KR880012786A - 고강도 내마모성 동합금 - Google Patents

고강도 내마모성 동합금 Download PDF

Info

Publication number
KR880012786A
KR880012786A KR870003452A KR870003452A KR880012786A KR 880012786 A KR880012786 A KR 880012786A KR 870003452 A KR870003452 A KR 870003452A KR 870003452 A KR870003452 A KR 870003452A KR 880012786 A KR880012786 A KR 880012786A
Authority
KR
South Korea
Prior art keywords
high strength
copper alloy
wear resistant
resistant copper
strength wear
Prior art date
Application number
KR870003452A
Other languages
English (en)
Other versions
KR900006104B1 (ko
Inventor
이근수
박동규
Original Assignee
이영세
풍산금속공업주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이영세, 풍산금속공업주식회사 filed Critical 이영세
Priority to KR1019870003452A priority Critical patent/KR900006104B1/ko
Priority to JP63-81174A priority patent/JPH01237A/ja
Priority to US07/179,774 priority patent/US4851191A/en
Publication of KR880012786A publication Critical patent/KR880012786A/ko
Application granted granted Critical
Publication of KR900006104B1 publication Critical patent/KR900006104B1/ko

Abstract

내용 없음

Description

고강도 내마모성 동합금
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (2)

  1. Cu=54-66%, Al=1.0-0.5%, Mn=1.0-5.0%, Si=0.1-2.0%, Sn=0.1-3.0%, B=0.01-1.0%와 나머지가 아연과 불가피한 불순물로 구성된 조성을 갖는 고강도 내마모성 동합금.
  2. Cu=54-66%, Al=1.0-5.0%, Mn=1.0-5.0%, Si=0.1-2.0%, Sn=0.1-3.0%, B=0.01-1.0%와 Fe, Ni, Cr 중 1종 또는 2종 이상을 0.1-0.4% 함유하고 나머지가 아연 및 불가피한 불순물로 구성된 조성을 갖는 고강도 내마모성 동합금.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019870003452A 1987-04-10 1987-04-10 고강도 내마모성 동합금 KR900006104B1 (ko)