KR890003979A - 차량의 문을 강화하기 위한 튜브용 강합금의 이용방법 - Google Patents

차량의 문을 강화하기 위한 튜브용 강합금의 이용방법 Download PDF

Info

Publication number
KR890003979A
KR890003979A KR1019880006105A KR880006105A KR890003979A KR 890003979 A KR890003979 A KR 890003979A KR 1019880006105 A KR1019880006105 A KR 1019880006105A KR 880006105 A KR880006105 A KR 880006105A KR 890003979 A KR890003979 A KR 890003979A
Authority
KR
South Korea
Prior art keywords
vehicle
tube
steel alloy
use steel
door
Prior art date
Application number
KR1019880006105A
Other languages
English (en)
Other versions
KR920000529B1 (ko
Inventor
클라쩌 슈테판
파우벨 게르트
Original Assignee
베노 나우요크스, 요헨호르스트마이어
벤텔러 아크티엔 게젤샤프트
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 베노 나우요크스, 요헨호르스트마이어, 벤텔러 아크티엔 게젤샤프트 filed Critical 베노 나우요크스, 요헨호르스트마이어
Publication of KR890003979A publication Critical patent/KR890003979A/ko
Application granted granted Critical
Publication of KR920000529B1 publication Critical patent/KR920000529B1/ko

Abstract

내용 없음

Description

차량의 문을 강화하기 위한 튜브용 강합금의 이용방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (2)

  1. 최고 0.35%의 탄소, 최고 0.50%의 실리콘, 최고 1.80%의 망간, 최고 0.30%ㅇ의 인, 최고 0.030%의 황, 1.8 내지 2.25의 크롬, 0.4 내지 0.7%의 몰리브덴, 최고 1.5% 바람직하게는 0.5 내지 1.0%의 니켈, 0.025 내지 0.050%의 알루미늄, 잔부의 철로 구성되고 열간 압연공정으로 제조되는 것을 특징으로 하는 차량의 문을 강화하기 위한 튜브용 강합금 이용방법.
  2. 제1항에 있어서, 최종 압연온도는 적어도 750℃, 바람직하게는 980 내지 1080℃인 것을 특징으로 하는 차량의 문을 강화하기 위한 튜브용 강합금의 이용방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019880006105A 1987-08-26 1988-05-25 차량의 문을 보강하기 위한 튜브용 강합금의 제조방법 KR920000529B1 (ko)