CN101718005B - 抗菌耐老化网衣 - Google Patents

抗菌耐老化网衣 Download PDF

Info

Publication number
CN101718005B
CN101718005B CN2009102305446A CN200910230544A CN101718005B CN 101718005 B CN101718005 B CN 101718005B CN 2009102305446 A CN2009102305446 A CN 2009102305446A CN 200910230544 A CN200910230544 A CN 200910230544A CN 101718005 B CN101718005 B CN 101718005B
Authority
CN
China
Prior art keywords
polyethylene
kilograms
resistant
master batch
etting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009102305446A
Other languages
English (en)
Other versions
CN101718005A (zh
Inventor
景发岐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG SHENGBON PLASTIC PIPE SYSTEM GROUP CO Ltd
Original Assignee
SHANDONG SHENGBON PLASTIC PIPE SYSTEM GROUP CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG SHENGBON PLASTIC PIPE SYSTEM GROUP CO Ltd filed Critical SHANDONG SHENGBON PLASTIC PIPE SYSTEM GROUP CO Ltd
Priority to CN2009102305446A priority Critical patent/CN101718005B/zh
Publication of CN101718005A publication Critical patent/CN101718005A/zh
Application granted granted Critical
Publication of CN101718005B publication Critical patent/CN101718005B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种聚乙烯抗菌耐老化网衣制做技术。其技术方案是:利用聚乙烯基料,添加抗菌剂(兼具增重作用)、耐老化助剂及加工助剂,按比例造粒为母料,然后与聚乙烯原料按一定比例混合生产聚乙烯网衣用丝线,并织成聚乙烯网衣,提高聚乙烯网衣的抗菌、耐老化性能,延长网衣的使用寿命;同时改变聚乙烯网衣的浮力,使聚乙烯网衣下沉或悬浮于水中。

Description

抗菌耐老化网衣
技术领域:
本发明涉及聚乙烯网衣制品领域中的一种抗菌耐老化聚乙烯网衣。
现有技术:
现有聚乙烯网衣主要采用聚乙烯基料经拉丝及织结而成,其抗菌耐老化性能较差,长期使用受海洋生物污损严重,且网衣使用寿命较短,一般为3至5年;同时,现有聚乙烯网衣易漂浮,不利于网衣固定。
发明内容:
本发明目的是针对现有技术存在的缺陷,为提高网衣抗菌耐老化性能及易漂浮的特点,结合抗菌剂、耐老化助剂、加工助剂对聚乙烯基料进行改性,研究成功了具有较好抗菌、耐老化性能且不易漂浮的抗菌耐老化网衣。
此发明技术方案是:以(4.5%-5.5%)的氧化铝、(4.5%-5.5%)黑色母(PE2747)、(1%-1.1%)的加工助剂(PPA)以及(80.1%-89%)高密度聚乙烯原料(YGH041)(质量百分比)经混合造粒成为抗菌、耐老化功能母料,然后将功能母料与拉丝级聚乙烯基料按(15%-40%)比例混合生产聚乙烯网衣丝线,最后织结成聚乙烯网衣。
工艺流程:氧化铝和黑色母、加工助剂、高密度聚乙烯四种原料挤出造粒作为功能母料,然后将功能母料与拉丝聚乙烯基料按比例混合生产聚乙烯网衣丝线,最后织结成聚乙烯网衣。
在本发明的技术方案中,充分利用氧化铝的抗菌抑菌性能及密度大的特点、黑色母的耐老化性能,结合加工助剂PPA对聚乙烯基料进行造粒改性,研究开发出一种具有较好抗菌、耐老化性能聚乙烯网衣,同时,改变聚乙烯网衣在水中的浮力。该网衣在抗菌、耐老化方面性能优异,且可下沉或悬浮于海水中,具有良好的应用前景。
具体实施方式:
实施例1,将4.5千克氧化铝、5.5千克黑色母PE2747、1千克加工助剂(PPA)及89千克高密度聚乙烯原料(YGH041)混合均匀,然后挤出造粒为功能母料,将功能母料与拉丝聚乙烯原料按一定100千克:500千克比例混合拉成聚乙烯网衣丝线,最后织成聚乙烯网衣。
实施例2,将5.5千克氧化铝、5.5千克黑色母PE2747、1.1千克加工助剂(PPA)及87.9千克高密度聚乙烯原料(YGH041)混合均匀,然后挤出造粒为功能母料,将功能母料与拉丝聚乙烯原料按一定100千克:300千克比例混合拉成聚乙烯网衣丝线,最后织成聚乙烯网衣。
实施例3,将5千克氧化铝、5千克黑色母PE2747、1千克加工助剂(PPA)及89千克高密度聚乙烯原料(YGH041)混合均匀,然后挤出造粒为功能母料,将功能母料与拉丝聚乙烯原料按一定100千克:450千克比例混合拉成聚乙烯网衣丝线,最后织成聚乙烯网衣。
说明:上述实施例中,采用拉丝级聚乙烯原料,保证聚乙烯网衣具有良好的物理力学性能。抗菌剂成份为氧化铝粉末,具有良好的抗菌抑菌作用;同时,氧化铝粉末具有增重作用,可增加网衣重量,改变聚乙烯网衣的浮力,使聚乙烯网衣可下沉或悬浮于海水中。耐老化助剂采用卡博特黑色母粒PE2747,该母料具有良好的抗老化功能。加工助剂为PPA,其主要作用为保证混合原料具有良好的加工性能。

Claims (3)

1.一种抗菌耐老化网衣,其特征是:将4.5千克氧化铝、5.5千克耐老化助剂、1千克加工助剂及89千克高密度聚乙烯原料混合均匀,然后挤出造粒为功能母料,将功能母料与拉丝聚乙烯原料按100千克:500千克比例混合拉成聚乙烯网衣丝线,最后织成聚乙烯网衣;
所述耐老化助剂为黑色母PE2747,加工助剂产品型号为PPA,高密度聚乙烯产品型号为YGH041。
2.一种抗菌耐老化网衣,其特征是:将5.5千克氧化铝、5.5千克耐老化助剂、1.1千克加工助剂及87.9千克高密度聚乙烯原料混合均匀,然后挤出造粒为功能母料,将功能母料与拉丝聚乙烯原料按100千克:300千克比例混合拉成聚乙烯网衣丝线,最后织成聚乙烯网衣;
所述耐老化助剂为黑色母PE2747,加工助剂产品型号为PPA,高密度聚乙烯产品型号为YGH041。
3.一种抗菌耐老化网衣,其特征是:将5千克氧化铝、5千克耐老化助剂、1千克加工助剂及89千克高密度聚乙烯原料混合均匀,然后挤出造粒为功能母料,将功能母料与拉丝聚乙烯原料按100千克:450千克比例混合拉成聚乙烯网衣丝线,最后织成聚乙烯网衣;
所述耐老化助剂为黑色母PE2747,加工助剂产品型号为PPA,高密度聚乙烯产品型号为YGH041。
CN2009102305446A 2009-11-27 2009-11-27 抗菌耐老化网衣 Expired - Fee Related CN101718005B (zh)