CN102321898A - 直插式led支架杯碗内电镀层过薄解决设备 - Google Patents

直插式led支架杯碗内电镀层过薄解决设备 Download PDF

Info

Publication number
CN102321898A
CN102321898A CN201110240862A CN201110240862A CN102321898A CN 102321898 A CN102321898 A CN 102321898A CN 201110240862 A CN201110240862 A CN 201110240862A CN 201110240862 A CN201110240862 A CN 201110240862A CN 102321898 A CN102321898 A CN 102321898A
Authority
CN
China
Prior art keywords
anode
cup bowl
led support
titaniums
blue
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201110240862A
Other languages
English (en)
Other versions
CN102321898B (zh
Inventor
朱虬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUXI DINGYA ELECTRONIC PARTS CO Ltd
Original Assignee
WUXI DINGYA ELECTRONIC PARTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI DINGYA ELECTRONIC PARTS CO Ltd filed Critical WUXI DINGYA ELECTRONIC PARTS CO Ltd
Priority to CN201110240862.8A priority Critical patent/CN102321898B/zh
Publication of CN102321898A publication Critical patent/CN102321898A/zh
Application granted granted Critical
Publication of CN102321898B publication Critical patent/CN102321898B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种直插式LED支架杯碗内电镀层过薄解决设备,包括电镀槽,所述电镀槽内部两侧分别设置两个钛蓝阳极,在所述两个钛蓝阳极的中间位置的上方设置一根电镀白金的钛管冲水阳极,所述钛管冲水阳极分别通过连接扣与相邻的两个钛蓝阳极连接。所述钛管冲水阳极的作用是将电镀液直接冲入电镀杯碗内并使杯碗内的电镀液快速更换,从而确认杯碗内的电镀液浓度在规定范围内。同时钛管冲水阳极与钛篮阳极相连接有阳极的作用,使LED支架的杯碗面的电流增强。本发明可以完全解决电镀烧焦问题,并且能提高50%的电镀效率。

Description

直插式LED支架杯碗内电镀层过薄解决设备
技术领域
本发明涉及LED技术领域,特别涉及一种直插式LED支架杯碗内电镀层过薄解决设备。
背景技术
直插式LED支架杯碗内电镀层过薄解决设备来讲,现有技术主要是支架浸渍电镀方式,存在的技术缺陷:由于直插式LED支架固发光芯片的杯碗有凹陷,现有浸镀工艺在电镀的时候杯碗内的电镀液难以循环,电镀后杯碗内的电镀液的金属离子瞬间置换为金属导致在镀液浓度严重降低,镀液中的金属离子浓度降低后使支架杯碗内部的电镀容易出现烧焦,电镀层厚度较薄等问题。
发明内容
为了克服上述现有技术存在的缺陷,本发明提供一种直插式LED支架杯碗内电镀层过薄解决设备,可以完全解决电镀烧焦问题,并且能提高50%的电镀效率。
为了实现上述目的,本发明的技术方案如下:
直插式LED支架杯碗内电镀层过薄解决设备,包括电镀槽,所述电镀槽内部两侧分别设置两个钛蓝阳极,在所述两个钛蓝阳极的中间位置的上方设置一根电镀白金的钛管冲水阳极。
进一步,所述钛管冲水阳极分别通过连接扣与相邻的两个钛蓝阳极连接。
所述钛管冲水阳极的作用是将电镀液由镀白金的钛管以从上之下的高速喷淋的方式直接冲入电镀杯碗内并使杯碗内的电镀液快速更换,从而确认杯碗内的电镀液浓度在规定范围内。
同时钛管冲水阳极与钛篮阳极相连接有阳极的作用,使LED支架的杯碗面的电流增强。
所述LED支架杯碗是固定LED芯片的地方,作用为固定芯片,反射光线。
本发明的有益效果是,结构新颖,设计巧妙,完全解决了以前LED支架杯碗内部电镀烧焦问题,并能有效提高电镀效率。
附图说明
图1为本发明的主视图;
图2为与图1对应的俯视图;
图3为与图1对应的侧视图。
图中,1、电镀槽,2、钛管冲水阳极,3、钛蓝阳极,4、连接扣;
具体实施方式:
为了使本发明的创作特征、技术手段与达成目的易于明白理解,以下结合具体实施例进一步阐述本发明。
实施例:
参看图1、图2与图3,直插式LED支架杯碗内电镀层过薄解决设备,包括电镀槽1,电镀槽1内部两侧分别设置两个钛蓝阳极3,共四个钛蓝阳极3,一般是一套设备两个钛蓝阳极3,两套设备放在一起是由于生产设备是一机台两条生产线,正如图中所示。
在每组两个钛蓝阳极3的中间位置的上方设置一根电镀白金的钛管冲水阳极2。
每个钛管冲水阳极2分别通过连接扣4与相邻的两个钛蓝阳极3连接,图中所示共四个连接扣4,连接两组钛管冲水阳极2与钛蓝阳极3;
所述LED支架杯碗是固定LED芯片的地方,作用为固定芯片,反射光线。
钛管冲水阳极2的作用是将电镀液由镀白金的钛管以从上之下的高速喷淋的方式直接冲入电镀杯碗内并使杯碗内的电镀液快速更换,从而确认杯碗内的电镀液浓度在规定范围内。
同时钛管冲水阳极2与钛篮阳极3相连接有阳极的作用,使LED支架的杯碗面的电流增强。
本发明所述的直插式LED支架杯碗内电镀层过薄解决设备,使用方便,可以完全解决电镀烧焦问题,并且能提高50%的电镀效率。
以上显示和描述了本发明的基本原理、主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等同物界定。

Claims (2)

1.直插式LED支架杯碗内电镀层过薄解决设备,其特征在于,包括电镀槽,所述电镀槽内部两侧分别设置两个钛蓝阳极,在所述两个钛蓝阳极的中间位置的上方设置一根电镀白金的钛管冲水阳极。
2.根据权利要求1所述的直插式LED支架杯碗内电镀层过薄解决设备,其特征在于,所述钛管冲水阳极分别通过连接扣与相邻的两个钛蓝阳极连接。
CN201110240862.8A 2011-08-22 2011-08-22 直插式led支架杯碗内电镀层过薄解决设备 Active CN102321898B (zh)