CN102423899A - 青铜色澄泥砚台的生产方法 - Google Patents
青铜色澄泥砚台的生产方法 Download PDFInfo
- Publication number
- CN102423899A CN102423899A CN201110304238XA CN201110304238A CN102423899A CN 102423899 A CN102423899 A CN 102423899A CN 201110304238X A CN201110304238X A CN 201110304238XA CN 201110304238 A CN201110304238 A CN 201110304238A CN 102423899 A CN102423899 A CN 102423899A
- Authority
- CN
- China
- Prior art keywords
- mud
- inkstone
- bronze
- blank
- fire
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种青铜色澄泥砚台的生产方法,解决了澄泥砚台生产方法失传多年且颜色无法人为控制的问题。一种青铜色澄泥砚台的生产方法,包括以下步骤:将取自山西省五台县境内滹沱河中的古沉泥晾晒干;将晒干后的古沉泥放入水缸浸泡两小时;将浸泡后的古沉泥搅拌成泥浆;将泥浆进行过滤;对过滤后的泥浆进行揉制拍打,使其成型为泥团;将泥团放入模具中制成毛坯;将毛坯放入耐火盒,用铅粉将毛坯全部埋住;将耐火盒放入窑中,窑温控制在980℃~1050℃,烧制72小时,获得青铜色澄泥砚台。本发明承古而创新,恢复了失传已久的澄泥砚台的生产工艺,生产出的澄泥砚台质地优良,形色兼备。
Description
技术领域
本发明涉及一种澄泥砚台的生产方法,具体为一种青铜色澄泥砚台的生产方法。
背景技术
澄泥砚是我国四大名砚之一,它与端砚、歙砚、洮河砚并称为中国“四大名砚”。澄泥砚开我国砚界精细的先河。它的前身是古代的陶砚。古人受砖、瓦当生产的启示,结合陶砚再精工制作,遂步升华为澄泥砚。此砚始于唐代,宋代发展到顶峰,此后逐步衰落,最后失传。澄泥砚的特点是质坚细腻,坚而不燥,细而不滑,储水不涸,历寒不冰,发墨益毫,浓淡相宜,温润沉静,色泽雅美,有多种不同颜色。《文房四谱》中说:“宋代以后,开采天然石琢砚,类澄泥砚,亦名‘澄泥砚’。其品类有‘鳝鱼黄’、‘蟹壳青’、‘绿豆砂’、‘玫瑰紫’、‘豆瓣砂’等”;文物专家指出:“因泥沙的来源及制作过程的天气、烧制火候的不同而各有不同的颜色。”看来古人并非是有意烧制各种颜色,而是烧制过程中客观形成的,颜色的形成带有偶然性,非人为所能控制。
澄泥砚台具体的烧制过程及工艺,则至清代就已失传。今日所见古澄泥砚极为稀少,上品更是难求,究其原因,恐怕就在于制作工艺繁复而产量甚低。
发明内容
本发明针对澄泥砚台生产方法失传、且砚台颜色无法人为控制的问题,提供一种青铜色澄泥砚台的生产方法。
本发明是通过以下步骤实现的:一种青铜色澄泥砚台的生产方法,包括以下步骤:将取自山西省五台县境内滹沱河中的古沉泥晾晒干;将晒干后的古沉泥放入水缸加水浸泡两小时;将浸泡后的古沉泥搅拌成泥浆;对泥浆进行过滤;对过滤后的泥浆进行揉制拍打,使其成型为泥团;将泥团放入模具中制成毛坯;将毛坯放入耐火盒,用铅粉将耐火盒中的毛坯全部埋住;将耐火盒放入窑中,窑温控制在980℃~1050℃,烧制72小时,获得青铜色澄泥砚台。
本发明承古而创新,恢复了失传已久的澄泥砚台的生产工艺,生产出的澄泥砚台质地细腻,坚实厚古,形制多样,并在此基础上实现了人为控制澄泥砚台外观色泽的目的,生产出的澄泥砚台形色兼备。所述生产方法具备可操作性,为本领域技术人员容易实现的。本发明取法民间传统工艺,经过大量的实验及多年的工艺探索,成功实现了澄泥砚台的工业化生产,所生产出的澄泥砚台具有古籍中记载的多种优良特性,并在此基础上取得了突破,实现了对澄泥砚台外观色彩的控制。烧制出的澄泥砚台可以把色彩与形制结合起来,使其更具有艺术效果。本发明对于弘扬民间传统工艺,保护民间珍贵文化遗产亦具有重要意义。
具体实施方式
一种青铜色澄泥砚台的生产方法,包括以下步骤:(a)将取自山西省五台县境内滹沱河中的古沉泥晾晒干;(b)将晒干后的古沉泥放入水缸加水浸泡两小时;(c)将浸泡后的古沉泥搅拌成泥浆;(d)对泥浆进行过滤;(e)对过滤后的泥浆进行揉制拍打,使其成型为泥团;(f)将泥团放入模具中制成毛坯;(g)将毛坯放入耐火盒,用铅粉将耐火盒中的毛坯全部埋住;(h)将耐火盒放入窑中,窑温控制在980℃~1050℃,烧制72小时,获得青铜色澄泥砚台。步骤(d)所述过滤分两步进行,第一步采用万孔筛过滤,第二步将过滤后的泥浆装入布袋中吊起,过滤掉其中的水分。
取自山西省五台县境内滹沱河中的古沉泥,细润而又有柔性,泥中含有十多种矿物质;经过万孔筛过滤和布袋过滤水分后留下的极为细致的泥浆就是澄泥;对澄泥进行揉制拍打使其成型为泥团,再放入模具中制成砚台毛坯,此时可以按照艺术要求进行雕刻加工,使其具备各种形制;所述铅粉为磨碎成粉状的铅;烧制时,用铅粉将耐火盒中的砚台毛坯全部埋住;窑中的温度控制在980℃~1050℃之间(可选择980℃、990℃、1000℃、1050℃),保持这一温度范围将装有毛坯的耐火盒烧制72小时,就可得到具有青铜色色泽的质地细腻、发墨而不损毫的澄泥砚台。
Claims (2)
1.一种青铜色澄泥砚台的生产方法,其特征在于,包括以下步骤:
(a)将取自山西省五台县境内滹沱河中的古沉泥晾晒干;
(b)将晒干后的古沉泥放入水缸加水浸泡两小时;
(c)将浸泡后的古沉泥搅拌成泥浆;
(d)对泥浆进行过滤;
(e)对过滤后的泥浆进行揉制拍打,使其成型为泥团;
(f)将泥团放入模具中制成毛坯;
(g)将毛坯放入耐火盒,用铅粉将耐火盒中的毛坯全部埋住;
(h)将耐火盒放入窑中,窑温控制在980℃~1050℃,烧制72小时,获得青铜色澄泥砚台。
2.如权利要求1所述的青铜色澄泥砚台的生产方法,其特征在于所述过滤步骤分两步进行,第一步采用万孔筛过滤,第二步将过滤后的泥浆装入布袋中吊起,过滤掉其中的水分。