WO2020195181A1 - 表示装置、および表示装置の製造方法 - Google Patents

表示装置、および表示装置の製造方法 Download PDF

Info

Publication number
WO2020195181A1
WO2020195181A1 PCT/JP2020/004110 JP2020004110W WO2020195181A1 WO 2020195181 A1 WO2020195181 A1 WO 2020195181A1 JP 2020004110 W JP2020004110 W JP 2020004110W WO 2020195181 A1 WO2020195181 A1 WO 2020195181A1
Authority
WO
WIPO (PCT)
Prior art keywords
guide
dam
film
display device
display
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2020/004110
Other languages
English (en)
French (fr)
Japanese (ja)
Inventor
大輔 加藤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Japan Display Inc
Original Assignee
Japan Display Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Japan Display Inc filed Critical Japan Display Inc
Publication of WO2020195181A1 publication Critical patent/WO2020195181A1/ja
Priority to US17/474,749 priority Critical patent/US12178069B2/en
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Links

Images

Classifications

    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10K—ORGANIC ELECTRIC SOLID-STATE DEVICES
    • H10K59/00—Integrated devices, or assemblies of multiple devices, comprising at least one organic light-emitting element covered by group H10K50/00
    • H10K59/10—OLED displays
    • H10K59/12—Active-matrix OLED [AMOLED] displays
    • H10K59/124—Insulating layers formed between TFT elements and OLED elements
    • G—PHYSICS
    • G09—EDUCATION; CRYPTOGRAPHY; DISPLAY; ADVERTISING; SEALS
    • G09F—DISPLAYING; ADVERTISING; SIGNS; LABELS OR NAME-PLATES; SEALS
    • G09F9/00—Indicating arrangements for variable information in which the information is built-up on a support by selection or combination of individual elements
    • G—PHYSICS
    • G09—EDUCATION; CRYPTOGRAPHY; DISPLAY; ADVERTISING; SEALS
    • G09F—DISPLAYING; ADVERTISING; SIGNS; LABELS OR NAME-PLATES; SEALS
    • G09F9/00—Indicating arrangements for variable information in which the information is built-up on a support by selection or combination of individual elements
    • G09F9/30—Indicating arrangements for variable information in which the information is built-up on a support by selection or combination of individual elements in which the desired character or characters are formed by combining individual elements
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10K—ORGANIC ELECTRIC SOLID-STATE DEVICES
    • H10K50/00—Organic light-emitting devices
    • H10K50/80—Constructional details
    • H10K50/84—Passivation; Containers; Encapsulations
    • H10K50/844—Encapsulations
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10K—ORGANIC ELECTRIC SOLID-STATE DEVICES
    • H10K59/00—Integrated devices, or assemblies of multiple devices, comprising at least one organic light-emitting element covered by group H10K50/00
    • H10K59/10—OLED displays
    • H10K59/12—Active-matrix OLED [AMOLED] displays
    • H10K59/1201—Manufacture or treatment
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10K—ORGANIC ELECTRIC SOLID-STATE DEVICES
    • H10K59/00—Integrated devices, or assemblies of multiple devices, comprising at least one organic light-emitting element covered by group H10K50/00
    • H10K59/80—Constructional details
    • H10K59/87—Passivation; Containers; Encapsulations
    • H10K59/873—Encapsulations
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10K—ORGANIC ELECTRIC SOLID-STATE DEVICES
    • H10K71/00—Manufacture or treatment specially adapted for the organic devices covered by this subclass

Definitions

  • An embodiment of the present invention relates to a display device and a method for manufacturing the display device.
  • an embodiment of the present invention relates to a display device having an organic light emitting element in each pixel, and a method for manufacturing the same.
  • the organic EL display device includes an organic light emitting element (hereinafter referred to as a light emitting element) as a display element in each of a plurality of pixels formed on the substrate.
  • the light emitting element has a layer containing an organic compound (hereinafter referred to as an EL layer) between the pair of electrodes, and is driven by supplying an electric current between the pair of electrodes.
  • the organic compound is oxidized or reduced to take a charged state, and further, these are recombined to generate an excited state.
  • One of the embodiments according to the present invention is intended to provide a highly reliable display device and a method for manufacturing the same.
  • the display device includes a substrate, a transistor, a flattening film, a display element, a dam, and a guide.
  • the substrate has a display area and a peripheral area surrounding the display area.
  • the transistor is located on the display area.
  • the flattening film is located on the transistor and covers the transistor.
  • the display element is located on the flattening film and is electrically connected to the transistor.
  • the dam is located on the peripheral area and surrounds the display area.
  • the guide is located between the flattening membrane and the dam and surrounds the display area.
  • the guide contains a first organic compound contained in the flattening membrane.
  • the display device includes a substrate, a transistor, a flattening film, a display element, a first dam, a second dam, and a guide.
  • the substrate has a display area and a peripheral area surrounding the display area.
  • the transistor is located on the display area.
  • the flattening film is located on the transistor and covers the transistor.
  • the display element is located on the flattening film and is electrically connected to the transistor.
  • the first dam is located on the peripheral area and surrounds the display area.
  • the second dam is located on the surrounding area and surrounds the first dam.
  • the guide is located at least between the flattening membrane and the first dam, and between the first dam and the second dam.
  • the guide contains a first organic compound contained in the flattening membrane.
  • One of the embodiments of the present invention is a method for manufacturing a display device.
  • This manufacturing method encloses a flattening film and a flattening film on a transistor by forming a transistor on a substrate, forming a first resin so as to cover the transistor, and processing the first resin. It involves forming a guide and a dam surrounding the guide, as well as forming a display element that is electrically connected to the transistor.
  • the guide includes a plurality of insulating films formed from the first resin.
  • the schematic top view of the display device of this invention An equivalent circuit of the pixel circuit of the display device of the present invention.
  • Schematic cross-sectional view of the display device of the present invention The schematic top view of the display device of this invention.
  • the schematic top view of the display device of this invention Schematic cross-sectional view of the display device of the present invention.
  • the schematic top view of the display device of this invention Schematic cross-sectional view of the display device of the present invention.
  • the schematic top view of the display device of this invention. Schematic cross-sectional view of the display device of the present invention.
  • Schematic cross-sectional view of the display device of the present invention Schematic cross-sectional view of the guide and dam of the display device of the present invention. Schematic top view and sectional view of the guide of the display device of the present invention.
  • a schematic cross-sectional view for explaining an example of a manufacturing process of a conventional display device The upper surface schematic diagram which shows the state of the passivation film at the time of manufacturing of the display device of this invention.
  • the schematic top view of the guide of the display device of this invention The schematic top view of the display device of this invention.
  • Schematic cross-sectional view of the display device of the present invention A schematic cross-sectional view for explaining an example of a manufacturing process of a conventional display device.
  • the upper surface schematic diagram which shows the state of the passivation film at the time of manufacturing of the display device of this invention.
  • the schematic top view of the guide of the display device of this invention The schematic top view of the guide of the display device of this invention.
  • the schematic top view of the display device of this invention The schematic top view of the display device of this invention.
  • the schematic cross-sectional view for demonstrating the manufacturing method of the display device of this invention The schematic cross-sectional view for demonstrating the manufacturing method of the display device of this invention.
  • the schematic cross-sectional view for demonstrating the manufacturing method of the display device of this invention The schematic cross-sectional view for demonstrating the manufacturing method of the display device of this invention.
  • the schematic cross-sectional view for demonstrating the manufacturing method of the display device of this invention The schematic cross-sectional view for demonstrating the manufacturing method of the display device of this invention.
  • the plurality of films when one film is processed to form a plurality of films, the plurality of films may have different functions and roles. However, these plurality of films are derived from the films formed as the same layer in the same process and have the same material. Therefore, these multiple films are defined as existing in the same layer.
  • a structure is exposed from another structure means an aspect in which a part of one structure is not covered by another structure, and other structures.
  • the portion not covered by the structure also includes an embodiment covered by yet another structure.
  • FIG. 1 shows a schematic top view of the display device 100 according to the embodiment of the present invention.
  • the display device 100 has a substrate 102, on which a plurality of pixels 104 are provided.
  • a single region including the plurality of pixels 104 and a region surrounding the single region are defined as a display region 106 and a peripheral region of the substrate 102, respectively.
  • a drive circuit for driving the pixel 104 is provided in the peripheral region.
  • two scanning line driving circuits 108 sandwiching the display area 106 and a signal line driving circuit 110 including an analog switch and the like are provided.
  • Wiring (not shown) extends from the display area 106, the scanning line drive circuit 108, and the signal line drive circuit 110 to one side of the substrate 102, and is exposed at the end of the substrate 102 to form the terminal 112.
  • the terminal 112 is electrically connected to a connector 116 such as a flexible printed circuit (FPC) board.
  • a drive IC 114 for controlling the pixel 104 may be further mounted on the connector 116 or the substrate 102.
  • the signal line drive circuit 110 may not be provided on the peripheral region, and this function may be realized by the drive IC 114.
  • the terminal 112 side of the display device 100 is referred to as the lower portion, and the opposite side of the terminal 112 is referred to as the upper portion.
  • the substrate 102 and the display area 106 can be regarded as a quadrangle mainly composed of four sides, the side on the terminal 112 side is called the lower side, and the side opposite to the terminal 112 is called the upper side.
  • Each pixel 104 is provided with a pixel circuit including a display element 130.
  • the pixel circuit is driven by a scanning line drive circuit 108, a signal line drive circuit 110, or the like.
  • the operation of the display element 130 is controlled, and as a result, the image can be displayed on the display area 106.
  • the pixel circuit will be described with reference to an example in which a light emitting element is used as the display element 130.
  • the configuration of the pixel circuit can be arbitrarily selected, and an example thereof is shown in FIG. 2 as an equivalent circuit.
  • the pixel circuit shown in FIG. 2 has a drive transistor 150, a light emission control transistor 154, a correction transistor 152, an initialization transistor 156, a write transistor 158, a holding capacity 140, and an additional capacity 170 in addition to the display element 130. ..
  • the high-potential power supply line 180 is given a high-potential P VDD, and this potential is given to the pixels 104 connected to each row via the current supply line 182.
  • the display element 130, the drive transistor 150, the light emission control transistor 154, and the correction transistor 152 are connected in series between the high potential power supply line 180 and the low potential power supply line 184.
  • the low potential power line 184 is given a low potential PVSS.
  • the gate of the drive transistor 150 is electrically connected to the first signal line 188 via the initialization transistor 156 and also electrically connected to the second signal line 186 via the write transistor 158.
  • An initialization signal Vini is given to the first signal line 188, and a video signal Vsig is given to the second signal line 186.
  • the operation of the write transistor 158 is controlled by the scan signal SG given to the write control scan line 190 connected to the gate.
  • the gate of the initialization transistor 156 is connected to the initialization control scanning line 192 to which the initialization control signal IG is given, and the operation is controlled by the initialization control signal IG.
  • a correction control scanning line 194 to which the correction control signal CG is applied and a light emission control scanning line 198 to which the light emission control signal BG is applied are connected to the gates of the correction transistor 152 and the light emission control transistor 154, respectively.
  • a reset control line 196 is connected to the drain of the drive transistor 150 via the correction transistor 152.
  • the reset control line 196 is connected to a reset transistor 160 provided in the scanning line drive circuit 108.
  • the reset transistor 160 is controlled by the reset control signal RG, whereby the reset potential Vrst given to the reset signal line 200 can be applied to the drain of the drive transistor 150 via the correction transistor 152.
  • a holding capacity 140 is provided between the source and the gate of the drive transistor 150, and an additional capacity 170 is provided between the source of the drive transistor 150 and the low potential power supply line 184.
  • the additional capacitance 170 may be arranged so that both terminals are connected to the source of the drive transistor 150 and the high potential power line 180, respectively.
  • the signal line drive circuit 110 or the drive IC 114 outputs the initialization signal Vini and the video signal Vsig to the first signal line 188 and the second signal line 186, respectively.
  • the scan line drive circuit 108 outputs the scan signal SG to the write control scan line 190, outputs the initialization control signal IG to the initialization control scan line 192, and outputs the correction control signal CG to the correction control scan line 194.
  • the light emission control signal BG is output to the light emission control scanning line 198
  • the reset control signal RG is output to the gate of the reset transistor 160.
  • the pixel circuit shown in FIG. 2 is just an example, and there are no restrictions on the number of elements such as transistors and capacitances and the connection relationship.
  • FIG. 3 shows a display element 130, a holding capacity 140 connected to the display element 130, a drive transistor 150, and an additional capacity 170.
  • the substrate 102 has a function of supporting a circuit formed on the substrate 102, and may contain glass, quartz, or a polymer.
  • a polymer such as polyimide, polyamide, or polycarbonate for the substrate 102, flexibility can be imparted to the display device 100, and it is also possible to provide a so-called flexible display.
  • the drive transistor 150 includes a semiconductor film 204, a gate insulating film 206 on the semiconductor film 204, a gate electrode 210 on the gate insulating film 206, a first interlayer film 212 on the gate electrode 210, and a drain on the first interlayer film 212. It has an electrode 214, a source electrode 216, and the like.
  • the semiconductor film 204 may have an active region 204a, a low-concentration impurity region 204b sandwiching the active region 204a, a high-concentration impurity region 204c sandwiching these, and the like.
  • the drive transistor 150 is depicted as a transistor having a top gate structure in FIG. 3, there are no restrictions on the structure of the transistors constituting the pixel circuit, and transistors having various structures can be used.
  • the holding capacity 140 is a part of the semiconductor film 204 (high-concentration impurity region 204c), the gate insulating film 206 on the semiconductor film 204, the capacitance electrode 208 existing in the same layer as the gate electrode 210, and the first interlayer film on the capacitance electrode 208. It is composed of 212 and a part of the source electrode 216.
  • the gate insulating film 206 and the first interlayer film 212 function as a dielectric having a holding capacity of 140.
  • a flattening film 220 on the second interlayer film 218 and the second interlayer film 218 is further provided on the drive transistor 150 and the holding capacity 140.
  • the second interlayer film 218 is provided to prevent impurities from entering elements such as transistors and capacitances in the pixel circuit.
  • the flattening film 220 absorbs irregularities caused by the pixel circuit including the drive transistor 150, the holding capacity 140, and the like, and forms a flat surface.
  • the flattening film 220 and the second interlayer film 218 are provided with openings that reach the source electrode 216.
  • a connection pad 224 that covers this opening and a part of the flattening film 220 is provided so as to be in contact with the source electrode 216, and an additional capacitance electrode 172 is formed on the flattening film 220.
  • a third interlayer film 174 is further formed so as to cover the connection pad 224 and the additional capacitance electrode 172.
  • the third interlayer film 174 does not cover a part of the connection pad 224 at the opening provided in the flattening film 220, and exposes the upper surface of the connection pad 224.
  • the third interlayer film 174 may be provided with an opening 226 for allowing contact between the partition wall (also called a rib or a bank) 222 provided on the interlayer film 174 and the flattening film 220.
  • the formation of the connection pad 224 and the opening 226 is arbitrary. By providing the connection pad 224, it is possible to prevent oxidation of the surface of the source electrode 216 in the subsequent process, and it is possible to suppress an increase in contact resistance due to this.
  • the opening 226 can function as an opening for releasing impurities such as water and oxygen from the flattening film 220, and by providing this, the reliability of the semiconductor element and the display element 130 in the pixel circuit can be improved. Can be done.
  • a pixel electrode 132 is provided on the third interlayer film 174 so as to overlap the connection pad 224 and the additional capacitance electrode 172.
  • the pixel electrode 132 is electrically connected to the source electrode 216 via the connection pad 224 at the openings provided in the third interlayer film 174 and the flattening film 220.
  • the additional capacitance 170 is formed by the additional capacitance electrode 172, the third interlayer film 174, and the pixel electrode 132. Therefore, the pixel electrode 132 is shared by the additional capacitance 170 and the display element 130.
  • an inorganic compound containing silicon can be used for the undercoat 202, the gate insulating film 206, the first interlayer film 212, the second interlayer film 218, and the third interlayer film 174.
  • the silicon-containing inorganic compound include silicon oxide containing oxygen and silicon, oxygen and silicon, silicon nitride and silicon nitride containing nitrogen, and silicon nitride containing silicon and nitrogen. These films may have a single layer structure or a laminated structure.
  • the flattening film 220 and the partition wall 222 contain an organic compound. Examples of typical organic compounds include acrylic resin, epoxy resin, polysiloxane resin, polyimide resin, and polyamide resin.
  • the gate electrode 210, the capacitance electrode 208, the drain electrode 214, and the source electrode 216 are configured to include titanium, molybdenum, tungsten, tantalum, aluminum, copper, or an alloy thereof. These electrodes may be configured to have a structure in which a metal having high conductivity such as aluminum or copper is sandwiched between refractory metals such as titanium, molybdenum, tungsten and tantalum.
  • the display element 130 is composed of a pixel electrode 132, a counter electrode 136 on the pixel electrode 132, and an EL layer 134 sandwiched between the pixel electrode 132 and the counter electrode 136.
  • the pixel electrode 132 is a conductive oxide that is transparent to visible light, such as a mixed oxide of indium and tin (ITO) or a mixed oxide of indium and zinc (IZO), or a metal such as silver or aluminum. Alternatively, it includes an alloy of these metals.
  • the pixel electrode 132 may have either a single-layer structure or a laminated structure. When it has a laminated structure, for example, a structure in which a film containing a metal is sandwiched between a film containing a conductive oxide such as ITO or IZO can be adopted.
  • the EL layer 134 is provided so as to cover the pixel electrode 132 and the partition wall 222.
  • the EL layer 134 refers to the entire layer provided between the pixel electrode 132 and the counter electrode 136.
  • the EL layer 134 can be composed of a plurality of layers, and can be formed by combining various functional layers such as a charge injection layer, a charge transport layer, a light emitting layer, a charge block layer, and an exciton block layer.
  • the display element 130 can be configured so that the structure of the EL layer 134 is the same among all the pixels 104, or the structure is different among the adjacent pixels 104.
  • the EL layer 134 by forming the EL layer 134 so that the structure and material of the light emitting layer are different between the adjacent pixels 104, different light emission can be obtained from the adjacent pixels 104.
  • the same EL layer 134 is used for all the pixels 104, it is possible to obtain a plurality of emission colors by providing a color filter.
  • FIG. 3 a structure in which a hole injection / transport layer, a light emitting layer, and an electron injection / transport layer are laminated in order from the pixel electrode 132 is shown as a typical functional layer in consideration of visibility.
  • the counter electrode 136 is formed over a plurality of pixels 104. That is, the counter electrode 136 is shared by a plurality of pixels 104.
  • the counter electrode 136 includes, for example, a translucent conductive oxide such as ITO or IZO, a metal such as aluminum, magnesium, or silver, or an alloy thereof.
  • a translucent conductive oxide such as ITO or IZO
  • a metal such as aluminum, magnesium, or silver
  • an alloy thereof e.g., aluminum, magnesium, or silver
  • the pixel electrode 132 is formed so as to contain a metal having a high reflectance to visible light such as aluminum and silver, and the counter electrode 136 is formed. It is formed so as to be transparent to visible light.
  • the counter electrode 136 is formed of a film containing a conductive oxide such as ITO or IZO, or a metal thin film containing a metal such as silver, magnesium, or aluminum and having a thickness capable of transmitting visible light. Can be done.
  • a protective film (hereinafter, passivation film) 230 for protecting the display element 130 is provided on the display element 130.
  • the structure of the passivation film 230 can be arbitrarily selected, and for example, as shown in FIG. 3, a first inorganic film 232 containing an inorganic compound, an organic film 234 containing an organic compound, and a second containing an inorganic compound.
  • a laminated structure having an inorganic film 236 can be applied to the passivation film 230.
  • the above-mentioned silicon-containing inorganic compound can be used as the inorganic compound.
  • a polymer such as an epoxy resin or an acrylic resin can be used.
  • the first inorganic film 232 and the second inorganic film 236, which have low gas permeability, can effectively suppress the invasion of impurities from the outside.
  • the organic film 234 can have a relatively large thickness, thereby absorbing unevenness caused by the partition wall 222, foreign matter, or the like to provide a flat upper surface. Due to the flattening function of the organic film 234, the flatness of the second inorganic film 236 formed on the organic film 234 can be improved, and cracks and pinholes can be prevented from occurring in the second inorganic film 236. , The display element 130 can be protected more effectively.
  • a resin film 240 is provided on the passivation film 230.
  • the resin film 240 protects the display area 106 and also serves as a mask for exposing the terminals 112 by removing the first inorganic film 232 and the second inorganic film 236 formed on the terminals 112 by etching treatment. It is a film used and has a function of protecting the passivation film 230 during an etching process.
  • the resin film 240 also contains a polymer which is an organic compound, and examples of the polymer include acrylic resin, epoxy resin, and polyolefin resin.
  • the display device 100 may include a touch sensor between the passivation film 230 and the resin film 240, or on the resin film 240.
  • FIG. 4 shows a schematic top view of the structure of the four corners of the display device 100.
  • the configurations of the display element 130, the passivation film 230, the resin film 240, and the like are omitted.
  • the display device 100 has at least one guide 260 surrounding the display area 106, and a plurality of dams 250.
  • the display device 100 has four dams (first dam 250-1, second dam 250-2, third dam 250-3, fourth dam 250-4) and four. It has two guides (first guide 260-1, second guide 260-2, third guide 260-3, fourth guide 260-4).
  • Each guide 260 includes a plurality of insulating films (hereinafter referred to as guide insulating films) 262.
  • the first guide 260-1, the second guide 260-2, the third guide 260-3, and the fourth guide 260-4 are each a plurality of first guide insulating films 262-1.
  • guide insulating films hereinafter referred to as guide insulating films
  • FIG. 5 A schematic top view of the area 118-1 (see FIG. 1) located on the opposite side of the display area 106 from the terminal 112 is shown in FIG. 5, and a schematic cross-sectional view taken along the chain line AA'in FIG. It is shown in FIG. In these figures, a peripheral region and a part of the pixel 104 in the vicinity of the peripheral region are shown.
  • one or a plurality of wires 270 extending substantially parallel to the upper side of the substrate 102, the low potential power supply line 184, and the first low potential power supply line 184 are connected.
  • Connection wiring 138 and the like are provided. There are no restrictions on the number, use, or function of the wiring 270, and it can function as, for example, a high-potential power supply line 180 for giving P VDD to the pixel electrode 132, or a signal line for transmitting various signals to the drive circuit. In the example shown in FIG.
  • the wiring 270 and the low potential power supply line 184 exist in the same layer as the gate electrode 210 and the source electrode 216 (drain electrode 214), respectively, but the wiring 270 is located in the source electrode 216 (drain electrode 214). ), And the low potential power supply line 184 may be present in the same layer as the gate electrode 210. Alternatively, both or one of the wiring 270 and the low potential power line 184 may be formed of a metal film formed in a layer different from the gate electrode 210 and the source electrode 216 (drain electrode 214).
  • the first connection wiring 138 is configured to contain a conductive oxide such as ITO or IZO, or a metal such as titanium, tungsten, molybdenum, or aluminum.
  • the counter electrode 136 extends from the display region 106 to the peripheral region and is electrically connected to the low potential power supply line 184 in the peripheral region. This makes it possible to supply substantially the same potential to the counter electrode 136 over the entire display region 106.
  • the counter electrode 136 and the low-potential power line 184 may be in direct contact with each other, but as shown in FIG. 6, an electrical connection may be made via the first connection wiring 138 and the second connection wiring 228. ..
  • the second connection wiring 228 is located on the flattening film 220, and a part of the second connection wiring 228 is exposed from the partition wall 222 in the plurality of openings 226 formed in the partition wall 222 (FIGS. 5 and 6). At this opening 226, the counter electrode 136 and the second connection wiring 228 are connected.
  • the second connection wiring 228 can be formed in the same process as the pixel electrode 132, so that they have the same structure and can exist in the same layer.
  • the first guide 260-1 is located in the region between the flattening film 220 and the first dam 250-1 (first region 280).
  • the second guide 260-2 is located in the region between the first dam 250-1 and the second dam 250-2 (second region 282).
  • the third guide 260-3 is located in the region between the second dam 250-2 and the third dam 250-3 (third region 284).
  • the fourth guide 260-4 is located in the region between the third dam 250-3 and the fourth dam 250-4 (fourth region 286).
  • the flattening film 220 provided in the display area 106 extends in the upper side direction of the substrate 102 so as to cover a part of the low potential power supply line 184 (FIGS. 5 and 6). However, in the peripheral region, a part of the flattening film 220 is removed, and the remaining flattening film 220 forms a plurality of dams 250 and guides 260.
  • the flattening film 220 located below the display element 130 and the flattening film 220 located below the second connection wiring 228 are drawn so as to be separated, but the source electrode The openings used for the electrical connection between the 216 and the display element 130 do not completely separate them.
  • the first dam 250-1 and the second dam 250-2 have a function of controlling the shape and position of the organic film 234, while the third dam 250-3 and the fourth dam 250-4 have a function.
  • the manufacturing method of the display device 100 will be described later, but the organic film 234 and the resin film 240 are formed by using a wet film forming method such as an inkjet method or a printing method. That is, a solution or suspension containing a resin as a raw material or a precursor thereof (hereinafter, these solutions and suspension are collectively referred to as a raw material solution) is referred to as a first inorganic film 232 or a second inorganic film.
  • the organic film 234 and the resin film 240 are formed by discharging and coating on 236, then distilling off the solvent of the raw material solution, and / or reacting the precursor.
  • the raw material liquid that gives the organic film 234 spreads on the first inorganic film 232 and is discharged and applied so as to cover the entire display region 106. At this time, a part of the raw material liquid protrudes from the display area 106, which is blocked by the first dam 250-1.
  • the organic film 234 can be selectively formed in the first dam 250-1.
  • the raw material liquid flows out from the first dam 250-1, the raw material liquid is blocked by the second dam 250-2, whereby the substrate 102 is more than the second dam 250-2. The formation of the organic film 234 on the end side of the dam is prevented.
  • the raw material liquid that gives the resin film 240 spreads on the second inorganic film 236, and is discharged and applied so as to cover the entire display area 106 and the organic film 234. At this time, a part of the raw material liquid protrudes from the display area 106 and the organic film 234, which is blocked by the third dam 250-3. As a result, the resin film 240 can be selectively formed in the third dam 250-3. When the raw material liquid flows out from the third dam 250-3, the raw material liquid is blocked by the fourth dam 250-4, whereby the substrate 102 is more than the fourth dam 250-4. It is prevented that the resin film 240 is formed on the end side.
  • the organic film 234 covers at least a part of the first guide 260-1.
  • the organic film 234 may cover a part of the first dam 250-1 as shown in FIG. 6, and although not shown, the end is located between the first dam 250-1 and the flattening film 220. It may be arranged so as to. If the organic film 234 covers the first dam 250-1, the organic film 234 may further cover a part of the second dam 250-2, or the ends of the second dam 250-2 and the first dam 250-2. It may be formed so as to be located between the dams 250-1.
  • the resin film 240 covers the end portion of the organic film 234. That is, the end portion of the resin film 240 is located between the end portion of the substrate 102 closest to the end portion and the end portion of the organic film 234.
  • the resin film 240 covers the first dam 250-1 and the second dam 250-2.
  • the resin film 240 may cover a part of the third dam 250-3, and although not shown, the ends of the resin film 240 may cover the third dam 250-3 and the second dam 250-2. It may be arranged so as to be located between. Alternatively, it covers the third dam 250-3 and a part of the fourth dam 250-4, or the end is located between the third dam 250-3 and the fourth dam 250-4.
  • the resin film 240 may be arranged on the surface.
  • the first inorganic film 232 and the second inorganic film 236 of the passivation film 230 cover at least the first dam 250-1, preferably the second dam 250-2, and the third. Covers part of Dam 250-3.
  • the guide 260 has the same composition as the flattening film 220. That is, the guide insulating film 262 contains the organic compound contained in the flattening film 220.
  • the dam 250 has a two-layer structure consisting of a first layer 250a and a second layer 250b located on the first layer 250a.
  • the first layer 250a has the same composition as the flattening film 220 and contains an organic compound contained in the flattening film 220. Therefore, the flattening film 220, the guide insulating film 262, and the first layer 250a of the dam 250 are present in the same layer.
  • the height of the guide 260 that is, the height of the guide insulating film 262 is smaller than the height of the flattening film 220 and the height of the first layer 250a.
  • the upper surface of the guide insulating film 262 is closer to the substrate 102 than the upper surface of the flattening film 220 and the first layer 250a.
  • the second layer 250b has the same composition as the partition wall 222. That is, the second layer 250b contains the organic compound contained in the partition wall 222.
  • FIG. 7 is a schematic top view of the region 118-2 (see FIG. 1) including a part of the long side of the display device 100
  • FIG. 8 is a schematic cross-sectional view along the chain line BB'of FIG. Shown in.
  • a peripheral region and a part of the pixel 104 in the vicinity of the peripheral region are shown.
  • the description of the configuration that is the same as or similar to that of region 118-1 may be omitted.
  • a transistor or the like included in the scanning line drive circuit 108 is provided in the peripheral region. Similar to region 118-1 (FIG. 6), the counter electrode 136 extends from the display region 106 to the peripheral region and is electrically connected to the low potential power line 184 in the peripheral region. As shown in FIGS. 4, 7, and 8 (FIG. 6), at least one guide 260 and a plurality of dams 250 are provided in the peripheral region.
  • FIG. 9 shows a schematic top view of the area 118-3 (see FIG. 1) located on the terminal 112 side of the display area 106
  • FIG. 10 shows a schematic cross-sectional view along the chain line CC'in FIG. ..
  • a peripheral region and a part of the pixel 104 in the vicinity of the peripheral region are shown. Also in the following description, the description may be omitted for configurations that are the same as or similar to the regions 118-1 and 118-2.
  • a signal line drive circuit 110 including an analog switch or the like is formed in the peripheral region, and one or a plurality of wirings 272 and low potential power lines extending substantially parallel to the lower side of the substrate 102.
  • the first connection wiring 138 and the second connection wiring 228 connected to the 184 and the low potential power supply line 184 are provided.
  • a wiring 122 for supplying various signals and power to the pixel 104 or the signal line drive circuit 110 is formed between the display area 106 and the end of the substrate 102.
  • the wiring 122 can be formed from a conductive film formed in a plurality of layers. For example, as shown in FIG. 10, the wiring 122a existing in the same layer as the gate electrode 210 of the drive transistor 150 and the source electrode 216 (drain).
  • the wiring 122 can be formed by connecting the wiring 122b existing in the same layer as the electrode 214).
  • the wiring 122 is exposed at the end of the substrate 102 to form the terminal 112.
  • the upper surface of the wiring 122 may be covered with the protective conductive film 124.
  • the protective conductive film 124 is formed at the same time as, for example, the pixel electrode 132 or the connection pad 224, and can exist in the same layer as these.
  • the counter electrode 136 extends from the display region 106 to the peripheral region
  • the low potential power supply line 184 extends from the display region 106 to the peripheral region via the first connection wiring 138 and the second connection wiring 228 in the peripheral region. Is electrically connected to.
  • at least one guide 260 and a plurality of dams 250 are provided in the peripheral area.
  • the first area 280 to the fourth Guide 260 may be provided in at least one of the regions 286.
  • guide 260s may be formed in both the area between the flattening film 220 and one dam 250 and the area between the two dams 250, or only in one area.
  • a guide 260 may be formed.
  • the guide 260 is not provided in the second area 282 and the fourth area 286, and the first area 280 and the third area 280 and the third area 286 are provided.
  • the guide 260 may be provided in each of the regions 284, or the guide 260 may not be provided in the first region 280 and the third region 284, and the guide 260 may be provided in the second region 282 and the fourth region 286, respectively. You may.
  • each guide 260 is composed of a plurality of guide insulating films 262 containing an organic compound contained in the flattening film 220.
  • the guide insulating film 262 is arranged so that the longest side faces the display area 106. That is, each of the guide insulating films 262 is arranged so that the longest side is perpendicular to or substantially perpendicular to the direction in which one side of the display region 106 closest to the guide insulating film 262 extends.
  • the sides of 102) are the upper side and the lower side, respectively.
  • the longest side of these first guide insulating films 262-1 is perpendicular to or substantially perpendicular to the direction in which the upper side or the lower side extends.
  • the sides of the display area 106 (or the substrate 102) closest to the first guide insulating film 262-1 located in the side peripheral region (for example, region 118-3) of the display device 100 are the upper side and the lower side thereof. The side between them (vertical side).
  • the longest side of these first guide insulating films 262-1 is perpendicular to or substantially perpendicular to the direction in which the vertical side extends. However, at the four corners of each guide 260, the longest side of the guide insulating film 262 may be inclined with respect to the direction in which the side of the display region 106 (or the substrate 102) extends.
  • the first guide insulating film 262-1 is physically separated from at least one of the flattening film 220 and the first dam 250-1.
  • the second guide insulating film 262-2 to the fourth guide insulating film 262-4 are also physically separated from at least one of the adjacent dams 250, respectively.
  • the second guide insulating film 262-2 is separated from both the adjacent first dam 250-1 and the second dam 250-2 (FIG. 11 (A)). Or, it is in contact with one of the first dam 250-1 and the second dam 250-2 (FIGS. 11 (B) and 11 (C)).
  • the second guide 260-2 is integrated with the first layer 150a of the dam 250 in contact with it.
  • the other guides 260 are also physically separated from at least one of the adjacent dams 250, respectively.
  • the flattening film 220, the first layer 250a of the dam 250, and the guide 260 are formed from a single film containing an organic compound in the same process.
  • a membrane containing an organic compound has a higher transmittance for impurities such as water and oxygen than a membrane containing an inorganic compound, and therefore serves as a transport route for impurities.
  • this film is divided in the peripheral region to provide a flattening film 220, a first layer 250a, and a guide 260. Therefore, there is no path for impurities to enter the display region 106 from the outside through this film, deterioration of the display element 130 is suppressed, and the display device 100 exhibits high reliability.
  • FIG. 12 (A) A schematic top view of the guide insulating film 262 is shown in FIG. 12 (A), and a schematic cross-sectional view taken along the chain line DD'of FIG. 12 (A) is shown in FIG. 12 (B).
  • FIG. 12B also depicts a first inorganic film 232 provided on the guide insulating film 262.
  • the plurality of guide insulating films 262 included in each guide 260 are preferably configured so that the distance S between the two adjacent guide insulating films 262 is at least twice the thickness t of the first inorganic film 232. ..
  • the interval S is preferably d / 2 or less, where d is the diameter of the droplet of the raw material liquid that gives the organic film 234 or the resin film 240. ..
  • the width W of each guide insulating film 262 can be 10 ⁇ m or more and 100 ⁇ m or less, 10 ⁇ m or more and 50 ⁇ m, or 20 ⁇ m or more and 50 ⁇ m.
  • the interval S can be 10 ⁇ m or more and 150 ⁇ m or less, 10 ⁇ m or more and 100 ⁇ m or less, or 20 ⁇ m or more and 50 ⁇ m or less.
  • the width W and the interval S may be different for each guide 260.
  • the discharged / applied raw material liquid is the first inorganic film 232 or the first inorganic film 232 or the first.
  • the inkjet method and the printing method are one of the methods capable of forming a thin film with relatively good regioselectivity, it is not always easy to appropriately adjust the above-mentioned parameters, and as a result, the resulting thin film can be formed. It may not be possible to precisely control the shape and position. For example, when the raw material liquid does not spread sufficiently on the first inorganic film 232 due to the high viscosity of the raw material liquid or the low affinity between the raw material liquid and the first inorganic film, the first one on the display area 106. The inorganic film 232 may be exposed from the raw material liquid. Further, as shown in FIG.
  • the guide 260 gives a fine uneven structure to the peripheral region. Further, the distance S between the adjacent guide insulating films 262 in each guide 260 is at least twice the thickness t of the first inorganic film 232. Therefore, the first inorganic film 232 formed on the guide 260 reflects the uneven structure caused by the plurality of guide insulating films 262 included in the guide 260. As a result, a plurality of fine grooves are formed on the upper surface of the first inorganic film 232 (FIG. 12 (B)).
  • the groove of the first inorganic film 232 caused by the second guide 260-2 can surely spread the raw material liquid to the end of the second guide 260-2.
  • the first guide 260-1 and the second guide 260-2 are formed in the first dam 250-1 by forming the first guide 260-1.
  • the organic film 234 can be selectively formed in the first dam 250-1 or the second dam 250-2, and the flat surface required by the second inorganic film 236 can be sufficiently provided. Can be secured.
  • the organic film 234 even if foreign matter adheres to the peripheral region, not only the foreign matter can be sufficiently covered by the organic film 234, but also defects such as pinholes can be prevented from occurring in the second inorganic film 236. it can. This contributes to the provision of a highly reliable display device.
  • the third guide 260-3 and the fourth guide 260-4 are effective for controlling the shape of the resin film 240.
  • the third guide 260-3 and the fourth guide 260-4 also provide a fine uneven structure in the peripheral region.
  • the third guide 260-3 and the fourth guide 260-4 are covered with the first inorganic film 232 and the second inorganic film 236, and the resin is placed on the first inorganic film 232 and the second inorganic film 236.
  • the raw material liquid that gives the film 240 is discharged and applied. Therefore, although not shown, this uneven structure is reflected in the second inorganic film 236, and a plurality of fine grooves are formed on the upper surface of the second inorganic film 236.
  • the raw material liquid that gives the resin film 240 comes into contact with one end of the groove caused by the third guide insulating film 262-3 or the fourth guide insulating film 262-4, the raw material liquid is inside the groove due to the capillary phenomenon. It extends through to the other end. Therefore, the raw material liquid can be reliably spread to the region where the third guide 260-3 or the fourth guide 260-4 is formed.
  • the resin film 240 is selectively placed in the third dam 250-3 or in the fourth dam 250-4. Can be formed.
  • the display area 106 and the passivation film 230 provided on the display area 106 can be reliably sealed and protected by the resin film 240.
  • the resin film 240 also functions as an etching mask for the first inorganic film 232 and the second inorganic film 236. Therefore, the third guide 260-3 and the fourth guide 260-4 also contribute to precise control of the shapes of the first inorganic film 232 and the second inorganic film 236.
  • the guide insulating films 262 may be arranged in a staggered arrangement. That is, the guide insulating film 262 can be arranged so that the straight line (dotted line in FIG. 15A) connecting the centers of gravity of each guide insulating film 262 draws a zigzag shape in the extending direction of the guide 260.
  • the longest side of all the guide insulating films 262 or some of the guide insulating films 262 of each guide 260 extends from the side of the substrate 102 or the display area 106 closest to the guide insulating film 262.
  • the guide insulating film 262 may be arranged so as to be inclined with respect to the direction.
  • the longest side of the guide insulating film 262 may be tilted with respect to the direction in which the guide 260 is stretched.
  • the pair of adjacent guide insulating films 262 may be tilted in opposite directions, and are arranged line-symmetrically about an axis perpendicular to the direction in which the guide 260 extends. You may.
  • the guide insulating films 262 need not all have the same length in each guide 260, and at least a part thereof may have a different length from the other parts.
  • the capillary phenomenon acts on the raw material liquid that gives the organic film 234 and the resin film 240 due to the uneven structure provided by the guide 260. Therefore, for example, the raw material liquid has a high viscosity, or the raw material liquid has a low affinity with the surface to be treated, and the raw material liquid has a high contact angle, so that the raw material liquid has a high contact angle on the first inorganic film 232 and the second inorganic film 236.
  • the display region 106 and the peripheral region can be reliably covered with the organic film 234 or the resin film 240, and the influence of foreign matter can be effectively eliminated. As a result, reliable sealing is achieved for the display device 100, and high reliability can be imparted.
  • the longest side of the guide insulating film 262 of each guide 260 is the display area 106 (or the substrate 102) closest to the guide insulating film 262. ) Is parallel to or substantially parallel to the extending direction. Specific examples are shown in a schematic top view of region 118-1 (FIG. 16) and a schematic cross-sectional view (FIG. 17) along the chain line EE'in FIG. As shown in FIG. 16, in each guide 260, the plurality of guide insulating films 262 take a staggered arrangement.
  • the plurality of guide insulating films 262 are arranged in two rows along the extending direction of the guide 260, and the lines connecting the centers of gravity of the adjacent guide insulating films 262 have a zigzag structure (FIGS. 16 and 16). 17). Focusing on one row, the distance between adjacent guide insulating films 262 is shorter than the length of the longest side of the guide insulating film 262. Further, when observed in a direction parallel to the main surface of the substrate 102 (direction of arrow 292), the space between the adjacent guide insulating films 262 in one row is blocked by the guide insulating film 262 in the other row. Since other configurations are the same as those of the display device 100, the description thereof will be omitted.
  • the viscosity of the raw material liquid used for forming the organic film 234 or the resin film 240 is low, or the affinity between the raw material liquid and the surface to be treated (first inorganic film 232, second inorganic film 236, etc.) is high. In that case, the raw material liquid may spread excessively. For example, as shown in FIG. 18, when the raw material liquid giving the organic film 234 flows out to the end side of the substrate 102 beyond the third dam 250-3, the organic film 234 is formed on the second dam 250-3. It is exposed from the inorganic film 236 and the resin film 240. As a result, impurities easily penetrate into the organic film 234, and the passivation film 230 loses its function.
  • the raw material liquid is spread in the direction in which the guide 260 is stretched by the guide insulating film 262, and the raw material liquid is spread in the direction perpendicular to the direction in which the guide 260 is stretched. It can be dammed.
  • the first region 280 sandwiched between the flattening film 220 and the first dam 250-1 will be described as an example.
  • the raw material liquid exceeding the flattening film 220 is subjected to the first guide insulation. Since the film 262-1 extends perpendicularly to the traveling direction of the raw material liquid (the direction of the arrow in the figure), it is blocked by the first guide insulating film 262-1.
  • the raw material liquid spreads in the direction in which the guide 260 stretches (the direction perpendicular to the direction of the arrow in the figure).
  • the organic film 234 can be selectively formed in the first dam 250-1.
  • a second guide 260-2 having a similar arrangement is provided in the second region 282 even when the raw material liquid exceeds the first guide 260-1 and the first dam 250-1. Therefore, the raw material liquid is not blocked by the second guide insulating film 262-2 and does not exceed the second dam 250-2, and the organic film 234 is selectively formed in the second dam 250-2. be able to. Based on such a mechanism, the shape and position of the organic film 234 can be precisely controlled.
  • a similar mechanism works when the resin film 240 is formed. That is, when the raw material liquid that gives the resin film 240 flows out from the third dam 250-3 to the end of the substrate 102, it is blocked by the fourth guide insulating film 262-4 of the fourth guide 260-4. It is possible to prevent the fourth dam 250-4 from being exceeded.
  • the resin film 240 is formed so that the end portion is located between the second dam 250-2 and the third dam 250-3, the raw material liquid is released by the third guide insulating film 262-3. It is prevented from flowing out beyond the dam 250-3 of 3. As a result, the shape and position of the resin film 240 are precisely controlled.
  • each guide 260 the arrangement and shape of the guide insulating film 262 in each guide 260 are not limited to those described above.
  • a plurality of guide insulating films 262 arranged in two rows are provided, and the guide insulating films 262 forming one row are integrated into one insulating film surrounding the display area 106.
  • Each guide 260 may be configured so as to be. In this case, in each guide 260, the guide insulating film 262 formed as one insulating film may be closer to or farther from the display area 106 than the plurality of guide insulating films 262 forming other rows. ..
  • each guide 260 may be composed of one guide insulating film 262 surrounding the display area 106 and one guide insulating film 262 surrounding the guide insulating film 262. ..
  • the guide insulating films 262 may be arranged in three rows or more in the direction in which the guide 260 is stretched. In this case, focusing on two adjacent rows, it is preferable to configure the guide 260 so that the plurality of guide insulating films 262 take a staggered arrangement.
  • 20 (A) to 20 (C) show guides 260 sandwiched between two adjacent dams 250, but these are also shown in the guide 260 sandwiched between the flattening film 220 and the first dam 250-1. A variant of is applicable.
  • each guide 260 is perpendicular to the guide insulating film 262 whose longest side is parallel or substantially parallel to the direction in which the side of the display area 106 (or the substrate 102) extends. Alternatively, it has a guide insulating film 262 that is substantially vertical.
  • each guide 260 has a plurality of guide insulating films 262 arranged in three rows, and in one row, the longest side of the guide insulating film 262 is the display area 106 closest to the guide insulating film 262. (Or the substrate 102) is perpendicular to or substantially perpendicular to the extending direction. On the other hand, in the other two rows, the longest side of the guide insulating film 262 is parallel to or substantially parallel to the direction in which the side of the display region 106 (or the substrate 102) closest to the guide insulating film 262 extends. In the latter row, the plurality of guide insulating films 262 can be staggered.
  • the guide insulating film 262 arranged in the former one row promotes the spread of the raw material liquid that gives the organic film 234 and the resin film 240, and the guide insulating film 262 arranged in the latter two rows excessively spreads the raw material liquid. Suppress that. As a result, the organic film 234 and the resin film 240 can be selectively formed in a desired region.
  • each guide 260 may include one or a plurality of comb-shaped guide insulating films 262.
  • the comb-shaped guide insulating film 262 also surrounds the display area 106.
  • the comb-shaped guide insulating film 262 has a portion perpendicular to the extending direction and a portion parallel to the side of the display region 106 (or the substrate 102) closest to the guide insulating film 262.
  • the former promotes the spread of the raw material liquid, and the latter suppresses the excessive spread of the raw material liquid.
  • the organic film 234 and the resin film 240 can be selectively formed in a desired region.
  • one or more comb-shaped guide insulating films 262 and the display region 106 (or substrate 102) having the longest side closest to the guide insulating film 262 are parallel to the extending direction.
  • the guide 260 may be configured to have a plurality of guide insulating films 262 to be arranged. The spread of the raw material liquid is promoted by the portion of the comb-tooth-shaped guide insulating film 262 in which the side of the display region 106 (or the substrate 102) closest to the guide insulating film 262 is perpendicular to the extending direction.
  • the raw material is provided by the remaining portion of the comb-shaped guide insulating film 262 and a plurality of guide insulating films 262 whose longest sides are arranged in parallel in the extending direction of the display region 106 (or substrate 102) closest to the remaining portion. Excessive spread of the liquid is suppressed.
  • a plurality of guides 260 may be configured so that the guides 260 having different arrangements of the guide insulating films 262 alternate.
  • the first guide insulating film 262-1 and the third guide insulating film 262-3 of the first guide 260-1 and the third guide 260-3 have the longest sides, respectively. Is arranged so that the side of the display region 106 (or the substrate 102) closest to the side is perpendicular to or substantially perpendicular to the extending direction.
  • the second guide insulating film 262-2 and the fourth guide insulating film 262-4 of the second guide 260-2 and the fourth guide 260-4 have the longest side closest to the display area 106. (Or the substrate 102) is arranged so as to be parallel to or substantially parallel to the extending direction.
  • the shapes and positions of the organic film 234 and the resin film 240 can be controlled more precisely. That is, the first guide 260-1 and the second guide 260-2 achieve promotion of the spread of the raw material liquid that gives the organic film 234 and suppression of excessive spread, respectively. Similarly, the third guide 260-3 and the fourth guide 260-4 achieve promotion of spreading of the raw material liquid that gives the resin film 240 and suppression of excessive spreading, respectively.
  • a guide insulating film having a function of promoting the spread of the raw material liquid that gives a film formed by the wet film forming method and a guide insulating film having a function of suppressing the excessive spread coexist.
  • FIGS. 6 and 23 (A) to 27 are schematic cross-sectional views corresponding to FIG. The description of the same or similar configurations as those of the first to third embodiments may be omitted.
  • FIG. 23 (A) shows a structure in which the drive transistor 150 and the second interlayer film 218 covering the drive transistor 150 are formed. Since this structure can be produced by applying a known method, the description thereof is omitted.
  • the second interlayer film 218 is etched to open an opening for electrical connection between the first connection wiring 138 and the low potential power line 184. It is formed on the second interlayer film 218. After that, the first connection wiring 138 is formed on the second interlayer film 218 so as to cover this opening (FIG. 23 (C)).
  • the first connection wiring 138 can be formed by applying a sputtering method, a chemical vapor deposition (CVD) method, or the like.
  • the photosensitive resin 219 is formed on the entire surface of the substrate 102 so as to cover the pixel circuit including the drive transistor 150 and the peripheral region.
  • the photosensitive resin 219 is a film that provides the flattening film 220 and the first layer 250a of the dam 250.
  • a solution or suspension of a photosensitive resin containing an organic compound such as an acrylic resin, an epoxy resin, a polysiloxane resin, a polyimide resin, or a polyamide resin, or a precursor thereof is spin-coated.
  • a method, a printing method, an inkjet method, a dip coating method, or the like is applied to apply the coating to the entire surface of the substrate 102, and then the solvent is distilled off.
  • a sheet-shaped photosensitive resin 219 containing the organic compound or a precursor thereof is attached.
  • the photomask 294 is placed on the substrate 102, and the photosensitive resin 219 is irradiated with light.
  • the photomask 294 is a so-called gray tone mask or a halftone mask, and has a translucent portion 294-1, a light-shielding portion 294-2, and a semi-transmissive portion 294-3.
  • the translucent portion 294-1 has a transmittance of 75% or more and 100% or less, or 80% or more and 100% or less with respect to the light (irradiation light) used for exposure.
  • the light-shielding portion 294-2 has a transmittance of, for example, 0% or more and 5% or less, 0% or more and 2% or less, 0% or more and 1% or less, or substantially 0%.
  • the transmittance of the semi-transmissive portion 294-3 with respect to the irradiation light is 20% or more and 60% or less, 30% or more and 50% or less, and typically 40%.
  • the region forming the guide 260 is a translucent portion so that the region forming the first layer 250a of the flattening film 220 and the dam 250 is covered by the light-shielding portion 294-2.
  • the photomask 294 is designed and arranged so that the remaining region (that is, the region from which the photosensitive resin 219 is completely removed) is covered by the translucent portion 294-1 so as to be covered by 294-3.
  • the region forming the guide 260 is covered by the translucent portion 294-1 so that the region forming the first layer 250a of the flattening film 220 and the dam 250 is covered.
  • the photomask 294 is designed and arranged so that the remaining area is covered by the light-shielding portion 294-2 so that is covered by the semi-transmissive portion 294-3. By arranging the photomask 294 in this way, exposing it, and then developing it, the flattening film 220, the first layer 250a of the dam 250, and the guide insulating film 262 are formed (FIG. 24 (B). )).
  • the photosensitive resin 219 When the photosensitive resin 219 is of the positive type, the high solubility of the photosensitive resin 219 in the developing solution is maintained in the unexposed portion, that is, the region covered by the light-shielding portion 294-2. Is maintained almost as it is.
  • the semi-exposed portion that is, the region covered by the semi-transmissive portion 294-3, only a part of the photosensitive resin 219 is exposed, and the solubility is increased. As a result, the exposed portion is dissolved in the developing solution, and the other portion remains.
  • the height of the first layer 250a of the flattening film 220 and the dam 250 corresponding to the unexposed portion is the same as or substantially the same as the height of the photosensitive resin 219 before exposure, whereas it is half.
  • the height of the guide 260 corresponding to the exposed portion is smaller than the height of the photosensitive resin 219 before exposure.
  • a guide insulating film 262 lower than the flattening film 220 and the first layer 250a is obtained.
  • the photosensitive resin 219 is a negative type.
  • the solubility of the photosensitive resin 219 in the developing solution is significantly reduced, so that the photosensitive resin 219 is not dissolved by the development, and the height of the photosensitive resin 219 is maintained substantially as it is.
  • the region covered by the translucent portion 294-3 only a part of the photosensitive resin 219 is exposed, so that a part is dissolved in the developing solution and the other part remains.
  • the height of the first layer 250a of the flattening film 220 and the dam 250 corresponding to the exposed portion is the same as or substantially the same as the height of the photosensitive resin 219 before exposure, whereas it is half.
  • the height of the guide 260 corresponding to the exposed portion is smaller than the height of the photosensitive resin 219 before exposure.
  • a flattening film 220 derived from the same photosensitive resin 219, a first layer 250a, and a guide insulating film 262 lower than the first layer 250a can be obtained.
  • a part of the opening for electrical connection between the drive transistor 150 and the display element 130 is formed in the flattening film 220 (FIG. 24 (B)). Further, although not shown, the photosensitive resin 219 is removed even in the region overlapping the terminal 112, and the terminal 112 is exposed (see FIG. 10). Then, the second interlayer film 218 is further etched in this opening, and the source electrode 216 is exposed from the flattening film 220 (FIG. 25 (A)).
  • connection pad 224 is formed so as to cover the openings formed in the flattening film 220 and the second interlayer film 218, and an additional capacitance electrode 172 is formed so as to cover a part of the upper surface of the flattening film 220. Will be done. These can also be formed by applying a CVD method or a sputtering method. At this time, the protective conductive film 124 that protects the wiring 122 may be formed at the terminal 112 at the same time (see FIG. 10).
  • a third interlayer film 174 covering a part of the additional capacitance electrode 172 and the connection pad 224 is formed. Further, the pixel electrode 132 is formed so as to overlap the additional capacitance electrode 172, and the second connection wiring 228 is formed so as to overlap a part of the flattening film 220 and the first connection wiring 138 (FIG. 25 (B)). These films and wirings can also be formed by applying a CVD method or a sputtering method. Since the pixel electrode 132 and the second connection wiring 228 can be formed at the same time, they can exist in the same layer.
  • the partition wall 222 and the second layer 250b of the dam 250 are formed so as to cover the end portion of the pixel electrode 132 and the first layer 250a of the dam 250 (FIG. 25B). These can also be formed by applying a photosensitive resin to almost the entire surface of the substrate 102 and exposing and developing the photosensitive resin with a photomask having a light-shielding portion and a translucent portion. At this time, the opening 226 is also formed at the same time. By simultaneously forming the partition wall 222 and the second layer 250b of the dam 250 in this way, they can exist in the same layer, have the same composition, and contain the same organic compound.
  • the EL layer 134 is formed so as to cover the partition wall 222 and the pixel electrode 132, and the counter electrode 136 is further formed on the EL layer 134 (FIG. 26 (A)).
  • These are formed by a wet film deposition method such as an inkjet method or a printing method, as well as a vapor deposition method or a sputtering method.
  • the counter electrode 136 is formed from the display region 106 to the peripheral region so as not only to cover the EL layer 134 but also to be connected to the second connection wiring 228 at the opening 226.
  • the display element 130 is formed by the above steps.
  • the first inorganic film 232 is formed on almost the entire surface of the substrate 102. As a result, not only the display element 130 but also the dam 250 is covered with the first inorganic film 232 (FIG. 26 (B)).
  • the organic film 234 is formed by using an inkjet method or a printing method (FIG. 26 (B)).
  • the display device 100 is provided with at least one guide 260 having a plurality of guide insulating films 262 in the peripheral region. Therefore, the mechanisms described in the first to third embodiments work, and the shape and position of the organic film 234 can be precisely controlled.
  • the organic film 234 is provided so as to cover the first guide insulating film 262-1 and overlap a part of the first dam 250-1.
  • the second inorganic film 236 is formed on the organic film 234 and the first inorganic film 232 by using the CVD method. Since the second inorganic film 236 is also formed on almost the entire surface of the substrate 102, the first inorganic film 232 comes into contact with the second inorganic film 236 on the third dam 250-3 and the fourth dam 250-4. (Fig. 26 (B)). With this configuration, the organic film 234 is sealed by the first inorganic film 232 and the second inorganic film 236, and the invasion of impurities into the organic film 234 from the outside is prevented.
  • the resin film 240 is subsequently formed (FIG. 27).
  • the resin film 240 is also formed by using a raw material liquid and using an inkjet method or a printing method.
  • the display device 100 is provided with at least one guide 260 having a plurality of guide insulating films 262 in the peripheral region. Therefore, the mechanisms described in the first to third embodiments work, and the shape and position of the resin film 240 can be precisely controlled.
  • the resin film 240 covers the first guide insulating film 262-1 to the third guide insulating film 262-3, the first dam 250-1, and the second dam 250-2. It is provided so as to overlap a part of the third dam 250-3.
  • etching processing is performed on the first inorganic film 232 and the second inorganic film 236 to partially remove the first inorganic film 232 and the second inorganic film 236.
  • etching processing is performed on the first inorganic film 232 and the second inorganic film 236 to partially remove the first inorganic film 232 and the second inorganic film 236.
  • Fig. 6 etching processing is performed on the first inorganic film 232 and the second inorganic film 236 to partially remove the first inorganic film 232 and the second inorganic film 236.
  • the fourth dam 250-4 and the fourth guide 260-4 are exposed, but also the first inorganic film 232 and the second inorganic film 236 formed on the terminal 112 are removed.
  • the conductive wiring 122 or the protective conductive film 124 is exposed, and electrical connection with the connector 116 becomes possible.
  • the display device 100 is manufactured by the above steps.
  • the manufacturing method of the present embodiment provides a highly reliable display device.
  • an EL display device is mainly illustrated as a disclosure example, but as another application example, an electronic paper type display having another self-luminous display device, a liquid crystal display device, an electrophoresis element, or the like. All flat panel type display devices such as devices can be mentioned. In addition, it can be applied from small to medium size to large size without any particular limitation.

Landscapes

  • Engineering & Computer Science (AREA)
  • Physics & Mathematics (AREA)
  • Microelectronics & Electronic Packaging (AREA)
  • General Physics & Mathematics (AREA)
  • Theoretical Computer Science (AREA)
  • Optics & Photonics (AREA)
  • Electroluminescent Light Sources (AREA)
  • Devices For Indicating Variable Information By Combining Individual Elements (AREA)
  • Manufacturing & Machinery (AREA)
PCT/JP2020/004110 2019-03-22 2020-02-04 表示装置、および表示装置の製造方法 Ceased WO2020195181A1 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
US17/474,749 US12178069B2 (en) 2019-03-22 2021-09-14 Display device and manufacturing method of the display device

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2019-054990 2019-03-22
JP2019054990A JP7269050B2 (ja) 2019-03-22 2019-03-22 表示装置、および表示装置の製造方法

Related Child Applications (1)

Application Number Title Priority Date Filing Date
US17/474,749 Continuation US12178069B2 (en) 2019-03-22 2021-09-14 Display device and manufacturing method of the display device

Publications (1)

Publication Number Publication Date
WO2020195181A1 true WO2020195181A1 (ja) 2020-10-01

Family

ID=72558908

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2020/004110 Ceased WO2020195181A1 (ja) 2019-03-22 2020-02-04 表示装置、および表示装置の製造方法

Country Status (3)

Country Link
US (1) US12178069B2 (enExample)
JP (1) JP7269050B2 (enExample)
WO (1) WO2020195181A1 (enExample)

Families Citing this family (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR102724697B1 (ko) * 2020-02-21 2024-11-01 삼성디스플레이 주식회사 표시 장치 및 가요성 표시 장치
KR102929009B1 (ko) * 2021-08-09 2026-02-24 삼성디스플레이 주식회사 표시 장치 및 그의 제조 방법
CN117425368A (zh) * 2022-07-08 2024-01-19 京东方科技集团股份有限公司 显示面板和显示装置
WO2024134878A1 (ja) * 2022-12-23 2024-06-27 シャープディスプレイテクノロジー株式会社 表示装置、および表示装置の製造方法
JP2025072823A (ja) 2023-10-25 2025-05-12 株式会社ジャパンディスプレイ 表示装置および表示装置用マザー基板

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2012003989A (ja) * 2010-06-17 2012-01-05 Hitachi Displays Ltd 有機エレクトロルミネッセンスパネルの製造方法
JP2017147165A (ja) * 2016-02-19 2017-08-24 株式会社ジャパンディスプレイ 表示装置
WO2018179035A1 (ja) * 2017-03-27 2018-10-04 シャープ株式会社 表示装置
WO2019012680A1 (ja) * 2017-07-14 2019-01-17 シャープ株式会社 電気光学装置の製造方法および電気光学装置

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7109653B2 (en) * 2002-01-15 2006-09-19 Seiko Epson Corporation Sealing structure with barrier membrane for electronic element, display device, electronic apparatus, and fabrication method for electronic element
KR102391361B1 (ko) * 2015-01-14 2022-04-27 삼성디스플레이 주식회사 유기 발광 표시 장치
KR102409060B1 (ko) 2015-09-11 2022-06-16 삼성디스플레이 주식회사 표시 장치

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2012003989A (ja) * 2010-06-17 2012-01-05 Hitachi Displays Ltd 有機エレクトロルミネッセンスパネルの製造方法
JP2017147165A (ja) * 2016-02-19 2017-08-24 株式会社ジャパンディスプレイ 表示装置
WO2018179035A1 (ja) * 2017-03-27 2018-10-04 シャープ株式会社 表示装置
WO2019012680A1 (ja) * 2017-07-14 2019-01-17 シャープ株式会社 電気光学装置の製造方法および電気光学装置

Also Published As

Publication number Publication date
JP7269050B2 (ja) 2023-05-08
US20210408480A1 (en) 2021-12-30
US12178069B2 (en) 2024-12-24
JP2020154235A (ja) 2020-09-24

Similar Documents

Publication Publication Date Title
US12178067B2 (en) Display device
US12178083B2 (en) Display device
US12268047B2 (en) Display device
JP7269050B2 (ja) 表示装置、および表示装置の製造方法
JP5284544B2 (ja) 半導体装置および表示装置
US9831391B2 (en) Light emitting display device and manufacturing method of the light emitting display device
JP2019179696A (ja) 有機el表示装置および有機el表示装置の製造方法
JP6726973B2 (ja) 表示装置
US11349098B2 (en) Display device with an improved sealing layer
US12382791B2 (en) Display device including a micro lens array
US20200091258A1 (en) Display device, display device production method, display device production apparatus, and controller
WO2020008583A1 (ja) 表示デバイス、表示デバイスの製造方法、表示デバイスの製造装置
KR20230140314A (ko) 표시 장치
JP2021048048A (ja) 表示装置及び表示装置の製造方法
TWI912873B (zh) 顯示裝置及其製造方法
CN112599562A (zh) 显示装置

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 20777397

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 20777397

Country of ref document: EP

Kind code of ref document: A1