Prior art keywords
copper
ore
gram
tons
atacamite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN 200910038842
Other languages
English (en)
Other versions
CN101524669A (zh
Inventor
胡真
李汉文
张慧
陈志强
陈治泉
严更生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WENGYUAN HONGLING MINING CO., LTD.
Original Assignee
Guangzhou Research Institute of Non Ferrous Metals
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Research Institute of Non Ferrous Metals filed Critical Guangzhou Research Institute of Non Ferrous Metals
Priority to CN 200910038842 priority Critical patent/CN101524669B/zh
Publication of CN101524669A publication Critical patent/CN101524669A/zh
Application granted granted Critical
Publication of CN101524669B publication Critical patent/CN101524669B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Landscapes

  • Manufacture And Refinement Of Metals (AREA)

Abstract

一种以卤化物形式存在的铜矿物的选矿方法。其特征是将氯铜矿原矿粉碎到-0.074;加入矿浆调整剂,捕收剂,起泡剂,进行粗选,得到粗选精矿和粗选尾矿;精选粗选精矿,获得铜精矿和精选中矿,精选中矿回收再精选;粗选尾矿加入捕收剂扫选,得到扫选中矿和尾矿,扫选中矿回收进入氯铜矿的粗选。本发明的选矿方法获得的铜精矿铜品位大于20%,铜回收率大于68%,可回收铜的回收率大于90%。本发明的选矿方法是一种低成本,少污染的以卤化物形式存在的铜矿物的选矿方法。

Description

一种以卤化物形式存在的铜矿物的选矿方法
技术领域
本发明涉及一种稀有矿物的选矿方法,特别涉及一种以卤化物形式存在的铜矿物-氯铜矿的选矿方法。
背景技术
铜在自然界形成的矿物有两百多种,其中以卤化物形式存在的铜矿物,如氯铜矿、碘铜矿、羟氯铜矿等却很少,仅国外有少量报导。
氯铜矿【Cu2Cl(OH)3】是一种稀有矿物,是含铜硫化物经氧化后所产生的硫酸铜溶液与下渗的含卤族元素的地面水反应而成的次生矿铜矿物。斜方晶系。柱状、板状晶体,纤维状、放射状、粒状、块状等集合体。颜色有美绿色、翠绿色或黑绿色。玻璃光泽到金属光泽,透明到半透明。硬度3~3.5,比重3.76。
由于氯铜矿的颜色、光泽和晶形等物理特征和产状特征均类似于孔雀石,与孔雀石在外观上非常相似,肉眼难以区分,显微镜下也不易分辨,因此常将其误认为孔雀石。采用选别孔雀石的硫化-浮选,即用硫、硫化钠或硫化氢钠等作氧化铜矿物的硫化剂的常规氧化铜矿的选矿方法进行选别,造成矿石中硫化铜矿被抑制,铜回收率低、铜精矿表面透明的金属绿色被破坏的、矿山环境污染等问题。
发明内容
本发明的目的提供一种低成本,少污染的以卤化物形式存在的铜矿物的选矿方法。
本发明的选矿方法由以下步骤组成:①将氯铜矿原矿粉碎到-0.074毫米占55~75%;②加入矿浆调整剂200~1000克/吨,捕收剂100~400克/吨,起泡剂20~40克/吨,进行粗选,得到粗选精矿和粗选尾矿;③两次空白精选粗选精矿,获得铜精矿和精选中矿,精选中矿回收再精选;④粗选尾矿加入捕收剂20~50克/吨,两次扫选,得到扫选中矿和尾矿,扫选中矿回收进入氯铜矿的粗选。
所述矿浆调整剂为碳酸钠、氢氧化钠或石灰。
所述捕收剂为丁基黄药、丁胺黑药或乙硫氮。
所述起泡剂为2号油、煤油或柴油。
本发明的原矿铜品位为0.38~0.55%,铜物相分析结果表明,结合铜占有率18~25%。主要铜矿物以卤化物氯铜矿为主,少量金属硫化矿物-黄铜矿,黄铁矿,极少量的斑铜矿,蓝辉铜矿,铜蓝。其它金属氧化矿物为磁铁矿,赤铁矿,褐铁矿,钛铁矿。脉石矿物为石英,长石,绿泥石,绢云母,方解石、白云石,少量高岭石、锆石等。
本发明具有如下优点:利用氯铜矿与脉石矿物自然的可浮选差异,只加铜矿物的捕收剂和起泡剂,实现了铜矿物与脉石矿物的分离。由于流程中不加硫化剂,保持了铜精矿表面翠绿色半透明的金属光泽,避免了硫化剂对矿石中硫化铜矿物(例如黄铜矿)的抑制,并减少了硫化剂对矿山环境的污染。结果表明,以卤化物形式存在的铜矿物氯铜矿,虽然分子式中有(OH)3的存在,但其可浮选比氧化铜矿物强,不需要硫化剂对其进行硫化,只要选择合适的介质调整剂和捕收剂,就能够从脉石矿中将铜矿物有效富集。本发明的选矿方法获得的铜精矿铜品位大于20%,铜回收率大于68%,可回收铜的回收率大于90%。
附图说明
图1是本发明的选矿流程图。
图2本发明选矿所获得的氯铜矿精矿。
图3硫化-浮选所获得的氯铜矿精矿。
具体实施方式
实施例1
原矿铜品位为0.42%,结合铜占有率为19%的某氯化铜矿。粉碎到-0.074毫米占55%,单体解离度大于70%;加入碳酸钠200克/吨,丁基黄药400克/吨,2号油40克/吨,进行氯铜矿的粗选,得到粗选精矿和粗选尾矿;粗选精矿两次空白精选获得铜精矿和精选中矿。铜精矿铜品位为32.49%,铜回收率73.62%,可回收铜的回收率为90.89%。精选中矿进入回路再选;粗选尾矿加入丁基黄药50克/吨,进行两次扫选,得到扫选中矿和尾矿,扫选中矿进入氯铜矿的粗选。尾矿铜品位较低,达到氯铜矿与脉石矿物的分离。
实施例2
原矿铜品位为0.44%,结合铜占有率为20%的某氯化铜矿。粉碎到-0.074毫米占70%,单体解离度大于90%;加入氢氧化钠1000克/吨,丁胺黑药200克/吨,煤油30克/吨,进行氯铜矿的粗选,得到粗选精矿和粗选尾矿;粗选精矿两次空白精选获得铜精矿和精选中矿。铜精矿铜品位为29.28%,铜回收率74.56%,可回收铜的回收率为93.20%。精选中矿进入回路再选;粗选尾矿加入丁胺黑药30克/吨,进行两次扫选,得到扫选中矿和尾矿,扫选中矿进入氯铜矿的粗选。
实施例3
原矿铜品位为0.38%,结合铜占有率为25%的某氯化铜矿。粉碎到-0.074毫米占65%,单体解离度大于80%;加入石灰800克/吨,乙硫氮300克/吨,柴油40克/吨,进行氯铜矿的粗选,得到粗选精矿和粗选尾矿;粗选精矿两次空白精选获得铜精矿和精选中矿。铜精矿铜品位为24.49%,铜回收率68.85%,可回收铜的回收率为91.80%。精选中矿进入回路再选;粗选尾矿加入乙硫氮30克/吨,进行两次扫选,得到扫选中矿和尾矿,扫选中矿进入氯铜矿的粗选。

Claims (4)

1.一种以卤化物形式存在的铜矿物的选矿方法,其特征是①将氯铜矿原矿粉碎到-0.074毫米占55~75%;②加入矿浆调整剂200~1000克/吨,捕收剂100~400克/吨,起泡剂20~40克/吨,进行粗选,得到粗选精矿和粗选尾矿;③两次空白精选粗选精矿,获得铜精矿和精选中矿,精选中矿回收再精选;④粗选尾矿加入捕收剂20~50克/吨,两次扫选,得到扫选中矿和尾矿,扫选中矿回收进入氯铜矿的粗选。
2.根据权利要求1所述的一种以卤化物形式存在的铜矿物的选矿方法,其特征是所述的矿浆调整剂为碳酸钠、氢氧化钠或石灰。
3.根据权利要求1所述的一种以卤化物形式存在的铜矿物的选矿方法,其特征是所述的捕收剂为丁基黄药、丁胺黑药或乙硫氮。
4.根据权利要求1所述的一种以卤化物形式存在的铜矿物的选矿方法,其特征是所述的起泡剂为2号油、煤油或柴油。
CN 200910038842 2009-04-21 2009-04-21 一种以卤化物形式存在的铜矿物的选矿方法 Active CN101524669B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 200910038842 CN101524669B (zh) 2009-04-21 2009-04-21 一种以卤化物形式存在的铜矿物的选矿方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 200910038842 CN101524669B (zh) 2009-04-21 2009-04-21 一种以卤化物形式存在的铜矿物的选矿方法

Publications (2)

Publication Number Publication Date
CN101524669A CN101524669A (zh) 2009-09-09
CN101524669B true CN101524669B (zh) 2012-12-26

Family

ID=41092826

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 200910038842 Active CN101524669B (zh) 2009-04-21 2009-04-21 一种以卤化物形式存在的铜矿物的选矿方法

Country Status (1)

Country Link
CN (1) CN101524669B (zh)

Families Citing this family (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101871044B (zh) * 2010-05-29 2011-08-03 大冶有色设计研究院有限公司 一种高次生泥铜混合矿石矿物加工方法
CN102019232A (zh) * 2010-11-29 2011-04-20 广州有色金属研究院 一种亚甲基双(二丁基二硫代氨基甲酸酯)的用途
CN102205274A (zh) * 2011-03-23 2011-10-05 昆明理工大学 氧化铜矿浮选体系硫化过程抗抑制的方法
CN106170343B (zh) * 2013-11-26 2017-10-17 华北理工大学 一种黄铜矿的选矿方法
US9885095B2 (en) 2014-01-31 2018-02-06 Goldcorp Inc. Process for separation of at least one metal sulfide from a mixed sulfide ore or concentrate
CN105413879B (zh) * 2015-12-08 2018-01-16 中南大学 一种黄铜矿与黄铁矿的浮选分离方法
CN111330740B (zh) * 2020-03-05 2021-10-15 中南大学 一种提高含镁层状硅酸盐矿物与硫化铜矿物浮选分离效率的方法
CN112337652B (zh) * 2020-10-19 2022-06-03 沈阳有色金属研究院有限公司 一种从氧化铜矿中浮选硫化铜的捕收剂及应用

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1651148A (zh) * 2005-02-04 2005-08-10 吉林吉恩镍业股份有限公司 硫化镍、铜尾矿综合回收工艺
CN101172267A (zh) * 2007-12-03 2008-05-07 西部矿业股份有限公司 一种提高复杂硫化铜矿矿石浮选指标的工艺

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1651148A (zh) * 2005-02-04 2005-08-10 吉林吉恩镍业股份有限公司 硫化镍、铜尾矿综合回收工艺
CN101172267A (zh) * 2007-12-03 2008-05-07 西部矿业股份有限公司 一种提高复杂硫化铜矿矿石浮选指标的工艺

Non-Patent Citations (5)

* Cited by examiner, † Cited by third party
Title
刘守信等.云南某氧化铜矿德选矿试验.《矿冶》.2007,第16卷(第4期),14-16. *
李崇德等.永平铜矿铜硫浮选工艺技术进展.《有色金属(选矿部分)》.2000,(第2期),5-10. *
程琼.氧化铜矿浮选方法研究.《矿产保护与利用》.2005,(第5期),32-35. *
赵福刚等.铜矿的选矿技术发展.《铜业工程》.2006,(第4期),13-18. *
金锐等.复杂铜冶炼渣浮选试验研究.《江西有色冶金》.2009,第23卷(第1期),12-14. *

Also Published As

Publication number Publication date
CN101524669A (zh) 2009-09-09

Similar Documents

Publication Publication Date Title
CN101524669B (zh) 一种以卤化物形式存在的铜矿物的选矿方法
CN101537388B (zh) 一种铋钼铜硫混合精矿的分离方法
CN101585017B (zh) 一种难选铜锌硫矿的选矿方法
CN105413854A (zh) 一种高氧化率铜钼共生矿的选矿方法
CN102218376B (zh) 一种高碳钼镍矿高效浮选分离回收钼镍的方法
CN102029220B (zh) 低品位复杂铅锑锌分离浮选的方法
CN101549326B (zh) 一种难选铜锌硫化矿浮选分离的工艺
CN102896037B (zh) 一种矿石中含离子态铜钴镍矿的选矿方法
CN111617880B (zh) 一种高砷铅锌矿的选矿方法
CN101254484A (zh) 一种复杂硫化矿的高效清洁选矿方法
CN101884951A (zh) 细粒和微细粒锡石联合选矿工艺
CN109092563A (zh) 一种高硫铅锌矿高效浮选的方法
CN101259451B (zh) 一种选矿捕收剂的制备方法
CN104209183A (zh) 一种彩钼铅矿的选矿方法
CN101402071A (zh) 铜铅锌硫化矿电位调控优先浮选工艺
CN103386359A (zh) 一种氧化铜钴矿的选矿方法
Asadi et al. A successful operational initiative in copper oxide flotation: Sequential sulphidisation-flotation technique
CN102029221B (zh) 一种多金属矿石选别工艺
CN102764701B (zh) 一种高泥质碱性脉石氧化铜矿浮选方法
CN1017686B (zh) 一种从含铜、铅、锌多金属复杂硫化矿中浮选铜精矿的方法
CN110947523B (zh) 一种从选铁尾矿中回收铜铅锌矿物的捕收剂
CN1215909C (zh) 一种浮选硫化铜矿石的捕收剂
CN108262156A (zh) 高泥质高碱性脉石低品位难选氧化铜矿的选矿方法
Lager et al. Current processing technology for antimony-bearing ores a review, part 2
O'Connor et al. The practice of pyrite flotation in South Africa and Australia

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20180207

Address after: 510651 Changxin Road, Guangzhou, Guangdong, No. 363, No.

Patentee after: GUANGDONG INSTITUTE OF RESOURCES COMPREHENSIVE UTILIZATION

Address before: 510651 Changxin Road, Guangzhou, Guangdong, No. 363, No.

Patentee before: Guangzhou Research Institute of Non-ferrous Metals

CB03 Change of inventor or designer information
CB03 Change of inventor or designer information

Inventor after: Yi Jinwu

Inventor after: Zhang Hui

Inventor after: Chen Zhiqiang

Inventor after: Chen Zhiquan

Inventor after: Yan Gengsheng

Inventor after: Cui Zeqi

Inventor after: Lin Yongsheng

Inventor after: Zhang Xueyi

Inventor after: Luo Rengui

Inventor after: Gong Nairui

Inventor after: Chen Lunliang

Inventor after: Hu Zhen

Inventor after: Li Hanwen

Inventor before: Hu Zhen

Inventor before: Li Hanwen

Inventor before: Zhang Hui

Inventor before: Chen Zhiqiang

Inventor before: Chen Zhiquan

Inventor before: Yan Gengsheng

TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20180509

Address after: 512638 Hongling mine of Jiangwei Town, Wengyuan County, Guangdong

Patentee after: WENGYUAN HONGLING MINING CO., LTD.

Address before: 510651 Changxin Road, Tianhe District, Guangzhou, Guangdong Province, No. 363

Patentee before: GUANGDONG INSTITUTE OF RESOURCES COMPREHENSIVE UTILIZATION