CN101805997A - 一种新型的纯棉厚重织物平幅短流程前处理工艺 - Google Patents

一种新型的纯棉厚重织物平幅短流程前处理工艺 Download PDF

Info

Publication number
CN101805997A
CN101805997A CN201010126935A CN201010126935A CN101805997A CN 101805997 A CN101805997 A CN 101805997A CN 201010126935 A CN201010126935 A CN 201010126935A CN 201010126935 A CN201010126935 A CN 201010126935A CN 101805997 A CN101805997 A CN 101805997A
Authority
CN
China
Prior art keywords
fabric
pure cotton
pretreatment process
cotton fabric
novel open
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010126935A
Other languages
English (en)
Inventor
陈晓华
吴中杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHAOXING ZHIREN TEXTILE PRINTING CO Ltd
Original Assignee
SHAOXING ZHIREN TEXTILE PRINTING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHAOXING ZHIREN TEXTILE PRINTING CO Ltd filed Critical SHAOXING ZHIREN TEXTILE PRINTING CO Ltd
Priority to CN201010126935A priority Critical patent/CN101805997A/zh
Publication of CN101805997A publication Critical patent/CN101805997A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种新型的纯棉厚重织物平幅短流程前处理工艺。本发明包括如下步骤:(1)配制处理液;(2)织物通过浸轧30-100℃处理液,进蒸箱,采用液煮堆置或汽蒸堆置30-100分钟,后进行水洗、烘干,即完成前处理工艺;处理液的pH值在6-10之间。本发明具有如下的有益效果:本发明的工艺对厚重织物前处理达到了一步完成。缩短工艺流程,节约人力,提高生产效率;同时由于大量减小使用液碱,双氧水的用量增加,大大的降低了废水的COD值。经本发明工艺处理的产品,各项前处理指标,达到生产要求,同时白度、强力、减量等指标优于传统工艺处理方法。

Description

一种新型的纯棉厚重织物平幅短流程前处理工艺
技术领域
本发明涉及一种新型的纯棉厚重织物平幅短流程前处理工艺。
背景技术
纯棉织物的前处理主要是去除织物上的浆料、天然杂质、蜡质、棉籽壳等。织物的浆料的主要成份是淀粉、PVA、聚丙烯酰胺类高分厂化合物;棉纤维中存在的杂质主是果胶杂、蜡质、色素、矿物盐等。
纯棉织物的前处理生产工艺,传统上一直采用高温强碱的化学方法进行处理,这种工艺要消耗大量的能源、水源、并产生大量对环境有害的物质。对薄型织物而言,可以采用酶氧一浴法进行处理,但对厚重织物(厚重织物是指克重大于250克/平方米或纱支小于40S))的酶氧一浴法的前处理,由于厚型织物比薄型织物在组织结构上更为紧密,浆料、杂质含量更高,前处理更为困难,采用酶氧一浴法进行前处理时工艺不稳定,得不到前处理效果稳定的半制品。致使酶氧一浴法在生产小于棉40S织物时或克重超过250克以上中厚型织物时,即无法得到有效应用。
发明内容
本发明的目的在于克服现有技术存在的不足,提供一种新型的纯棉厚重织物平幅短流程前处理工艺。本发明工艺具有绿色、环保、生产效率高,降低了生产成本等优点。
为达到上述目的,本发明采取了如下的技术方案:
一种新型的纯棉厚重织物平幅短流程前处理工艺,包括如下步骤:
(1)配制处理液:
(2)织物通过浸轧30-100℃处理液,进蒸箱,采用液煮堆置或汽蒸堆置30-100分钟,后进行水洗、烘干,即完成前处理工艺;处理液的pH值在6-10之间。
处理液温度为优选为60-80℃;处理液的pH值优选为9-10。
上述技术方案中,处理液包括代碱剂、双氧水及水,其组成为:代碱剂的浓度为5-50克/升,优选浓度为20-30克/升;双氧水的浓度为5-15克/升,优选浓度为9-10克/升。
本发明的代碱剂产品可使用的市场上目前销售的一些代碱剂产品,如常州市金源绿色化工助剂厂生产的的标号为CB-98的产品。
在处理液中,也可以加入硫酸钠、净水剂,不需加其它类助剂,如稳定剂、分散剂。加入硫酸钠、净水剂的重量用量为0.1-5%,最好为0.5-2%。
与现有技术相比,本发明具有如下的有益效果:
本发明的工艺对厚重织物前处理达到了一步完成。缩短工艺流程,节约人力,提高生产效率;同时由于大量减小使用液碱,双氧水的用量增加,大大的降低了废水的COD值。经本发明工艺处理的产品,各项前处理指标,达到生产要求,同时白度、强力、减量等指标优于传统工艺处理方法。
具体实施方式
以下通过具体实施例来对本发明作进一步的描述。
实施例1:
按照下述配方制备处理液,然后将全棉纱卡21*16/128*60坯布门幅63”,浸轧处理液(60℃),进L-BOX进行堆置、液煮102℃*50分钟。然后出L-BOX,进过三次高效平洗。经纯棉厚重织物平幅短流程前处理工艺处理的织物性能对比见表1。
配方:
代碱剂CB-98:30g/l
双氧水:9g/l。
实施例2:
按实施例1的处方及工艺,在相同的条件下处理全棉帆布21*7/78*30 60”,经纯棉厚重织物平幅短流程前处理工艺处理的织物性能对比见表2。
表1:经纯棉厚重织物平幅短流程前处理工艺处理的织物性能
处理工艺 白度   毛效(cm/30min)   强力(N)经向/纬向 失重(%) 手感
  传统工艺   76.8   11.5   1146/486   -6.2   比较硬
  短流程   80.1   11.6   1184/500   -4.2   柔软
表2:经纯棉厚重织物平幅短流程前处理工艺处理的织物性能
处理工艺 白度   毛效(cm/30min)   强力(N)经向/纬向 失重(%) 手感
  传统工艺   76.8   11.5   1103/380   -5.2   比较硬
  短流程   80.1   11.6   1150/450   -4.1   柔软

Claims (6)

1.一种新型的纯棉厚重织物平幅短流程前处理工艺,其特征在于:包括如下步骤:
(1)配制处理液:
(2)织物通过浸轧30-100℃处理液,进蒸箱,采用液煮堆置或汽蒸堆置30-100分钟,后进行水洗、烘干,即完成前处理工艺;处理液的pH值在6-10之间。
2.根据权利要求1所述的新型的纯棉厚重织物平幅短流程前处理工艺,其特征在于:处理液温度为60-80℃。
3.根据权利要求1所述的新型的纯棉厚重织物平幅短流程前处理工艺,其特征在于:处理液的pH值在9-10。
4.根据权利要求1所述的新型的纯棉厚重织物平幅短流程前处理工艺,其特征在于:
处理液包括代碱剂、双氧水及水,其组成为:代碱剂的浓度为5-50克/升,双氧水的浓度为5-15克/升。
5.根据权利要求4所述的新型的纯棉厚重织物平幅短流程前处理工艺,其特征在于:
代碱剂的浓度为20-30克/升;双氧水的浓度为9-10克/升。
6.根据权利要求4或5所述的新型的纯棉厚重织物平幅短流程前处理工艺,其特征在于:所述的代碱剂为常州市金源绿色化工助剂厂生产的的标号为CB-98的产品。
CN201010126935A 2010-03-18 2010-03-18 一种新型的纯棉厚重织物平幅短流程前处理工艺 Pending CN101805997A (zh)