CN103666175B - 一种高环保离型涂布材料及其制备方法 - Google Patents

一种高环保离型涂布材料及其制备方法 Download PDF

Info

Publication number
CN103666175B
CN103666175B CN201210330924.9A CN201210330924A CN103666175B CN 103666175 B CN103666175 B CN 103666175B CN 201210330924 A CN201210330924 A CN 201210330924A CN 103666175 B CN103666175 B CN 103666175B
Authority
CN
China
Prior art keywords
coating material
release coating
environmental protection
preparation
consumption
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210330924.9A
Other languages
English (en)
Other versions
CN103666175A (zh
Inventor
吕新民
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Yongguan Zhongcheng New Material Science And Technology (group) Ltd By Share Ltd
Original Assignee
Shanghai Yongguan Zhongcheng New Material Science And Technology (group) Ltd By Share Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Yongguan Zhongcheng New Material Science And Technology (group) Ltd By Share Ltd filed Critical Shanghai Yongguan Zhongcheng New Material Science And Technology (group) Ltd By Share Ltd
Priority to CN201210330924.9A priority Critical patent/CN103666175B/zh
Publication of CN103666175A publication Critical patent/CN103666175A/zh
Application granted granted Critical
Publication of CN103666175B publication Critical patent/CN103666175B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种高环保离型涂布材料及其制备方法。该离型涂布材料的原料配方由以下组分组成:丙烯腈-丙烯酸丁酯共聚物5-9%,氢氧化铵0.5-1.5%和纯净水90-94%,其中,各百分比均为质量百分比。该离型涂布材料的制备方法包括下列步骤:将上述环保离型涂布材料的各组分混合,密闭搅拌即可。本发明的这种涂布材料形成的高环保离型涂布材料成本低,安全环保,涂布均匀,离型效果好。

Description

一种高环保离型涂布材料及其制备方法
技术领域
本发明涉及一种高环保离型涂布材料,尤其涉及该离型涂布材料的原料配方及其制备方法。
背景技术
离型涂布材料在使用时与120号汽油、甲苯等溶剂充分混合后,利用涂布设备将其均匀涂在产品的涂胶背面基材上,使产品在涂胶后,使用时能将该产品顺利的解卷,才能正常的张贴使用。
离型涂布材料用于生产布基、薄膜、纸张和铝箔等基材,须用合理的溶剂稀释至合理的浓度涂覆于基材上,涂覆后需要用热量蒸发基材表面的油分,使离型剂得到有机的固化。
离型涂布材料是影响胶带品质的重要因素之一,同时随着人们环保意识的增强,使用环保型的离型涂布材料更是人类努力的方向。
现有技术中用的是溶剂型的非硅离型涂布材料,它是由氨基甲酸酯、聚乙烯醇、氨基酯、甲苯组分组成,具体配比为:氨基甲酸酯0.5-0.7%、聚乙烯醇0.075-0.125%、氨基酯0.075-0.125%、甲苯99.1-99.3%。
但这种溶剂型的非硅离型涂布材料存在诸多的缺陷:
第一:利用120号汽油、甲苯等溶剂作为稀释剂,基材的表面存有毒性的残留物,长期使用容易使人致癌:且溶剂均为石油化工材料,居高的成本,给公司产品销售带来巨大的压力。
第二:溶剂是易燃易爆品,在涂布的过程极易产生静电导致大型火灾,给人身安全造成威胁,并且中挥发大量的有毒气体排放到空气中,严重的污染环境。
第三,由于溶剂型的非硅离型涂布材料的分子量分布不够活跃,硅溶液易沉淀、不均匀,导致涂硅更不均匀,经常使母卷复卷时无法解卷,造成大量浪费;因为涂硅不均匀,导致产品解卷出现无法解卷的而被抛弃,造成产品的严重浪费。
第四,溶剂型的非硅离型涂布材料价格高昂,其原料十八氨基甲酸酯每千克达人民币捌佰多元,且分子量分布不够活跃,要保证产品的品质的前提下,涂布量须在每平方5g以上,更是使产品失去了竞争力。
发明内容
本发明所要解决的技术问题是为了克服现有的离型涂布材料高成本、高污染、涂布不均匀的缺陷,而提供了一种高环保离型涂布材料及其制备方法。本发明的这种涂布材料形成的高环保离型涂布材料成本低,安全环保,涂布均匀,离型效果好。
本发明提供了一种环保离型涂布材料,该原料由以下组分组成:丙烯腈-丙烯酸丁酯共聚物5-9%,氢氧化铵0.5-1.5%和水90-94%,其中,各百分比均为质量百分比。
其中,所述的丙烯腈-丙烯酸丁酯共聚物按下列步骤制得:在引发剂的作用下,丙烯腈和丙烯酸丁酯在含有乳化剂的水中进行乳液共聚反应,即可。
其中,按照重量份数计,所述的丙烯腈的用量为4-6份,所述的丙烯酸丁酯的用量为1-3份,所述的乳化剂的用量为0.2-0.5份,所述的引发剂的用量为0.3-0.8份,所述的水的用量为40-45份。
其中,所述的乳化剂可为本领域常规使用的乳化剂,较佳的为十二烷基硫酸钠和/或十二烷基二苯醚二磺酸钠。
其中,所述的引发剂可为本领域常规使用的引发剂,较佳的为过硫酸铵。
其中,所述的水可为本领域常规使用的水,较佳的为去离子水。
其中,所述的乳液共聚的温度较佳的75-83℃,更佳的为80℃。
其中,所述的乳液共聚的时间较佳的为0.5-1小时。
其中,所述的丙烯腈链段与丙烯酸丁酯链段的比值为70:30。
本发明还提供一种环保离型涂布材料的制备方法,其包括以下步骤:将所述的环保离型涂布材料的各组分混合,密闭搅拌即可。
所述的搅拌的转速较佳的为75-90转/分钟。
所述的搅拌的时间较佳的为4-6分钟。
在符合本领域常识的基础上,上述各优选条件,可任意组合,即得本发明各较佳实例。
本发明所用试剂和原料均市售可得。
本发明的积极进步效果在于:
与纯净水的相容性好;溶解后易分散,不产生沉淀;涂布均匀,离型效果好;使用时更安全、更环保。
具体实施方式
下面通过实施例的方式进一步说明本发明,但并不因此将本发明限制在所述的实施例范围之中。下列实施例中未注明具体条件的实验方法,按照常规方法和条件。
实施例
将42kg去离子水加入反应釜中,再加入乳化剂十二烷基硫酸钠0.3kg,以转速为90转/分钟的速度搅拌20分钟,通入氮气置换釜内的空气,加入引发剂过硫酸铵0.5kg,然后加入5kg丙烯腈和2kg丙烯酸丁酯的混合物,混合均匀后开始升温,温度控制在80℃,维持反应1小时,得到丙烯腈-丙烯酸丁酯共聚物。
再将1kg氢氧化铵和50kg去离子水加入上述反应釜中,密闭,启动搅拌开关,5分钟后,搅拌均匀即可得到高环保离型涂布材料。

Claims (4)

1.一种环保离型涂布材料,其特征在于,其原料配方由以下组分组成:丙烯腈-丙烯酸丁酯共聚物5-9%,氢氧化铵0.5-1.5%和纯净水90-94%,各百分比均为质量百分比;
所述的丙烯腈-丙烯酸丁酯共聚物按下列步骤制得:在引发剂的作用下,丙烯腈和丙烯酸丁酯在含有乳化剂的水中进行乳液共聚反应,即可;
所述的丙烯腈的用量为4-6份,所述的丙烯酸丁酯的用量为1-3份,所述的乳化剂的用量为0.2-0.5份,所述的引发剂的用量为0.3-0.8份,所述的水的用量为40-45份;所述的份为质量份;
所述的乳化剂为十二烷基硫酸钠,所述的引发剂为过硫酸铵;
所述的乳液共聚反应的温度为75-83℃,所述的乳液共聚反应的时间为0.5-1小时。
2.一种如权利要求1所述的环保离型涂布材料的制备方法,其特征在于,其包括以下步骤:根据所述的环保离型涂布材料的原料配方,将各组分混合,密闭搅拌即可。
3.如权利要求2所述的环保离型涂布材料的制备方法,其特征在于,所述的搅拌的转速为75-90转/分钟。
4.如权利要求2所述的环保离型涂布材料的制备方法,其特征在于,所述的搅拌的时间为4-6分钟。
CN201210330924.9A 2012-09-07 2012-09-07 一种高环保离型涂布材料及其制备方法 Active CN103666175B (zh)