CN102358099A - Processing method of surface-engraved multicolor aluminum profile - Google Patents
Processing method of surface-engraved multicolor aluminum profile Download PDFInfo
- Publication number
- CN102358099A CN102358099A CN2011102487827A CN201110248782A CN102358099A CN 102358099 A CN102358099 A CN 102358099A CN 2011102487827 A CN2011102487827 A CN 2011102487827A CN 201110248782 A CN201110248782 A CN 201110248782A CN 102358099 A CN102358099 A CN 102358099A
- Authority
- CN
- China
- Prior art keywords
- paint
- carving
- section bar
- aluminium section
- decorative pattern
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a processing method of a surface-engraved multicolor aluminum profile, which can be used for engraving convex and concave floral designs on the surface of the aluminum profile and applying multiple colors of paint so as to achieve the advantages of strong third dimension and good decoration effect. The processing method comprises the following steps of: 1, engraving the surface of the aluminum profile; 2, primarily coloring; and 3, secondarily coloring comprising the procedures of (1), scribing engraving patterns on scribing paper, (2), adhering the scribing paper, (3), blending metal patient, (4), spraying the patient,(5), complementing color, and (6), washing.
Description
Technical field
The present invention relates to the aluminium shape surface processing technique field, particularly a kind of processing method of surperficial carving polychrome aluminium section bar.
Background technology
At present, the aluminium shape surface method of colouring is mainly contained integral colouring, electrolytic coloring, chemical staining, coating dip coating etc., these are all based on to the aluminium anode oxide film method of colouring.These colorize methods can only obtain monochromatic rete, have shortcomings such as dull coloring, no third dimension, decorative effect be relatively poor.
Summary of the invention
The object of the invention is to provide a kind of processing method of surperficial carving polychrome aluminium section bar, and it can have the concave, convex floral designs and impose the paint of multiple color at aluminium shape surface carving, reaches that third dimension is strong, good decorating effect.
Technical solution proposed by the invention is such:
A kind of processing method of surperficial carving polychrome aluminium section bar, the processing step of this processing method is following:
(1) aluminium shape surface carving: make wooden bed die and aluminium section bar is made even be fixed on this aluminium section bar; In the data input numerical control carving machine of intending the carving line shape and the degree of depth; To being carried out carving, with refiner the burr of the docking point of decorative pattern and decorative pattern are ground off and to make even by the carving plane;
(2) colouring for the first time: aluminium shape surface is carried out the painted processing of anode oxide film;
(3) colouring for the second time:
1. paint to carve on the paper at quarter with art weave special purpose computer engraving machine and paint the carving style;
2. paste to carve and paint paper: for the decorative pattern of recessed flower; Paint paper the quarter of painting style and once stick on the corresponding aluminium section bar carving face carving; And carved and also will paste several layers after painting paper the quarter of painting style and carved and paint paper the quarter of painting style having pasted ground floor on the aluminium section bar carving face of correspondence for the decorative pattern of protruding flower, up to exceeding the outstanding peak of this decorative pattern a little;
3. allotment is painted, and the proportioning of this paint is by weight percentage:
Metallic paint 40-50, mill base or toner 12-20, curing agent 18-26, diluent 14-20; The mill base color will be confirmed by the decorative pattern required color and the depth;
4. spray paint: raise to carve and paint the decorative pattern part that need spray paint in the paper, to this decorative pattern part primer spray, then, the paint of selecting to meet the color requirement sprays paint to this decorative pattern aluminium section bar partly with alkali resistant priming paint in elder generation;
5. complementary color: add look again one time with the writing brush point, paint thickness is wanted evenly;
6. wash plate: under 50-80 ° of C temperature, dry the metallic paint of carving part, with alcohol unnecessary paint is removed from aluminium section bar, and aluminium section bar is cleaned up with cleaning solution.
The pattern depth that aluminium section bar is carved face is 1/5-1/4 of this aluminium section bar thickness.
Curing agent adopts polyurethane curing agent.Diluent adopts Tianna solution.
Compared with prior art, the present invention has following remarkable result: (1) strengthens the third dimension of its floral designs greatly owing to be carved with the concave, convex floral designs at aluminium shape surface.(2) because aluminium section bar is carried out twice colouring; The technology that particularly adopts metallic paint to match with alkali resistant priming paint; Make multicoloured metallic paint painted ten minutes on said ridge design firm, decolouring, variable color can not appear in long-term the use, and decorative effect is fine.
The specific embodiment
Embodiment 1
A kind of processing method of surperficial carving polychrome aluminium section bar, its processing step is following.
(1) aluminium shape surface carving: because the shape of aluminium section bar is very irregular; Before aluminium section bar engraving, will make wooden bed die makes even aluminium section bar and is fixed on this aluminium section bar; To intend in the data inputs numerical control carving machine of the carving line shape and the degree of depth (highly), and to being carried out carving, with refiner the burr of the docking point of decorative pattern and decorative pattern ground off and to make even by the carving plane; Pattern depth is 1/5-1/4 of this aluminium section bar thickness; Because general aluminium section bar thickness is 1-4mm, so the concavo-convex degree of depth of decorative pattern is generally 0.2-1mm.
(2) colouring for the first time: aluminium shape surface is carried out the painted processing of anode oxide film.
(3) colouring for the second time: 1. paint to carve on the paper at quarter and paint the carving style with art weave special purpose computer engraving machine.2. paste to carve and paint paper: for the decorative pattern of recessed flower; Be to carve to paint paper the quarter of painting style and once stick on the corresponding aluminium section bar carving face; And carved and also will paste several layers after painting paper the quarter of painting style and carved and paint paper the quarter of painting style having pasted ground floor on the aluminium section bar carving face of correspondence for the decorative pattern of protruding flower, up to exceeding the outstanding peak of this decorative pattern a little.3. allotment is painted, and the proportioning of this paint is by weight percentage: metallic paint 40-50, mill base or toner 12-20, curing agent 18-26, diluent 14-20; Mill base or toner color are confirmed that by the decorative pattern required color and the depth in the present embodiment, curing agent adopts polyurethane curing agent; Diluent adopts Tianna solution, and the proportioning of this metallic paint is by weight percentage: metallic paint 40, mill base 20; Polyurethane curing agent 26, Tianna solution 14.4. spray paint: raise to carve and paint the ridge design part that need spray paint in the paper, at first use alkali resistant priming paint to this decorative pattern part primer spray, then, the metallic paint of selecting to meet the color requirement partly sprays paint to this decorative pattern; If the decorative pattern in aluminium section bar requires multiple color; Then to spray paint step by step, at first open and paint paper the 1st roughly the same color patterned quarter and spray paint, treat that paint is done after; With gluing this place that seals of paper; Open again and paint paper the 2nd roughly the same color patterned quarter and carry out another kind of color and spray paint, so analogize, just can spray the floral designs of multiple color.5. complementary color: add look again one time with the writing brush point, paint thickness is wanted evenly.6. wash plate: under 50 ° of-80 ° of C temperature, dry the metallic paint of carving part, with alcohol unnecessary metallic paint is removed from aluminium section bar, and aluminium section bar is cleaned up with cleaning solution.
Embodiment 2
The paint proportioning of present embodiment is by weight percentage: metallic paint 45, toner 16, polyurethane curing agent 22, Tianna solution 17.
After this decorative pattern is partly sprayed paint, at its surface spraying layer of transparent varnish, prevent that toner from coming off again.All the other, the processing method of said surperficial carving polychrome aluminium section bar is identical with embodiment 1.
Embodiment 3
The paint proportioning of present embodiment is by weight percentage: metallic paint 50, mill base 12, polyurethane curing agent 18, Tianna solution 20.The processing method of all the other said surperficial carving polychrome aluminium section bars is identical with embodiment 1.
Claims (4)
1. the processing method of a surperficial carving polychrome aluminium section bar, it is characterized in that: the processing step of this processing method is following:
(1) aluminium shape surface carving: make wooden bed die and aluminium section bar is made even be fixed on this aluminium section bar; In the data input numerical control carving machine of intending the carving line shape and the degree of depth; To being carried out carving, with refiner the burr of the docking point of decorative pattern and decorative pattern are ground off and to make even by the carving plane;
(2) colouring for the first time: aluminium shape surface is carried out the painted processing of anode oxide film;
(3) colouring for the second time:
1. paint to carve on the paper at quarter with art weave special purpose computer engraving machine and paint the carving style;
2. paste to carve and paint paper: will carve for the decorative pattern of recessed flower and paint paper the quarter of painting style and once stick on the corresponding aluminium section bar carving face; And carved and also will paste several layers after painting paper the quarter of painting style and carved and paint paper the quarter of painting style having pasted ground floor on the aluminium section bar carving face of correspondence for the decorative pattern of protruding flower, up to exceeding the outstanding peak of this decorative pattern a little;
3. allotment is painted, and the proportioning of this paint is by weight percentage:
Metallic paint 40-50, mill base or toner 12-20, curing agent 18-26, diluent 14-20; The mill base color will be confirmed by the decorative pattern required color and the depth;
4. spray paint: raise to carve and paint the decorative pattern part that need spray paint in the paper, to this decorative pattern part primer spray, then, the metallic paint of selecting to meet the color requirement partly sprays paint to this decorative pattern with alkali resistant priming paint in elder generation;
5. complementary color: add look again one time with the writing brush point, paint thickness is wanted evenly;
6. wash plate: under 50-80 ° of C temperature, dry the paint of carving part, with alcohol unnecessary paint is removed from aluminium section bar, and aluminium section bar is cleaned up with cleaning solution.
2. the processing method of surperficial carving polychrome aluminium section bar according to claim 1 is characterized in that: the pattern depth that said aluminium section bar is carved face is 1/5-1/4 of this aluminium section bar thickness.
3. the processing method of surperficial carving polychrome aluminium section bar according to claim 1 is characterized in that: said curing agent is a polyurethane curing agent; Said diluent is a Tianna solution.
4. the processing method of surperficial carving polychrome aluminium section bar according to claim 1 is characterized in that: adopt the paint of toner allotment, after this decorative pattern is partly sprayed paint, again at its surface spraying clear varnish.