou City, Zhejiang Province

Patentee after: Zhejiang Jia run new material Co., Ltd.

Address before: Room 512a, building 1, No. 98, Yingchun East Road, hailing Industrial Park, Taizhou City, Jiangsu Province

Patentee before: Jiangsu Wanglong Machinery Co., Ltd

TR01 Transfer of patent right