SU410109A1 - - Google Patents

Info

Publication number
SU410109A1
SU410109A1 SU1779270A SU1779270A SU410109A1 SU 410109 A1 SU410109 A1 SU 410109A1 SU 1779270 A SU1779270 A SU 1779270A SU 1779270 A SU1779270 A SU 1779270A SU 410109 A1 SU410109 A1 SU 410109A1
Authority
SU
USSR - Soviet Union
Prior art keywords
castings
aging
cast iron
heat treatment
residual stresses
Prior art date
Application number
SU1779270A
Other languages
English (en)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1779270A priority Critical patent/SU410109A1/ru
Application granted granted Critical
Publication of SU410109A1 publication Critical patent/SU410109A1/ru

Description

Изобретение относитс  к маитиностроению, в частности к термической обработке фасонных деталей из чугуна.
Р1звестен сиособ термической обработки чугунных отливок, включающий нагрев до температур старени , выдержку и охлаждение на воздухе.
Цель изобретени  - сокращение длительности процесса и снижение остаточных напр жений .
Эта цель достигаетс  тем, что отливки нагревают со скоростью 240-600 град/час до температуры, например 200-280°С и выдерживают в теченне 80-300 мин.
Обща  продолжительность термообработки по предлагаемому способу не превьпнает 4- 5 час, что дает возможность повысить нроизводительность действующих печей на операци х старени  чугунных деталей не менее, чем в 5-6 раз.
Предложенный снособ нозволит сннзить остаточные нанр женн , уменьщнть коробление и сократить цикл обработки.
Предложенный способ можно также прнмен ть дл  чугуппых отливок с высокими остаточными напр жени ми, составл ющими более 20-30% от предела нрочности чугуна.
Предмет изобретени 

Claims (2)

1.Снособ термической обработки чугунных отливок, включающий нагрев до температур старени , выдержку и охлаждеиие па воздухе , отличающийс  тем, что, с целью снижени  остаточных напр жеиий, и сокран1енн  цикла обработки, иагрев отливок производ т со скоростью 240-600 град/час.
2.Способ по п. 1, отличающийс  тем, что выдержку отливок производ т в течение 80-300 мин.
SU1779270A 1972-04-30 1972-04-30 SU410109A1 (ru)