TR19319A - Cam imalinde veya bununla ilgili islahat - Google Patents

Cam imalinde veya bununla ilgili islahat

Info

Publication number
TR19319A
TR19319A TR19319A TR1931976A TR19319A TR 19319 A TR19319 A TR 19319A TR 19319 A TR19319 A TR 19319A TR 1931976 A TR1931976 A TR 1931976A TR 19319 A TR19319 A TR 19319A
Authority
TR
Turkey
Prior art keywords
improvement
glass
Prior art date
Application number
TR19319A
Other languages
English (en)
Original Assignee
Pilkington Brothers Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Pilkington Brothers Ltd filed Critical Pilkington Brothers Ltd
Publication of TR19319A publication Critical patent/TR19319A/tr

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C03GLASS; MINERAL OR SLAG WOOL
    • C03BMANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
    • C03B5/00Melting in furnaces; Furnaces so far as specially adapted for glass manufacture
    • C03B5/16Special features of the melting process; Auxiliary means specially adapted for glass-melting furnaces
    • C03B5/23Cooling the molten glass
    • CCHEMISTRY; METALLURGY
    • C03GLASS; MINERAL OR SLAG WOOL
    • C03BMANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
    • C03B5/00Melting in furnaces; Furnaces so far as specially adapted for glass manufacture
    • C03B5/16Special features of the melting process; Auxiliary means specially adapted for glass-melting furnaces
    • C03B5/18Stirring devices; Homogenisation
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P40/00Technologies relating to the processing of minerals
    • Y02P40/50Glass production, e.g. reusing waste heat during processing or shaping
    • Y02P40/57Improving the yield, e-g- reduction of reject rates
TR19319A 1975-01-31 1976-01-30 Cam imalinde veya bununla ilgili islahat TR19319A (tr)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
GB4359/75A GB1533979A (en) 1975-01-31 1975-01-31 Thermally conditioning molten glass

Publications (1)

Publication Number Publication Date
TR19319A true TR19319A (tr) 1978-11-28

Family

ID=9775696

Family Applications (1)

Application Number Title Priority Date Filing Date
TR19319A TR19319A (tr) 1975-01-31 1976-01-30 Cam imalinde veya bununla ilgili islahat

Country Status (21)

Country Link
JP (1) JPS51101013A (tr)
AR (1) AR209470A1 (tr)
AU (1) AU498434B2 (tr)
BE (1) BE838129A (tr)
BR (1) BR7600588A (tr)
CA (1) CA1071407A (tr)
CS (1) CS208179B2 (tr)
DE (1) DE2603612C2 (tr)
ES (1) ES444812A1 (tr)
FI (1) FI59578C (tr)
FR (1) FR2299278A1 (tr)
GB (1) GB1533979A (tr)
IE (1) IE42253B1 (tr)
LU (1) LU74284A1 (tr)
MX (1) MX144271A (tr)
NL (1) NL169986C (tr)
NO (1) NO142905C (tr)
NZ (1) NZ179874A (tr)
PL (1) PL110994B1 (tr)
SE (1) SE416947B (tr)
TR (1) TR19319A (tr)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
GB1557630A (en) * 1977-06-03 1979-12-12 Pilkington Brothers Ltd Glass manufacture
GB8430312D0 (en) * 1984-11-30 1985-01-09 Pilkington Brothers Plc Glass melting tanks
KR100414175B1 (ko) * 1999-10-12 2004-01-07 한국전기초자 주식회사 유리용융로
ES2192423B1 (es) * 2000-04-18 2005-02-16 Avacon, S.A. Horno de fusion de vidrio.

Family Cites Families (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US1879718A (en) * 1929-04-17 1932-09-27 Owens Illinois Glass Co Glass furnace
US2049600A (en) * 1933-07-21 1936-08-04 Libbey Owens Ford Glass Co Method and apparatus for conditioning molten glass
US2982522A (en) * 1957-06-05 1961-05-02 Owens Illinois Glass Co Water cooled glass stirrer
DE1210520B (de) * 1962-01-11 1966-02-10 Glaverbel Glasschmelzofen
US3321288A (en) * 1964-02-28 1967-05-23 Owens Corning Fiberglass Corp Method for controlling the temperature of heat-softenable material
GB1060622A (en) * 1964-02-29 1967-03-08 Elemelt Ltd Improvements relating to a method of melting and supplying glass along a feeder duct
LU50619A1 (tr) * 1966-03-10 1967-09-11
DE1796318A1 (de) * 1967-03-31 1972-05-18 Owens Corning Fiberglass Corp Vorrichtung zur thermischen Aufbereitung von Stoffschmelzen
US3573017A (en) * 1968-11-04 1971-03-30 Owens Corning Fiberglass Corp Method and apparatus for melting and supplying heat-softenable materials in a process
US3658505A (en) * 1969-05-22 1972-04-25 Ppg Industries Inc Glass melting furnace
JPS4856713A (tr) * 1971-11-22 1973-08-09
AR204404A1 (es) * 1973-01-12 1976-02-06 Pilkington Brothers Ltd Metodo para producir vidrio en un tanque de fundir vidrio y tanque para su realizacion

Also Published As

Publication number Publication date
FR2299278B1 (tr) 1982-05-21
FR2299278A1 (fr) 1976-08-27
GB1533979A (en) 1978-11-29
NO142905B (no) 1980-08-04
BR7600588A (pt) 1976-08-31
CA1071407A (en) 1980-02-12
IE42253L (en) 1976-07-31
PL110994B1 (en) 1980-08-30
LU74284A1 (tr) 1976-07-23
NL7600957A (nl) 1976-08-03
FI760234A (tr) 1976-08-01
JPS51101013A (tr) 1976-09-07
CS208179B2 (en) 1981-08-31
BE838129A (fr) 1976-07-30
SE416947B (sv) 1981-02-16
NZ179874A (en) 1978-04-03
FI59578C (fi) 1981-09-10
NO142905C (no) 1980-11-12
NL169986C (nl) 1982-09-16
AU498434B2 (en) 1979-03-15
NL169986B (nl) 1982-04-16
MX144271A (es) 1981-09-23
NO760299L (tr) 1976-08-03
DE2603612A1 (de) 1976-08-05
SE7601005L (sv) 1976-08-02
FI59578B (fi) 1981-05-29
ES444812A1 (es) 1977-08-16
AR209470A1 (es) 1977-04-29
IE42253B1 (en) 1980-07-02
DE2603612C2 (de) 1984-11-08
AU1027476A (en) 1977-07-21

Similar Documents

Publication Publication Date Title
TR19246A (tr) Cam imalinde veya bununla ilgili islahat
TR18884A (tr) Cam kaplamasinda veya bununla ilgili islahat
MX143761A (es) Mejoras en turbo-bombas
IT1053603B (it) Perfezionamento negli elettreti
ATA597476A (de) Lichtdurchlaessige schichtglasplatte
MX144462A (es) Mejoras en dirigible
TR18595A (tr) Cam eritme
TR17475A (tr) Cam imali usullerinde veya bunlarla ilgili islahat
AT365159B (de) Beschussfeste verbundglasscheibe
IT1057369B (it) Perfezionamento nei dispositivi per illuminazione
TR18688A (tr) Duez cam ihalinde veya bununla ilgili islahat
TR18556A (tr) Cam eritmede veya bununla ilgili islahat
TR19319A (tr) Cam imalinde veya bununla ilgili islahat
SE405697B (sv) Monteringsdistans i notspont
BR7608135A (pt) Composicao de vidro
TR18341A (tr) Cam imalinde veya bununla ilgili islahat
TR19744A (tr) Duez cam imalinde veya bununla ilgili islahat
NO138594C (no) Fototropt glass i systemet p2o5 - sio2 -al2o3 - r2o - ro
IT1073680B (it) Perfezionamento nei congelatori
JPS51109939A (ja) Butsushitsuokanetsuyokaishitetososuruhoho to kyujobifunmatsunoseiho to sonosochinitsuite
SE7613715L (sv) Tendning i slaghammartendare
IT1110894B (it) Perfezionamento nei trasprotatori
ATA936875A (de) Transparente glasmikrokugeln
SE385609B (sv) Festanordning for prydnadsprojsar i fonster
JPS5184708A (ja) Seikoyoaakuro