CN102582349A - Manufacturing method for ceramic painting - Google Patents

Manufacturing method for ceramic painting Download PDF

Info

Publication number
CN102582349A
CN102582349A CN2012100529105A CN201210052910A CN102582349A CN 102582349 A CN102582349 A CN 102582349A CN 2012100529105 A CN2012100529105 A CN 2012100529105A CN 201210052910 A CN201210052910 A CN 201210052910A CN 102582349 A CN102582349 A CN 102582349A
Authority
CN
China
Prior art keywords
ceramic
glaze
pottery
paint
painting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012100529105A
Other languages
Chinese (zh)
Inventor
杨舒童
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012100529105A priority Critical patent/CN102582349A/en
Publication of CN102582349A publication Critical patent/CN102582349A/en
Pending legal-status Critical Current

Abstract

The invention relates to a manufacturing method for ceramic painting. The manufacturing method comprises the following steps of: painting ceramic pigment on a ceramic product, arranging a circular shielding object on the surface of a ceramic ware or a ceramic plate by dropwise adding a thinning agent or rotatably pressing a thumb and cotton fiber, removing the shielding object after spraying to form a water-and-light mist pattern, and shaping a subject on the water-and-light mist pattern by combining the painting. Or the manufacturing method comprises the following steps of: spreading underglazed ceramic pigment and colored glaze on a ceramic green body, removing part of the pigment or the glaze by using a scraper or in a washing subtraction mode, etc., or arranging the circular shielding object on the surface of the ceramic green tire, removing the circular shielding object after spraying to form the water-and-light mist pattern, and shaping the subject on the water-and-light mist pattern by combining the painting. The manufacturing method has the advantages that the water-and-light mist pattern serves as the background and atmosphere, an imaginary virtual space is created, and the subject is shaped on the water-and-light mist pattern, the perfect combination of the ceramic painting and western painting styles is realized, and the traditional western painting is blended with the traditional Chinese ceramic painting, so that the unique artistic feeling and charm of the ceramic are fully released.

Description

A kind of preparation method of ceramic drawing
Technical field
The present invention relates to a kind of ceramic drawing, be specifically related to a kind of preparation method of ceramic drawing.
Background technology
The West drawing method covers comprehensively, is different from state's technique of painting, and rare reflection relies on the material of material.Borrow the covering power and the properties of transparency of pigment to show rendered object more fully, rich color, third dimension is strong.Its form characteristics are to be full of picture, through the drawing performance imaginary space and theme.Pottery be with the clay be that primary raw material and various natural minerals are mixing through pulverizing, material and various goods that moulding and calcining make.The Chinese pottery drawing is on ceramic or ceramic plain tire, to carry out the works that painting creation obtains, and leaves a large amount of negative spaces, demonstrates fully the glamour of porcelain.How the form with western drawing combines with the pottery drawing, becomes an emerging graphics art form.But according to the western drawing method, ceramic paint has been paved with ceramic product, lets the people experience the unique artistic glamour less than ceramic material.Therefore, need a kind of western drawing form and preparation method that manifests the ceramic drawing of ceramic quality of having concurrently.
Summary of the invention
Technical problem to be solved by this invention provides a kind of preparation method of ceramic drawing, and this technology is simple, and processing and fabricating is easy, is skillfully constructed, with ceramic quality and the perfect adaptation of western drawing form of painting.
For solving the problems of the technologies described above, so the new producing method of a kind of ceramic drawing of invention may further comprise the steps:
(1) selects pottery or ceramic wafer; Ceramic paint in ceramic paint or the glaze on the modulation treatment glaze; Spray repeatedly, drip and spill through Spray painting tool, ceramic paint in ceramic paint or the glaze on the glaze of modulation treatment acquisition is evenly coated in the surface of said pottery or ceramic wafer;
(2) treat that said ceramic paint is not dried before; Diluent is dripped respectively on the ceramic paint that is sprinkled upon said pottery surface or ceramic wafer surface diverse location; The ceramic paint that contacts with said diluent looses towards periphery, and the formation shape is similar, not of uniform size on the ceramic paint on pottery or ceramic wafer surface, actual situation is alternate, cross one another circle points;
(3) on pottery that step (2) obtains or ceramic wafer, paint, fire through 600-1400 ℃ in the porcelain stove afterwards, firing time 3-8 hour, 10-12 hour cool time; Can repeat above-mentioned steps as required.
Said diluent is alcohol or turpentine oil or rosin.
Said circle points is through pressing thumb or cotton-wool respectively on the said ceramic paint of said pottery or ceramic wafer surface diverse location, and rotation thumb or cotton-wool form.
Said circle points is provided with circular shelter through the surface at described pottery of step (1) or ceramic wafer, removes shelter behind the ceramic coated material and forms.
Circular shelter on said pottery or the ceramic wafer perhaps blocks liquid formation through smearing for through pasting the scraps of paper, plastic sheeting formation.
The present invention also can realize that a kind of preparation method of ceramic drawing may further comprise the steps through following technical scheme:
(1) select ceramic plain embryo, ceramic paint or coloured glaze under the modulation treatment glaze spray repeatedly, drip and spill the surface that ceramic paint or coloured glaze under the glaze of modulation treatment acquisition is evenly coated in the plain embryo of said pottery through Spray painting tool;
(2) treat under the said glaze that ceramic paint or coloured glaze dry after; Scrape picture or wash subtraction and respectively ceramic paint or coloured glaze under the part glaze of diverse location on the plain embryo surface of pottery are got rid of through scraper, the ceramic plain embryo surface that is paved with pigment occurs that shape is similar, not of uniform size, actual situation is alternate, cross one another circle points;
(3) on the ceramic plain embryo that step (2) obtains, paint; Fire through stove 1300-1500 ℃ afterwards, coat the layer of transparent glaze, firing time 7-12 hour before the ceramic plain embryo of ceramic paint is fired under the glaze for being paved with; Cooled off 12-14 hour, and can repeat above-mentioned steps as required.
Said Spray painting tool is tack pen, writing brush, airbrush or sponge.
The said ceramic plain tire that scribbles coloured glaze forms said circle points through dripping the glaze colours that spills different tones before said coloured glaze is not dried.
Said circle points is removed circular shelter behind ceramic paint or the coloured glaze under the spraying glaze and is formed through on the plain tire of the described pottery of step (1) surface circular shelter being set.
Circular shelter on said pottery or the ceramic wafer perhaps blocks liquid formation through smearing through pasting the scraps of paper, plastic sheeting formation.
The present invention is skillfully constructed; Form on ceramic that shape is similar, not of uniform size, actual situation is alternate, intersect each other or overlapping circle points through several different methods; Ceramic material in the circle points is visible; Fine artistic conception with the aqueous vapor of ascension on the lake surface and water light haze gas that rain and dew form in the sun forms water light haze gas pattern.With water light haze gas pattern as a setting and atmosphere; Created the imaginary space that can give free rein to one's imagination, drawing is moulded theme above that, can clearly experience the quality of pottery; Realized the perfect adaptation of pottery with Western form of painting; Draw the mutual blending of full Western traditional drawing and Chinese traditional ceramics, fully discharge the unique artistic impression and the glamour of ceramic material, Western traditional drawing form has found the home to return on Chinese pottery.
The specific embodiment
Embodiment 1
A kind of preparation method of ceramic drawing may further comprise the steps:
(1) selects suitable pottery or ceramic wafer; Need based on form of painting; Buy on the required glaze ceramic paint ceramic paint or the glaze from market; The modulation treatment ceramic paint; Through the tack pen; Writing brush; Airbrush; Spray painting tools such as sponge spray repeatedly; Drip and spill; The ceramic paint that modulation treatment is obtained evenly is coated with the surface that is drawn in said pottery or ceramic wafer; When spraying; Based on needs; Pigment can be sprayed into the whole surface of pottery or ceramic wafer, also can be that part of surface that need paint on pottery or the ceramic wafer;
(2) treat that said ceramic paint is not dried before; Diluents such as alcohol or turpentine oil or rosin are dripped respectively on the ceramic paint that is sprinkled upon said pottery surface or ceramic wafer surface diverse location; The ceramic paint that contacts with said diluent looses towards periphery; The formation shape is similar, not of uniform size on the ceramic paint on pottery or ceramic wafer surface, actual situation is alternate, cross one another circle points, exposes pottery in the circle points, forms water light haze gas pattern; Said circle points also can be by on the said ceramic paint that objects such as thumb or cotton-wool is pressed on said pottery or ceramic wafer surface diverse location respectively, and rotation thumb or cotton-wool form; Said circle points can also be by forming circular shelter at the surperficial paste shape of described pottery of step (1) or the ceramic wafer circular or oval scraps of paper, plastic sheeting same or similar, not of uniform size; Also can block liquid and form circular shelter by smearing at the diverse location on the surface of described pottery or ceramic wafer; Circular shelter is being to form space under the required circle points reservation on pottery or the ceramic wafer, and the circular shelter of the outer back removal of ceramic coated pigment forms circle points;
(3) on pottery that step (2) obtains or ceramic wafer, paint and mould theme, fire for 600-1400 ℃ in porcelain stove back warp afterwards, firing time 3-8 hour, 10-12 hour cool time; Can repeat above-mentioned steps 1,2,3 as required.
Embodiment 2
A kind of preparation method of ceramic drawing may further comprise the steps:
(1) selects the plain embryo of suitable ceramic; According to the form of painting needs; Buy ceramic paint under the glaze, coloured glaze from market, ceramic paint or coloured glaze under the modulation treatment glaze spray repeatedly, drip and to spill under the glaze that modulation treatment is obtained ceramic paint or coloured glaze evenly is coated with the surface that is drawn in the plain embryo of said pottery through Spray painting tools such as tack pen, writing brush, airbrush, sponges; When spraying; As required, can pigment be sprayed into the whole surface of ceramic plain tire, also can be that part of surface that need paint on the ceramic plain tire;
(2) treat under the said glaze that ceramic paint or coloured glaze dry after, scrape picture or wash subtraction through scraper, respectively ceramic paint or coloured glaze under the part glaze of diverse location on the plain embryo surface of pottery are got rid of.The ceramic plain embryo surface that is paved with pigment occurs that shape is similar, not of uniform size, actual situation is alternate, cross one another circle points; The said ceramic plain tire that scribbles coloured glaze also can form said circle points through dripping the glaze colours that spills different tones through before coloured glaze is not dried; Said circle points can also be through forming circular shelter at the plain tire of pottery surface the paste shape circular or oval scraps of paper, plastic sheeting same or similar, not of uniform size; Also can through on the plain tire of described pottery surface diverse location smear and block liquid and form circular shelter; Circular shelter is being to form space under the required circle points reservation on the plain tire of pottery, removes circular shelter formation under the spraying glaze behind ceramic paint or the coloured glaze;
(3) on the ceramic plain embryo that step (2) obtains the drawing after; In the porcelain stove, fire through 1300-1500 ℃; Coat the layer of transparent glaze for being paved with before the ceramic plain embryo of ceramic paint is fired under the glaze; Firing time 7-12 hour, cooled off 12-14 hour, can repeat above-mentioned steps 1,2,3 as required.
The present invention is skillfully constructed; Form on ceramic that shape is similar, not of uniform size, actual situation is alternate, intersect each other or overlapping circle points through several different methods; Ceramic material in the circle points is visible; Fine artistic conception with the aqueous vapor of ascension on the lake surface and water light haze gas that rain and dew form in sunlight forms water light haze gas pattern.With water light haze gas pattern as a setting and atmosphere, created the imaginary space that can give free rein to one's imagination, drawing is moulded theme above that, can clearly experience the quality of pottery.Realized the perfect adaptation of pottery with the western drawing form of painting; Draw the mutual blending of full Western traditional drawing and Chinese traditional ceramics; Fully discharge the unique artistic impression and the glamour of ceramic material; The West traditional drawing form has found the home to return on Chinese pottery, realized the dream that western drawing and Chinese pottery drawing organically combines.

Claims (10)

1. the preparation method of a ceramic drawing is characterized in that, may further comprise the steps:
(1) selects pottery or ceramic wafer; Ceramic paint in ceramic paint or the glaze on the modulation treatment glaze; Spray repeatedly, drip and spill through Spray painting tool, ceramic paint in ceramic paint or the glaze on the glaze of modulation treatment acquisition is evenly coated in the surface of said pottery or ceramic wafer;
(2) treat that said ceramic paint is not dried before; Diluent is dripped respectively on the ceramic paint that is sprinkled upon said pottery surface or ceramic wafer surface diverse location; The ceramic paint that contacts with said diluent looses towards periphery, and the formation shape is similar, not of uniform size on the ceramic paint on pottery or ceramic wafer surface, actual situation is alternate, cross one another circle points;
(3) on pottery that step (2) obtains or ceramic wafer, paint, in ceramics furnace, fire through 600-1400 ℃ afterwards, firing time 3-8 hour, 10-12 hour cool time; Can repeat above-mentioned steps as required.
2. the preparation method of ceramic drawing according to claim 1 is characterized in that, said diluent is alcohol or turpentine oil or rosin.
3. the preparation method of ceramic drawing according to claim 1 is characterized in that, said circle points is through pressing thumb or cotton-wool respectively on the said ceramic paint of said pottery or ceramic wafer surface diverse location, and rotation thumb or cotton-wool form.
4. according to the preparation method of claim 1 or 3 described ceramic drawings, it is characterized in that said circle points is provided with circular shelter through the surface at described pottery of step (1) or ceramic wafer, remove circular shelter behind the ceramic coated pigment and form.
5. the preparation method of ceramic drawing according to claim 4 is characterized in that, the circular shelter on said pottery or the ceramic wafer perhaps blocks liquid formation through smearing for through pasting the scraps of paper, plastic sheeting formation.
6. the preparation method of a ceramic drawing is characterized in that, may further comprise the steps:
(1) select ceramic plain embryo, ceramic paint or coloured glaze under the modulation treatment glaze spray repeatedly, drip and spill the surface that ceramic paint or coloured glaze under the glaze of modulation treatment acquisition is evenly coated in the plain embryo of said pottery through Spray painting tool;
(2) treat under the said glaze that ceramic paint or coloured glaze dry after; Scrape picture or wash subtraction and respectively ceramic paint or coloured glaze under the part glaze of diverse location on the plain embryo surface of pottery are got rid of through scraper, the ceramic plain embryo surface that is paved with pigment occurs that shape is similar, not of uniform size, actual situation is alternate, cross one another circle points;
(3) on the ceramic plain embryo that step (2) obtains, paint; In stove, fire through 1300-1500 ℃ afterwards, coat the layer of transparent glaze, firing time 7-12 hour before the ceramic plain embryo of ceramic paint is fired under the glaze for being paved with; Cooled off 12-14 hour, and can repeat above-mentioned steps as required.
7. the preparation method of ceramic drawing according to claim 6 is characterized in that, said Spray painting tool is tack pen, writing brush, airbrush or sponge.
8. the preparation method of ceramic drawing according to claim 6 is characterized in that, the said ceramic plain tire that scribbles coloured glaze forms said circle points through dripping the glaze colours that spills different tones before said coloured glaze is not dried.
9. according to the preparation method of claim 6 or 8 described ceramic drawings, it is characterized in that said circle points is removed circular shelter behind ceramic paint or the coloured glaze under the spraying glaze and formed through on the plain tire of the described pottery of step (1) surface circular shelter being set.
10. the preparation method of ceramic drawing according to claim 9 is characterized in that, the circular shelter on said pottery or the ceramic wafer perhaps blocks liquid formation through smearing through pasting the scraps of paper, plastic sheeting formation.
CN2012100529105A 2012-03-02 2012-03-02 Manufacturing method for ceramic painting Pending CN102582349A (en)