Prior art keywords
glue
wooden
pressing
wood door
wooden skin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201210377816
Other languages
English (en)
Inventor
何书洪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 201210377816 priority Critical patent/CN102886798A/zh
Publication of CN102886798A publication Critical patent/CN102886798A/zh
Pending legal-status Critical Current

Links

Abstract

本发明的操作方法为:1、使用万能胶,在木皮和被粘物体的表面,均匀地涂刷上万能胶,等到涂刷的胶水干了,用涂胶将木门横向贴压一层;2、用涂胶将木门再竖向贴压一层,涂胶要适量、均匀,所贴板面一定要平整,不得有板筋、凹陷、孔洞等,否则容易鼓泡、离层;3、横竖交叉,用此双层贴压的方法确保实木门板面的质量稳定。

Description

一种实木门制作过程中的压贴木皮方法
技术领域
本发明涉及一种实木门制作过程中的压贴木皮方法。
背景技术
在传统的制作家具过程中,使用单层贴压,实木门的面容易开裂,造成实木门的质量不稳定。本技术针对木质的生长特点,运用竖丝拉力强度高、横丝拉力差的原理,使用双层贴压来完成。
发明内容
本发明针对木质的生长特点,横竖交叉,使用双层贴压的方法确保实木门板面的质量稳定。首先将要贴木皮的家具表面做平整,刷上第一遍白乳胶,等待胶水干后,刷第二遍,然后等胶水半干,将木皮平整的放置到刷过胶水的家具上,每放置一张要压在之前那张木皮的上面,也就是两张木皮只要有2-4厘米的边缘是重叠的。用手将木皮抚平,不能有褶皱,让后用木工刀之类的锋利的刀片在木皮与木皮重叠的部分的中间用锋利的刀或刀片划开。最后需要用熨斗熨平整。没有气孔,没有褶皱,然后再用砂纸磨一下。边缘和边角有线条部分操作是一样的。用涂胶先将木门横向贴压一层,然后再竖向贴压一层,以此防止实木门的开裂现象。
具体实施方式
本发明的操作方法为:
1、使用万能胶,在木皮和被粘物体的表面,均匀地涂刷上万能胶,等到涂刷的胶水干了,用涂胶将木门横向贴压一层;
2、用涂胶将木门再竖向贴压一层,涂胶要适量、均匀,所贴板面一定要平整,不得有板筋、凹陷、孔洞等,否则容易鼓泡、离层;
3、横竖交叉,用此双层贴压的方法确保实木门板面的质量稳定。

Claims (1)

1.本发明针对木质的生长特点,横竖交叉,使用双层贴压的方法确保实木门板面的质量稳定。首先将要贴木皮的家具表面做平整,刷上第一遍白乳胶,等待胶水干后,刷第二遍,然后等胶水半干,将木皮平整的放置到刷过胶水的家具上,每放置一张要压在之前那张木皮的上面,也就是两张木皮只要有2—4厘米的边缘是重叠的。用手将木皮抚平,不能有褶皱,让后用木工刀之类的锋利的刀片在木皮与木皮重叠的部分的中间用锋利的刀或刀片划开。最后需要用熨斗熨平整。没有气孔,没有褶皱,然后再用砂纸磨一下。边缘和边角有线条部分操作是一样的。用涂胶先将木门横向贴压一层,然后再竖向贴压一层,以此防止实木门的开裂现象。
CN 201210377816 2012-09-26 2012-09-26 一种实木门制作过程中的压贴木皮方法 Pending CN102886798A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201210377816 CN102886798A (zh) 2012-09-26 2012-09-26 一种实木门制作过程中的压贴木皮方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201210377816 CN102886798A (zh) 2012-09-26 2012-09-26 一种实木门制作过程中的压贴木皮方法

Publications (1)

Publication Number Publication Date
CN102886798A true CN102886798A (zh) 2013-01-23

Family

ID=47530580

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201210377816 Pending CN102886798A (zh) 2012-09-26 2012-09-26 一种实木门制作过程中的压贴木皮方法

Country Status (1)

Country Link
CN (1) CN102886798A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104493924A (zh) * 2014-11-28 2015-04-08 湖北燕加隆木制品有限公司 一种用于多层实木地板的压痕熨烫方法
CN107139304A (zh) * 2017-07-01 2017-09-08 安徽省扬子家居新材料有限公司 一种实木门制作过程中的压贴木皮方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104493924A (zh) * 2014-11-28 2015-04-08 湖北燕加隆木制品有限公司 一种用于多层实木地板的压痕熨烫方法
CN107139304A (zh) * 2017-07-01 2017-09-08 安徽省扬子家居新材料有限公司 一种实木门制作过程中的压贴木皮方法

Similar Documents

Publication Publication Date Title
CN102950638B (zh) 木质书画纸材及制作方法
CN102922568B (zh) 一种板材贴三聚氰胺面纸的方法
CN105922422A (zh) 拼花重组竹木地板及其生产工艺
CN104044197A (zh) 一种软木地板的生产工艺
CN103753900A (zh) 一种柔性装饰木皮
CN106493802B (zh) 一种含有定向结构板的集装箱底板及其制备方法
RU2016140386A (ru) Способ изготовления декорированных плит на основе древесного материала и изготовленная из плиты на основе древесного материала панель, прежде всего половая панель, а также применение изготовленной этим способом плиты на основе древесного материала
CN102886798A (zh) 一种实木门制作过程中的压贴木皮方法
CN107471361A (zh) 一种科技木贴面实木复合地板的生产工艺
CN208290089U (zh) 一种复合实木板
CN104149140A (zh) 杉木集成板的制作方法
CN204109102U (zh) 一种实木胶合拼板结构
CN203266833U (zh) Osb高强复合饰面板
CN104400843A (zh) 一种实木门制作过程中的压贴木皮方法
CN105034093A (zh) 一种实木门制作过程中的压贴木皮方法
CN207808670U (zh) 电子线固化膜多层复合地板
CN102581899B (zh) 防腐木板及其制备方法和用途以及由其制成的篮球板
CN104234359A (zh) 一种再生风化快装墙饰板及制作方法
CN204081362U (zh) 一种再生风化快装墙饰板
CN103963118A (zh) 一种实木薄板及其拼板工艺
CN108481470A (zh) 大规格实木复合板材的制备方法及制备的实木复合板材
CN206030109U (zh) 一种新型复合细木工板
CN203266834U (zh) Osb高强复合贴面板
CN202753245U (zh) 实木锯切复合板
CN206953190U (zh) 一种握钉加强的复合板材

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130123