SU708990A3 - Способ непрерывного получени прутка из алюминиевого сплава - Google Patents
Способ непрерывного получени прутка из алюминиевого сплава Download PDFInfo
- Publication number
- SU708990A3 SU708990A3 SU772476553A SU2476553A SU708990A3 SU 708990 A3 SU708990 A3 SU 708990A3 SU 772476553 A SU772476553 A SU 772476553A SU 2476553 A SU2476553 A SU 2476553A SU 708990 A3 SU708990 A3 SU 708990A3
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- aluminum alloy
- rod
- bar
- continuous production
- ingot
- Prior art date
Description
I
Изобретение относитс к металлургии, ко кретнее к способам непрерывного получени заготовок.
Известен способ непрерывного получени прутка из алюминиевого сплава, включающий подачу жидкого металла в кристаллизатор, криталлизащпо и охлаждение слитка, извлечение и прокатку слитка в пруток, лакалку и намотку Прутка 1. Полученный этим способом пруток имеет неудовлетворительную прочность на разрыв.
С целью устранени указанного недостатка, согласно предложенному способу, непосредственно после прокатки пруток нагревают до температуры 371-566° С.
На черте-же показана схема непрерывного получени прутка из алюминиевого сплава.
Дл получени прутка используют агрегат, содержащи1 разливочную машину 1, прокатный стап 2, {агреватель 3, закалочную трубу 4 и намоточное устройство 5.
Способ осуществл етс следующим образом.
Расплавленный металл из печи подают на разливочное колесо разливочной машины 1, откуда извлекают слиток, которьп направл ют в прокатный стан 2. В прокатном с.тане слиток прокатывают в пруток, который на выходе из стана имеет температуру лх 371°С, пруток подают далее в нагреватель 3, где его температура повышаетс приблизительно до 566°С. После прохождени через нагреватель пруток попадает в закалочную трубу 4, где его температура быстро снижаетс до , и после
этого он охлаждаетс в змеевике (на чертеже не показан) и далее подаетс на намоточное устройство 5.
Описан 1ый способ предназначен в основном дл получени нрутка из алюминиевого сплава марки 6201. Благодар предложенному способу получени значительно повысилась прочность прутка на разрыв.
Ф о рмула изобретени
Способ непрерывного получени прутка из шпоминиевого сплава, включаюший подачу жидкого металла в кристаллизатор, кристаллизацию и охлажде ше слитка, извлечение и прокатку слитка в пруток, закалку и намотку прутка , отличающийс тем, что, с целью повышени прочности прутка на разрыв после прокатки, пруток нагревают до температуры 371-566°С.
Источники информа1щи, прин тые во внимание при экспертизе 1. Патент США № 583720, кл. В 22 D 11/00, 1975.
Claims (2)
- Фо рмула изобретения
- 2° Способ непрерывного получения прутка из алюминиевого сплава, включающий подачу жидкого металла в кристаллизатор, кристаллизацию и охлаждение слитка, извлечение и прокатку слитка в пруток, закалку и намотку прут3 ка, отличающийся тем, что, с целью повышения прочности прутка на разрыв после прокатки, пруток нагревают до температуры 371—5 66° С.