NL8100197A - Werkwijze voor het verbeteren van de corrosiebestendigheid van installatiebuizen uit koper. - Google Patents

Werkwijze voor het verbeteren van de corrosiebestendigheid van installatiebuizen uit koper. Download PDF

Info

Publication number
NL8100197A
NL8100197A NL8100197A NL8100197A NL8100197A NL 8100197 A NL8100197 A NL 8100197A NL 8100197 A NL8100197 A NL 8100197A NL 8100197 A NL8100197 A NL 8100197A NL 8100197 A NL8100197 A NL 8100197A
Authority
NL
Netherlands
Prior art keywords
tube
copper
corrosion
corrosion resistance
improving
Prior art date
Application number
NL8100197A
Other languages
English (en)
Dutch (nl)
Original Assignee
Wieland Werke Ag
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wieland Werke Ag filed Critical Wieland Werke Ag
Publication of NL8100197A publication Critical patent/NL8100197A/nl

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C22METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
    • C22FCHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
    • C22F1/00Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
    • C22F1/08Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of copper or alloys based thereon

Landscapes

  • Chemical & Material Sciences (AREA)
  • Physics & Mathematics (AREA)
  • Thermal Sciences (AREA)
  • Crystallography & Structural Chemistry (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Mechanical Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Heat Treatment Of Articles (AREA)
  • Preventing Corrosion Or Incrustation Of Metals (AREA)
NL8100197A 1980-01-30 1981-01-16 Werkwijze voor het verbeteren van de corrosiebestendigheid van installatiebuizen uit koper. NL8100197A (nl)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
DE3003228A DE3003228C2 (de) 1980-01-30 1980-01-30 Verfahren zur Verbesserung der Korrosionsbeständigkeit von Installationsrohren aus Kupfer
DE3003228 1980-01-30

Publications (1)

Publication Number Publication Date
NL8100197A true NL8100197A (nl) 1981-09-01

Family

ID=6093232

Family Applications (1)

Application Number Title Priority Date Filing Date
NL8100197A NL8100197A (nl) 1980-01-30 1981-01-16 Werkwijze voor het verbeteren van de corrosiebestendigheid van installatiebuizen uit koper.

Country Status (7)

Country Link
BE (1) BE887195A (fr)
DE (1) DE3003228C2 (fr)
FI (1) FI66209B (fr)
FR (1) FR2474532A1 (fr)
IT (1) IT1143270B (fr)
NL (1) NL8100197A (fr)
SE (1) SE8100269L (fr)

Families Citing this family (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE3760510D1 (en) 1987-03-07 1989-10-05 Wieland Werke Ag Process for improving the corrosion resistance of hard or semi-hard copper fitting tubes
EP0335999A1 (fr) * 1988-04-08 1989-10-11 Wieland-Werke AG Méthode de nettoyage des tubes métalliques, en particulier des tubes en cuivre
DE3827353A1 (de) * 1988-08-12 1990-02-22 Kabelmetal Ag Innenoxidierte rohre
FI107543B (fi) * 1998-07-30 2001-08-31 Outokumpu Oy Menetelmä kupariputken valmistamiseksi
FI20001467A (fi) * 2000-06-20 2001-12-21 Outokumpu Oy Menetelmä sisäpuolelta pinnoitettujen kupari- tai kupariseosputkien valmistamiseksi

Family Cites Families (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
LU67959A1 (fr) * 1973-07-06 1975-04-11
DE2337022A1 (de) * 1973-07-20 1975-02-13 Liege Usines Cuivre Zinc Verfahren zur reinigung der innenflaeche von kupferrohren zur vermeidung der durch einen kohlenstoffueberzug bedingten korrosion
FR2308436A1 (fr) * 1975-04-25 1976-11-19 Cit Alcatel Traitement des tubes en cuivre et alliages en vue de l'elimination des produits carbones subsistant a leur surface
BE841148A (fr) * 1976-04-26 1976-08-16 Procede de fabrication de rouleaux de tube en cuivre ou alliage de cuivre

Also Published As

Publication number Publication date
IT1143270B (it) 1986-10-22
BE887195A (nl) 1981-05-14
FI810160L (fi) 1981-07-31
IT8167042A0 (it) 1981-01-15
FR2474532A1 (fr) 1981-07-31
FR2474532B1 (fr) 1983-03-04
DE3003228C2 (de) 1981-11-26
SE8100269L (sv) 1981-07-31
FI66209B (fi) 1984-05-31
DE3003228B1 (de) 1981-03-26

Similar Documents

Publication Publication Date Title
Carter Metallic coatings for corrosion control: corrosion control series
CN101517115B (zh) 搪瓷施釉用加工产品以及搪瓷加工产品
KR930006494B1 (ko) 스테인레스 강대의 스케일 제거방법
NL8100197A (nl) Werkwijze voor het verbeteren van de corrosiebestendigheid van installatiebuizen uit koper.
GB1581172A (en) Surface-layered stainless steel products and method of producing the same
US3231971A (en) Method of producing fusion coated metal base
Ray et al. The influence of non-metallic inclusions on the corrosion fatigue of mild steel
Hinton et al. The inhibition of hydrogen embrittlement in SAE 4340 steel in an aqueous environment with the rare earth compound lanthanum 4 hydroxy cinnamate
GB2041483A (en) Corrosion-resistant phosphorous copper, or phosphorous copper alloy pipes for sanitary plumbing applications and method of making the same
JP6685161B2 (ja) 耐食性に優れたステンレス鋼加工品
JP3216571B2 (ja) 高Crステンレス鋼の脱スケール用アルカリ溶融塩浴
JP2001140081A (ja) 耐食性皮膜付き銅又は銅合金管
Tuthill Stainless steel: surface cleanliness
US2106227A (en) Surface treatment of metal to prevent localized corrosive attack
US4473412A (en) Annealing steel strip using molten B2 O3, SiO2 Na2 O, NaF glass bath
US2172421A (en) Corrosion-resistant ferrous alloys
JP6778499B2 (ja) 耐食性に優れたステンレス鋼板及びその製造方法
GB2055061A (en) Improvements concerning copper or copper-alloy tubes for pipes used in sanitary, condenser and other installations
JP6778500B2 (ja) 耐食性に優れたステンレス鋼加工品及びその製造方法
Adamy et al. Inhibition of pitting in ferrous materials by carbonate as a function of temperature and alkalinity
US1527538A (en) Calorizing iron or steel surfaces
US7115174B2 (en) Method for producing and oxide layer on metallic elements
Sproles Jr et al. A new interpretation of the mechanism of fretting and fretting corrosion damage
CN113646459B (zh) 经镀覆形成的黑心可锻铸铁部件的制造方法、及经镀覆形成的黑心可锻铸铁部件
JP3245806B2 (ja) フェライト系ステンレス鋼の製造方法

Legal Events

Date Code Title Description
A85 Still pending on 85-01-01
BV The patent application has lapsed