CN102950847B - 用于软硬结合板的两面性粘结片及其制作方法 - Google Patents

用于软硬结合板的两面性粘结片及其制作方法 Download PDF

Info

Publication number
CN102950847B
CN102950847B CN201210452502.9A CN201210452502A CN102950847B CN 102950847 B CN102950847 B CN 102950847B CN 201210452502 A CN201210452502 A CN 201210452502A CN 102950847 B CN102950847 B CN 102950847B
Authority
CN
China
Prior art keywords
bonding sheet
prepreg
rigid flex
glass resin
dual character
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210452502.9A
Other languages
English (en)
Other versions
CN102950847A (zh
Inventor
俞宜
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangxi Zhangda Circuit Technology Co. Ltd.
Original Assignee
CHANGZHOU ZHANHUA ROBOT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGZHOU ZHANHUA ROBOT Co Ltd filed Critical CHANGZHOU ZHANHUA ROBOT Co Ltd
Priority to CN201210452502.9A priority Critical patent/CN102950847B/zh
Publication of CN102950847A publication Critical patent/CN102950847A/zh
Application granted granted Critical
Publication of CN102950847B publication Critical patent/CN102950847B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种用于软硬结合板的两面性粘结片及其制作方法,包括:该两面性粘结片是采用两种粘结片复合在一起而制成,所述两种粘结片分别为玻璃树脂粘结片和半固化片。所述的制作方法包括以下步骤:a、备料:玻璃树脂粘结片和半固化片;b、复合:将玻璃树脂粘结片和半固化片分别加热到180℃,再将两者进行压合,得到所述两面性粘结片。通过上述方式,本发明弥补了软硬结合板的结合强度不足与流胶不规律的缺陷,使软硬结合板具有完美的抗高温热冲击能力与恶劣环境下的稳定使用效果。

Description

用于软硬结合板的两面性粘结片及其制作方法
技术领域
本发明涉及软硬结合板技术领域,特别是涉及一种用于软硬结合板的两面性粘结片及其制作方法。
背景技术
软硬结合板是一种兼具刚性印刷电路板(PCB,printedcircuitboard)的耐久力和柔性PCB的适应力的新型印刷电路板,在所有类型的PCB中,软硬结合是对恶劣应用环境的抵抗力最强的,因此受到医疗与军事设备生产商的青睐,我国的企业也正在逐步提高软硬结合板占总体产量的比例。
现有的软硬结合板,由于所用的粘结片的问题,存在着结合强度不足、流胶不规律、粘结不方便的缺陷。因此,开发一种新的、能够解决上述问题的粘结片显得很有必要。
发明内容
本发明主要解决的技术问题是提供一种用于软硬结合板的两面性粘结片及其制作方法,能够解决现有技术中存在的问题,弥补了软硬结合板的结合强度不足与流胶不规律的缺陷,使软硬结合板具有完美的抗高温热冲击能力与恶劣环境下的稳定使用效果。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种用于软硬结合板的两面性粘结片,包括:该两面性粘结片是采用两种粘结片复合在一起而制成,所述两种粘结片分别为玻璃树脂粘结片和半固化片。
本发明还提供了上述用于软硬结合板的两面性粘结片的制作方法,包括以下步骤:
a、备料:玻璃树脂粘结片和半固化片;
b、复合:将玻璃树脂粘结片和半固化片分别加热到180℃,再将两者进行压合,得到所述两面性粘结片。
在本发明一个较佳实施例中,所述玻璃树脂粘结片采用低流动的玻璃树脂粘结片。
在本发明一个较佳实施例中,所述半固化片采用低溢胶量半固化片。
在本发明一个较佳实施例中,所述玻璃树脂粘结片与半固化片的厚度相同。
在本发明一个较佳实施例中,所述玻璃树脂粘结片与半固化片的厚度不相同。
本发明的有益效果是:本发明用于软硬结合板的两面性粘结片及其制作方法,弥补了软硬结合板的结合强度不足与流胶不规律的缺陷,使软硬结合板具有完美的抗高温热冲击能力与恶劣环境下的稳定使用效果。
附图说明
图1是本发明一较佳实施例的用于软硬结合板的两面性粘结片的结构示意图;
图2是本发明一较佳实施例的用于软硬结合板的两面性粘结片的制作方法的流程图;
附图中各部件的标记如下:1、玻璃树脂粘结片,2、半固化片。
具体实施方式
下面结合附图对本发明的较佳实施例进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
请参阅图1,本发明实施例包括:
一种用于软硬结合板的两面性粘结片,包括:所述两面性粘结片是采用两种粘结片复合在一起而制成,所述两种粘结片分别为玻璃树脂粘结片1和半固化片2。
常规性单一玻璃树脂粘结片1与半固化片2两者各有特点,但两种材料对应软硬结合板的两种基材不能单一同时满足结合后的产品需求,玻璃树脂粘结片1的玻璃转化温度为170℃,恒压40KG,但转化过程所需时间至少需要30分钟,且必须在真空状态下进行,半固化片2压合过程简便快捷,其预贴定型温度180℃,压力50KG,时间仅需10秒,此种操作参数在普通过塑机或快压机上均可实现,但其结合力仅有1KG/cm2,不能具备玻璃树脂粘结片1.5KG/cm2以上的结合强度。
本发明的用于软硬结合板的两面性粘结片,将玻璃树脂粘结片1和半固化片2压合在一起,得到新的两面性粘结片,采用半固化片2的低温、定型时间短的特点组合玻璃树脂粘结片1,弥补软硬结合板的第一基材(FR4)与第二基材(聚醯亚胺)间的结合强度不足与流胶不规律的缺陷,从而使第一基材(FR4)与第二基材(聚醯亚胺)在压合成型后具有完美的抗高温热冲击能力与恶劣环境下的稳定使用效果。
请一并参阅图2,本发明还提供了上述用于软硬结合板的两面性粘结片的制作方法,包括以下步骤:
a、备料:玻璃树脂粘结片1和半固化片2;
b、复合:将玻璃树脂粘结片1和半固化片2分别加热到180℃,再将两者进行压合,得到所述两面性粘结片。
所述玻璃树脂粘结片1采用低流动的玻璃树脂粘结片1。
所述半固化片2采用低溢胶量半固化片2。
所述玻璃树脂粘结片1与半固化片2的厚度相同,也可以不相同。
以下是实验测试结果:
采用本发明的用于软硬结合板的两面性粘结片作为第一基材(FR4)和第二基材(聚醯亚胺)之间的粘结材料,经工艺测试,流胶量为0.2mm,且流胶位置均匀,便于在资料设计过程中给出准确的涨缩系数,第一基材与第二基材结合强度为1.5KG/cm2,满足了产品整体的结合强度要求。产品高温热冲击测试为300℃/30秒,不产生气泡和分层。
下表为不同粘结片的覆盖层性能比较,其中,最后一列为本发明的用于软硬结合板的两面性粘结片的性能。
实验表明,组合后的两面性粘结片便于软硬结合板的基材复合制作,解决了基材结合中所产生的结合力不足与粘结不方便的问题,为软硬结合板的制作提供了可靠的工艺条件。
本发明用于软硬结合板的两面性粘结片及其制作方法,弥补了软硬结合板的结合强度不足与流胶不规律的缺陷,使软硬结合板具有完美的抗高温热冲击能力与恶劣环境下的稳定使用效果。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书及附图内容所作的等效结构或等效流程变换,或直接或间接运用在其他相关的技术领域,均同理包括在本发明的专利保护范围内。

Claims (3)

1.一种用于软硬结合板的两面性粘结片,其特征在于,包括:该两面性粘结片是采用两种粘结片复合在一起而制成,所述两种粘结片分别为玻璃树脂粘结片和半固化片,所述玻璃树脂粘结片与半固化片的厚度相同或不相同,所述半固化片采用低溢胶量半固化片。
2.一种用于软硬结合板的两面性粘结片的制作方法,其特征在于,包括以下步骤:
a、备料:玻璃树脂粘结片和半固化片;
b、复合:将玻璃树脂粘结片和半固化片分别加热到180℃,再将两者进行压合,得到所述两面性粘结片。
3.根据权利要求2所述的用于软硬结合板的两面性粘结片的制作方法,其特征在于,所述玻璃树脂粘结片采用低流动的玻璃树脂粘结片。
CN201210452502.9A 2012-11-13 2012-11-13 用于软硬结合板的两面性粘结片及其制作方法 Active CN102950847B (zh)