- CN103171817A CN103171817A CN2013101232177A CN201310123217A CN103171817A CN 103171817 A CN103171817 A CN 103171817A CN 2013101232177 A CN2013101232177 A CN 2013101232177A CN 201310123217 A CN201310123217 A CN 201310123217A CN 103171817 A CN103171817 A CN 103171817A
- Authority
- CN
- China
- Prior art keywords
- film
- bonding
- temperature
- printing
- flexo
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Bag Frames (AREA)
- Wrappers (AREA)
Abstract
柔印耐高温食品塑料包装袋的制作方法,生产工艺是尼龙膜柔版印刷,双膜粘合,烘烤固化,制袋机制袋。先用柔版印刷机和水性油墨在尼龙膜里面印刷图文;再用聚氨酯胶水加乙酯搅拌均匀后上胶至尼龙膜,将尼龙膜与耐高温蒸煮膜粘合复膜;复合膜经50~75℃恒温烘烤熟化24~55小时,使复合膜通过恒温熟化将胶水固化;最后用三边封制袋机经4Pa高压210℃‐230℃热封制成食品包装袋。这种食品包装袋安全无毒,具有良好的耐高温蒸煮性和阻隔性及阻湿性等特点,可保证食品包装抽真空耐135℃30min高温杀菌的要求,从而保证食品安全。
Description
技术领城
本发明涉及柔印耐高温食品塑料包装袋的制作方法。
背景技术
现在我国彩印塑料包装食品袋,普遍使用的是聚氨酯复合里印油墨的凹版印刷方式,印刷油墨需要用甲苯、乙酯、异丙醇等溶剂来稀释油墨的粘度,以保证印刷质量效果。但溶剂中含有苯和各种重金属物质,大部分在印刷过程中迅速挥发出来污染空气,影响车间生产员工的身体健康;同时,食品包装印刷中遗留的小量溶剂,在较短时间内慢慢渗透到包装袋内的食品中,从而影响消费者的身体健康。目前世界上所有印刷方式中唯一经美国食品药品协会认可的无毒油墨是柔印水墨。因而,柔版印刷又被称之为绿色印刷,被广泛用于不耐高温的食品和药品包装印刷,这是其他印刷方式可望而不可及的。但柔版印刷应用于需要耐高温的食品包装袋目前未见报导。
发明内容
本发明要解决的技术问题是:提供一种柔印耐高温食品塑料包装袋的印制方法,实现食品塑料彩印包装袋生产安全无毒,同时食品包装袋能耐高温。
本发明的技术方案是:柔印耐高温食品塑料包装袋由尼龙膜(BOPA)与耐高温蒸煮膜(RCPP)复合而成。生产工艺是尼龙膜柔版印刷,双膜粘合,烘烤固化,制袋机制袋。
a、柔版印刷:用柔版印刷机和水性油墨在尼龙膜里面印刷图文;
b、双膜粘合:将柔印后的尼龙膜与耐高温蒸煮膜通过复合机粘合,先用聚氨酯胶水加乙酯按重量比1:1.1~1.3搅拌均匀后上胶至柔印后的尼龙膜,再将两膜粘合;
c、烘烤固化:将粘合膜放入专用烘房,经过50~75℃恒温烘烤熟化24~55小时,使粘合胶水由液体熟化成固体,双层粘合膜形成固化的复合膜。
最后通过三边封制袋机经4Pa高压210℃‐230℃热封制成包装袋,可耐高温135℃30min蒸煮杀菌。
尼龙膜厚度1.5丝米;耐高温蒸煮膜选用延流薄膜,其厚度7~9丝米。
尼龙膜与耐高温蒸煮膜在温度55~75℃的烘道内先粘合,残留溶剂通过烘道内的空气对流排出烘道外。粘合膜经过55‐75℃恒温烘烤熟化24‐36小时,或50‐65℃恒温烘烤45‐55小时固化成复合膜。
本发明的积极效果在于:这种食品塑料包装袋生产过程安全无毒,有利于生产工人身体健康,同时具有良好的耐高温蒸煮性和阻隔性及阻湿性等特点,可保证食品包装抽真空耐135℃30min高温杀菌的要求,从而保证食品安全。
具体实施方式
1、图文设计:根据客户的要求做好图文设计,图文尽量简单明了,有别于凹版印刷的“浓妆艳抹”;
2、柔版印刷:将在专业厂家做好的印刷版辊,利用柔版印刷机和水性油墨在尼龙膜里面印刷图文;
3、双膜粘合:将柔印后的尼龙膜通过专用复合机与耐高温蒸煮膜用胶水粘合,原料用量:尼龙膜18‐33%,油墨与胶水5‐10%,耐高温蒸煮膜60‐75%。尼龙膜厚度1.5C(丝米);耐高温蒸煮膜厚度7‐9C(丝米);先将柔印后的尼龙膜送入复合工序,用聚氨酯胶水加乙酯按重量比1:1.1~1.3搅拌均匀后上胶至柔印后的尼龙膜,再将两膜粘合。粘合膜通过烘道加热,烘道温度55‐75℃。复合机设有一个进风口,一个排风口,使空气在烘道内对流,通过烘道内空气对流将残留溶剂排出烘道外;
4、烘烤固化:将复合薄膜放入专用烘房,经过55‐75℃恒温烘烤熟化24‐36小时,或50‐65℃恒温烘烤45‐55小时,使粘合胶水由液体熟化成固体,将两层或两层以上的薄膜完全复合成一体;
5、制袋机制袋:用三边封制袋机经4Pa高压210℃‐230℃热封制成包装袋。
本发明虽然以较佳实例揭露如上,但并非限定本发明,凡与本发明功能相近似的改进,皆被本发明申请所涵盖。
Claims (4)
1.柔印耐高温食品塑料包装袋的制作方法,包括尼龙膜印刷,制袋机制袋,其特征在于:柔版印刷,双膜粘合,烘烤固化工艺;
a、柔版印刷:用柔版印刷机和水性油墨在尼龙膜里面印刷图文;
b、双膜粘合:将柔印后的尼龙膜与耐高温蒸煮膜通过复合机粘合,先用聚氨酯胶水加乙酯按重量比1:1.1~1.3搅拌均匀后上胶至柔印后的尼龙膜,再将两膜粘合;
c、烘烤固化:将粘合膜放入专用烘房,经过50~75℃恒温烘烤熟化24~55小时,使粘合胶水由液体熟化成固体,双层粘合膜形成固化的复合膜。
2.根据权利要求1所述的柔印耐高温食品塑料包装袋的制作方法,其特征是:材料选择尼龙膜厚度1.5C;耐高温蒸煮膜选用延流薄膜,其厚度7~9C。
3.根据权利要求1所述的柔印耐高温食品塑料包装袋的制作方法,其特征是:尼龙膜与耐高温蒸煮膜在温度55~75℃的烘道内先粘合,残留胶水通过烘道内的空气对流排出烘道外。
4.根据权利要求1所述的柔印耐高温食品塑料包装袋的制作方法,其特征是:粘合膜经过55~75℃恒温烘烤24~36小时,或50~65℃恒温烘烤45~55小时。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2013101232177A CN103171817A (zh) | 2013-04-10 | 2013-04-10 | 柔印耐高温食品塑料包装袋的制作方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2013101232177A CN103171817A (zh) | 2013-04-10 | 2013-04-10 | 柔印耐高温食品塑料包装袋的制作方法 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN103171817A true CN103171817A (zh) | 2013-06-26 |
Family
ID=48632112
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN2013101232177A Pending CN103171817A (zh) | 2013-04-10 | 2013-04-10 | 柔印耐高温食品塑料包装袋的制作方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN103171817A (zh) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN105109220A (zh) * | 2015-09-15 | 2015-12-02 | 永新股份(黄山)包装有限公司 | 软包装防伪柔印工艺 |
CN109591413A (zh) * | 2018-11-12 | 2019-04-09 | 江阴升辉包装材料有限公司 | 一种复合彩色片材及其制备方法与应用 |
CN112389842A (zh) * | 2020-11-30 | 2021-02-23 | 重庆鼎盛印务股份有限公司 | 食品包装用塑料袋及其生产方法 |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US20090022434A1 (en) * | 2005-02-07 | 2009-01-22 | Eisuke Chiba | Packaging bag and drying agent with moisture absorption indicator function |
CN101837855A (zh) * | 2010-01-31 | 2010-09-22 | 赵秀雄 | 食品真空蒸煮包装袋的制作方法 |
-
2013
- 2013-04-10 CN CN2013101232177A patent/CN103171817A/zh active Pending
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US20090022434A1 (en) * | 2005-02-07 | 2009-01-22 | Eisuke Chiba | Packaging bag and drying agent with moisture absorption indicator function |
CN101837855A (zh) * | 2010-01-31 | 2010-09-22 | 赵秀雄 | 食品真空蒸煮包装袋的制作方法 |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN105109220A (zh) * | 2015-09-15 | 2015-12-02 | 永新股份(黄山)包装有限公司 | 软包装防伪柔印工艺 |
CN109591413A (zh) * | 2018-11-12 | 2019-04-09 | 江阴升辉包装材料有限公司 | 一种复合彩色片材及其制备方法与应用 |
CN112389842A (zh) * | 2020-11-30 | 2021-02-23 | 重庆鼎盛印务股份有限公司 | 食品包装用塑料袋及其生产方法 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN103171817A (zh) | 柔印耐高温食品塑料包装袋的制作方法 | |
CN101837855A (zh) | 食品真空蒸煮包装袋的制作方法 | |
CN104859326A (zh) | 一种食品用软包装的制备工艺 | |
CN106461469A (zh) | 显示装置 | |
CN106003963B (zh) | 一种不沾奶热封口膜及其制备方法 | |
CN102303434A (zh) | 耐拉伸高阻隔耐蒸煮的复合包装膜 | |
CN109263330A (zh) | 一种可热转印的模具硅胶转印标的制备方法 | |
CN105666951A (zh) | 药品包装袋的生产方法 | |
CN104369559A (zh) | 一种食品包装纸印刷方法 | |
CN103057236A (zh) | 一种彩印高温蒸煮袋的制备方法 | |
CN107901522A (zh) | 一种纸铝塑复合膜的生产方法 | |
CN101407264A (zh) | 一种定位激光防伪复合膜及其制造方法 | |
CN104118182A (zh) | 一种冷饮包装用纸塑复合膜及其制造方法 | |
CN104972725A (zh) | 耐拉伸耐蒸煮高阻隔复合包装膜 | |
CN202124180U (zh) | 食品保鲜包装袋 | |
CN208701417U (zh) | 一种水基涂层的复合铝箔纸 | |
CN108384461A (zh) | 一种无底纸不干胶的制备方法 | |
CN106188586B (zh) | 一种高强度薄膜的制备工艺 | |
CN104844897A (zh) | 一种耐热包装用蒸煮膜 | |
CN102785836A (zh) | 一种抗紫外线透明食品包装膜及其制备方法 | |
CN201817432U (zh) | 广告喷绘热裱膜 | |
CN102268846A (zh) | 一种食品包装纸的制作工艺 | |
CN110370739A (zh) | 一种贴体包装膜及其制备方法 | |
CN107059468A (zh) | 一种热塑性保润涂布材料及其制备方法 | |
CN207389931U (zh) | 链式脱氧剂用自动化作业包装袋 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
C02 | Deemed withdrawal of patent application after publication (patent law 2001) | ||
WD01 | Invention patent application deemed withdrawn after publication |
Application publication date: 20130626 |