KR920016622A - 스피닝 노즐 팁 구조체 - Google Patents
스피닝 노즐 팁 구조체 Download PDFInfo
- Publication number
- KR920016622A KR920016622A KR1019910018602A KR910018602A KR920016622A KR 920016622 A KR920016622 A KR 920016622A KR 1019910018602 A KR1019910018602 A KR 1019910018602A KR 910018602 A KR910018602 A KR 910018602A KR 920016622 A KR920016622 A KR 920016622A
- Authority
- KR
- South Korea
- Prior art keywords
- spinning nozzle
- piece
- spinning
- nozzle
- nozzle body
- Prior art date
Abstract
내용 없음
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도 내지 3도는 본 발명의 실시예의 스피닝 노즐의 부분 단면도.
Claims (11)
- 세라믹, 세멧 및 세멘트 카바이트 합금중의 어느 하나로 이루어진 스피닝 노즐 피이스가 금속으로 이루어진 노즐 몸체에 형성된 수용 구멍내로 끼워 맞춤되도록된 스피닝 노즐 칩 구조체에 있어서, 금속링은 스피닝 노즐 피이스와 노즐 몸체와의 사이에 삽입되어, 스피닝 노즐 피이스를 수밀하게 밀봉시키는 것을 특징으로하는 스피닝 노즐 팁 구조체.
- 세라믹, 세멧 및 세멘트 카바이트 합금중의 어느 하나로 이루어진 스피닝 노즐 피이스가 금속으로 이루어진 노즐 몸체에 형성된 수용 구멍내로 끼워 맞춤되도록된 스피닝 노즐 칩 구조체에 있어서, 금속링은 동축인 수용구멍의 한끝에서 패인 홈에 설치되어 노즐 피이스 및 노즐 몸체를 수밀하게 밀봉시키는 것을 특징으로하는 스피닝 노즐 팁 구조체.
- 제1항 또는 제2항에 있어서, 노즐 몸체에 형성된 수용 구멍은 출구 방향으로 점점 더 작아지는 스텝핑을 가진 구멍의 축구끝 가까이에 형성되고, 이 스텝핑은 노즐 몸체의 대응 스텝핑과 맞물림하는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제2항에 있어서, 상기 금속링은 스피닝 노즐 피이스의 외주면과 노즐 몸체에 패인 홈의 내주면과의 사이에서 압축 끼워 맞춤되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제2항에 있어서, 상기 금속링은 땜질로써 상기 스피닝 노즐 피이스와 결합되고, 이 금속링 결합 스피닝 노즐 피이스는 노즐 몸체와 결합하기 위하여 대응 흠내로 압력 끼워 맞춤되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제1항 또는 제2항에 있어서, 상기 금속링은 노즐 몸체의 재질보다 열팽창 계수가 낮은 재질로 이루어지고, 상기 금속링은 스피닝 노즐 피이스 및 노즐 몸체와 함께 땜질 되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 세라믹, 서멧 또는 세멘트 카바이드 합금으로 이루어지고, 금속으로 이루어진 노즐 몸체내로 끼워 맞춤되는 각각의 하나의 스피닝 노즐로 구비된 스피닝노즐 피이스로 구성되어 있는 스피닝 노즐 팁 구조체에 있어서, 상기 스피닝 노즐 피이스는 브리넬 경도가 150㎏/㎟ 이하인 금속으로 이루어진 소프트 금속링을 상기 수용 구멍의 한끝에서 동축으로 돋축으로 패인 홈의 저면에 설치하고, 유연하게 변형되고, 하드금속으로 이루어진 압축링이 소프트 금속링을 카바하도록 위치함으로써, 스피닝 노즐 피이스 및 노즐 몸체와 수밀하게 접촉되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제7항에 있어서, 상기 압축링은 스피닝 노즐 피이스의 외주면과 노즐 몸체에 패인 홈의 내주면과의 사이에 압축 시킴으로써 끼원 맞춤되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제7항에 있어서, 상기 압축링은 스피닝 노즐 피이스에 땜질되고, 노즐 몸체에 패인홈의 내주면에 대해서 밀봉되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제7항에 있어서, 상기 압축링은 스피닝 노즐 피이스 및 노즐 몸체에 땜질되는 것을 특징으로 하는 스피닝 노즐 팁 구조체.
- 제7항에 있어서, 상기 압축링은 직경 방향으로 탄성을 주로 형상인 것을 특징으로 하는 스피닝 노즐 팁 구조체.※ 참고사항 : 최초출원 내용에 의하여 공개되는 것임.