SU72448A1 - The method of obtaining resin from wood - Google Patents

The method of obtaining resin from wood

Info

Publication number
SU72448A1
SU72448A1 SU377468A SU377468A SU72448A1 SU 72448 A1 SU72448 A1 SU 72448A1 SU 377468 A SU377468 A SU 377468A SU 377468 A SU377468 A SU 377468A SU 72448 A1 SU72448 A1 SU 72448A1
Authority
SU
USSR - Soviet Union
Prior art keywords
wood
obtaining resin
resin
kerosene
subjected
Prior art date
Application number
SU377468A
Other languages
Russian (ru)
Inventor
А.К. Славянский
нский А.К. Слав
Original Assignee
А.К. Славянский
нский А.К. Слав
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.К. Славянский, нский А.К. Слав filed Critical А.К. Славянский
Priority to SU377468A priority Critical patent/SU72448A1/en
Application granted granted Critical
Publication of SU72448A1 publication Critical patent/SU72448A1/en

Description

За влено 16 апрел  1948 г. за .Yg 377468 в Комитет по изобретени м и открыти м при Совете Л инистров СССРIt was filed on April 16, 1948 for. Yg 377468 to the Committee on Inventions and Discoveries at the Council of Ministers of the USSR

Древесину в виде кружков толщиной около 100 мм подвергают пирогенетической обработке в среде керосина при 275° и- нормальном давлении. При этом в интервале температур 100-220° вместе с керосином отгон етс  влага, а при 220-275° отгон етс  концентрированный погон лесохимикатов. Остатки керосина удал ют из древесины путем продувки ее вод ным паром (лучше перегретым до 150-200°).Wood in the form of circles with a thickness of about 100 mm is subjected to pyrogenetic treatment in kerosene at 275 ° and normal pressure. At the same time, moisture is distilled off along with kerosene in the temperature range of 100–220 ° C, and at 220–275 ° C, concentrated condensate of chemical chemicals is distilled. Kerosene residues are removed from the wood by blowing it out with water vapor (preferably overheated to 150-200 °).

Полученную бурую древесину измельчают в щепу и подвергают экстракционной обработке ацетоном или спиртом. После отгонки экстракта до концентрации 30-40% получаетс  лак темно-красного цвета. Выход сухой смолы составл ет около 5% от веса исходной сухой древесины . Из 1 кг исходной сухой древесины можно получить до 15-17% (по весу) спиртового лака с 35%-ной концентрацией смолы (в среднем).The obtained brown wood is crushed into chips and subjected to extraction treatment with acetone or alcohol. After distilling off the extract to a concentration of 30-40%, a dark red lacquer is obtained. The dry resin yield is about 5% by weight of the original dry wood. From 1 kg of the original dry wood, you can get up to 15-17% (by weight) of alcohol varnish with a 35% resin concentration (on average).

Предмет изобретени Subject invention

1.Способ получени  смолы из древесины, подвергнутой пирогенетической обработке в среде нефтедестиллатов при температуре до 275°. отличающийс  тем, что обработанную древесину после пропаривани  дл  удалени  остатков нефтедестиллатов измельчают и обрабатывают пол рными органическими растворител ми, в частности, спиртом ИЛИ; ацетоном, с последующей отгонкой растворителей из экстракта.1. A method of obtaining resin from wood subjected to pyrogenic treatment in the environment of petroleum distillates at temperatures up to 275 °. characterized in that the treated wood after steaming is crushed and treated with polar organic solvents, in particular, OR alcohol, to remove residues of petroleum distillates; acetone, followed by distillation of the solvent from the extract.

2.Применение смолы, полученной согласно п. 1, в качестве пленкообразующего .2. The use of the resin obtained according to p. 1, as a film-forming.

Редактор А. Г. Новожилов Техред А. А. Кудр вицка  Корректор С. Ю. ЦверинаEditor A. G. Novozhilov Tehred A. A. Kudr vitska Proofreader S. Yu. Tsverina

Поди, к печ. 15/1 - 62 г.Формат бум. 70 X 108 /1бОбъем 0,18 изд. л,Go to the furnace. 15/1 - 62 g. Format boom. 70 X 108 / 1bVolume 0,18 ed. lt

Зак. 3395/15Тираж 200Цена 5 коп.Zak 3395/15 Circulation 200Price 5 kopecks

ЦБТИ при Комитете по делам изобретений и открытийTsBTI under the Committee on Inventions and Discoveries

при Совете Министров СССР Москва, Центр, М. Черкасский пер., д. 2/6.under the Council of Ministers of the USSR, Moscow, Center, M. Cherkassky Lane, 2/6.

Типографи , птэ. Сапунова, 2.Typography pte. Sapunova, 2.

SU377468A 1948-04-16 1948-04-16 The method of obtaining resin from wood SU72448A1 (en)