太阳能光伏焊带着色工艺 Download PDFInfo
- Publication number
- CN102214731A CN102214731A CN2011101000096A CN201110100009A CN102214731A CN 102214731 A CN102214731 A CN 102214731A CN 2011101000096 A CN2011101000096 A CN 2011101000096A CN 201110100009 A CN201110100009 A CN 201110100009A CN 102214731 A CN102214731 A CN 102214731A
- Authority
- CN
- China
- Prior art keywords
- welding
- roller
- solar
- rod
- welding strip
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种太阳能光伏焊带着色工艺,包括对太阳能光伏焊带与太阳能电池连接的一面进行镀锡,以及利用氟碳涂料对另一面进行着色的加工工艺。本发明在不改变光伏焊带传统性能的基础上,根据用户的不同颜色需求,利用能够耐焊锡熔融温度的氟碳涂料在焊带的外表面着色,使其应用于光伏组件后既可实现导流光伏发电的目的,又与光伏组件外表面颜色协调一致,增强光伏组件的美观性,增加市场销售量。
Description
技术领域
本发明涉及一种对太阳能光伏组件焊带进行着色的加工工艺。
背景技术
焊带是用在光伏组件上的焊接材料,主要起连接导电的作用,传统的光伏组件焊带为铜质镀锡材质,采用热浸锡工艺制造,该工艺是在焊带加工过程中将铜带全部通过熔融状态的锡金属中,使焊带的正反面都浸上了焊锡,制作完毕后焊带两面颜色均为焊锡的自然颜色,焊带和电池片焊接成电池组起到导流光伏发电的作用。传统焊带应用于光伏组件后,其焊锡的自然颜色与光伏组件电池片和背板颜色不协调,影响了光伏组件的美观性。
氟碳涂料是以氟树脂为主要成膜物质的涂料,在各种涂料之中氟树脂涂料由于引入的氟元素电负性大,碳氟键能强,因此各项性能都比较优越。氟碳涂料优良的防腐蚀性能得益于极好的化学惰性,漆膜耐酸、碱、盐等化学物质和多种化学溶剂,为基材提供保护屏障;该漆膜坚韧,表面硬度高、耐冲击、抗屈曲、耐磨性好,显示出极佳的物理机械性能。氟碳涂层能够在摄氏300℃左右温度下对性能没有影响。氟碳涂层中含有大量的F--C键,决定了其超强的稳定性,不粉化、不褪色,使用寿命长达20年,具有比任何其他类涂料更为优异的性能。
发明内容
本发明需要解决的技术问题是提供一种能够为太阳能光伏焊带进行着色的加工工艺,以使整个太阳能光伏组件的颜色协调一致。
为解决上述技术问题,本发明所采取的技术方案是:
太阳能光伏焊带着色工艺,包括以下步骤:
a.将铜质焊带用于与太阳能光伏电池连接的一面浸入熔融状态的锡金属中,使焊带与太阳能光伏电池的连接面镀上锡层;
b.将焊带不镀锡金属的一面通过着色装置进行着色,着色剂采用氟碳涂料,着色装置包括放辊、收辊、涂色棍以及染料槽;进行着色时,将焊带镀锡面朝上固定在放辊和收辊上,放辊和收辊之间设置有涂色棍,涂色棍的下端浸泡在盛装氟碳涂料的染料槽中,然后同时向同一方向转动放辊、涂色棍和收辊,涂色棍转动时沾满染料槽中的氟碳涂料,与涂色棍接触的焊带即可印染上氟碳颜色。
由于采用了以上技术方案,本发明所取得技术进步在于:
本发明在不改变光伏焊带传统性能的基础上,根据用户的不同颜色需要,利用能够耐焊锡熔融温度的氟碳涂料在焊带的外表面着色,使其应用于光伏组件后既可实现导流光伏发电的目的,又与光伏组件外表面颜色协调一致,增强光伏组件的美观性,增加市场销售量。
通过本发明加工而成的太阳能光伏焊带,其外表面采用氟碳涂料进行着色,而与太阳能电池片的连接面则仍保持有焊锡层,不仅不影响焊带的焊接和导热性能;而且还使焊带的耐高温性大大增强,具有了硬度高、稳定性强、不褪色、不粉化、寿命长等优点。由于氟碳涂料具有优越的绝缘性能,所以太阳能光伏组件焊带、汇流带使用本发明的工艺方法制得的产品将大大提高太阳能光伏组件的耐高电压击穿性能。
附图说明
图1为本发明着色装置的侧视图;
图2为图1的俯视图。
其中:1.放辊,2.收辊,3.涂色棍,4.染料槽,5.焊带。
具体实施方式
下面将结合附图对本发明进行进一步详细说明。
太阳能光伏焊带着色时需要用到着色装置,其中着色装置的结构示意图如图1和图2所示,包括放辊1、收辊2、涂色棍3以及染料槽4,涂色棍位于放辊和收辊之间,涂色棍的下方设置有染料槽,涂色棍的下端浸在染料槽中。染料槽中盛装有氟碳涂料,可根据太阳能光伏电池的颜色调整氟碳涂料的颜色,使整个太阳能光伏组件的外观颜色一致。
太阳能光伏焊带着色工艺,如下所述:
a.首先将铜质焊带用于与太阳能光伏电池连接的一面浸入熔融状态的锡金属中,使焊带与太阳能光伏电池的连接面镀上锡层;
b.将焊带不镀锡金属的一面通过着色装置进行着色;进行着色时,将焊带镀锡面朝上固定在放辊和收辊上,然后同时向同一方向转动放辊、涂色棍和收辊,涂色棍转动时沾满染料槽中的氟碳涂料,与涂色棍接触的焊带即可印染上氟碳涂料的颜色。
通过本发明生产的焊带,与太阳能电池焊接的一面为镀锡层,焊带的外表面为着色面,与太阳能电池外表的颜色相同,大大提高了光伏组件的美观性。
Claims (1)
1.太阳能光伏焊带着色工艺,其特征在于包括以下步骤:
a.将铜质焊带用于与太阳能光伏电池连接的一面浸入熔融状态的锡金属中,使焊带与太阳能光伏电池的连接面镀上锡层;
b.将焊带不镀锡金属的一面通过着色装置进行着色,着色剂采用氟碳涂料,着色装置包括放辊、收辊、涂色棍以及染料槽;进行着色时,将焊带镀锡面朝上固定在放辊和收辊上,放辊和收辊之间设置有涂色棍,涂色棍的下端浸泡在盛装氟碳涂料的染料槽中,然后同时向同一方向转动放辊、涂色棍和收辊,涂色棍转动时沾满染料槽中的氟碳涂料,与涂色棍接触的焊带即可印染上氟碳颜色。