SU94055A1 - Method for the production of the retarder setting gypsum - Google Patents

Method for the production of the retarder setting gypsum

Info

Publication number
SU94055A1
SU94055A1 SU434292A SU434292A SU94055A1 SU 94055 A1 SU94055 A1 SU 94055A1 SU 434292 A SU434292 A SU 434292A SU 434292 A SU434292 A SU 434292A SU 94055 A1 SU94055 A1 SU 94055A1
Authority
SU
USSR - Soviet Union
Prior art keywords
production
gypsum
retarder
setting gypsum
retarder setting
Prior art date
Application number
SU434292A
Other languages
Russian (ru)
Inventor
В.В. Помазков
Original Assignee
В.В. Помазков
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by В.В. Помазков filed Critical В.В. Помазков
Priority to SU434292A priority Critical patent/SU94055A1/en
Application granted granted Critical
Publication of SU94055A1 publication Critical patent/SU94055A1/en

Description

Предлагаемый способ производства замедлител  схватывани  гипса из древесных опилок отличаетс  тем, что опилки подвергают гидролизу при повышенном давлении в автоклаве в присутствии кислоты. Полученна  масса нейтрализуетс  углекислым кальцием и подвергаетс  сушке и помолу.The proposed method for producing a retarder for setting gypsum from sawdust is characterized in that the sawdust is subjected to hydrolysis under increased pressure in the autoclave in the presence of acid. The resulting mass is neutralized with calcium carbonate and dried and ground.

Дл  гидролиза древесны.ч опилок примен етс  серна  2%-на  кислота , а давление в автоклаве повышаетс  до 8 атм.Sulfuric acid 2% is used to hydrolyze wood chips and the pressure in the autoclave rises to 8 atm.

Сушку производ т при температуре выше 170°, и просушенный порогиок дополнительно подвергают номолу в мельнице, например шаровой .Drying is carried out at a temperature above 170 °, and the dried threshold is additionally subjected to nomolum in a mill, such as a ball.

Полученный замедлитель схватывани  гипса хорошо раствор етс  в холодной воде, поэтому его можно вводить с перемешиванием в воду, идушую дл  затворени  гипса .The resulting gypsum setting retarder dissolves well in cold water, so it can be injected with stirring into water, and then mixed to set gypsum.

Нормальный расход замедлител  0,2-0,3% от веса гинса. Дл  замедлени  схватывани  гипса на 30- 40 мин. нужно вводить замедлитель в количестве около 0,5%.The normal consumption of the moderator is 0.2-0.3% of the weight of the gyns. To slow down the setting of gypsum by 30-40 minutes. It is necessary to introduce a retarder in an amount of about 0.5%.

Применение предложенного замедлител  повышает пластичность и водоудерживаюш.ую способностьThe use of the proposed retarder increases the plasticity and water retention ability

гипсового теста.gypsum dough.

Предмет изобретени Subject invention

Способ производства замедлител  схватывани  гипса из древесных опилок. отличаюн.ийс  тем, что опилки подвергают гидролизу в автоклаве при повышенном давлении в присутствии кислоты с дальнейп е; 1 нейтрализацией полученной массы углекислым кальцием , и полученный продукт подвергают сушке и помолу.Method for the production of a retarder setting gypsum from sawdust. the difference is that sawdust is subjected to hydrolysis in an autoclave at elevated pressure in the presence of acid with further e; 1 by neutralizing the resulting mass with calcium carbonate, and the resulting product is subjected to drying and grinding.

SU434292A 1919-09-04 1919-09-04 Method for the production of the retarder setting gypsum SU94055A1 (en)