NL303028A - - Google Patents
Info
- Publication number
- NL303028A NL303028A NL303028DA NL303028A NL 303028 A NL303028 A NL 303028A NL 303028D A NL303028D A NL 303028DA NL 303028 A NL303028 A NL 303028A
- Authority
- NL
- Netherlands
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C21/00—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
- Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
- Y10T428/00—Stock material or miscellaneous articles
- Y10T428/31—Surface property or characteristic of web, sheet or block
- Y10T428/315—Surface modified glass [e.g., tempered, strengthened, etc.]
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Surface Treatment Of Glass (AREA)
- Glass Compositions (AREA)
Applications Claiming Priority (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US249790A US3287201A (en) | 1963-01-07 | 1963-01-07 | Method of strengthening glass by ion exchange and article made therefrom |
US26470863A | 1963-03-12 | 1963-03-12 | |
US26469063A | 1963-03-12 | 1963-03-12 |
Publications (1)
Publication Number | Publication Date |
---|---|
NL303028A true NL303028A (nl) |
Family
ID=27400244
Family Applications (3)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
NL302981D NL302981A (nl) | 1963-01-07 | ||
NL303028D NL303028A (nl) | 1963-01-07 | ||
NL63303028A NL141478B (nl) | 1963-01-07 | 1963-12-31 | Werkwijze ter vervaardiging van een glazen voorwerp met een oppervlaktelaag onder drukspanning en een daaronder liggende laag onder trekspanning, alsmede aldus vervaardigd glazen voorwerp. |
Family Applications Before (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
NL302981D NL302981A (nl) | 1963-01-07 |
Family Applications After (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
NL63303028A NL141478B (nl) | 1963-01-07 | 1963-12-31 | Werkwijze ter vervaardiging van een glazen voorwerp met een oppervlaktelaag onder drukspanning en een daaronder liggende laag onder trekspanning, alsmede aldus vervaardigd glazen voorwerp. |
Country Status (6)
Country | Link |
---|---|
US (1) | US3287201A (nl) |
BE (2) | BE641938A (nl) |
CH (1) | CH431835A (nl) |
DE (2) | DE1496624B1 (nl) |
GB (3) | GB1076603A (nl) |
NL (3) | NL141478B (nl) |
Families Citing this family (41)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB1107887A (en) * | 1964-06-23 | 1968-03-27 | Pilkington Brothers Ltd | Improvements in or relating to glass articles |
US3533888A (en) * | 1964-12-18 | 1970-10-13 | Corning Glass Works | Glass article and method of production |
US3395998A (en) * | 1964-12-18 | 1968-08-06 | Corning Glass Works | Method for production of glass article having increased mechanical strength |
US3403015A (en) * | 1965-05-25 | 1968-09-24 | Owens Illinois Inc | Method of treating glassware |
US3406279A (en) * | 1965-11-12 | 1968-10-15 | Corning Glass Works | Cooking surfaces |
US3486963A (en) * | 1966-03-07 | 1969-12-30 | Owens Illinois Inc | Surface treatment of crystalline glass ceramic |
US3490885A (en) * | 1966-12-30 | 1970-01-20 | Owens Illinois Inc | Manufacture of chemically-strengthened glass articles |
FR1589397A (nl) * | 1967-04-25 | 1970-03-31 | ||
GB1208153A (en) * | 1967-04-27 | 1970-10-07 | Glaverbel | Glass tempering processes and apparatus |
US3656923A (en) * | 1968-05-27 | 1972-04-18 | Corning Glass Works | Method for strengthening photochromic glass articles |
US3615322A (en) * | 1968-09-30 | 1971-10-26 | Anchor Hocking Glass Corp | Chemical strengthening of glass articles produced with flame treatment |
US4124733A (en) * | 1968-10-31 | 1978-11-07 | Pilkington Brothers Limited | Laminated glass units |
US3525658A (en) * | 1968-11-21 | 1970-08-25 | Ford Motor Co | Glass-plastic laminates having a layer of glass fiber filled polycarbonate |
US3630704A (en) * | 1969-03-10 | 1971-12-28 | Corning Glass Works | Method for strengthening glass articles |
GB1275653A (en) * | 1969-08-15 | 1972-05-24 | Glaverbel | Articles of chemically tempered glass |
BE755946A (fr) * | 1969-09-10 | 1971-03-09 | Saint Gobain Pont A Mousson | Perfectionnements aux procedes de traitement superficiel d'articles en verre ou en ceramique par echange d'ions |
US3650720A (en) * | 1969-11-14 | 1972-03-21 | Corning Glass Works | Decorating glass-ceramic articles |
US4102665A (en) * | 1970-02-03 | 1978-07-25 | Glaverbel-Mecaniver | Diffusion treatments for modifying the properties of glass and vitrocrystalline materials |
US3904460A (en) * | 1971-01-04 | 1975-09-09 | Ppg Industries Inc | Treating glass sheets |
US3791809A (en) * | 1973-01-12 | 1974-02-12 | Owens Illinois Inc | Method of strengthening glass articles using powdered salts for ion exchange |
FR2407897A1 (fr) * | 1977-11-03 | 1979-06-01 | Corning Glass Works | Procede de trempe chimique d'oculaires de lunetterie et pieces de verre analogues |
US4218230A (en) * | 1978-08-04 | 1980-08-19 | Brockway Glass Company, Inc. | Method of glass strengthening by ion exchange |
US4273832A (en) * | 1978-08-04 | 1981-06-16 | Brockway Glass Company, Inc. | Glass article strengthened by ion exchange substitution |
US4416930A (en) * | 1980-11-24 | 1983-11-22 | Ppg Industries, Inc. | Treating glass sheets to heal vents that result in breakage during thermal treatment |
US4824712A (en) * | 1984-07-16 | 1989-04-25 | Ppg Industries, Inc. | Treatment of glass to reduce venting during thermal treatment and a glass article made thereby |
JPH0818850B2 (ja) * | 1986-09-05 | 1996-02-28 | セントラル硝子株式会社 | 化学強化ガラス |
US4883523A (en) * | 1988-05-17 | 1989-11-28 | Raychem Corporation | Avoidance of surface deterioration of glass during strengthening processes |
WO2000047529A1 (en) * | 1999-02-12 | 2000-08-17 | The Pennsylvania State University | Strengthening, crack arrest and multiple cracking in brittle materials using residual stresses |
DK1688398T3 (da) | 2005-02-08 | 2014-07-21 | Ivoclar Vivadent Ag | Lithiumsilikat-glaskeramik |
DE102007009786B4 (de) * | 2007-02-27 | 2013-09-05 | Schott Ag | Beschichtetes vorgespanntes Glas, Verfahren zu dessen Herstellung und dessen Verwendung |
DE102007011337A1 (de) * | 2007-03-06 | 2008-09-11 | Hermsdorfer Institut Für Technische Keramik E.V. | Verblendkeramik für dentale Restaurationen aus yttriumstabilisiertem Zirkoniumdioxid und Verfahren zur Verblendung von dentalen Restaurationen aus yttriumstabilisiertem Zirkoniumdioxid |
US7666511B2 (en) * | 2007-05-18 | 2010-02-23 | Corning Incorporated | Down-drawable, chemically strengthened glass for cover plate |
US8075999B2 (en) | 2008-08-08 | 2011-12-13 | Corning Incorporated | Strengthened glass articles and methods of making |
US8584354B2 (en) * | 2010-08-26 | 2013-11-19 | Corning Incorporated | Method for making glass interposer panels |
CN106232543A (zh) | 2014-02-27 | 2016-12-14 | 康宁股份有限公司 | 用于三维成形的可离子交换玻璃制品 |
TWI749160B (zh) | 2017-01-31 | 2021-12-11 | 美商康寧公司 | 具有工程應力分佈的塗層玻璃基底製品及包含其之消費性電子產品 |
CN107721195A (zh) * | 2017-10-27 | 2018-02-23 | 福州瑞克布朗医药科技有限公司 | 一种增强齿科微晶玻璃理化性能的方法 |
CN107572828A (zh) * | 2017-10-27 | 2018-01-12 | 福州大学 | 一种铜/锌离子强化齿科微晶玻璃理化性能的方法 |
CO2018001322A1 (es) * | 2017-12-27 | 2018-04-30 | Agp America Sa | Método para fortalecer y curvar capas de vidrio |
FI12216U1 (fi) * | 2018-09-03 | 2018-11-15 | Boldan Oy | Putkenpuhdistus- tai avauslaitteen teräpala |
CN117129119A (zh) * | 2023-10-26 | 2023-11-28 | 西安中星测控有限公司 | 一种基于玻璃熔合技术的mcs压力传感器及其制做方法 |
Family Cites Families (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2154490A (en) * | 1936-12-09 | 1939-04-18 | Owens Illinois Glass Co | Method of treating hollow glass articles |
BE524291A (nl) * | 1951-04-21 | |||
AT202724B (de) * | 1955-07-06 | 1959-04-10 | Corning Glass Works | Verfahren zur Herstellung von Glasgegenständen mit hoher mechanischer Festigkeit |
BE549285A (nl) * | 1955-07-06 | |||
US3218220A (en) * | 1964-11-20 | 1965-11-16 | Brockway Glass Co Inc | Strengthened glass article and method of producing same |
-
0
- NL NL302981D patent/NL302981A/xx unknown
- NL NL303028D patent/NL303028A/xx unknown
-
1963
- 1963-01-07 US US249790A patent/US3287201A/en not_active Expired - Lifetime
- 1963-12-10 GB GB4155/65A patent/GB1076603A/en not_active Expired
- 1963-12-20 DE DE19631496624D patent/DE1496624B1/de active Pending
- 1963-12-30 BE BE641938D patent/BE641938A/xx unknown
- 1963-12-31 NL NL63303028A patent/NL141478B/nl unknown
-
1964
- 1964-01-22 DE DE19641496627 patent/DE1496627B2/de active Pending
- 1964-03-11 GB GB10173/64A patent/GB1018890A/en not_active Expired
- 1964-03-11 BE BE645046D patent/BE645046A/xx unknown
- 1964-03-12 CH CH323364A patent/CH431835A/fr unknown
-
1965
- 1965-12-10 GB GB48685/65D patent/GB1076602A/en not_active Expired
Also Published As
Publication number | Publication date |
---|---|
NL141478B (nl) | 1974-03-15 |
DE1496627A1 (de) | 1969-03-27 |
DE1496624B1 (de) | 1971-05-19 |
CH431835A (fr) | 1967-03-15 |
BE641938A (nl) | 1964-06-30 |
DE1496627B2 (de) | 1970-08-13 |
US3287201A (en) | 1966-11-22 |
NL302981A (nl) | |
GB1018890A (en) | 1966-02-02 |
GB1076603A (en) | 1967-07-19 |
GB1076602A (en) | 1967-07-19 |
BE645046A (nl) | 1964-09-11 |