CN101289587B - 一种用于无水胶印油墨的连接料 - Google Patents
一种用于无水胶印油墨的连接料 Download PDFInfo
- Publication number
- CN101289587B CN101289587B CN 200710172397 CN200710172397A CN101289587B CN 101289587 B CN101289587 B CN 101289587B CN 200710172397 CN200710172397 CN 200710172397 CN 200710172397 A CN200710172397 A CN 200710172397A CN 101289587 B CN101289587 B CN 101289587B
- Authority
- CN
- China
- Prior art keywords
- portions
- ink
- printing
- oil
- high boiling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明为一种无水胶印油墨连接料,其特征在于,该连接料的重量配比为:酚醛树脂30-55%;苯酐2-10%;长油度醇酸5-10%;植物油10-25%;高沸点矿油15-30%;以及助剂0.1-2%。其中,高沸点矿油为沸点240-320度的石油馏分。本发明连接料的内聚能较高,而且粘弹性和流动性较佳,因此采用本发明制成的油墨在印刷后网点还原性能好,印刷质量令人满意。
Description
技术领域
本发明涉及油墨的连接料,尤其是一种用于无水胶印油墨的连接料。
背景技术
油墨由颜料、连接料、填料、附加料等组成。连接料,俗称调墨油,是油墨的主要组成成分,起着分散颜料,给予油墨以适当的粘着、流动性和转印性能,以及印刷后通过成膜使颜料固着于印刷品表面的作用。
油墨的流变性、粘度、中性、酸值、色泽、抗水性以及印刷性能等主要取决于连接料,同一种颜料,使用不同的连接料,可制成不同类型的油墨;而同一种连接料,使用不同的颜料。所制成的仍为同一类型的油墨,因它不能改变油墨的根本性能,所以油墨的质量好坏,除与颜料有关外,主要取决于连接料。
现有的无水胶印油墨中的连接料与普通胶印油墨中所用的相似,常用的松香改性酚醛树脂、胶质化松香改性酚醛树脂及用亚麻油等植物油改性醉酸树脂等为主体。但由于无水胶印过程中没有润版液的冷却,油墨印刷过程对温度的敏感性相对较高,因而对组成油墨的树脂有特殊流变学性能要求。一般要求比普通胶印油墨的粘弹性要高些,而性状要略柔软些,也就是说流动性要好。这两者是有矛盾的,但力求找到一个合适的平衡范围是油墨配方的重点。此外,树脂连结料要有适当的高内聚能物质这样才能促使油墨完整、清洁地从印版上和橡皮布上实现剥离和转移。
发明内容
本发明在于提供一种无水胶印油墨连接料,其具有高粘弹性和较好的流动性,并具有高内聚能,从而能达到更佳的印刷效果。
为实现上述目的,本发明提供一种无水胶印油墨连接料,其其重量配比为:
酚醛树脂30-55%;
苯酐2-10%;
长油度醇酸5-10%;
植物油10-25%;
高沸点矿油15-30%;以及
助剂0.1-2%。
较佳地,高沸点矿油为沸点240-320度的石油馏分。
将按照以下的重量配比,用本发明的连接料制成的无水胶印油墨与现有的无水胶印油墨相比较:
连接料50-70%;
颜料13-20%;
油墨油5-15%;以及
助剂5-15%。
印刷承印物:铜版纸
印刷速度:8000张/小时
测定结果:
表一:网点扩大表
本发明 | 对照例 | |||||||
Y | M | C | BK | Y | M | C | BK | |
0% | 0 | 0 | 0 | 0 | 1 | 0 | 0 | 0 |
15% | 23 | 25 | 24 | 25 | 26 | 25 | 25 | 29 |
25% | 37 | 39 | 38 | 38 | 40 | 38 | 36 | 44 |
50% | 66 | 67 | 66 | 66 | 67 | 66 | 65 | 71 |
75% | 86 | 87 | 86 | 87 | 86 | 86 | 87 | 91 |
100% | 100 | 100 | 100 | 100 | 100 | 100 | 100 | 100 |
上表中:Y、M、C和BK分别代表黄色、红色、蓝色和黑色。
由于本发明的连接料的内聚能较高,而且粘弹性和流动性较佳,因此从上表可以看出,采用本发明制成的油墨在印刷后网点还原性能好,印刷质量令人满意。
具体实施方式
本发明为一种无水胶印油墨连接料,其重量配比为:
酚醛树脂30-55%,较佳为45%;
苯酐2-10%,较佳为6%;
长油度醇酸5-10%,较佳为8%;
植物油10-25%,较佳为18%;
高沸点矿油15-30%,较佳为22%;以及
助剂0.1-2%,较佳为1%。
上述的高沸点矿油为沸点为240-320度的石油馏分。
本发明的连接料制造工艺如下:
1.在反应釜中加入植物油、酚醛树脂和苯酐;
2.在150-220度的温度范围内,以转速100-300RPM搅拌30-60分钟;
3.在搅拌后的物料中加入部分(例如40%、50%或60%)高沸点矿物油、醇酸和助剂,在130-180度的温度范围内,以转速100-300RPM搅拌30-60分钟;
4.加入剩余的矿物油(例如60%、50%或40%),将连接料调整到规定的指标范围内;
5.出料至油墨配料处,进行油墨的进一步操作。
Claims (1)
1.一种无水胶印油墨连接料,其特征在于,该连接料的重量配比为:
酚醛树脂30-55%;
苯酐2-10%;
长油度醇酸5-10%;
植物油10-25%;
高沸点矿油15-30%;以及
助剂0.1-2%;
其中所述高沸点矿油为沸点240-320度的石油馏分。