SU375980A1 - Способ восстановления двуокиси германия - Google Patents

Способ восстановления двуокиси германия

Info

Publication number
SU375980A1
SU375980A1 SU1484121A SU1484121A SU375980A1 SU 375980 A1 SU375980 A1 SU 375980A1 SU 1484121 A SU1484121 A SU 1484121A SU 1484121 A SU1484121 A SU 1484121A SU 375980 A1 SU375980 A1 SU 375980A1
Authority
SU
USSR - Soviet Union
Prior art keywords
bioxide
germany
germanium
restoration method
rate
Prior art date
Application number
SU1484121A
Other languages
English (en)
Original Assignee
КНТ. айК
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by КНТ. айК filed Critical КНТ. айК
Priority to SU1484121A priority Critical patent/SU375980A1/ru
Application granted granted Critical
Publication of SU375980A1 publication Critical patent/SU375980A1/ru

Description

1
Изобретение относитс  к области металлургии редких металлов.
Известен способ получени  металлического германи  восстановлением его двуокиси водородом при 700-850°С. При этом не исключены потери германи ; процесс длитс  продолжительное врем .
Отличительной особенностью предлагаемого способа  вл етс  то, что температуру повышают со скоростью не более 1 град/мин, что позвол ет исключить потери германи  и сократить врем  процесса.
Пример. Двоукись германи  загружают в кварцевые лодочки высотой 10 мм и помещают в электропечь. В печь подают водород, а температуру печи повышают по программе, обеспечивающей повыщение скорости восстановлени  летучей моноокпси по сравнению со
скоростью диффузии в слое порощкообразного германи . При этом верхние слои двуокиси германи  успевают восстановитьс  при более низкой температуре. Далее процесс приобретает диффузионный характер (процесс лимитируетс  скоростью проникновени  водорода в слой материала).
Наилучшей  вл етс  скорость подъема температуры , равна  1 град/мин. Врем  процесса не более 2 час, извлечение германи  .
Предмет изобретени 
Способ восстановлени  двуокиси германи 
водородом при 700-850°С, отличающийс  тем,
что, с целью исключени  потерь германи  и
сокращени  времени процесса, температуру
повышают со скоростью не более 1 град/мин.
SU1484121A 1970-10-16 1970-10-16 Способ восстановления двуокиси германия SU375980A1 (ru)