CN102059809A - 硅胶烘烤垫的生产方法 - Google Patents

硅胶烘烤垫的生产方法 Download PDF

Info

Publication number
CN102059809A
CN102059809A CN201010545999XA CN201010545999A CN102059809A CN 102059809 A CN102059809 A CN 102059809A CN 201010545999X A CN201010545999X A CN 201010545999XA CN 201010545999 A CN201010545999 A CN 201010545999A CN 102059809 A CN102059809 A CN 102059809A
Authority
CN
China
Prior art keywords
silica gel
food
baking pad
baking
pad
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010545999XA
Other languages
English (en)
Inventor
王红霞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201010545999XA priority Critical patent/CN102059809A/zh
Publication of CN102059809A publication Critical patent/CN102059809A/zh
Pending legal-status Critical Current

Abstract

硅胶烘烤垫的生产方法,涉及食品烘烤垫的生产工艺。将食品级液体硅胶稀释后置于胶槽中,将无腊玻璃纤维布自胶槽中浸透后,于60~120℃烘箱烘干,经压光机压光成型硫化,再经裁片后,于220℃高温处理3~4小时。本发明工艺简单,易于生产,经过本发明方法生产的烘烤垫中间不夹带气泡,强度高、使用寿命长,外观好,不但可耐受250℃的高温烘烤,还具有耐40℃低温的特性,无毒、环保,可将食物直接置于其上,与食品不粘粘。还可直接放于洗碗机中清洗,可重复使用。

Description

硅胶烘烤垫的生产方法
技术领域
本发明涉及食品烘烤垫的生产工艺。
背景技术
硅胶烘烤垫用于食品的烘烤,可作桌垫,餐垫,隔热垫。缺陷是在生产过程中如温度时间掌握不好,就会在垫体中产生气泡,影响美观,还会影响使用的寿命。
发明内容
本发明目的在于提供一种无气泡的硅胶烘烤垫的生产方法。
本发明生产方法是:将食品级液体硅胶稀释后置于胶槽中,将无腊玻璃纤维布自胶槽中浸透后,于60~120℃烘箱烘干,经压光机压光成型硫化,再经裁片后,于220℃高温处理3~4小时。
本发明工艺简单,易于生产,经过本发明方法生产的烘烤垫中间不夹带气泡,强度高、使用寿命长,外观好,不但可耐受250℃的高温烘烤,还具有耐40℃低温的特性,无毒、环保,可将食物直接置于其上,与食品不粘粘。还可直接放于洗碗机中清洗,可重复使用。
本发明用于稀释食品级液体硅胶的稀释剂与食品级液体硅胶的混合投料质量比为30︰100。合适的稀释配比,利于将硅胶附着于玻璃纤维布上,使最终产品具有一定的厚度和质感。
本发明用于稀释食品级液体硅胶的稀释剂为120号溶剂汽油。该稀释剂可在高温后挥发,以确保最终产品的无毒性和环保性。
具体实施方式
一、制备胶体
将100kg的食品级液体硅胶和30kg的120号溶剂汽油均匀混合,置于胶槽中。
二、生产工艺
放卷,将无腊的玻璃纤维布自胶槽中浸透后,经60~120℃烘箱反复烘干,再经压光机成型硫化,同时将硫化定型后的连续的垫体收卷。
三、裁片
将硫化后的垫体整卷放卷,置于分切机上,按客户要求的形状、尺寸裁成片。
四、高温处理
将裁片后的垫体于220℃高温处理3~4小时,检测通过即成正品。

Claims (3)

1.硅胶烘烤垫的生产方法,其特征在于将食品级液体硅胶稀释后置于胶槽中,将无腊玻璃纤维布自胶槽中浸透后,于60~120℃烘箱烘干,经压光机压光成型硫化,再经裁片后,于220℃高温处理3~4小时。
2.根据权利要求1所述硅胶烘烤垫的生产方法,其特征在于用于稀释食品级液体硅胶的稀释剂与食品级液体硅胶的混合投料质量比为30︰100。
3.根据权利要求1或2所述硅胶烘烤垫的生产方法,其特征在于用于稀释食品级液体硅胶的稀释剂为120号溶剂汽油。
CN201010545999XA 2010-11-17 2010-11-17 硅胶烘烤垫的生产方法 Pending CN102059809A (zh)