Prior art keywords
active material
manufacturing
electrode
electrode material
treatment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2023/027221
Other languages
English (en)
French (fr)
Japanese (ja)
Inventor
行央 高野
英二郎 岩瀬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujifilm Corp
Original Assignee
Fujifilm Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fujifilm Corp filed Critical Fujifilm Corp
Priority to CN202380055001.3A priority Critical patent/CN119585880A/zh
Priority to EP23846516.5A priority patent/EP4564467A4/en
Priority to JP2024537749A priority patent/JPWO2024024786A1/ja
Publication of WO2024024786A1 publication Critical patent/WO2024024786A1/ja
Priority to US19/015,659 priority patent/US20250149577A1/en
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Links

Classifications

    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/13—Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
    • H01M4/139—Processes of manufacture
    • C—CHEMISTRY; METALLURGY
    • C01—INORGANIC CHEMISTRY
    • C01B—NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C
    • C01B25/00—Phosphorus; Compounds thereof
    • C01B25/16—Oxyacids of phosphorus; Salts thereof
    • C01B25/26—Phosphates
    • C01B25/45—Phosphates containing plural metal, or metal and ammonium
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M10/00—Secondary cells; Manufacture thereof
    • H01M10/05—Accumulators with non-aqueous electrolyte
    • H01M10/052—Li-accumulators
    • H01M10/0525—Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/04—Processes of manufacture in general
    • H01M4/043—Processes of manufacture in general involving compressing or compaction
    • H01M4/0433—Molding
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/13—Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/62—Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
    • H01M4/624—Electric conductive fillers
    • H01M4/625—Carbon or graphite
    • C—CHEMISTRY; METALLURGY
    • C01—INORGANIC CHEMISTRY
    • C01P—INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
    • C01P2004/00—Particle morphology
    • C01P2004/60—Particles characterised by their size
    • C01P2004/61—Micrometer sized, i.e. from 1-100 micrometer
    • C—CHEMISTRY; METALLURGY
    • C01—INORGANIC CHEMISTRY
    • C01P—INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
    • C01P2006/00—Physical properties of inorganic compounds
    • C01P2006/40—Electric properties
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M2004/021—Physical characteristics, e.g. porosity, surface area
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M2004/026—Electrodes composed of, or comprising, active material characterised by the polarity
    • H01M2004/028—Positive electrodes
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/13—Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
    • H01M4/131—Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/13—Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
    • H01M4/136—Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/13—Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
    • H01M4/139—Processes of manufacture
    • H01M4/1391—Processes of manufacture of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/13—Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
    • H01M4/139—Processes of manufacture
    • H01M4/1397—Processes of manufacture of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/36—Selection of substances as active materials, active masses, active liquids
    • H01M4/362—Composites
    • H01M4/366—Composites as layered products
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/36—Selection of substances as active materials, active masses, active liquids
    • H01M4/48—Selection of substances as active materials, active masses, active liquids of inorganic oxides or hydroxides
    • H01M4/50—Selection of substances as active materials, active masses, active liquids of inorganic oxides or hydroxides of manganese
    • H01M4/505—Selection of substances as active materials, active masses, active liquids of inorganic oxides or hydroxides of manganese of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/36—Selection of substances as active materials, active masses, active liquids
    • H01M4/48—Selection of substances as active materials, active masses, active liquids of inorganic oxides or hydroxides
    • H01M4/52—Selection of substances as active materials, active masses, active liquids of inorganic oxides or hydroxides of nickel, cobalt or iron
    • H01M4/525—Selection of substances as active materials, active masses, active liquids of inorganic oxides or hydroxides of nickel, cobalt or iron of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
    • H—ELECTRICITY
    • H01—ELECTRIC ELEMENTS
    • H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00—Electrodes
    • H01M4/02—Electrodes composed of, or comprising, active material
    • H01M4/36—Selection of substances as active materials, active masses, active liquids
    • H01M4/58—Selection of substances as active materials, active masses, active liquids of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
    • H01M4/5825—Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines
    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10—Energy storage using batteries

Definitions

  • the present disclosure relates to a method of manufacturing an electrode material, a method of manufacturing an electrode for a battery, and a method of manufacturing a battery.
  • Electrodes applied to semi-solid batteries are manufactured using, for example, an electrode material that includes at least a powdered active material and an electrolyte.
  • JP-A No. 2012-234808 discloses a method for producing a lithium manganese oxide positive electrode active material for a lithium ion secondary battery in which two or more types of spinel-type lithium manganese oxide particles having a spherical shape and different sizes are mixed. An electrode material containing the produced positive electrode active material is also disclosed. Furthermore, JP 2012-234808A also discloses controlling the size and shape of manganese oxide particles using milling.
  • the electrode material used to manufacture electrodes applied to semi-solid batteries is Bingham fluid, which contains more active material in the form of powder than the electrolyte, is clay-like, and has a yield value. many. Therefore, it is desired that the electrode material, which is a Bingham fluid, has a low yield value so that it can exhibit fluidity with a smaller shearing force, from the viewpoint of increasing the efficiency of operations such as molding when manufacturing the electrode.
  • An object of an embodiment of the present disclosure is to provide a method for manufacturing an electrode material that can obtain an electrode material with a low yield value.
  • Another embodiment of the present disclosure aims to provide a method for manufacturing an electrode or a method for manufacturing a battery using the method for manufacturing the electrode material described above.
  • the present disclosure includes the following aspects. ⁇ 1> A classification step of classifying the active material into two or more active material groups having different average particle sizes; a first treatment step of performing a surface smoothing treatment on each of the two or more active material groups; a mixing step of mixing two or more active material groups after surface smoothing treatment with an electrolyte; A method for manufacturing an electrode material having the following. ⁇ 2> The method for producing an electrode material according to ⁇ 1>, wherein the surface smoothing treatment in the first treatment step is mechanochemical surface treatment.
  • a conductive additive is mixed with each of the two or more active material groups after the surface smoothing treatment, and the resulting mixture of two or more
  • ⁇ 5> A method for manufacturing an electrode for a battery, comprising the steps of manufacturing an electrode material by the manufacturing method according to any one of ⁇ 1> to ⁇ 4>, and molding the manufactured electrode material.
  • ⁇ 6> A method for manufacturing a battery, including the step of manufacturing a positive electrode by the manufacturing method according to ⁇ 5>.
  • a method for manufacturing an electrode material that provides an electrode material with a low yield value.
  • a method for manufacturing an electrode or a method for manufacturing a battery using the method for manufacturing the electrode material described above is provided.
  • a numerical range expressed using " ⁇ " means a range that includes the numerical values written before and after " ⁇ " as lower and upper limits.
  • the upper limit or lower limit described in a certain numerical range may be replaced with the upper limit or lower limit of another numerical range described step by step.
  • the upper limit or lower limit described in a certain numerical range may be replaced with the value shown in the Examples.
  • the term "process” includes not only an independent process but also a process that is not clearly distinguishable from other processes, as long as the intended purpose of the process is achieved. .
  • the amount of each component in the composition means the total amount of the multiple substances present in the composition, unless otherwise specified. .
  • a combination of two or more preferred aspects or forms is a more preferred aspect or form.
  • the term “solid component” refers to a component that is solid at 25°C and 1 atm
  • the term “liquid component” refers to a component that is liquid at 25°C and 1 atm.
  • the method for manufacturing an electrode material according to the present disclosure includes a classification step of classifying an active material into two or more active material groups having different average particle sizes, and a surface smoothing treatment for each of the two or more active material groups.
  • lithium iron phosphate a typical positive electrode active material
  • LFP lithium iron phosphate
  • an active material having a large surface area and having irregularities on its surface is used as an electrode material like this LFP, the yield value of the electrode material tends to be high. This is presumed to be because the electrolyte is easily retained on the surface of the active material, which reduces the proportion of freely movable electrolyte in the electrode material, which reduces the dispersibility of the active material and increases the viscosity of the electrode material. Ru.
  • the present inventors conducted a study and performed surface smoothing treatment separately on each of two or more active material groups with different average particle sizes obtained by the classification process, and then We have found a method for manufacturing an electrode material according to the present disclosure, which involves mixing two or more treated active material groups with an electrolyte.
  • the method for manufacturing an electrode material according to the present disclosure includes a classification step of classifying an active material into two or more active material groups having different average particle sizes.
  • the active material prepared in advance that is, the active material before classification
  • the active material before classification is classified into two or more active material groups having different average particle sizes. Details of the active material before classification will be described later.
  • the number of compound groups obtained by classification may be two or more, but from the viewpoint of efficiency of classification and restriction by classification means that can be applied to active materials, two or three is preferable, and two or more is preferable. More preferred. In other words, in this step, it is preferable to classify the active material prepared in advance into two or three active material groups with different average particle sizes, and it is preferable to classify the active material prepared in advance into two or three active material groups with different average particle sizes. More preferred.
  • the conditions for classification in this step may be determined depending on, for example, the particle size distribution of the active material before classification, the type of surface smoothing treatment, etc.
  • the classification point for classification in this step can be determined by taking into consideration the fact that differences tend to appear in the progress of the surface smoothing treatment and the balance between the efficiency of the surface smoothing treatment.
  • the active materials so that, for example, the ratio of specific surface areas between the classified active material groups is 4 or more (preferably 9 or more).
  • D 10 particle size that accounts for 10% cumulatively from the small diameter side of the volume frequency
  • D 90 particle size that cumulatively accounts for 90% from the small diameter side of the volume frequency
  • the particle size distribution ranges from 1 ⁇ m to 6 ⁇ m.
  • the average particle size on the small diameter side is 1.5 ⁇ m and the average particle size on the large diameter side is 3 ⁇ m or more.
  • the average particle size on the large diameter side more than twice the average particle size on the small diameter side (that is, by making the particle size ratio 2 or more)
  • the ratio can be 4 or more. In the above case, it is more preferable to classify the particles so that the average particle size on the small diameter side is 1.5 ⁇ m and the average particle size on the large diameter side is 4.5 ⁇ m or more.
  • the average particle size on the large-diameter side three times or more as compared to the average particle size on the small-diameter side (that is, by making the particle size ratio 3 or more)
  • the specific surface area of the large-diameter side relative to the small-diameter side can be increased.
  • the ratio can be 9 or more.
  • the average particle diameter in the active material group is the particle diameter at which the cumulative volume frequency is 50% from the small diameter side in the particle size distribution, the so-called median diameter (D 50 ).
  • the average particle diameter in the active material group can be measured with a laser diffraction/scattering particle size distribution measuring device (for example, LA-960 manufactured by Horiba, Ltd.). Note that the particle size may be measured by either a wet method or a dry method.
  • the classification means in this step is not particularly limited, and any known dry classification means or wet classification means that can be used for classifying active materials can be used, but it is preferable to use a dry classification means. From the viewpoint of suitability for classifying active materials, it is preferable to use an air classifier as the classification means, and more preferably to use an air classifier that utilizes the Coanda effect. Examples of the airflow classifier include an elbow jet classifier (Nippon Steel Mining Co., Ltd.), a Hyprec classifier (Powder Systems Co., Ltd.), and a Turboplex (registered trademark) ATP (Hosokawa Micron Co., Ltd.). . In this step, in addition to classification into two or more active material groups having different average particle sizes, coarse powder or fine powder may be removed.
  • First treatment step In the method for manufacturing an electrode material according to the present disclosure, after the classification treatment, a first treatment step of performing a surface smoothing treatment on each of two or more active material groups is performed.
  • the surface smoothing treatment in this step is not particularly limited as long as the unevenness on the surface of the active material can be reduced, and any known surface smoothing treatment for powder can be used. Among these, from the viewpoint of the efficiency of the surface smoothing treatment and from the viewpoint of easily suppressing the crushing of the active material, it is preferable that the surface smoothing treatment in this step is a mechanochemical surface treatment.
  • Devices used for mechanochemical surface treatment generally treat the surface of the powder using shear energy generated by the rotation of the shear blades or the metal kiln, by injecting the powder into the clearance between the shear blades and the metal kiln. It is a device that performs The surface of the powder is polished by the shear energy applied to the powder introduced into the device, and the surface is smoothed. In particular, when the powder is a hard material, the surface of the powder is polished even by shearing between the powders, and the surface is smoothed. In this step, it is preferable to utilize this principle to reduce unevenness on the surface of the active material and achieve surface smoothing.
  • the equipment used for surface treatment with mechanochemicals is the circulating Mechanofusion (registered trademark) system AMS (Hosokawa Micron Co., Ltd.), Nobilta (registered trademark) NOB (Hosokawa Micron Co., Ltd.), and the hybridization system (Nara Kikai Co., Ltd.). Seisakusho), Composite (Nippon Coke Industry Co., Ltd.), Mechano Hybrid (Nippon Coke Industry Co., Ltd.), etc.
  • mechanochemical refers to causing a chemical change by applying a mechanical action to an object to be treated. Therefore, the device used for mechanochemical surface treatment can not only smooth the surface of the powder but also fix the powder. However, in this step, it is only necessary to smooth the surface of each of the two or more active material groups, so the mechanochemical surface treatment may be performed under conditions that polish the irregularities on the surface of the active material. Normally, the surface smoothing treatment of the active material on the larger diameter side is difficult to progress, so of the two or more active material groups, the active material group on the larger diameter side is treated under longer or stronger conditions. , it is preferable that surface treatment is performed using mechanochemicals. For example, of the two or more active material groups, the mechanochemical surface treatment may be performed on the active material group on the larger diameter side for a longer time than on the active material group on the smaller diameter side.
  • the surface smoothing treatment for the active material is preferably carried out until, for example, when applied to an electrode material, a yield value required for the electrode material can be achieved.
  • the degree of surface smoothing treatment applied to the active material can be determined based on, for example, the amount of liquid absorbed by the active material.
  • the surface smoothing treatment on the active material is preferably performed until the amount of liquid absorbed by the active material is reduced by, for example, 5% or more, and more preferably until it is reduced by 10% or more.
  • the amount of liquid absorbed by the active material is determined by the following method. That is, when an electrolytic solution having the following composition is continuously added to 100 g of active material while gradually reducing the amount added from 10 g to 0.1 g, the mixture of active material and electrolytic solution becomes a slurry (sludge).
  • the mechanochemical surface treatment can be performed, for example, under the following conditions.
  • the circumferential speed of the shear blade is preferably 15 m/s or more, more preferably 30 m/s or more, and may be even higher. The faster the circumferential speed of the shear blades, the greater the mill energy and the shorter the processing time. However, the circumferential speed of the shearing blades is appropriately selected so that unintended changes in the active material (alteration, deterioration, crushing, etc. of the active material) do not occur.
  • mill energy is measured from the difference between the load power when loading powder (active material) and the no-load power of the device.
  • the mill energy may be calculated as energy per amount of input powder (active material).
  • the mill energy may be appropriately selected depending on conditions such as the desired degree of surface smoothness, the circumferential speed of the shear blades, and the temperature during surface treatment. good.
  • the mill energy of each of the active material on the small diameter side and the active material on the large diameter side may be appropriately selected based on the ratio of specific surface areas. For example, if the ratio of the specific surface area of the large diameter side to the small diameter side is 6, the mill energy of the active material on the large diameter side is approximately 3 to 9 times that of the active material on the small diameter side. Note that the higher the mill energy, the higher the processing temperature.
  • the surface treatment temperature is preferably controlled at 10°C to 200°C. Further, in order to prevent oxidation of the active material, it is also preferable to fill the device with an inert gas.
  • a mixing step is performed in which two or more active material groups subjected to surface smoothing treatment are mixed with an electrolyte solution.
  • two or more active material groups subjected to surface smoothing treatment may be mixed with an electrolytic solution, and there are no particular restrictions on the mixing means.
  • the mixing means for example, a ball mill, bead mill, planetary mixer, blade mixer, roll mill, kneader, disk mill, etc. are used.
  • two or more active material groups after surface smoothing treatment may be mixed first, and then the electrolyte may be mixed therein, or two or more active material groups after surface smoothing treatment may be mixed together.
  • the electrolyte and the electrolyte may be mixed at once.
  • other components such as a conductive additive may be mixed in addition to the two or more active material groups and the electrolytic solution after the surface smoothing treatment.
  • a conductive additive is mixed with each of two or more active material groups after surface smoothing treatment, and the resulting
  • the method further includes a second treatment step of performing a mechanochemical treatment on each of the two or more mixtures obtained.
  • the mixture of the active material and the conductive agent is treated with mechanochemicals, so that the conductive agent bites into the active material, resulting in a composite in which the conductive agent is attached and fixed to the surface of the active material. particles are obtained.
  • the electrode material contains aggregates of the conductive aid, the electrolyte may be restrained by the aggregates of the conductive aid, and the proportion of freely movable electrolyte in the electrode material may decrease.
  • the aggregates of the conductive agent are reduced, and the electrolyte that is bound by the aggregates of the conductive agent is reduced, resulting in a higher yield value.
  • a low electrode material can be obtained.
  • the above-mentioned composite particles easily exhibit conductivity because the active material and the conductive aid are in contact with each other. Therefore, by performing this step and obtaining composite particles as described above, it is also possible to obtain an electrode material that can improve electrode performance and battery performance.
  • the mechanochemical treatment may be performed under conditions that the conductive additive penetrates into the surface of the active material.
  • the apparatus used for the mechanochemical treatment may be similar to the apparatus used for the mechanochemical surface treatment in the first treatment step described above.
  • the mechanochemical treatment of the active material and the conductive additive is preferably carried out until, for example, when applied to the electrode material, a yield value required for the electrode material can be achieved.
  • the degree of mechanochemical treatment of the active material and the conductive additive can be determined based on, for example, the amount of liquid absorbed between the active material and the conductive additive.
  • the mechanochemical treatment of the active material and the conductive additive reduces the liquid absorption of the composite material of the active material and the conductive additive by, for example, 5%, similar to the reduction in the amount of liquid absorbed by the active material in the first treatment step. It is preferable to carry out the process until the amount is reduced by 10% or more, and more preferably until the amount is reduced by 10% or more.
  • the mechanochemical treatment of the active material and the conductive additive is more effective than the surface smoothing treatment of the active material alone in the first treatment step when the purpose is to combine the active material and the conductive additive.
  • the mill energy is the same or smaller.
  • the mill energy during the mechanochemical treatment of the active material and the conductive additive is 1/20 to about the same as the mill energy during the surface smoothing treatment of the active material alone in the first treatment step. It is desirable that there be.
  • the mill energy during the mechanochemical treatment of the active material and the conductive aid may be greater than the mill energy during the surface smoothing treatment of the active material alone in the first treatment step.
  • the method for manufacturing an electrode material according to the present disclosure may include any steps as necessary.
  • the active material is a substance that can insert and release ions of metal elements belonging to Group 1 or Group 2 of the periodic table.
  • the active material is included in the solid component. Examples of the active material include a positive electrode active material and a negative electrode active material.
  • the positive electrode active material is not limited, and any known active material used for positive electrodes can be used.
  • the positive electrode active material is preferably a positive electrode active material that can reversibly insert and release lithium ions.
  • the positive electrode active material include transition metal oxides and elements that can be composited with lithium (for example, sulfur).
  • the positive electrode active material is preferably a transition metal oxide.
  • the transition metal oxide is at least one transition metal element selected from the group consisting of Co (cobalt), Ni (nickel), Fe (iron), Mn (manganese), Cu (copper), and V (vanadium).
  • element Ma is preferably a transition metal oxide.
  • the molar ratio of Li to Ma (Li/Ma) is preferably 0.3 to 2.2.
  • transition metal oxides include Group 1 elements other than lithium, Group 2 elements, Al (aluminum), Ga (gallium), In (indium), Ge (germanium), Sn (tin), Pb ( At least one transition metal element (hereinafter referred to as "element Mb") selected from the group consisting of lead), Sb (antimony), Bi (bismuth), Si (silicon), P (phosphorus), and B (boron). .) may be included.
  • element Mb transition metal element selected from the group consisting of lead
  • Sb antimony
  • Bi bismuth
  • Si silicon
  • P phosphorus
  • B boron
  • transition metal oxides include transition metal oxides having a layered rock salt structure, transition metal oxides having a spinel structure, lithium-containing transition metal phosphate compounds, lithium-containing transition metal halide phosphate compounds, and lithium-containing transition metal phosphate compounds.
  • transition metal-containing silicate compounds include transition metal-containing silicate compounds.
  • transition metal oxides having a layered rock salt structure examples include LiCoO 2 (lithium cobalt oxide [LCO]), LiNi 2 O 2 (lithium nickel oxide), LiNi 0.85 Co 0.10 Al 0.05 O 2 (nickel cobalt lithium aluminate [NCA]), LiNi 1/3 Co 1/3 Mn 1/3 O 2 (nickel manganese cobalt lithium [NMC]), and LiNi 0.5 Mn 0.5 O 2 (manganese nickel lithium oxide).
  • LiCoO 2 lithium cobalt oxide [LCO]
  • LiNi 2 O 2 lithium nickel oxide
  • LiNi 0.85 Co 0.10 Al 0.05 O 2 nickel cobalt lithium aluminate [NCA]
  • LiNi 1/3 Co 1/3 Mn 1/3 O 2 nickel manganese cobalt lithium [NMC]
  • LiNi 0.5 Mn 0.5 O 2 mangaganese nickel lithium oxide
  • transition metal oxides having a spinel structure examples include LiCoMnO 4 , Li 2 FeMn 3 O 8 , Li 2 CuMn 3 O 8 , Li 2 CrMn 3 O 8 , and Li 2 NiMn 3 O 8 .
  • lithium-containing transition metal phosphate compounds include olivine-type iron phosphates (e.g., LiFePO 4 and Li 3 Fe 2 (PO 4 ) 3 ), iron pyrophosphates (e.g., LiFeP 2 O 7 ), and phosphorus.
  • Acid cobalt salts eg, LiCoPO 4
  • monoclinic nasicon-type vanadium phosphate salts eg, Li 3 V 2 (PO 4 ) 3 (lithium vanadium phosphate)).
  • lithium-containing transition metal halogenated phosphate compounds include iron fluorophosphates (e.g., Li 2 FePO 4 F), manganese fluorophosphates (e.g., Li 2 MnPO 4 F), and phosphorus fluorides. Acid cobalt salts (eg, Li 2 CoPO 4 F) are included.
  • lithium-containing transition metal silicate compound examples include Li 2 FeSiO 4 , Li 2 MnSiO 4 , and Li 2 CoSiO 4 .
  • the transition metal oxide is preferably a transition metal oxide having a layered rock salt structure, such as LiCoO 2 (lithium cobalt oxide [LCO]), LiNi 0.85 Co 0.10 Al 0.05 O 2 (nickel cobalt oxide), Lithium aluminate [NCA]), and LiNi 1/3 Co 1/3 Mn 1/3 O 2 (lithium nickel manganese cobalt oxide [NMC]). preferable.
  • LiCoO 2 lithium cobalt oxide [LCO]
  • LiNi 0.85 Co 0.10 Al 0.05 O 2 nickel cobalt oxide
  • NCA Lithium aluminate
  • NMC lithium nickel manganese cobalt oxide
  • the positive electrode active material may be a commercially available product or a synthetic product manufactured by a known method (for example, a calcination method).
  • the positive electrode active material obtained by the calcination method may be washed using water, an acidic aqueous solution, an alkaline aqueous solution, or an organic solvent.
  • the positive electrode active material may have a carbon film on its surface.
  • the shape of the positive electrode active material is not limited, but from the viewpoint of ease of handling, it is preferably particulate.
  • the volume average particle size of the positive electrode active material is not limited, and can be, for example, 0.1 ⁇ m to 50 ⁇ m.
  • the volume average particle size of the positive electrode active material is preferably 0.3 ⁇ m to 40 ⁇ m, more preferably 0.5 ⁇ m to 30 ⁇ m.
  • the volume average particle diameter of the positive electrode active material is 0.3 ⁇ m or more, an aggregate of electrode materials can be easily formed, and scattering of the electrode material during handling can be suppressed.
  • the volume average particle size of the positive electrode active material is 40 ⁇ m or less, the thickness of the electrode molded body can be easily adjusted, and the generation of voids can be suppressed during the molding process.
  • the volume average particle size of the positive electrode active material is measured by the following method.
  • a dispersion containing 0.1% by mass or less of the positive electrode active material is prepared by mixing the positive electrode active material and a solvent (for example, pure water, ethanol, heptane, octane, toluene, or xylene).
  • a dispersion liquid irradiated with 1 kHz ultrasonic waves for 10 minutes is used as a measurement sample.
  • a laser diffraction/scattering particle size distribution analyzer for example, LA-960 manufactured by Horiba, Ltd.
  • data was acquired 50 times at a temperature of 25°C, and the volume frequency particle size distribution and median diameter were measured. seek.
  • a quartz cell is used as the measurement cell.
  • Examples of methods for adjusting the particle size of the positive electrode active material include methods using a crusher, a crusher, and a classifier. Further, as a method for adjusting the particle size of the positive electrode active material, a known milling method may be applied.
  • the manufactured electrode material may contain one type of positive electrode active material, or may contain two or more types of positive electrode active materials. Further, even if the manufactured electrode material contains one type of positive electrode active material, positive electrode active materials having different particle sizes may be used in combination.
  • the content of the positive electrode active material in the total volume of the electrode material to be produced is preferably 30% to 75% by volume, more preferably 35% to 70% by volume, and 40% to 65% by volume. % is more preferable.
  • the negative electrode active material is not limited, and any known active material used for negative electrodes can be used.
  • the negative electrode active material is preferably a negative electrode active material that can reversibly insert and release lithium ions.
  • negative electrode active materials include carbonaceous materials, metal oxides (e.g., tin oxide), silicon oxide, metal composite oxides, lithium alone, lithium alloys (e.g., lithium-aluminum alloys), and those capable of forming alloys with lithium. metals such as Sn, Si, and In.
  • the negative electrode active material is preferably a carbonaceous material or a lithium composite oxide from the viewpoint of reliability.
  • a carbonaceous material is a material consisting essentially of carbon.
  • Examples of carbonaceous materials include petroleum pitch, carbon black (e.g., acetylene black), graphite (e.g., natural graphite, and artificial graphite (e.g., vapor-grown graphite)), hard carbon, and synthetic resins (e.g., polyester).
  • Examples include carbonaceous materials made by firing acrylonitrile (PAN) and furfuryl alcohol resins.
  • carbonaceous materials include carbon fibers (e.g., polyacrylonitrile carbon fibers, cellulose carbon fibers, pitch carbon fibers, vapor grown carbon fibers, dehydrated PVA (polyvinyl alcohol) carbon fibers, lignin carbon fibers, glass carbon fibers, and activated carbon fibers).
  • carbon fibers e.g., polyacrylonitrile carbon fibers, cellulose carbon fibers, pitch carbon fibers, vapor grown carbon fibers, dehydrated PVA (polyvinyl alcohol) carbon fibers, lignin carbon fibers, glass carbon fibers, and activated carbon fibers.
  • Graphite also includes, for example, mesophase microspheres, graphite whiskers, and tabular graphite.
  • "flat plate shape” means a shape having two main planes facing in opposite directions.
  • the metal composite oxide is preferably a metal composite oxide capable of intercalating and deintercalating lithium.
  • the metal composite oxide capable of intercalating and deintercalating lithium preferably contains at least one element selected from the group consisting of titanium and lithium, from the viewpoint of high current density charge/discharge characteristics.
  • the metal oxide and metal composite oxide are particularly preferably amorphous oxides.
  • the metal oxide and metal composite oxide are chalcogenides.
  • Chalcogenides are reaction products of metal elements and elements of group 16 in the periodic table.
  • amorphous oxides of metalloid elements and chalcogenides are preferred, and elements of groups 13 to 15 in the periodic table, Al, Ga, Si, Sn , Ge, Pb, Sb, and Bi, and chalcogenide.
  • the negative electrode active material further contains titanium.
  • a negative electrode containing titanium has excellent rapid charging and discharging characteristics due to small volume fluctuations during intercalation and desorption of lithium ions, and from the viewpoint of suppressing electrode deterioration and extending the life of lithium ion secondary batteries.
  • the active material is preferably Li 4 Ti 5 O 12 (lithium titanate [LTO]).
  • the negative electrode active material may be a commercially available product or a synthetic product produced by a known method (for example, a calcination method).
  • the negative electrode active material obtained by the calcination method may be washed using water, an acidic aqueous solution, an alkaline aqueous solution, or an organic solvent.
  • the negative electrode active material is available, for example, as CGB20 (Nippon Graphite Industries Co., Ltd.).
  • the composition of the negative electrode active material is measured using inductively coupled plasma (ICP) emission spectrometry.
  • ICP inductively coupled plasma
  • the shape of the negative electrode active material is not limited, but is preferably particulate from the viewpoint of ease of handling and easy control of uniformity during mass production.
  • the volume average particle diameter of the negative electrode active material is preferably 0.1 ⁇ m to 60 ⁇ m, more preferably 0.3 ⁇ m to 50 ⁇ m, and particularly preferably 0.5 ⁇ m to 40 ⁇ m.
  • the volume average particle size of the negative electrode active material is measured by a method similar to the method for measuring the volume average particle size of the positive electrode active material.
  • Examples of methods for adjusting the particle size of the negative electrode active material include a method using a pulverizer or a classifier.
  • the manufactured electrode material may contain only one type of negative electrode active material, or may contain two or more types of negative electrode active materials.
  • the content of the negative electrode active material relative to the total volume of the electrode material to be produced is preferably 30% to 75% by volume, more preferably 35% to 73% by volume, and 45% to 70% by volume. It is more preferable that
  • the surfaces of the positive electrode active material and the negative electrode active material may each be coated with a surface coating agent.
  • the surface coating agent include metal oxides containing Ti, Nb, Ta, W, Zr, Si, or Li.
  • the metal oxides include spinel titanate, tantalum oxides, niobium oxides, and lithium niobate compounds.
  • the electrolytic solution is not particularly limited, and any known electrolytic solution can be used.
  • the electrolytic solution include an electrolytic solution containing an electrolyte and a solvent.
  • Specific examples of the electrolytic solution include, for example, an electrolytic solution containing a lithium salt compound as an electrolyte and a carbonate compound as a solvent.
  • the lithium salt compound examples include lithium hexafluorophosphate.
  • the electrolytic solution may contain one type of lithium salt compound alone, or may contain two or more types of lithium salt compounds.
  • carbonate compounds include chain carbonate compounds such as ethyl methyl carbonate (also referred to as EMC), dimethyl carbonate (also referred to as DMC), and diethyl carbonate (DEC), ethylene carbonate (also referred to as EC), and propylene carbonate (PC).
  • chain carbonate compounds such as ethyl methyl carbonate (also referred to as EMC), dimethyl carbonate (also referred to as DMC), and diethyl carbonate (DEC), ethylene carbonate (also referred to as EC), and propylene carbonate (PC).
  • Examples include cyclic carbonate compounds such as (also referred to as).
  • the electrolytic solution may contain one type of carbonate compound alone, two or more types of carbonate compounds, or a combination of one or more types of chain carbonate compounds and one or more types of cyclic carbonate compounds. You may.
  • the electrolyte contained in the electrolytic solution for example, a known inorganic solid electrolyte can also be used.
  • an ionic liquid may be used as a component of the electrolytic solution.
  • Ionic liquids can be used either as electrolytes or as solvents.
  • the content of the electrolyte in the total volume of the electrode material to be manufactured is preferably 70% by volume or less, more preferably 60% by volume or less, and even more preferably 55% by volume or less.
  • the lower limit of the electrolyte content in the electrode material may be more than 0% by volume, and preferably 30% by volume or more.
  • the manufactured electrode material may contain, as a liquid component, a solvent other than the solvent contained as a component of the electrolytic solution (hereinafter also simply referred to as "solvent").
  • solvent include alcohol compound solvents, ether compound solvents, amide compound solvents, amino compound solvents, ketone compound solvents, aromatic compound solvents, aliphatic compound solvents, and nitrile compound solvents.
  • the boiling point of the solvent is preferably 50°C or higher, more preferably 70°C or higher at normal pressure (ie, 1 atm).
  • the upper limit of the boiling point of the solvent is preferably 250° C. or lower, more preferably 220° C. or lower at normal pressure (ie, 1 atm).
  • the manufactured electrode material may contain one type of solvent alone, or may contain two or more types of solvents.
  • the content of liquid components (i.e., electrolyte and solvent) relative to the total volume of the electrode material to be manufactured is preferably 70% by volume or less, more preferably 60% by volume or less, and 55% by volume or less. It is even more preferable that there be.
  • the content of the liquid component in the electrode material is 70% by volume or less, it is possible to suppress the liquid component from seeping out when the electrode material is molded. Moreover, when the liquid component contains a solvent, deterioration of battery performance can be suppressed.
  • the lower limit of the content of the liquid component in the electrode material may be more than 0% by volume, and preferably 30% by volume or more.
  • the liquid component in the electrode material is preferably liquid even at -10°C, and is preferably liquid even at -20°C. It is preferable that there be. That is, the component in the electrode material that is liquid at 25°C is preferably a component that does not solidify at -10°C, and is preferably a component that does not solidify even at -20°C.
  • the manufactured electrode material preferably contains a conductive additive from the viewpoint of improving the electronic conductivity of the active material.
  • the conductive aid is not limited, and any known conductive aid can be used.
  • the conductive aid is included in the solid component.
  • Examples of conductive aids include graphite (e.g., natural graphite and artificial graphite), carbon black (e.g., acetylene black, Ketjen black, and furnace black), amorphous carbon (e.g., needle coke), and carbon fiber (e.g., needle coke). other carbonaceous materials (e.g., graphene, and fullerenes); metal powders (e.g., copper powders, and nickel powders); metal fibers (e.g., copper fibers, and nickel powders); fibers), and conductive polymers (eg, polyaniline, polypyrrole, polythiophene, polyacetylene, and polyphenylene derivatives).
  • graphite e.g., natural graphite and artificial graphite
  • carbon black e.g., acetylene black, Ketjen black, and furnace black
  • amorphous carbon e.g., needle coke
  • carbon fiber e.g., needle coke
  • the manufactured electrode material may contain one type of conductive aid, or may contain two or more types of conductive aid.
  • the content of the conductive additive is 0.05% to 5% by volume based on the total volume of the electrode material, from the viewpoint of improving the electronic conductivity of the active material. It is preferably 0.1% to 4% by volume, and even more preferably 0.5% to 3% by volume.
  • the manufactured electrode material may contain a binder, a dispersant, other additives, etc. in addition to the above-mentioned components.
  • the binder include fluororesins, hydrocarbon thermoplastic resins, acrylic resins, and urethane resins.
  • the dispersant may be any known dispersant that can disperse the object to be dispersed.
  • known additives added to electrode materials can be used.
  • the electrode material manufactured by the method for manufacturing an electrode material according to the present disclosure has a low yield value.
  • the yield value of the manufactured electrode material is preferably 120 kPa or less, more preferably 60 kPa or less, even more preferably 40 kPa or less, and particularly preferably 30 kPa or less.
  • the yield value is 120 kPa or less, the material exhibits fluidity with a small shearing force, which improves the working efficiency of molding.
  • the yield value of the electrode material is measured as follows. That is, the mixed electrode material is put into a container (for example, a cylindrical cup, etc.), and is pushed through a jig or the like from above by applying a pressure of 0.1 MPa to 1 MPa as a guide, to create a gap between the constituent components of the electrode material. Prepare the measurement sample by solidifying it so that there are no gaps. Using a precision rotational viscometer with a vane-type spindle (e.g. Brookfield Soft Solid Tester, RST-SST), when the probe is inserted into the measurement sample (i.e. solidified electrode material) and rotated at a constant speed. Read the stress change and measure the yield value (yield stress).
  • a container for example, a cylindrical cup, etc.
  • RST-SST Brookfield Soft Solid Tester
  • the manufactured electrode material contains an active material and has a solid component concentration of 30% by volume or more.
  • the solid component concentration is 30% by volume or more means that the content rate of the solid component with respect to the total volume of the electrode material is 30% by volume or more.
  • the solid component concentration in the electrode material is preferably 40% by volume or more, more preferably 45% by volume or more.
  • the upper limit of the solid component concentration in the electrode material may be less than 100% by volume, and preferably 70% by volume or less.
  • the solid component concentration of the electrode material is calculated from the composition ratio of each component contained in the electrode material and the specific gravity of those components.
  • the manufactured electrode materials may have been obtained through a classification process, and therefore often contain active materials that have two or more peaks in their particle size distribution.
  • the particle size distribution here is obtained by the same method as the volume frequency particle size distribution of the positive electrode active material described above.
  • An active material having two or more peaks in the particle size distribution means that a distribution having two or more peaks is observed on the obtained volume frequency particle size distribution.
  • the method of manufacturing an electrode for a battery according to the present disclosure includes a step of manufacturing an electrode material by the method of manufacturing an electrode material according to the present disclosure (also referred to as an electrode material manufacturing step), and a step of molding the manufactured electrode material (molding step). (also referred to as).
  • a step of manufacturing an electrode material by the method of manufacturing an electrode material according to the present disclosure also referred to as an electrode material manufacturing step
  • a step of molding the manufactured electrode material molding step.
  • Electrode material manufacturing process In the method for manufacturing a battery electrode according to the present disclosure, the electrode material manufacturing step of manufacturing an electrode material by the method for manufacturing an electrode material according to the present disclosure described above is performed. The details of this step are the same as the method for manufacturing an electrode material according to the present disclosure, and the preferred embodiments are also the same.
  • a molding step is performed in which the electrode material obtained in the electrode material manufacturing step is molded.
  • the method for forming the electrode material There are no particular restrictions on the method for forming the electrode material, and the method may be selected depending on the shape, size, filling rate, etc. of the battery electrode.
  • this step may be, for example, a step of applying the electrode material onto a support to obtain a sheet-like molded body, or a step of injecting the electrode material into a mold to obtain the desired shape. It may also be a process of obtaining a molded body.
  • a molding method described in Japanese Patent Publication No. 2017-533548, Japanese Patent Application Publication No. 2021-530829, etc., which discloses a method for manufacturing an electrode can also be used.
  • this step is preferably a step of applying an electrode material onto a support to obtain a sheet-like molded body (also referred to as an electrode film).
  • the support used in the step of obtaining the sheet-like molded body will be explained.
  • the support is not particularly limited as long as it can form a sheet-like molded body made of electrode material on its surface.
  • a current collector is preferred as the support.
  • the current collector which is an example of the support, is not particularly limited, and known current collectors (positive electrode current collector and negative electrode current collector) can be used.
  • Examples of the positive electrode current collector include aluminum, aluminum alloy, stainless steel, nickel, and titanium.
  • the positive electrode current collector is preferably made of aluminum or an aluminum alloy.
  • the positive electrode current collector may be made of aluminum having a coating layer containing one or more of carbon, nickel, titanium, silver, gold, platinum, and vanadium oxide on the surface.
  • Examples of the negative electrode current collector include aluminum, copper, copper alloy, stainless steel, nickel, and titanium.
  • the negative electrode current collector is preferably made of aluminum, copper, a copper alloy, or stainless steel, and more preferably copper or a copper alloy.
  • the negative electrode current collector may be made of copper or stainless steel, with a coating layer containing one or more of carbon, nickel, titanium, silver, and lithium on the surface.
  • the current collector is preferably aluminum foil (including aluminum foil having the above-mentioned coating layer on the surface) or copper foil (including copper foil having the above-mentioned coating layer on the surface).
  • Aluminum foil is commonly utilized as a current collector in positive electrodes.
  • Copper foil is typically utilized as a current collector in the negative electrode.
  • the current collector used as the support may be a laminate of a metal layer exemplified as the above-mentioned positive electrode current collector or negative electrode current collector and a resin film.
  • resin films used in the laminate include polyethylene terephthalate (PET) film, polypropylene (PP) film, polyethylene (PE) film, cyclic olefin polymer (COP, COC) film, triacetylcellulose (TAC) film, and polyimide (PI) film. ) films, and resin films such as polyamide (PA) films.
  • a mold release material is mentioned as an example of a support.
  • the release material which is an example of a support, include release paper (for example, release paper manufactured by Lintec Corporation), a film having a release layer, and paper having a release layer. is preferred.
  • release paper for example, release paper manufactured by Lintec Corporation
  • the sheet-like molded object formed on the mold release material can be transferred to a current collector using the mold release property which the mold release material has.
  • the average thickness of the support is, for example, preferably 3 ⁇ m or more, more preferably 5 ⁇ m or more, and particularly preferably 10 ⁇ m or more.
  • the average thickness of the support is preferably 100 ⁇ m or less, more preferably 70 ⁇ m or less, particularly preferably 50 ⁇ m or less, from the viewpoint of flexibility and lightness.
  • the average thickness of the support is the arithmetic mean of the thicknesses at three locations measured by cross-sectional observation. In cross-sectional observation, a known microscope (for example, a scanning electron microscope) can be used.
  • a battery electrode is manufactured by the method for manufacturing a battery electrode according to the present disclosure.
  • the shape and size of the battery electrode may be determined depending on the battery to which it is applied.
  • the method of manufacturing a battery according to the present disclosure includes a step of manufacturing a positive electrode (also referred to as a positive electrode manufacturing step) by the method of manufacturing an electrode for a battery according to the present disclosure.
  • a positive electrode manufacturing step of manufacturing at least a positive electrode by the above-described battery electrode manufacturing method according to the present disclosure is performed.
  • the details of this step are the same as the method for manufacturing a battery electrode according to the present disclosure, and the preferred embodiments are also the same.
  • a negative electrode may also be manufactured. That is, the negative electrode may be manufactured by the method for manufacturing a battery electrode according to the present disclosure.
  • steps include preparing a negative electrode or manufacturing the negative electrode using a method different from the positive electrode manufacturing process, preparing or manufacturing a separator, and bonding (laminating) the positive electrode, separator, and negative electrode. Examples include processes. Furthermore, other steps include stacking a single cell made by bonding a positive electrode, a separator, and a negative electrode together, and forming a tab shape for connecting the positive electrode current collector and negative electrode current collector to the outside in the stacked unit cell. Examples include a step of attaching electrodes, a step of sealing a stack of single cells with an exterior member, and the like. A laminated cell can be manufactured through these steps. In addition, as other processes, various processes described in Japanese Patent Publication No.
  • a battery is manufactured by the battery manufacturing method according to the present disclosure.
  • the manufactured battery is a semi-solid battery.
  • Example 1 (Classification process) The positive electrode active material (lithium iron phosphate: “LFP NCO M121” manufactured by Aleees) was classified using an air flow classifier (Elbow jet classifier manufactured by Nippon Steel Mining Co., Ltd.) to classify it into a small diameter group with a peak at 2 ⁇ m.
  • the active materials were classified into two groups: , a large diameter group with a peak at 5 ⁇ m, and a large diameter group with a peak at 5 ⁇ m.
  • fine powder of 0.2 ⁇ m or less was removed.
  • the large-diameter group obtained in the classification step was subjected to the same mechanochemical surface smoothing treatment as described above for 48 hours. At this time, the peripheral speed of the shear blade was 20 m/s, and the mill energy was 30,000 kJ/kg.
  • electrolyte A 64 g was added to the obtained kneaded material (176 g), and the mixture was stirred at 1500 rpm for 120 seconds using a mixer (Awatori Rentaro ARE-310, manufactured by Shinky Co., Ltd.) to prepare a positive electrode.
  • An electrode material (P1) was obtained.
  • 13.4 g of LiPF 6 (electrolyte) was mixed into a mixed solution of 45 g of ethylene carbonate (EC), 10 g of propylene carbonate (PC), and 45 g of diethyl carbonate (DEC), vinylene carbonate (VC) was added. ) 2.3g were mixed.
  • 64 g was taken out and used as electrolyte solution A.
  • the yield value of the obtained positive electrode material (P1) was measured by the method described above and was found to be 20 kPa.
  • the obtained positive electrode material (P1) had a volume ratio of solid component to liquid component of 48:52.
  • the maximum space filling rate was determined from the particle size distribution of the active material in the obtained positive electrode material (P1) and was 68%. It was found that the maximum space filling factor was greater than about 64%. It is therefore presumed that by using the positive electrode material (P1), an electrode containing an active material at a high filling rate can be obtained.
  • Example 2 After performing the classification step and first treatment step of Example 1, the following second treatment step and mixing step were performed to obtain a positive electrode material (P2) in the same manner as in Example 1. Ta.
  • the yield value of the obtained positive electrode material (P2) was measured by the method described above and was found to be 15 kPa.
  • the obtained positive electrode material (P2) had a volume ratio of solid component to liquid component of 48:52.
  • the maximum space filling rate was found to be 68% from the particle size distribution of the active material in the obtained positive electrode material (P2), and the maximum space filling rate was approximately 66% due to only the small diameter group, and approximately 66% due to only the large diameter group. It was found that the maximum space filling factor was greater than about 64%. It is presumed that by using the positive electrode material (P2), an electrode containing an active material at a high filling rate can be obtained.
  • the small-diameter group obtained in the classification process was processed using a circulation type Mechanofusion (registered trademark) system AMS manufactured by Hosokawa Micron Co., Ltd., at a rotation speed of 2500 rpm, a temperature of 35°C to 60°C (temperature rise was suppressed by a refrigerant), and N Surface smoothing treatment using mechanochemical was performed for 10 hours under a two- purge environment.
  • the peripheral speed of the shear blade was 20 m/s, and the mill energy was 8000 kJ/kg.
  • the large-diameter group obtained in the classification step was subjected to the same mechanochemical surface smoothing treatment as described above for 84 hours. At this time, the peripheral speed of the shear blade was 20 m/s, and the mill energy was 67,200 kJ/kg.
  • the above electrolyte A 64 g was added to the obtained kneaded material (176 g), and the mixture was stirred at 1500 rpm for 120 seconds using a mixer (Awatori Rentaro ARE-310, manufactured by Shinky Co., Ltd.) to prepare a positive electrode.
  • An electrode material (P3) was obtained.
  • the yield value of the obtained positive electrode material (P3) was measured by the method described above and was found to be 40 kPa.
  • the obtained positive electrode material (P3) had a volume ratio of solid component to liquid component of 48:52.
  • the maximum space filling rate was determined from the particle size distribution of the active material in the obtained positive electrode material (P3) and was found to be 70%. It was found that the maximum space filling factor was greater than about 62%. It is presumed that by using the positive electrode material (P3), an electrode containing an active material at a high filling rate can be obtained.
  • a positive electrode material (C1) was obtained in the same manner as in Example 1, except that the classification process in Example 1 was not performed and the following surface treatment process and mixing process were performed.
  • the positive electrode active material lithium iron phosphate: "LFP NCO M121" manufactured by Aleees
  • the positive electrode active material was prepared using a circulating Mechanofusion (registered trademark) system AMS manufactured by Hosokawa Micron Co., Ltd. at a rotation speed of 2500 rpm and a temperature of 25 to 40 degrees Celsius
  • Surface treatment using mechanochemicals was performed for 8 hours under an N 2 purge environment (temperature rise was suppressed by a refrigerant).
  • the yield value of the obtained positive electrode material (C1) was measured by the method described above and was found to be 45 kPa.
  • the obtained positive electrode material (C1) had a volume ratio of solid component to liquid component of 48:52.
  • a positive electrode material (C2) was obtained in the same manner as in Example 3, except that the classification step in Example 3 was not performed and the following surface treatment step and mixing step were performed.
  • the positive electrode active material lithium iron phosphate: "LFP NCO M23" manufactured by Aleees
  • the positive electrode active material was prepared using a circulating Mechanofusion (registered trademark) system AMS manufactured by Hosokawa Micron Co., Ltd. at a rotation speed of 2500 rpm and a temperature of 35 to 60 degrees Celsius
  • Surface treatment using mechanochemicals was performed for 10 hours under an N 2 purge environment (temperature rise was suppressed by a refrigerant).
  • the yield value of the obtained positive electrode material (C2) was measured by the method described above and was found to be 84 kPa.
  • the obtained positive electrode material (C2) had a volume ratio of solid component to liquid component of 48. :52.
  • Positive electrode current collector (147.6 mm x 203.6 mm x 20 ⁇ m rectangular body with 30.0 mm x 34.4 mm x 20 ⁇ m convex part (connection part with tab-shaped electrode) on PET film (20 ⁇ m) with aluminum foil welded ) was prepared.
  • a frame (148.6 mm x 204.6 mm x 325 ⁇ m) having an opening was placed on the aluminum foil of the positive electrode current collector.
  • the blade was moved along the frame to form the electrode material along the shape of the frame and remove excess electrode material. . Thereafter, the frame was removed to obtain a positive electrode in which a positive electrode film (148.6 mm x 204.6 mm x 325 ⁇ m) was formed on the positive electrode current collector.
  • Negative electrode current collector with copper foil welded on PET film (20 ⁇ m) (150.3 mm x 206.3 mm x 20 ⁇ m rectangular body with 30.0 mm x 33.0 mm x 20 ⁇ m convex part (connection part with tab-shaped electrode) ) was prepared.
  • a frame (151.3 mm x 207.3 mm x 335 ⁇ m) having an opening was placed on the copper foil of the negative electrode current collector.
  • PA negative electrode material
  • the electrode material is molded according to the shape of the frame, and the excess electrode material is removed. was removed. Thereafter, the frame was removed to obtain a negative electrode in which a negative electrode film (151.3 mm x 207.3 mm x 335 ⁇ m) was formed on the negative electrode current collector.
  • Electrode material for negative electrode (PA) - First, the above electrolytic solution A (64 g) was prepared. Next, a conductive additive (carbon black: "C-NERGY SUPER C45” manufactured by Imerys Graphite & Carbon) and a negative electrode active material ("MESOPHASE GRAPHITE POW” manufactured by China Steel Chemical Corporation) were added. DER A(M GP-A)'') and a total of 159 g so that the mass ratio was 2.7; 63.4, and both were placed in a mixer (Awatori Rentaro ARE-310, manufactured by Shinky Co., Ltd.). The mixture was stirred at 900 rpm for 18 seconds to prepare a kneaded product.
  • a conductive additive carbon black: "C-NERGY SUPER C45” manufactured by Imerys Graphite & Carbon
  • MEOPHASE GRAPHITE POW manufactured by China Steel Chemical Corporation
  • electrolytic solution A 64 g was added to the obtained kneaded material (159 g), and the mixture was stirred at 900 rpm for 30 seconds using a mixer (Awatori Rentaro ARE-310, manufactured by Shinky Co., Ltd.) to form a negative electrode.
  • a material (PA) was obtained.
  • the yield value of the obtained negative electrode material (PA) was measured by the method described above and was found to be 20 kPa.
  • the obtained negative electrode material (PA) had a volume ratio of solid component to liquid component of 52:48.
  • a separator manufactured by Double Scope Co., Ltd., polyethylene, 220 mm x 260 mm x 20 ⁇ m
  • the positive electrode obtained by the above method was placed on the separator. was placed so that the positive electrode film faced the negative electrode film.
  • the PET film portion around the electrode film (specifically, the four peripheral sides approximately 3 mm outside the formed electrode film) was heat welded and laminated at 200°C.
  • the surrounding excess PET film was cut to produce a single cell (an example of a battery). A total of 16 single cells were produced using the same procedure.
  • a tab-shaped electrode (30 mm x 42 mm x 0.3 mm, an electrode made of copper coated with nickel, and a polypropylene resin welded to the base) was attached to the end of the negative electrode current collector of each single cell of the obtained laminate. ) were heat welded using an ultrasonic welding machine.
  • an aluminum sheet was prepared in which a nylon film (thickness 25 ⁇ m) was adhered to the surface of an aluminum foil (thickness 40 ⁇ m) with an adhesive, and a polypropylene film (thickness 45 ⁇ m) was welded to the back surface. Two depressions of 155 mm x 212 mm x 5 mm were formed inside this aluminum sheet (300 mm x 260 mm).
  • the above-mentioned single cell laminate was wrapped from above and below with the two obtained molded aluminum sheets, and three sides around the molded aluminum sheets were heat welded at 230° C. using a heat welding machine.
  • the laminate wrapped in a formed aluminum sheet was set in a restraint jig.
  • the restraint jig consists of two rectangular metal plates that sandwich the laminate wrapped in formed aluminum sheets from the front and back sides, and spring-loaded bolts installed at the four corners of the two rectangular metal plates.
  • a jig was used to hold the laminate wrapped in a sheet with the tightening load of a spring, and the set load was 100 kgf.
  • the laminate wrapped in the formed aluminum sheet still set in the restraint jig was placed in a vacuum heat welding machine, and after vacuuming to -85 kPa, the remaining side of the formed aluminum sheet that was not heat welded was It was sealed by heat welding at °C. Thereafter, the vacuum heat welding machine was opened to the atmosphere, and the sealant was taken out to obtain a laminated cell (S1).
  • the battery performance of the obtained laminated cell (S1) was confirmed as follows.
  • the front and back sides of the laminated cell obtained as described above were tightened again using the above-mentioned restraint jig at a set load of 150 kgf.
  • the laminated cell still set in the restraint jig was set in a charging/discharging machine equipped with a constant temperature bath.
  • the laminated cell was placed in a constant temperature bath at 25° C. ⁇ 3° C., and the laminated cell was connected to positive and negative terminals installed in the constant temperature bath. Note that the cables connected to the positive and negative terminals go outside the thermostatic oven and are connected to the charger/discharger.
  • BCS-815 manufactured by Bio-Logic Science Instruments was used as the charge/discharge machine
  • BTC-408Hb manufactured by Espec was used as the constant temperature bath.
  • the laminated cell was charged to about 15% of the designed battery capacity (37 Ah) (constant current 6.2 A, up to about 555 mAh).
  • the battery capacity 37 Ah
  • excess reactive gas was generated from the electrode films within the laminated cell, and the gas accumulated in the margins of the formed aluminum sheet in areas where no load was applied by the restraint jig. Therefore, one side of the formed aluminum sheet was unsealed, and the sheet was again placed in the thermal vacuum welding machine to remove excess gas, and then resealed.
  • the laminated cell was set in the charger/discharger again and fully charged to 100% of the designed battery capacity (37 Ah).
  • the charging sequence using the charger/discharger was to charge the battery at a constant current of 10.9 A until the battery voltage reached 3.6 V, and then to fully charge the battery while adjusting the current value so as not to exceed 3.6 V.
  • the fully charged laminated cell was stored in a constant temperature bath at 38 ⁇ 3° C. for 21 days. Thereafter, the laminated cell was stored in a constant temperature bath at 25°C ⁇ 3°C for 24 hours.

Landscapes

  • Chemical & Material Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • General Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Inorganic Chemistry (AREA)
  • Organic Chemistry (AREA)
  • Materials Engineering (AREA)
  • Manufacturing & Machinery (AREA)
  • Crystallography & Structural Chemistry (AREA)
  • Battery Electrode And Active Subsutance (AREA)
PCT/JP2023/027221 2022-07-28 2023-07-25 電極材料の製造方法、電池用電極の製造方法、及び、電池の製造方法 Ceased WO2024024786A1 (ja)

Priority Applications (4)

Application Number Priority Date Filing Date Title
CN202380055001.3A CN119585880A (zh) 2022-07-28 2023-07-25 电极材料的制造方法、电池用电极的制造方法及电池的制造方法
EP23846516.5A EP4564467A4 (en) 2022-07-28 2023-07-25 METHOD FOR MANUFACTURING ELECTRODE MATERIAL, METHOD FOR MANUFACTURING BATTERY ELECTRODE AND METHOD FOR MANUFACTURING BATTERIES
JP2024537749A JPWO2024024786A1 (cg-RX-API-DMAC7.html) 2022-07-28 2023-07-25
US19/015,659 US20250149577A1 (en) 2022-07-28 2025-01-10 Production method of electrode material, manufacturing method of electrode for battery, and manufacturing method of battery

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2022-120973 2022-07-28
JP2022120973 2022-07-28

Related Child Applications (1)

Application Number Title Priority Date Filing Date
US19/015,659 Continuation US20250149577A1 (en) 2022-07-28 2025-01-10 Production method of electrode material, manufacturing method of electrode for battery, and manufacturing method of battery

Publications (1)

Publication Number Publication Date
WO2024024786A1 true WO2024024786A1 (ja) 2024-02-01

Family

ID=89706353

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2023/027221 Ceased WO2024024786A1 (ja) 2022-07-28 2023-07-25 電極材料の製造方法、電池用電極の製造方法、及び、電池の製造方法

Country Status (5)

Country Link
US (1) US20250149577A1 (cg-RX-API-DMAC7.html)
EP (1) EP4564467A4 (cg-RX-API-DMAC7.html)
JP (1) JPWO2024024786A1 (cg-RX-API-DMAC7.html)
CN (1) CN119585880A (cg-RX-API-DMAC7.html)
WO (1) WO2024024786A1 (cg-RX-API-DMAC7.html)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2025206397A1 (ja) * 2024-03-29 2025-10-02 富士フイルム株式会社 電極の製造方法、電極の製造装置、及び電極膜の製造方法

Citations (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2011125577A1 (ja) * 2010-03-31 2011-10-13 住友金属工業株式会社 改質天然黒鉛粒子およびその製造方法
JP2012124121A (ja) * 2010-12-10 2012-06-28 Hitachi Chem Co Ltd リチウム二次電池用負極材の製造方法
JP2012234808A (ja) 2011-05-02 2012-11-29 Samsung Corning Precision Materials Co Ltd リチウムイオン二次電池用リチウムマンガンオキサイド正極活物質の製造方法、これによって製造された正極活物質及びこれを含むリチウムイオン二次電池
JP2017533548A (ja) 2014-11-05 2017-11-09 24エム・テクノロジーズ・インコーポレイテッド24M Technologies, Inc. 半固体電極を有する電気化学セルおよびその製造方法
JP2018139219A (ja) 2012-05-18 2018-09-06 24エム・テクノロジーズ・インコーポレイテッド24M Technologies, Inc. 電気化学セル及びその製造方法
JP2019021456A (ja) * 2017-07-14 2019-02-07 株式会社半導体エネルギー研究所 正極活物質、正極、正極の作製方法、および二次電池
JP2019067586A (ja) * 2017-09-29 2019-04-25 三洋化成工業株式会社 リチウムイオン電池用電極の製造方法及び電極組成物の充填装置
JP2021530829A (ja) 2018-07-09 2021-11-11 24エム・テクノロジーズ・インコーポレイテッド24M Technologies, Inc. 半固体電極および電池製造の連続的および半連続的方法
JP2022120973A (ja) 2021-02-08 2022-08-19 国立大学法人 名古屋工業大学 無線電力伝送用レクテナ用電力変換回路、無線電力伝送用レクテナ及びそれを用いた電力伝送方法

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5881943B2 (ja) * 2010-12-10 2016-03-09 日立化成株式会社 リチウム二次電池
JP7525984B2 (ja) * 2018-05-30 2024-07-31 三洋化成工業株式会社 電極活物質層の製造方法、リチウムイオン電池用電極の製造方法及びリチウムイオン電池の製造方法
JP7242868B2 (ja) * 2019-08-19 2023-03-20 富士フイルム株式会社 電極用成形体の製造方法

Patent Citations (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2011125577A1 (ja) * 2010-03-31 2011-10-13 住友金属工業株式会社 改質天然黒鉛粒子およびその製造方法
JP2012124121A (ja) * 2010-12-10 2012-06-28 Hitachi Chem Co Ltd リチウム二次電池用負極材の製造方法
JP2012234808A (ja) 2011-05-02 2012-11-29 Samsung Corning Precision Materials Co Ltd リチウムイオン二次電池用リチウムマンガンオキサイド正極活物質の製造方法、これによって製造された正極活物質及びこれを含むリチウムイオン二次電池
JP2018139219A (ja) 2012-05-18 2018-09-06 24エム・テクノロジーズ・インコーポレイテッド24M Technologies, Inc. 電気化学セル及びその製造方法
JP2017533548A (ja) 2014-11-05 2017-11-09 24エム・テクノロジーズ・インコーポレイテッド24M Technologies, Inc. 半固体電極を有する電気化学セルおよびその製造方法
JP2019021456A (ja) * 2017-07-14 2019-02-07 株式会社半導体エネルギー研究所 正極活物質、正極、正極の作製方法、および二次電池
JP2019067586A (ja) * 2017-09-29 2019-04-25 三洋化成工業株式会社 リチウムイオン電池用電極の製造方法及び電極組成物の充填装置
JP2021530829A (ja) 2018-07-09 2021-11-11 24エム・テクノロジーズ・インコーポレイテッド24M Technologies, Inc. 半固体電極および電池製造の連続的および半連続的方法
JP2022120973A (ja) 2021-02-08 2022-08-19 国立大学法人 名古屋工業大学 無線電力伝送用レクテナ用電力変換回路、無線電力伝送用レクテナ及びそれを用いた電力伝送方法

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
See also references of EP4564467A4

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2025206397A1 (ja) * 2024-03-29 2025-10-02 富士フイルム株式会社 電極の製造方法、電極の製造装置、及び電極膜の製造方法

Also Published As

Publication number Publication date
JPWO2024024786A1 (cg-RX-API-DMAC7.html) 2024-02-01
US20250149577A1 (en) 2025-05-08
CN119585880A (zh) 2025-03-07
EP4564467A1 (en) 2025-06-04
EP4564467A4 (en) 2025-11-26

Similar Documents

Publication Publication Date Title
EP4266418B1 (en) Cathode active material for secondary battery, preparation method therefor, and lithium secondary battery comprising same
KR102657451B1 (ko) 이차전지용 양극재 및 이를 포함하는 리튬 이차전지
US10199646B2 (en) Anodes for lithium-ion devices
EP4462502A2 (en) Positive electrode active material for secondary battery, method of preparing the same, and lithium secondary battery including the positive electrode active material
EP3486979A1 (en) Cathode active material for secondary battery, and preparation method therefor
KR102581795B1 (ko) 폐-양극 활물질을 이용한 리튬 이차전지용 양극 활물질의 제조 방법
JP7612642B2 (ja) 正極活物質及びこれを含むリチウム二次電池
JP2022529817A (ja) リチウム二次電池用正極活物質の製造方法および前記方法により製造されたリチウム二次電池用正極活物質
WO2019131519A1 (ja) リチウム二次電池用複合活物質およびその製造方法
KR20200030287A (ko) 이차전지용 양극재, 그 제조방법 및 이를 포함하는 리튬 이차전지
KR102697188B1 (ko) 리튬 이차전지의 제조 방법 및 이에 의하여 제조된 리튬 이차전지
KR102924383B1 (ko) 양극 활물질 및 이를 포함하는 리튬 이차전지
JP2024540133A (ja) 正極材、これを含む正極およびリチウム二次電池
JP2026511565A (ja) 正極活物質、それを含む正極およびリチウム二次電池
KR20250048222A (ko) 양극 활물질 및 이를 사용하는 리튬 이차전지
KR102724217B1 (ko) 리튬 이차전지, 전지 팩 및 이를 포함하는 전자 기기
US20250149577A1 (en) Production method of electrode material, manufacturing method of electrode for battery, and manufacturing method of battery
KR20250096661A (ko) 양극재, 이를 포함하는 양극 및 리튬 이차전지
JP2026510385A (ja) 正極活物質、それを含む正極、およびリチウム二次電池
KR102792103B1 (ko) 양극 활물질 및 이를 사용하는 리튬 이차전지
JP2026509601A (ja) 正極活物質、それを含む正極、およびリチウム二次電池
KR20250108354A (ko) 양극재, 이를 포함하는 양극 및 리튬 이차전지
JP7448657B2 (ja) 全固体二次電池用シート及び全固体二次電池の製造方法、並びに、全固体二次電池用シート及び全固体二次電池
JP2017117539A (ja) 電池用活物質、電池用電極、非水電解質電池、及び電池パック
KR102929048B1 (ko) 리튬 이차 전지용 양극 활물질, 이의 제조방법 및 이를 포함하는 리튬 이차 전지

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 23846516

Country of ref document: EP

Kind code of ref document: A1

WWE Wipo information: entry into national phase

Ref document number: 2024537749

Country of ref document: JP

WWE Wipo information: entry into national phase

Ref document number: 202380055001.3

Country of ref document: CN

WWE Wipo information: entry into national phase

Ref document number: 2023846516

Country of ref document: EP

NENP Non-entry into the national phase

Ref country code: DE

ENP Entry into the national phase

Ref document number: 2023846516

Country of ref document: EP

Effective date: 20250228

WWP Wipo information: published in national office

Ref document number: 202380055001.3

Country of ref document: CN

WWP Wipo information: published in national office

Ref document number: 2023846516

Country of ref document: EP