TWI378905B - - Google Patents
Download PDFInfo
- Publication number
- TWI378905B TWI378905B TW98120003A TW98120003A TWI378905B TW I378905 B TWI378905 B TW I378905B TW 98120003 A TW98120003 A TW 98120003A TW 98120003 A TW98120003 A TW 98120003A TW I378905 B TWI378905 B TW I378905B
- Authority
- TW
- Taiwan
- Prior art keywords
- bottle
- bottle mouth
- mouth
- heat
- layer
- Prior art date
Links
Landscapes
- Containers Having Bodies Formed In One Piece (AREA)
- Blow-Moulding Or Thermoforming Of Plastics Or The Like (AREA)
- Processing And Handling Of Plastics And Other Materials For Molding In General (AREA)
- Apparatus Associated With Microorganisms And Enzymes (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW98120003A TW201100344A (en) | 2009-06-16 | 2009-06-16 | Weight reduction method for container with crystallized bottle mouth |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW98120003A TW201100344A (en) | 2009-06-16 | 2009-06-16 | Weight reduction method for container with crystallized bottle mouth |
Publications (2)
Publication Number | Publication Date |
---|---|
TW201100344A TW201100344A (en) | 2011-01-01 |
TWI378905B true TWI378905B (enrdf_load_stackoverflow) | 2012-12-11 |
Family
ID=44836587
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW98120003A TW201100344A (en) | 2009-06-16 | 2009-06-16 | Weight reduction method for container with crystallized bottle mouth |
Country Status (1)
Country | Link |
---|---|
TW (1) | TW201100344A (enrdf_load_stackoverflow) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TW201700357A (zh) * | 2015-06-22 | 2017-01-01 | Chance Mate Develop Industry Co Ltd | Pet瓶胚構造 |
-
2009
- 2009-06-16 TW TW98120003A patent/TW201100344A/zh not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
TW201100344A (en) | 2011-01-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN1231341C (zh) | 非晶体塑料制品的局部结晶方法和装置 | |
EP2578380B1 (en) | Preform opening crystallization method | |
JPS6359513A (ja) | ポリエステル中空成形体の製造 | |
EP1413420A4 (en) | METHOD AND DEVICE FOR HEATING PREFORMS | |
WO2016067658A1 (ja) | 熱収縮性ポリエステル系フィルム及び包装体 | |
TWI378905B (enrdf_load_stackoverflow) | ||
JP3218670B2 (ja) | パリソンの温度調節方法 | |
JP2005531445A5 (enrdf_load_stackoverflow) | ||
WO2002076712A1 (fr) | Goulot cristallise de bouteille de biere en polyester et son procede de fabrication | |
WO2004012925A1 (ja) | 耐熱性を有するプラスチック製のカップ状容器およびその一次成形品 | |
CN1223451C (zh) | 延伸吹塑容器及其成形方法 | |
JP4562320B2 (ja) | 合成樹脂製容器の口元高速白化方法 | |
AU2003237109B2 (en) | Biaxial orientation blow molding process | |
CN101934581B (zh) | 结晶瓶口容器轻量化方法 | |
JP3044348B1 (ja) | プリフォ―ム口首部の内径規制用コア | |
JP2006181756A (ja) | プリフォームの口部結晶化装置 | |
JP2004009633A (ja) | プリフォーム首部の結晶化方法およびプリフォームホルダ | |
JPS6061228A (ja) | プラスチックボトルの成形方法 | |
JP4775791B2 (ja) | プリフォーム用の保持治具および熱結晶化処理設備 | |
JPH0443498B2 (enrdf_load_stackoverflow) | ||
JPS6225491B2 (enrdf_load_stackoverflow) | ||
JP2007233176A5 (enrdf_load_stackoverflow) | ||
JPH1142696A (ja) | 耐熱性延伸樹脂容器及びその製法 | |
JP7727187B2 (ja) | ラベル付き樹脂容器の製造方法 | |
TWI276532B (en) | Method for crystallizing and heating bottle opening |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |