CN103736650A - 一种特氟龙喷涂工艺 - Google Patents

一种特氟龙喷涂工艺 Download PDF

Info

Publication number
CN103736650A
CN103736650A CN201410029031.XA CN201410029031A CN103736650A CN 103736650 A CN103736650 A CN 103736650A CN 201410029031 A CN201410029031 A CN 201410029031A CN 103736650 A CN103736650 A CN 103736650A
Authority
CN
China
Prior art keywords
teflon
spraying
coating process
described step
spraying coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410029031.XA
Other languages
English (en)
Inventor
陆华平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou New District Teflon Plastic Products Factory
Original Assignee
Suzhou New District Teflon Plastic Products Factory
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou New District Teflon Plastic Products Factory filed Critical Suzhou New District Teflon Plastic Products Factory
Priority to CN201410029031.XA priority Critical patent/CN103736650A/zh
Publication of CN103736650A publication Critical patent/CN103736650A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种特氟龙喷涂工艺,包含以下操作步骤,首先用机溶剂进行30~50min的侵泡并进行加热,去除待涂物品表面的油脂类杂质;然后用清水冲洗物品表面的有机溶剂,采用喷砂处理的机械方式进行清洁物品表面剩余杂质,并使其表面毛糙;毛糙步骤之后进行底漆的喷涂;最后用进行特氟龙层的喷涂。通过上述方式,本发明能够提供一种特氟龙涂料的喷涂工艺,操作步骤简单,且喷涂效果佳。

Description

一种特氟龙喷涂工艺
技术领域
本发明涉及一种特氟龙制品的喷涂方法,特别是涉及一种特氟龙喷涂工艺。
背景技术
铁氟龙涂料是一种高性能涂料,通过结合耐热性、化学惰性和优异的绝缘稳定性及低摩擦性使其具有其他涂料无法抗衡的综合优势。它的灵活性使得它能用于几乎所有形状和大小的产品上。因此本发明提供一种能够用于喷涂产品表面的特氟龙制品的制作工艺。
发明内容
本发明主要解决的技术问题是提供一种特氟龙喷涂工艺,能够提供一种特氟龙涂料的喷涂工艺,操作步骤简单,且喷涂效果佳。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种特氟龙喷涂工艺,包括以下操作步骤:
(1)用机溶剂进行30~50min的侵泡并进行加热,去除待涂物品表面的油脂类杂质;
(2)用清水冲洗物品表面的有机溶剂;
(3)采用喷砂处理的机械方式进行清洁物品表面剩余杂质,并使其表面毛糙;
(4)毛糙步骤之后进行底漆的喷涂;
(5)最后用进行特氟龙层的喷涂。
在本发明一个较佳实施例中,所述步骤(1)中加热的温度为60~100℃。
在本发明一个较佳实施例中,所述步骤(5)中特氟龙层的厚度为0.1~0.3um。
在本发明一个较佳实施例中,所述步骤(4)中底漆的厚度为0.1~1um。
在本发明一个较佳实施例中,所述步骤(2)中清水的温度为80~95℃。
本发明的有益效果是:本发明提供一种特氟龙涂料的喷涂工艺,操作步骤简单,且喷涂效果佳。
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅是本发明的一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其它实施例,都属于本发明保护的范围。
本发明实施例提供如下技术方案。
在一个实施例中,一种特氟龙喷涂工艺,包括以下操作步骤:
(1)用机溶剂进行30~50min的侵泡并进行加热,去除待涂物品表面的油脂类杂质;
(2)用清水冲洗物品表面的有机溶剂;
(3)采用喷砂处理的机械方式进行清洁物品表面剩余杂质,并使其表面毛糙;
(4)毛糙步骤之后进行底漆的喷涂;
(5)最后用进行特氟龙层的喷涂。
区别于现有技术,在一个实施例中,优选地,所述步骤(1)中加热的温度为60~100℃。
优选地,所述步骤(5)中特氟龙层的厚度为0.1~0.3um。
优选地,所述步骤(4)中底漆的厚度为0.1~1um。
优选地,所述步骤(2)中清水的温度为80~95℃。
本发明能够提供一种特氟龙涂料的喷涂工艺,操作步骤简单,且喷涂效果佳。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其它相关的技术领域,均同理包括在本发明的专利保护范围内。

Claims (5)

1.一种特氟龙喷涂工艺,其特征在于:包含以下操作步骤,
(1)用机溶剂进行30~50min的侵泡并进行加热,去除待涂物品表面的油脂类杂质;
(2)用清水冲洗物品表面的有机溶剂;
(3)采用喷砂处理的机械方式进行清洁物品表面剩余杂质,并使其表面毛糙;
(4)毛糙步骤之后进行底漆的喷涂;
(5)最后用进行特氟龙层的喷涂。
2.根据权利要求1所述的一种特氟龙喷涂工艺,其特征在于:所述步骤(1)中加热的温度为60~100℃。
3.根据权利要求1所述的一种特氟龙喷涂工艺,其特征在于:所述步骤(2)中清水的温度为80~95℃。
4.根据权利要求1所述的一种特氟龙喷涂工艺,其特征在于:所述步骤(4)中底漆的厚度为0.1~1um。
5.根据权利要求1所述的一种特氟龙喷涂工艺,其特征在于:所述步骤(5)中特氟龙层的厚度为0.1~0.3um。
CN201410029031.XA 2014-01-22 2014-01-22 一种特氟龙喷涂工艺 Pending CN103736650A (zh)