CN103409076B - 金属粘膏及其制备方法 - Google Patents

金属粘膏及其制备方法 Download PDF

Info

Publication number
CN103409076B
CN103409076B CN201310310043.5A CN201310310043A CN103409076B CN 103409076 B CN103409076 B CN 103409076B CN 201310310043 A CN201310310043 A CN 201310310043A CN 103409076 B CN103409076 B CN 103409076B
Authority
CN
China
Prior art keywords
parts
metal paste
adhesive
paste adhesive
metal
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201310310043.5A
Other languages
English (en)
Other versions
CN103409076A (zh
Inventor
徐志坚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wujiang Longshuo Metal Products Co., Ltd.
Original Assignee
WUJIANG LONGSHUO METAL PRODUCTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUJIANG LONGSHUO METAL PRODUCTS CO Ltd filed Critical WUJIANG LONGSHUO METAL PRODUCTS CO Ltd
Priority to CN201310310043.5A priority Critical patent/CN103409076B/zh
Publication of CN103409076A publication Critical patent/CN103409076A/zh
Application granted granted Critical
Publication of CN103409076B publication Critical patent/CN103409076B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种金属粘膏及其制备方法。金属粘膏包括以下重量份计的原料:氧化锌10-20份、环氧乙烷1-10份、二氯甲烷2-6份、磷酸二钠10-20份、聚氧乙烯壬基酚醚20-30份、正丁醇10-15份、二氧化硅10-11份、醋酸异戊酯2-8份。本发明的金属粘膏可以将金属之间牢牢的连接在一起,粘结力达到168N/cm2以上,而普通的胶水粘结金属的粘接力仅为26N/cm2,远远小于本发明的粘结力,具有良好的粘接金属的能力。在高温条件下,加热后本发明的粘膏的粘结力为63-70N/cm2,而普通的胶水在加热高温条件下,几乎没有粘结作用,因此,本发明还具有稳定的耐热性能。

Description

金属粘膏及其制备方法
技术领域
本发明涉及一种粘膏,尤其涉及一种金属粘膏及其制备方法。
背景技术
胶水就是能够粘接二个物体的物质。胶水不是独立存在的,它必须涂在二个物体之间才能发挥粘接作用。胶水中的化学成分,在水性环境里。胶水中的高分子体(白胶中的醋酸乙烯是石油衍生物的一种)都是呈圆形粒子,一般粒子的半径是在0.5~5μm之间。物体的粘接,就是靠胶水中的高分子体间的拉力来实现的。在胶水中,水就是中高分子体的载体,水载着高分子体慢慢地浸入到物体的组织内。当胶水中的水分消失后,胶水中的高分子体就依靠相互间的拉力,将两个物体紧紧的结合在一起。在胶水的使用中,涂胶量过多就会使胶水中的高分子体相互拥挤在一起;高分子体间产生不了很好的拉力。高分子体相互拥挤,从而形成不了相互间最强的吸引力。同时,高分子体间的水分也不容易挥发掉。但是金属之间的粘接通过胶水链接,易剥落,稳定性低,尤其是在高温条件下胶水融化失效。
发明内容
针对现有技术的不足,本发明提供了一种稳定性好、粘接能力强的金属粘膏及其制备方法。
本发明采用以下技术方案解决技术问题:
一种金属粘膏,包括以下重量份计的原料:氧化锌10份、环氧乙烷1份、二氯甲烷2份、磷酸二钠10份、聚氧乙烯壬基酚醚20份、正丁醇10份、二氧化硅10份、醋酸异戊酯2份。
上述金属粘膏的制备方法,包括以下步骤:将氧化锌、环氧乙烷、二氯甲烷、磷酸二钠、聚氧乙烯壬基酚醚、正丁醇、二氧化硅、醋酸异戊酯混匀,加热到90℃保持10min,冷凝即可。
本发明的有益效果是,本发明的金属粘膏可以将金属之间牢牢的连接在一起,粘结力达到168N/cm2以上,而普通的胶水粘结金属的粘接力仅为26N/cm2,远远小于本发明的粘结力,因此,具有良好的粘接金属的能力。在高温条件下,加热后本发明制备的粘膏的粘结力为63-70N/cm2,而普通的胶水在加热高温条件下,几乎没有粘结作用,因此,本发明还具有稳定的耐热性能。
具体实施方式
下面通过具体实施例对本发明作进一步详细介绍。
实施例1
一种金属粘膏,包括以下重量份计的原料制成:氧化锌10份、环氧乙烷1份、二氯甲烷2份、磷酸二钠10份、聚氧乙烯壬基酚醚20份、正丁醇10份、二氧化硅10份、醋酸异戊酯2份。
上述金属粘膏的制备方法包括以下步骤:将氧化锌、环氧乙烷、二氯甲烷、磷酸二钠、聚氧乙烯壬基酚醚、正丁醇、二氧化硅、醋酸异戊酯混匀,加热到90℃保持10min,冷凝即可。
实施例2
一种金属粘膏,包括以下重量份计的原料制成:氧化锌20份、环氧乙烷10份、二氯甲烷6份、磷酸二钠20份、聚氧乙烯壬基酚醚30份、正丁醇15份、二氧化硅11份、醋酸异戊酯8份。
上述金属粘膏的制备方法包括以下步骤:将氧化锌、环氧乙烷、二氯甲烷、磷酸二钠、聚氧乙烯壬基酚醚、正丁醇、二氧化硅、醋酸异戊酯混匀,加热到100℃保持15min,冷凝即可。
实施例3
一种金属粘膏,包括以下重量份计的原料制成:氧化锌15份、环氧乙烷5份、二氯甲烷4份、磷酸二钠15份、聚氧乙烯壬基酚醚25份、正丁醇13份、二氧化硅10.5份、醋酸异戊酯5份。
上述金属粘膏的制备方法包括以下步骤:将氧化锌、环氧乙烷、二氯甲烷、磷酸二钠、聚氧乙烯壬基酚醚、正丁醇、二氧化硅、醋酸异戊酯混匀,加热到95℃保持13min,冷凝即可。
下面通过试验测试本发明的性能:
试验:选择在两块厚度均为2mm的薄铁片,在其中一块铁片上涂覆本发明的粘膏,然后将两块铁片压紧粘合10min,测试粘接力。
对比:选择在两块厚度均为2mm的薄铁片,在其中一块铁片上涂覆普通胶水,然后将两块铁片压紧粘合10min,测试粘接力。
由上可知,本发明的粘膏可以将金属之间牢牢的连接在一起,粘结力达到168N/cm2以上,而普通的胶水粘结金属的粘接力仅为26N/cm2,远远小于本发明的粘结力,因此,本发明具有良好的粘接金属的能力。在高温条件下,加热后本发明的粘膏的粘结力为63-70N/cm2,而普通的胶水在加热高温条件下,几乎没有粘结作用,因此,本发明还具有稳定的耐热性能。
另外,本发明不限于上述实施方式,只要在不超出本发明的范围内,可以采取各种方式实施本发明。

Claims (2)

1.一种金属粘膏,其特征在于包括以下重量份计的原料:氧化锌10份、环氧乙烷1份、二氯甲烷2份、磷酸二钠10份、聚氧乙烯壬基酚醚20份、正丁醇10份、二氧化硅10份、醋酸异戊酯2份。
2.权利要求1所述的金属粘膏的制备方法,其特征在于包括以下步骤:将氧化锌、环氧乙烷、二氯甲烷、磷酸二钠、聚氧乙烯壬基酚醚、正丁醇、二氧化硅、醋酸异戊酯混匀,加热到90℃保持10min,冷凝即可。
CN201310310043.5A 2013-07-23 2013-07-23 金属粘膏及其制备方法 Expired - Fee Related CN103409076B (zh)