JPS6356912B2 - - Google Patents
Info
- Publication number
- JPS6356912B2 JPS6356912B2 JP57001050A JP105082A JPS6356912B2 JP S6356912 B2 JPS6356912 B2 JP S6356912B2 JP 57001050 A JP57001050 A JP 57001050A JP 105082 A JP105082 A JP 105082A JP S6356912 B2 JPS6356912 B2 JP S6356912B2
- Authority
- JP
- Japan
- Prior art keywords
- water
- present
- oil
- group
- repellency
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Materials Applied To Surfaces To Minimize Adherence Of Mist Or Water (AREA)
- Treatments For Attaching Organic Compounds To Fibrous Goods (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP105082A JPS58118882A (ja) | 1982-01-08 | 1982-01-08 | 高性能撥水撥油剤 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP105082A JPS58118882A (ja) | 1982-01-08 | 1982-01-08 | 高性能撥水撥油剤 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58118882A JPS58118882A (ja) | 1983-07-15 |
JPS6356912B2 true JPS6356912B2 (en, 2012) | 1988-11-09 |
Family
ID=11490717
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP105082A Granted JPS58118882A (ja) | 1982-01-08 | 1982-01-08 | 高性能撥水撥油剤 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS58118882A (en, 2012) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0428419A (ja) * | 1990-05-24 | 1992-01-31 | Nkk Corp | プレス曲げ治具の雌型 |
US6872605B2 (en) | 1992-12-04 | 2005-03-29 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device and method of fabricating the same |
US6964890B1 (en) | 1992-03-17 | 2005-11-15 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device and method for forming the same |
US6987283B2 (en) | 1993-03-12 | 2006-01-17 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device structure |
US7622335B2 (en) | 1992-12-04 | 2009-11-24 | Semiconductor Energy Laboratory Co., Ltd. | Method for manufacturing a thin film transistor device |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6375178A (ja) * | 1986-07-29 | 1988-04-05 | フエイドガ−ド,インコ−ポレ−テツド | 有機及び類似の繊維、布帛などに紫外線安定性及び吸収性並びに撥油性を同時に付与する方法及び材料、並びに紫外線遮断性及び撥水性を有する薄い固化被膜 |
JP2007169419A (ja) * | 2005-12-21 | 2007-07-05 | Kao Corp | 睫用化粧料用ポリマーエマルジョン |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3532659A (en) * | 1967-04-26 | 1970-10-06 | Pennsalt Chemicals Corp | Fluorinated organic compounds and polymers thereof |
US3637614A (en) * | 1969-02-27 | 1972-01-25 | Du Pont | Solvent soluble dry soil resistant fluoropolymers |
-
1982
- 1982-01-08 JP JP105082A patent/JPS58118882A/ja active Granted
Cited By (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0428419A (ja) * | 1990-05-24 | 1992-01-31 | Nkk Corp | プレス曲げ治具の雌型 |
US6964890B1 (en) | 1992-03-17 | 2005-11-15 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device and method for forming the same |
US7564057B1 (en) | 1992-03-17 | 2009-07-21 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device having an aluminum nitride film |
US6872605B2 (en) | 1992-12-04 | 2005-03-29 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device and method of fabricating the same |
US7622335B2 (en) | 1992-12-04 | 2009-11-24 | Semiconductor Energy Laboratory Co., Ltd. | Method for manufacturing a thin film transistor device |
US6987283B2 (en) | 1993-03-12 | 2006-01-17 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device structure |
US7391051B2 (en) | 1993-03-12 | 2008-06-24 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device forming method |
US7238558B2 (en) | 1993-06-30 | 2007-07-03 | Semiconductor Energy Laboratory Co., Ltd. | Semiconductor device and method of fabricating the same |
Also Published As
Publication number | Publication date |
---|---|
JPS58118882A (ja) | 1983-07-15 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN103788288B (zh) | 拒水和拒油组合物 | |
US5055538A (en) | Novel copolymer and water- and oil-repellent comprising the same | |
EP2799458B1 (en) | Fluorine-containing composition and fluorine-containing polymer | |
JP5567334B2 (ja) | 撥水撥油剤を用いる処理 | |
WO2009119911A1 (en) | Fluorine-containing polymer and water- and oil-repellent agent | |
EP2762504A1 (en) | Water-repellent and oil-repellent composition | |
JP5862745B2 (ja) | 含フッ素重合体および処理剤 | |
JPH0432873B2 (en, 2012) | ||
JP3820593B2 (ja) | 防汚加工剤 | |
JP3820694B2 (ja) | 新規共重合体および防汚加工剤 | |
JP2013100494A (ja) | 含フッ素組成物 | |
JPS6356912B2 (en, 2012) | ||
JPS5859277A (ja) | 撥水撥油剤 | |
JP3300424B2 (ja) | 新規共重合体および防汚加工剤 | |
JPS5871977A (ja) | 低温キユア型撥水撥油剤 | |
EP1127898B1 (en) | Process for production of copolymer composition and water-repellent, oil-repellent agent | |
JP3064388B2 (ja) | 撥水撥油剤 | |
JP2968366B2 (ja) | 撥水撥油剤組成物 | |
JP5895975B2 (ja) | 表面処理剤および含フッ素重合体 | |
JP2968364B2 (ja) | 耐久性の優れた撥水撥油剤および撥水撥油剤組成物 | |
JPS58118883A (ja) | 高性能撥水撥油剤 | |
JP2968365B2 (ja) | 耐久性撥水撥油剤および撥水撥油剤組成物 | |
JPS6410556B2 (en, 2012) |