WO2017049808A1 - Procédé de production de soufflage de film - Google Patents

Procédé de production de soufflage de film Download PDF

Info

Publication number
WO2017049808A1
WO2017049808A1 PCT/CN2016/000418 CN2016000418W WO2017049808A1 WO 2017049808 A1 WO2017049808 A1 WO 2017049808A1 CN 2016000418 W CN2016000418 W CN 2016000418W WO 2017049808 A1 WO2017049808 A1 WO 2017049808A1
Authority
WO
WIPO (PCT)
Prior art keywords
thickness
bubble
point
normal
control mechanism
Prior art date
Application number
PCT/CN2016/000418
Other languages
English (en)
Chinese (zh)
Inventor
李子平
林洁波
林蔚
Original Assignee
广东金明精机股份有限公司
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 广东金明精机股份有限公司 filed Critical 广东金明精机股份有限公司
Publication of WO2017049808A1 publication Critical patent/WO2017049808A1/fr

Abstract

La présente invention concerne un procédé de production de soufflage de film qui comprend les étapes suivantes : (1) un dispositif de mesure d'épaisseur de bulle mesure en continu les épaisseurs initiales de divers points sur une bulle le long d'une direction circonférentielle ; (2) divers mécanismes de régulation d'épaisseur de bosse initiale commencent à effectuer une opération de réduction d'épaisseur de bulle ; (3) sélectionner certains mécanismes parmi tous les mécanismes de régulation d'épaisseur de point normal pour effectuer une opération d'épaississement de bulle ; (4) calculer une valeur absolue d de la différence entre c et b, c'est-à-dire, d =|c - b|, c étant une valeur moyenne des épaisseurs réelles de tous les points normaux de la bulle, y compris celles épaissies, après l'opération d'épaississement et b étant une valeur moyenne des épaisseurs de bosse initiale ajustées des différentes bosses initiales de la bulle après l'opération de réduction d'épaisseur ; (5) comparer d à e, e étant la différence maximale admissible entre c et b et passer à l'étape (6) ; et (6) un mécanisme de régulation d'épaisseur de circonférence complète réduit l'épaisseur de circonférence complète de la bulle selon le résultat de mesure du dispositif de mesure d'épaisseur de bulle, pour réduire l'épaisseur moyenne de circonférence complète de la bulle à a, a étant une valeur désignée pour l'épaisseur de la bulle. Après que la bulle produite est enroulée, l'erreur cumulée d'épaisseurs de divers points est répartie uniformément le long d'une direction axiale du rouleau, ce qui permet d'éviter des faux pli à la bobineuse et de supprimer également un procédé et un appareil de traction rotationnelle mécanique classique.
PCT/CN2016/000418 2015-09-25 2016-07-29 Procédé de production de soufflage de film WO2017049808A1 (fr)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
CN201510619894.7 2015-09-25
CN201510619894.7A CN106553330B (zh) 2015-09-25 2015-09-25 吹膜生产工艺

Publications (1)

Publication Number Publication Date
WO2017049808A1 true WO2017049808A1 (fr) 2017-03-30

Family

ID=58385800

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/CN2016/000418 WO2017049808A1 (fr) 2015-09-25 2016-07-29 Procédé de production de soufflage de film

Country Status (2)

Country Link
CN (1) CN106553330B (fr)
WO (1) WO2017049808A1 (fr)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2018185597A1 (fr) * 2017-04-07 2018-10-11 Brampton Engineering Inc. Anneau venturi réglable
CN117183302A (zh) * 2023-09-10 2023-12-08 苏州鸿科新材料科技有限公司 一种离型膜生产用吹膜机

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN116653273B (zh) * 2023-08-01 2023-09-22 沈阳东源包装制品有限公司 一种塑料膜吹膜工艺及控制方法

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5804221A (en) * 1996-09-05 1998-09-08 Macro Engineering & Technology Inc. Air ring for cooling blown plastic film
CN202572976U (zh) * 2012-05-10 2012-12-05 广州市金威龙实业股份有限公司 吹膜机的膜厚度检测装置
CN103978669A (zh) * 2014-05-15 2014-08-13 西安交通大学 一种吹塑薄膜自动厚度控制系统及控制方法
CN204183889U (zh) * 2014-10-09 2015-03-04 广东金明精机股份有限公司 能局部调节膜泡厚度的吹膜设备冷却风环
CN204604888U (zh) * 2015-03-18 2015-09-02 广东金明精机股份有限公司 能局部调节膜泡厚度的吹膜设备模头

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0825463A (ja) * 1994-07-21 1996-01-30 Tomy Kikai Kogyo Kk 押出成形方法および装置
DE10248366B4 (de) * 2002-10-17 2005-06-02 U.B.Tech.Gmbh Vorrichtung zur Regelung der Materialstärke, insbesondere während der Herstellung eines Blasfolienschlauches
CN1817616A (zh) * 2006-03-27 2006-08-16 王根乐 自动控制出膜厚度的方法及实施该方法的称量装置

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US5804221A (en) * 1996-09-05 1998-09-08 Macro Engineering & Technology Inc. Air ring for cooling blown plastic film
CN202572976U (zh) * 2012-05-10 2012-12-05 广州市金威龙实业股份有限公司 吹膜机的膜厚度检测装置
CN103978669A (zh) * 2014-05-15 2014-08-13 西安交通大学 一种吹塑薄膜自动厚度控制系统及控制方法
CN204183889U (zh) * 2014-10-09 2015-03-04 广东金明精机股份有限公司 能局部调节膜泡厚度的吹膜设备冷却风环
CN204604888U (zh) * 2015-03-18 2015-09-02 广东金明精机股份有限公司 能局部调节膜泡厚度的吹膜设备模头

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2018185597A1 (fr) * 2017-04-07 2018-10-11 Brampton Engineering Inc. Anneau venturi réglable
US11065799B2 (en) 2017-04-07 2021-07-20 Brampton Engineering Inc. Adjustable venturi ring
CN117183302A (zh) * 2023-09-10 2023-12-08 苏州鸿科新材料科技有限公司 一种离型膜生产用吹膜机
CN117183302B (zh) * 2023-09-10 2024-04-16 苏州鸿科新材料科技有限公司 一种离型膜生产用吹膜机

Also Published As

Publication number Publication date
CN106553330B (zh) 2018-09-18
CN106553330A (zh) 2017-04-05

Similar Documents

Publication Publication Date Title
WO2017049808A1 (fr) Procédé de production de soufflage de film
US6905642B2 (en) Method and continuous production line of plastic tubes with bi-axial drawing, and resulting plastic tube
KR102293036B1 (ko) 필름성형장치
CN102990812B (zh) 轮胎硫化方法及轮胎硫化机
JP5467391B2 (ja) 熱収縮チューブの製造方法および製造装置
US3092874A (en) Production of thermoplastic polymeric film
US9193107B2 (en) Apparatus and method for cooling plastic film tube in blown film process
JP2015502262A (ja) ロールを冷却するための方法及び装置
CN112571776A (zh) 实现液晶高分子横向吹胀的吹膜装置及制备方法
CN102259481B (zh) 一种薄膜热伸缩定长方法
CN111672704B (zh) 一种自动非接触式面密度调节系统及调节方法
CN104002465A (zh) 一种胀-微缩式双轴向拉伸管连续成型方法及设备
US20170210664A1 (en) Apparatus for manufacturing an optical fiber
CN104723581A (zh) 含氟层聚酰亚胺复合材料的制备方法及用于该方法的设备
JP2019214158A (ja) タイヤ加硫用ブラダーのパンク検出方法
CN106769064B (zh) 一种孔板式背压调节装置
CN106548845B (zh) 提高非晶带材生产产品质量的方法
JP2022115223A (ja) ゴム被覆ワイヤの製造方法および装置
TW201932370A (zh) 吹袋機袋體厚度均衡控制方法與其裝置
CN116653273B (zh) 一种塑料膜吹膜工艺及控制方法
CN104384205A (zh) 轧机工艺油压力控制系统
CN106825466B (zh) 提高非晶带材产品叠片系数的方法
JP2019025779A (ja) タイヤ加硫方法及びタイヤ加硫装置
CN205762955U (zh) 延压机
KR102308063B1 (ko) 블로운 필름의 제조장치

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 16847706

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 16847706

Country of ref document: EP

Kind code of ref document: A1