AT159679B - Magnesiumlegierung. - Google Patents

Magnesiumlegierung.

Info

Publication number
AT159679B
AT159679B AT159679DA AT159679B AT 159679 B AT159679 B AT 159679B AT 159679D A AT159679D A AT 159679DA AT 159679 B AT159679 B AT 159679B
Authority
AT
Austria
Prior art keywords
magnesium alloy
magnesium
alloys
phosphorus
corrosion resistance
Prior art date
Application number
Other languages
English (en)
Inventor
Roland Dr Mitsche
Robert Dr Mueller
Original Assignee
Roland Dr Mitsche
Robert Dr Mueller
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Roland Dr Mitsche, Robert Dr Mueller filed Critical Roland Dr Mitsche
Application granted granted Critical
Publication of AT159679B publication Critical patent/AT159679B/de

Description


   <Desc/Clms Page number 1> 
 



    Magnesiumlegierung.   
 EMI1.1 
 

 <Desc/Clms Page number 2> 

 
 EMI2.1 
 widerstand und hohe Korrosionsbeständigkeit aufweisen. 



   In manchen Fällen sind auch höhere Phosphorzusätze zweckmässig. Die bereits erwähnte Le- 
 EMI2.2 
 ein besonders gutes Korrosionsverhalten, wenn die korrodierende Flüssigkeit die Proben abwechselnd vollkommen bedeckt und dann wieder freigibt. 
 EMI2.3 
 Festigkeit und Dehnung bei guter Korrosionsbeständigkeit. 



   Höhere Phosphorzusätze als 3% haben sich bei den untersuchten Legierungen nicht als zweckmässig herausgestellt, soweit es sich um Verbesserung der Korrosionsbeständigkeit handelt. Die unter- 
 EMI2.4 
 bis 40% Cu und bis 6% Be. Dabei ist aber darauf hinzuweisen, dass es z. B. nicht möglich war,   rei     binäre Mg-Be-Legierungen   herzustellen. Hingegen ist es möglich, Beryllium in ternäre und komplexe Magnesiumlegierungen einzuführen. 



   PATENT-ANSPRÜCHE :
1.   Magnesiumlegierung,   gekennzeichnet durch einen Phosphorgehalt bis zu 25% und gegebenenfalls mit einem Kupfergehalt bis zu 40%, Rest Magnesium. 
 EMI2.5 


AT159679D 1935-10-22 1935-10-22 Magnesiumlegierung. AT159679B (de)