KR940021750A - 프레스가공성과 내도금박리성이 우수한 합금화용융아연도금강판 - Google Patents

프레스가공성과 내도금박리성이 우수한 합금화용융아연도금강판 Download PDF

Info

Publication number
KR940021750A
KR940021750A KR1019940004192A KR19940004192A KR940021750A KR 940021750 A KR940021750 A KR 940021750A KR 1019940004192 A KR1019940004192 A KR 1019940004192A KR 19940004192 A KR19940004192 A KR 19940004192A KR 940021750 A KR940021750 A KR 940021750A
Authority
KR
South Korea
Prior art keywords
less
dip galvanized
steel sheet
galvanized steel
weight
Prior art date
Application number
KR1019940004192A
Other languages
English (en)
Other versions
KR100261522B1 (ko
Inventor
마꼬또 이소베
가즈아끼 교노
노부유끼 모리또
Original Assignee
도사끼 시노부
가와사끼 세이데쓰 가부시끼가이샤
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=12655038&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=KR940021750(A) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Application filed by 도사끼 시노부, 가와사끼 세이데쓰 가부시끼가이샤 filed Critical 도사끼 시노부
Publication of KR940021750A publication Critical patent/KR940021750A/ko
Application granted granted Critical
Publication of KR100261522B1 publication Critical patent/KR100261522B1/ko

Abstract

고도의 프레스가공성과 우수한 내도금박리를 갖는 합금화 용융아연도금강판을 제조하는 것을 목적으로하며, 극저탄소강판표면에 Fe 9~12중량%, A10.3~1.5중량% 함유하는 합금화 용융아연도금층을 부착량 25~70g/㎡의 범위로 형성함으로써, 성형성이 우수하고, 또 파우더링성과 플레이킹성 모두 우수한 합금화 용융아연도금강판을 얻을 수 있다.

Description

프레스가공성과 내도금박리성이 우수한 합금화용융아연도금강판
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 비드식 인발시험의 설명도.

Claims (2)

  1. C 0.0015중량% 이하, Si 0.1중량% 이하, Mn 0.03중량% 이상 0.3중량% 이하, Al 0.01중량% 이상, 0.1중량% 이하, P 0.01중량% 이하, S 0.005중량$ 이하, O 0.005중량% 이하, N 0.005중량% 이하를 함유하고, 다시 0.03중량% 이하의 Ti 또는 0.03중량% 이하의 Nb 적어도 1종 이상을, C/12≤Ti*/48+Nb/93≤C/2를 만족하는 범위로 함유하는 강판표면에, Fe 9중량% 이상, 12중량% 이하, Al 0.3중량% 이상, 1.5중량% 이하, Pb 0.1중량% 이하를 함유하는 합금화 용융아연도금층이 25g/㎡ 이상 70g/㎡ 이하인 것을 특징으로 하는 프레스가공성과 내도금박리성이 우수한 합금화용융아연 도금강판, 단 Ti*는 Ti-(48N/14+48S/32)≥0일때는 Ti*= Ti-(48N/14+48S/32), Ti-(48N/14*48S/32)〈0 일때는 Ti*=0으로함.
  2. 제1항에 있어서, 다시 B를 0.001중량% 이하로 함유하는 것인 프레스가공성과 내도금박리성이 우수한 합금화 용융아연도금강판.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019940004192A 1993-03-04 1994-03-04 프레스가공성과 내도금박리성이 우수한 합금화 용융아연도금강판 KR100261522B1 (ko)