JPS6360152B2 - - Google Patents
Info
- Publication number
- JPS6360152B2 JPS6360152B2 JP58183692A JP18369283A JPS6360152B2 JP S6360152 B2 JPS6360152 B2 JP S6360152B2 JP 58183692 A JP58183692 A JP 58183692A JP 18369283 A JP18369283 A JP 18369283A JP S6360152 B2 JPS6360152 B2 JP S6360152B2
- Authority
- JP
- Japan
- Prior art keywords
- titanium
- coating
- carbon fibers
- film
- solution
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Manufacture Of Alloys Or Alloy Compounds (AREA)
- Treatments For Attaching Organic Compounds To Fibrous Goods (AREA)
- Reinforced Plastic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58183692A JPS6075671A (ja) | 1983-10-01 | 1983-10-01 | 複合材料用炭素繊維の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58183692A JPS6075671A (ja) | 1983-10-01 | 1983-10-01 | 複合材料用炭素繊維の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6075671A JPS6075671A (ja) | 1985-04-30 |
| JPS6360152B2 true JPS6360152B2 (enExample) | 1988-11-22 |
Family
ID=16140264
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58183692A Granted JPS6075671A (ja) | 1983-10-01 | 1983-10-01 | 複合材料用炭素繊維の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6075671A (enExample) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4961971A (en) * | 1988-12-19 | 1990-10-09 | United Technologies Corporation | Method of making oxidatively stable water soluble amorphous hydrated metal oxide sized fibers |
| JP5712470B2 (ja) * | 2009-07-28 | 2015-05-07 | 日東紡績株式会社 | 耐アルカリ性ガラス繊維及びその製造方法 |
| JP2017155172A (ja) * | 2016-03-03 | 2017-09-07 | 国立大学法人信州大学 | 炭素繊維強化プラスチック及びその製造方法並びに炭素繊維 |
-
1983
- 1983-10-01 JP JP58183692A patent/JPS6075671A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6075671A (ja) | 1985-04-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Tohge et al. | Fine-patterning on glass substrates by the sol-gel method | |
| US4937208A (en) | Catalyst for sol-gel method using metal alkoxide and sol-gel method using the same | |
| JPS61192735A (ja) | 金属アルコキシドから重合体を製造するための新規な方法 | |
| JPS6360152B2 (enExample) | ||
| US4434103A (en) | Substituted silicon-oxygen-aluminum oligomers and preparation thereof | |
| US4547402A (en) | Method of increasing the thermal shock resistance of phosphate laser glass | |
| US4460654A (en) | Aluminosilicate coating method, coated articles and organic substituted silicon-oxygen-aluminum oligomers | |
| JPS5837260B2 (ja) | 熱線反射ガラスの製造方法 | |
| TWI233938B (en) | Sol-gel process for the preparation of vitreous films possessing high adhesion properties and stable colloidal solutions suitable for its carrying out the same | |
| JPH054839A (ja) | ゾルゲル法による薄膜の作製方法 | |
| JPS6150903B2 (enExample) | ||
| JPH11124543A (ja) | 無機−有機ハイブリッド被膜を有する複合材料の製造方法 | |
| JPH04280812A (ja) | 基材上への多孔質シリカ被膜の形成法 | |
| JPH0465327A (ja) | Tiドープ層付石英光ファイバの製造方法 | |
| JPS6376881A (ja) | ジルコニア膜の製造方法 | |
| JPH02239112A (ja) | 金属基材上へのシリカ被膜の形成法 | |
| JPH04160020A (ja) | 薄膜の作製方法 | |
| KR100217465B1 (ko) | 발수성이 우수한 자동차의 후사경용 유리의 제조방법 | |
| JPH0217670B2 (enExample) | ||
| JPH0333062A (ja) | 耐酸化性炭素材料およびその製造方法 | |
| JPS5988701A (ja) | 光ファイバの被覆方法 | |
| JPH0376819A (ja) | TiO↓2中空ファイバーの製造法 | |
| KR100236479B1 (ko) | 자외선 차단 및 발수성 유리의 제조방법 | |
| JP2862283B2 (ja) | 導電性セラミックファイバーの製造方法 | |
| JPH0367978B2 (enExample) |