Известны способы восстановлени железной руды, нагретой до 850-950с, смес ми нефт ного газа и вод ного пара в шахтных печах. Однако применение известных способов сопровождаетс выделением сажистого углерода.Methods are known for reducing iron ore heated to 850-950s with mixtures of petroleum gas and steam in shaft furnaces. However, the application of known methods is accompanied by the release of black carbon.
Предлагаемый способ отличаетс тем, что с целью устранени выделени сажи и более тонного поддержани оптималь-г ной температуры в слое руды, восстановление железа осуществл етс в атмосфере факела горени смеси нефт ного газа с воздухом и вод ным паром.The proposed method is characterized in that in order to eliminate the release of soot and to maintain a more tonne optimum temperature in the ore layer, the iron is reduced in the atmosphere of the flame of the mixture of oil gas with air and water vapor.
Сущность способа заключаетс в том, что восстановление железной руды производитс в шахтной печи при 8ОО1100 С. Руда на восстановление поступает в виде гранул, брикетов иди окатышей .The essence of the method lies in the fact that the reduction of iron ore is carried out in a shaft furnace at 8OO1100 C. The ore is sent to the reduction in the form of pellets, briquettes or pellets.
Восстановление происхо/цит в восстановительной атмосфере факела горени па ровоздухогазовой смеси (нефт ной газ с паром и воздухом) с наиболее выгодным коэффициентом избытка воздуха в пределе 0,05-0,25. Состав паровоздухогазовой смеси дл факела устанавливаетс с расчетом получени бессажисто- го губчатого железа. Дл предупреждени выделени сажистого углерода, в зависимости от состава нефт ного газа, в газовую смесь ввод т 3-54% вод ного пара .Restoration took place in the reducing atmosphere of the flame of the gas-air mixture (oil gas with steam and air) with the most favorable air excess factor in the range of 0.05-0.25. The composition of the vapor-air mixture for the plume is determined with the expectation of production of bespistye sponge iron. To prevent the release of black carbon, depending on the composition of the petroleum gas, 3-54% water vapor is introduced into the gas mixture.
10ten
Claims (1)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU6100726350A SU142318A1 (en) | 1961-04-12 | 1961-04-12 | Method of obtaining sponge iron |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU6100726350A SU142318A1 (en) | 1961-04-12 | 1961-04-12 | Method of obtaining sponge iron |
Publications (1)
Publication Number | Publication Date |
---|---|
SU142318A1 true SU142318A1 (en) | 1978-09-15 |
Family
ID=20437215
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SU6100726350A SU142318A1 (en) | 1961-04-12 | 1961-04-12 | Method of obtaining sponge iron |
Country Status (1)
Country | Link |
---|---|
SU (1) | SU142318A1 (en) |
-
1961
- 1961-04-12 SU SU6100726350A patent/SU142318A1/en active
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1017360A (en) | Process for producing a furnace atmosphere for the heat treatment of metals, particularly steel | |
GB1004006A (en) | Process and plant for the production of sponge iron | |
SU142318A1 (en) | Method of obtaining sponge iron | |
GB1111608A (en) | Improvements in or relating to the manufacture of steel | |
US1889757A (en) | Process of operating cupola furnaces | |
GB424273A (en) | Process and apparatus for the production of spongy iron | |
GB883998A (en) | Method of operating blast furnaces | |
AT93333B (en) | Process for the production of sponge iron in a rotary kiln. | |
GB919681A (en) | Improvements in or relating to the reduction of iron oxide | |
GB442478A (en) | Improvements in and relating to blast furnaces and methods of operating same | |
SU529245A1 (en) | The method of obtaining carbon-manganese briquettes | |
GB396058A (en) | Process for eliminating arsenic and antimony from iron ores and manganese ores | |
US1773491A (en) | Method of producing the blast required for blast-furnace or similar plants by means of calcium carbide | |
US1388976A (en) | Annealing | |
SU147596A1 (en) | The method of heating metal | |
SU256789A2 (en) | Method of producing soot iron | |
GB418873A (en) | Improvements in the manufacture and production of malleable iron | |
GB353180A (en) | Improvements in or relating to the manufacture of sponge iron | |
GB573085A (en) | Improvements in the production of gaseous atmospheres for the cementation of iron and steel | |
GB815112A (en) | Improvements in or relating to blast furnaces | |
ES8303321A1 (en) | Blast furnace operation | |
GB500041A (en) | Process for the recovery of elementary sulphur from sulphur dioxide and gases containing same | |
GB338244A (en) | Improvements in the treatment of air-blast for furnaces | |
BE760948A (en) | Hearth furnace operation | |
GB980425A (en) | Improvements in methods of, and apparatus for, the preparation of ferrous oxide |