KR960704958A - 액체 에폭시 수지 중의 α-글리콜의 수준을 증가시키는 방법(Method to increase the level of α-glycol in liquid epoxy resin) - Google Patents

액체 에폭시 수지 중의 α-글리콜의 수준을 증가시키는 방법(Method to increase the level of α-glycol in liquid epoxy resin)

Info

Publication number
KR960704958A
KR960704958A KR1019960701984A KR19960701984A KR960704958A KR 960704958 A KR960704958 A KR 960704958A KR 1019960701984 A KR1019960701984 A KR 1019960701984A KR 19960701984 A KR19960701984 A KR 19960701984A KR 960704958 A KR960704958 A KR 960704958A
Authority
KR
South Korea
Prior art keywords
weight
resin
parts
epoxy resin
liquid epoxy
Prior art date
Application number
KR1019960701984A
Other languages
English (en)
Inventor
제이. 헤어스톤 토마스
Original Assignee
스티븐 에스. 그레이스
더 다우 케미칼 캄파니
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 스티븐 에스. 그레이스, 더 다우 케미칼 캄파니 filed Critical 스티븐 에스. 그레이스
Publication of KR960704958A publication Critical patent/KR960704958A/ko

Abstract

각각의 최종 용도에서 에폭시 수지의 성능은 α-글리콜 그룹으로 말단화된 소량의 가수분해된 수지에 의해 향상된다.
본 발명은 (1) 반응 온도가 130 내지 200℃이고, (2) 반응 혼합물이 수지 100중량부당 물 0.5 내지 10중량부를 포함하며, (3) 액체 에폭시 수지와 물을 포함하는 혼합물이 유기 용매 0 내지 1중량% 및 각각의 유기산, 유기 아산, 포스포늄 화합물 및 알칼리 또는 알칼리 토금속 및 이들의 염 0 내지 100ppm을 포함함을 특징으로 하여, 액체 에폭시 수지와 물을 포함하는 혼합물을 승온에서 반응시켜 에폭시 그룹을 α-글리콜 그룹으로 가수분해시키는 방법에 관한 것이다. 본 발명의 방법은 수지중의 α-글리콜 그룹의 수준은 증가시키나 용매 또는 촉매를 사용하지 않으므로 생성된수지를 세정하기가 용이하다.

Description

액체 에폭시 수지 중의 α-글리콜의 수준을 증가시키는 방법(Method to increase the level of α-glycol in liquid epoxy resin)
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (8)

  1. (1) 반응 온도가 130 내지 200℃이고, (2) 반응 혼합물이 수지 100중량부당 물 0.5 내지 10중량부를 포함하며, (3) 액체 에폭시 수지와 물을 포함하는 혼합물이 유기 용매 0 내지 1중량% 및 각각의 유기산, 유기 이산, 포스포늄 화합물 및 알칼리 또는 알칼리 토금속 및 이들의 염 0 내지 100ppm을 포함함을 특징으로 하여, 액체 에폭시 수지와 물을 포함하는 혼합물을 승온에서 반응시켜 에폭시 그룹을 α-글리콜 그룹으로 가수분해시키는 방법.
  2. 제1항에 있어서, 액체 에폭시 수지가 반응 개시시 모노-α-글리콜 수지를 2중량% 이하로 포함하는 방법.
  3. 제1항 또는 제2항에 있어서, 반응 혼합물이 수지 100중량부당 물 2 내지 8중량부를 포함하는 방법.
  4. 제1항 내지 제3항 중의 어느 한 항에 있어서, 액체 에폭시 수지가 반응 개시시 비스페놀 A의 디글리시딜에테르 70 내지 700중량부, 올리고머 0 내지 30중량부 및 모노-α-글리콜 수지 0 내지 2중량부를 포함하는 방법.
  5. 제1항 내지 제4항 중의 어느 한 항에 있어서, 반응 혼합물이 각각의 에피할로하이드린, 산 및 알칼리 및 알칼리 토금속 및 이들의 염을 50ppm 미만으로 포함하는 방법.
  6. 제1항 내지 제5항 중의 어느 한 항에 있어서, 반응 혼합물이 방향족 극성 유기 용매 0.5중량% 미만을 포함하는 방법.
  7. 제1항 내지 제6항 중의 어느 한 항에 있어서, 공정 온도가 145 내지 180℃이고, 압력이 680kPa내지 1.8MPa이며, 반응시간 또는 잔류 시간이 0.5 내지 8시간인 방법.
  8. 제1항 내지 제6항 중의 어느 한 항에 있어서, 반응 혼합물이 수지 100중량부당 물 2 내지 5중량부를 포함하는 방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019960701984A 1993-10-18 1994-02-14 액체 에폭시 수지 중의 α-글리콜의 수준을 증가시키는 방법(Method to increase the level of α-glycol in liquid epoxy resin) KR960704958A (ko)